SU114115A1 - The method of heat treatment of twisted yarn of fiber such as Perlon or nylon - Google Patents

The method of heat treatment of twisted yarn of fiber such as Perlon or nylon

Info

Publication number
SU114115A1
SU114115A1 SU360987A SU360987A SU114115A1 SU 114115 A1 SU114115 A1 SU 114115A1 SU 360987 A SU360987 A SU 360987A SU 360987 A SU360987 A SU 360987A SU 114115 A1 SU114115 A1 SU 114115A1
Authority
SU
USSR - Soviet Union
Prior art keywords
fiber
perlon
nylon
heat treatment
twisted yarn
Prior art date
Application number
SU360987A
Other languages
Russian (ru)
Inventor
Б.Я. Горовой
Original Assignee
Б.Я. Горовой
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Б.Я. Горовой filed Critical Б.Я. Горовой
Priority to SU360987A priority Critical patent/SU114115A1/en
Application granted granted Critical
Publication of SU114115A1 publication Critical patent/SU114115A1/en

Description

При выработке нити из волокна типа перлона или капрона нить носле нр дени , предварительного кручени , выт жки н окончательной крутки обычно промывают дл  удалени  из волокна лактама, центрифугируют , сушат и пе)ематывают на большие паковки.When making a yarn from a perlon or nylon fiber, the yarn is worn, pre-twisted, drawn, and the final twist is usually washed to remove lactam from the fiber, centrifuged, dried, and wrapped into large packages.

Предлагаемый способ термической обработки нити позвол ет совершенно устранить промывку и сушку и улучшить упругие свойства нити.The proposed method of heat treating a yarn makes it possible to completely eliminate washing and drying and to improve the elastic properties of the yarn.

Согласно изобретению, нить после обычной выт жки и крутки вторично выт гивают на 20-50% в гор чем воздухе нрн температуре 100- 195°, оптимально 190°, со скоростью питани  39-80 м/лшн и наматываютAccording to the invention, the thread after the usual stretching and twisting is secondarily drawn by 20-50% in hot air at a temperature of 100-195 ° C, optimally 190 °, with a feed rate of 39-80 m / l and wound

па шпули весом 1,5-1,6 кг. Выт жку производ т в трубе, в которой циркулирует гор чий воздух, подогреваемый калорифером.Pa spools weighing 1.5-1.6 kg. It is exhausted in a pipe in which hot air is circulated, heated by a heater.

Предмет изобретени Subject invention

Способ термической обработки крученой нити из волокна типа перлона или капрона, отличающийс   тем, что, дл  улучшени  упругих свойств нити и устранени  после кручени  операций промывки, центрифугировани , сушки и перемотки , НИТЬ, подаваемую со скоростью 39-80 м/мин, выт гивают на 20-50% в гор чем воздухе при температуре 100-195°, оптимально 190°. The method of heat treatment of a twisted yarn from a fiber of the perlon or nylon type, characterized in that, to improve the elastic properties of the yarn and to eliminate after twisting the washing, centrifuging, drying and rewinding operations, the THREAD supplied with a speed of 39-80 m / min 20-50% in hot air at a temperature of 100-195 °, optimally 190 °.

SU360987A 1947-11-25 1947-11-25 The method of heat treatment of twisted yarn of fiber such as Perlon or nylon SU114115A1 (en)