SU104597A1 - Способ закалки углеродистых и низколегированных сталей - Google Patents

Способ закалки углеродистых и низколегированных сталей

Info

Publication number
SU104597A1
SU104597A1 SU453585A SU453585A SU104597A1 SU 104597 A1 SU104597 A1 SU 104597A1 SU 453585 A SU453585 A SU 453585A SU 453585 A SU453585 A SU 453585A SU 104597 A1 SU104597 A1 SU 104597A1
Authority
SU
USSR - Soviet Union
Prior art keywords
alloy steels
low alloy
quenching
quenching carbon
carbon
Prior art date
Application number
SU453585A
Other languages
English (en)
Inventor
Я.Ю. Авдиев
Е.И. Малинкина
Original Assignee
Я.Ю. Авдиев
Е.И. Малинкина
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Я.Ю. Авдиев, Е.И. Малинкина filed Critical Я.Ю. Авдиев
Priority to SU453585A priority Critical patent/SU104597A1/ru
Application granted granted Critical
Publication of SU104597A1 publication Critical patent/SU104597A1/ru

Description

Изобретение касаетс  способа термической обработки, в частности закалки,. изделий из углеродистых и низколегированных сталей.
Известен способ закалки углеродистых и низколегированных сталей с применением в качестве охлаждающей среды водного раствора едкого натра или поваренной соли, который не обеспечивает низкую скорость охлаждени  в интервале температур мартенситного превращени  ( 300° -200°), что приводит к образованию трещин в закаливаемой стали.
Отличительна  особенность предложенного способа состоит в том, что в качестве охлаждающей среды примен ют 8-18-процентный раствор КМпО4.
Предложенный способ термической обработки обеспечивает высокую скорость охлаждени  в интервале закалочной температуры от 650° до 550, что способствует достижению высокой и равномерной твердости стали при отсутствии м гких п тен, а также низкую скорость охлаждени  в интервале температур 300° - 200°, что преп тствует образованию трещин в закаливаемой стали.
Предмет изобретени 
Способ закалки углеродистых и низколегированных сталей, отличающийс  тем, что, с целью устранени  трещин и м гких п тен в процессе закалки, а также повыщени  твердости, в качестве охлаждающей среды примен ют 8-18-процентный водный раствор КМпО4.
SU453585A 1955-03-09 1955-03-09 Способ закалки углеродистых и низколегированных сталей SU104597A1 (ru)