SG171545A1 - Backing device and welding method - Google Patents
Backing device and welding methodInfo
- Publication number
- SG171545A1 SG171545A1 SG201008375-6A SG2010083756A SG171545A1 SG 171545 A1 SG171545 A1 SG 171545A1 SG 2010083756 A SG2010083756 A SG 2010083756A SG 171545 A1 SG171545 A1 SG 171545A1
- Authority
- SG
- Singapore
- Prior art keywords
- backing
- welding
- copper plate
- steel plates
- flux
- Prior art date
Abstract
BACKINGEVICE AND WELDING GMETHOD Provided is a backing device that is used in one-side welding equipment for joining together steel plates, that performs welding using backing flux, and that includes a backing member having a minimum length larger than or equal to the length of a welding groove in the steel plates. The backing member includes a backing copper plate that is disposed along the welding groove and that holds the backing flux and a support frame that supports the backing copper plate in such a manner that it slides in the direction of the welding groove. The backing copper plate includes copper plate pieces each having a predetermined length and joined together by a joining member. According to such a configuration, a good welding shape can be obtained when performing one-side automatic welding.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2009269021A JP2011110582A (en) | 2009-11-26 | 2009-11-26 | Backing device and welding method |
Publications (1)
Publication Number | Publication Date |
---|---|
SG171545A1 true SG171545A1 (en) | 2011-06-29 |
Family
ID=43373362
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SG201008375-6A SG171545A1 (en) | 2009-11-26 | 2010-11-15 | Backing device and welding method |
Country Status (4)
Country | Link |
---|---|
JP (1) | JP2011110582A (en) |
CN (2) | CN102078998A (en) |
BR (1) | BRPI1004982B1 (en) |
SG (1) | SG171545A1 (en) |
Families Citing this family (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2011110582A (en) * | 2009-11-26 | 2011-06-09 | Kobe Steel Ltd | Backing device and welding method |
CN102319948B (en) * | 2011-08-26 | 2013-08-21 | 上汽通用五菱汽车股份有限公司 | Slidable copper plate backing welding mechanism and method using same to weld parts |
CN105033404B (en) * | 2015-07-22 | 2019-02-22 | 中国核电工程有限公司 | Deflection welding liner and its operating method |
CN105252118A (en) * | 2015-11-20 | 2016-01-20 | 辽宁忠旺特种车辆制造有限公司 | Welding process for rear door of self-supporting van vehicle |
CN105269167B (en) * | 2015-11-20 | 2017-06-23 | 辽宁忠旺特种车辆制造有限公司 | It is complete to carry van-type front part of the carriage plate weld technique |
CN107931904B (en) * | 2017-12-21 | 2024-03-01 | 无锡奥特维科技股份有限公司 | Lamination welding device and battery string repairing machine |
CN109079375A (en) * | 2018-09-27 | 2018-12-25 | 哈尔滨理工大学 | Welding procedure pallet device |
CN110293355B (en) * | 2019-06-25 | 2021-03-30 | 合肥创智汽车技术开发有限公司 | Improve welding copper plate structure of automobile body outward appearance solder joint quality |
Family Cites Families (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5660590U (en) * | 1979-10-17 | 1981-05-23 | ||
JP3930793B2 (en) * | 2002-09-30 | 2007-06-13 | 株式会社神戸製鋼所 | Single-side welding equipment |
JP4401238B2 (en) * | 2004-05-11 | 2010-01-20 | 株式会社神戸製鋼所 | Single-side welding equipment |
JP4401258B2 (en) * | 2004-08-13 | 2010-01-20 | 株式会社神戸製鋼所 | BACKING DEVICE AND ITS CONVEYING METHOD |
JP2011110582A (en) * | 2009-11-26 | 2011-06-09 | Kobe Steel Ltd | Backing device and welding method |
-
2009
- 2009-11-26 JP JP2009269021A patent/JP2011110582A/en active Pending
-
2010
- 2010-03-09 CN CN2010101276415A patent/CN102078998A/en active Pending
- 2010-03-09 CN CN2010201311113U patent/CN201685073U/en not_active Expired - Lifetime
- 2010-11-15 SG SG201008375-6A patent/SG171545A1/en unknown
- 2010-11-23 BR BRPI1004982-7A patent/BRPI1004982B1/en not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
CN201685073U (en) | 2010-12-29 |
BRPI1004982B1 (en) | 2018-02-06 |
JP2011110582A (en) | 2011-06-09 |
CN102078998A (en) | 2011-06-01 |
BRPI1004982A2 (en) | 2013-03-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
SG171545A1 (en) | Backing device and welding method | |
EP2813596A4 (en) | High tensile steel plate having excellent low-temperature toughness in weld heat-affected zones, and method for producing same | |
EP2907611A4 (en) | Method for producing heat exchanger plate and method for friction stir welding | |
EP2687315A4 (en) | Friction stir spot welding device and friction stir spot welding method | |
EP2703110A4 (en) | Friction stir welding method and device, and tool set | |
EP3653329A4 (en) | Double-sided friction stir welding method for metal plate and double-sided friction stir welding device | |
EP2745972A4 (en) | Friction stir welding method | |
EP2769797A4 (en) | Resistance spot welding method for high-tensile steel plates, and resistance spot welding joint | |
EP2881210A4 (en) | Welding tool used for double-acting type friction stir welding or double-acting type friction stir spot welding, and welding device using same | |
EP3067148A4 (en) | Friction stir welding method for high-strength steel sheets or plates | |
EP2511038A4 (en) | Friction stir welding apparatus and method | |
ZA201406337B (en) | Method for joining metal parts | |
SI3122510T1 (en) | Method and apparatus for improving the weld quality in friction stir welding | |
EP2524760A4 (en) | Method for producing joint member and friction stir welding apparatus | |
GB201203030D0 (en) | Forge welding of tubular articles | |
EP2436472A4 (en) | Submerged arc welding method for steel plate | |
GB2466865B (en) | Joining method and reflow apparatus | |
GB2475574B (en) | Method and apparatus for preheating in welding operations | |
SG171543A1 (en) | Backing device and welding method | |
DK2359974T3 (en) | Arc welding method and welding current source for carrying out the method | |
PH12014502019A1 (en) | Method for producing arc-welded structural member | |
EP2857542A4 (en) | High strength cold-rolled steel plate exhibiting little variation in strength and ductility, and manufacturing method for same | |
PL2758207T3 (en) | Weld gun part clamp device and method | |
EP3639965A4 (en) | Double-side friction stir joining method and double-side friction stir joining device for metal plates | |
EP2716917A4 (en) | Jig used for repairing pin-coupling component, and method using the same |