SE8106386L - PROCEDURE FOR PREPARING A CORROSION-RESISTANT GOLD PLATING THROUGH ELECTROLYTIC DEPOSIT - Google Patents
PROCEDURE FOR PREPARING A CORROSION-RESISTANT GOLD PLATING THROUGH ELECTROLYTIC DEPOSITInfo
- Publication number
- SE8106386L SE8106386L SE8106386A SE8106386A SE8106386L SE 8106386 L SE8106386 L SE 8106386L SE 8106386 A SE8106386 A SE 8106386A SE 8106386 A SE8106386 A SE 8106386A SE 8106386 L SE8106386 L SE 8106386L
- Authority
- SE
- Sweden
- Prior art keywords
- gold plating
- electrodeposition
- salt
- corrosion
- preparing
- Prior art date
Abstract
Improved corrosion resistance of base metal hardened gold plating is achieved by the electrodeposition of a ductile, low-stress nickel coating on the substrate prior to the electrodeposition of the metal-hardened gold plating. The nickel coating is electrodeposited from a bath containing a Ni salt, an electrolyte eg boric and/or formic acid, o-formyl benzene sulphonic acid, and optionally a blend of K perfluoroalkyl sulphonates as wetting agent. The gold coating is electrodeposited from a bath containing a Au salt, an electrolyte eg acetic, citric and/or formic acid, and a Au hardener metal salt, eg of Co, In, Ni and/or Zn. Both electrodeposition steps may use insoluble anodes.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US20241080A | 1980-10-31 | 1980-10-31 |
Publications (1)
Publication Number | Publication Date |
---|---|
SE8106386L true SE8106386L (en) | 1982-05-01 |
Family
ID=22749762
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SE8106386A SE8106386L (en) | 1980-10-31 | 1981-10-29 | PROCEDURE FOR PREPARING A CORROSION-RESISTANT GOLD PLATING THROUGH ELECTROLYTIC DEPOSIT |
Country Status (14)
Country | Link |
---|---|
JP (1) | JPS6053120B2 (en) |
AU (1) | AU530002B2 (en) |
BE (1) | BE890947A (en) |
BR (1) | BR8107041A (en) |
CA (1) | CA1162505A (en) |
DE (1) | DE3139815C2 (en) |
DK (1) | DK422081A (en) |
ES (1) | ES506573A0 (en) |
FR (1) | FR2493349A1 (en) |
GB (1) | GB2086428B (en) |
HK (1) | HK66886A (en) |
IT (1) | IT1171616B (en) |
NL (1) | NL8104859A (en) |
SE (1) | SE8106386L (en) |
Families Citing this family (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB2130602B (en) * | 1982-11-24 | 1986-04-16 | Stc Plc | Electroplating electrical contacts |
EP0127857B1 (en) * | 1983-05-28 | 1987-07-29 | Masami Kobayashi | Solderable stainless steel article and method for making same |
JPS607157A (en) * | 1983-06-25 | 1985-01-14 | Masami Kobayashi | Lead frame for ic |
JPS6033363A (en) * | 1983-08-02 | 1985-02-20 | Nippon Dento Kogyo Kk | Noble metal plating method |
GB2153386B (en) * | 1984-02-01 | 1987-08-26 | Omi Int Corp | Gold alloy plating bath |
GB2168381B (en) * | 1984-12-12 | 1988-03-09 | Stc Plc | Gold plated electrical contacts |
JP2693480B2 (en) * | 1988-04-28 | 1997-12-24 | シチズン時計株式会社 | Exterior parts for watch and manufacturing method thereof |
JP2780506B2 (en) * | 1991-03-04 | 1998-07-30 | 戸田工業株式会社 | Electric Ni plating method |
US9693672B2 (en) | 2011-09-22 | 2017-07-04 | Whirlpool Corporation | Dishwasher with sprayer |
Family Cites Families (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE1124780B (en) * | 1960-10-08 | 1962-03-01 | Schering Ag | Electrolyte for the deposition of high-gloss nickel coatings |
DE1496818C3 (en) * | 1964-03-12 | 1978-04-27 | Dr. Hesse & Cie, 4800 Bielefeld | Process for the electrolytic production of gold layers with a high, uniform gloss and good resistance to corrosion and tarnishing |
US3334032A (en) * | 1964-05-08 | 1967-08-01 | Hanson Van Winkle Munning Co | Electrodeposition of nickel |
GB1442325A (en) * | 1972-07-26 | 1976-07-14 | Oxy Metal Finishing Corp | Electroplating with gold and gold alloys |
FR2309203A1 (en) * | 1975-04-30 | 1976-11-26 | Parant Sa | Dental cap based on stainless steel - which is electrolytically deposited with nickel and gold and finally coated with ceramic |
DK422181A (en) * | 1980-10-23 | 1982-04-24 | Hooker Chemicals Plastics Corp | BATH AND METHOD FOR HIGH SPEED NICKEL ELECTROPLETING |
-
1981
- 1981-09-23 CA CA000386447A patent/CA1162505A/en not_active Expired
- 1981-09-24 DK DK422081A patent/DK422081A/en not_active Application Discontinuation
- 1981-09-25 AU AU75675/81A patent/AU530002B2/en not_active Ceased
- 1981-10-07 DE DE3139815A patent/DE3139815C2/en not_active Expired
- 1981-10-22 FR FR8119852A patent/FR2493349A1/en not_active Withdrawn
- 1981-10-24 JP JP56170635A patent/JPS6053120B2/en not_active Expired
- 1981-10-26 ES ES506573A patent/ES506573A0/en active Granted
- 1981-10-27 NL NL8104859A patent/NL8104859A/en not_active Application Discontinuation
- 1981-10-29 IT IT49589/81A patent/IT1171616B/en active
- 1981-10-29 SE SE8106386A patent/SE8106386L/en not_active Application Discontinuation
- 1981-10-30 BE BE0/206412A patent/BE890947A/en not_active IP Right Cessation
- 1981-10-30 BR BR8107041A patent/BR8107041A/en unknown
- 1981-11-02 GB GB8132943A patent/GB2086428B/en not_active Expired
-
1986
- 1986-09-11 HK HK668/86A patent/HK66886A/en unknown
Also Published As
Publication number | Publication date |
---|---|
AU7567581A (en) | 1982-05-06 |
IT1171616B (en) | 1987-06-10 |
BR8107041A (en) | 1982-07-20 |
JPS5798694A (en) | 1982-06-18 |
DK422081A (en) | 1982-05-01 |
GB2086428A (en) | 1982-05-12 |
FR2493349A1 (en) | 1982-05-07 |
CA1162505A (en) | 1984-02-21 |
IT8149589A0 (en) | 1981-10-29 |
DE3139815A1 (en) | 1982-06-16 |
BE890947A (en) | 1982-04-30 |
HK66886A (en) | 1986-09-18 |
ES8206671A1 (en) | 1982-08-16 |
DE3139815C2 (en) | 1986-05-22 |
GB2086428B (en) | 1983-11-30 |
ES506573A0 (en) | 1982-08-16 |
NL8104859A (en) | 1982-05-17 |
AU530002B2 (en) | 1983-06-30 |
JPS6053120B2 (en) | 1985-11-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE1496843A1 (en) | Electrodeposition process | |
EP0214667A1 (en) | Palladium and palladium alloy composite electrodeposits and method for their production | |
SE8106386L (en) | PROCEDURE FOR PREPARING A CORROSION-RESISTANT GOLD PLATING THROUGH ELECTROLYTIC DEPOSIT | |
SE8504517D0 (en) | Aqueous acidic electrolyte for electrolytic precipitation of zinc alloys and sets for electrolytic precipitation of such alloys using the electrolyte | |
US4384929A (en) | Process for electro-depositing composite nickel layers | |
US4411965A (en) | Process for high speed nickel and gold electroplate system and article having improved corrosion resistance | |
US3692641A (en) | Electrodeposition of low stress ruthenium alloy | |
US3183067A (en) | Metal having two coats of sulfurcontaining nickel and method of making same | |
GB1224680A (en) | Electroplating a ductile zinc nickel alloy onto a metallic article | |
SE7812869L (en) | ACID ZINK ELECTROPLETATION PROCEDURE AND COMPOSITION | |
SE8300416L (en) | ZINK COBOLT BASED ELECTROPLETING BATH, PROCEDURE FOR THE PREPARATION OF A ZINK COBOLT PLATING AND THEREFORE, PLETTERED FORM | |
Rosegren et al. | Hardened Gold Plating Process | |
US4746411A (en) | Acidic sulfate containing bath for the electrodeposition of zinc/iron alloys | |
SE8205087D0 (en) | PROCEDURES FOR RECOVERY OF THE CORROSION RESISTANCE OF A GALVANIC Separated Palladium-Nickel Alloy | |
ES420067A1 (en) | Electrolyte and method for electrodepositing microporous chromium-nickel composite coatings | |
US4411744A (en) | Bath and process for high speed nickel electroplating | |
CA1180677A (en) | Bath and process for high speed nickel electroplating | |
US3355263A (en) | Three-layer nickel laminate | |
ATE11796T1 (en) | PROCESS FOR ELECTROPLATING A ZINC-NICKEL ALLOY COATING ON A METAL OBJECT, ESPECIALLY STEEL STRIP. | |
ES8402368A1 (en) | Zinc-nickel electroplated article and method for producing the same. | |
GB891564A (en) | Composite chromium electroplate | |
GB1039797A (en) | Electro-deposition of a ternary alloy of nickel-iron and molybdenum | |
EP0415632A1 (en) | Palladium alloy electroplating process | |
JPS5767188A (en) | Zinc alloy electroplated steel plate with high corrosion resistance and its manufacture | |
EP0163944A3 (en) | Aqueous acid electrolytes containing nickel and cobalt ions for the galvanic deposition of hardly discolouring lustrous white alloy coatings |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
NAV | Patent application has lapsed |
Ref document number: 8106386-9 |