SE458214B - Fibre material treatment for chemical consolidation - Google Patents
Fibre material treatment for chemical consolidationInfo
- Publication number
- SE458214B SE458214B SE8502556A SE8502556A SE458214B SE 458214 B SE458214 B SE 458214B SE 8502556 A SE8502556 A SE 8502556A SE 8502556 A SE8502556 A SE 8502556A SE 458214 B SE458214 B SE 458214B
- Authority
- SE
- Sweden
- Prior art keywords
- polymer
- added
- dried
- fibers
- pulp
- Prior art date
Abstract
Description
'du 458 214 10 15 20 25 2 avvattnas fibermaterialet, torkas och finfördelas. En lösning av poly- propen i xylen i en koncentration av 1-2 % beredes och det torkade och finfördelade fibermaterialet tillsättes lösningen så att fiberkon- centrationen uppgår till ca 2 % och blandningen uppvärmes till en temperatur av 100-115 OC. Efter 15 minutef'tas fibermaterialet upp ur lösningen, pressas till en torrhalt av ca 20 % och torkas. 458 214 10 15 20 25 2 the fibrous material is dewatered, dried and comminuted. A solution of polypropylene in xylene in a concentration of 1-2% is prepared and the dried and finely divided fibrous material is added to the solution so that the fiber concentration amounts to about 2% and the mixture is heated to a temperature of 100-115 ° C. After 15 minutes, the fibrous material is taken out of the solution, pressed to a dry content of about 20% and dried.
EXEMPEL 2 En massasuspension innehållande tensid framställes på samma sätt som i exempel 1. Efter omrörning i 15 minuter avvattnas fiber- materialet, torkas och finfördelas. Till en massasuspension av den beredda massan tillsättes polypropen i form av ett fint pulver i en mängd av 5-10 % räknat på massan. Efter omrörning avvattnas materialet och torkas.EXAMPLE 2 A pulp suspension containing surfactant is prepared in the same manner as in Example 1. After stirring for 15 minutes, the fibrous material is dewatered, dried and comminuted. To a pulp suspension of the prepared pulp is added polypropylene in the form of a fine powder in an amount of 5-10% based on the pulp. After stirring, the material is dewatered and dried.
EXEMPEL 3 Materialet framställes på samma sätt som i exempel 2 men med den skillnad att i stället för polypropen användes polyeten i pulverform. n EXEMPEL ä En vattenlösning av en nonjonisk tensid som marknadsföres under namnet Berol 09 (Berol Aktiebolag) beredes och i exempel1 angivna massan tillsättes så att massakoncentrationen uppgår till ca 0,5 %. Den använda mängden tensid motsvarar 1-3 kg per ton massa. Efter omrörning i 15 minuter avvattnas massan, torkas och finfördelas. En lösning av polypropen i xylen beredes och den torkade och finfördelade massan tillsättes så att massakoncentrationen uppgår till ca 2 till en temperatur av 100- í en koncentration av 1-2 % % och uppvärmes 115 OC. Efter 15 minuter tas massan upp ur lös- ningen, pressas till en torrhalt av ca 20 % och torkas.EXAMPLE 3 The material is prepared in the same manner as in Example 2 but with the difference that instead of polypropylene polyethylene in powder form is used. n EXAMPLE ä An aqueous solution of a nonionic surfactant marketed under the name Berol 09 (Berol Aktiebolag) is prepared and the pulp specified in Example 1 is added so that the pulp concentration amounts to about 0.5%. The amount of surfactant used corresponds to 1-3 kg per tonne of pulp. After stirring for 15 minutes, the mass is dehydrated, dried and comminuted. A solution of polypropylene in xylene is prepared and the dried and comminuted pulp is added so that the pulp concentration amounts to about 2 to a temperature of 100- at a concentration of 1-2%% and heated to 115 ° C. After 15 minutes, the pulp is taken out of the solution, pressed to a dry content of about 20% and dried.
Uppfinningen är icke begränsad till de angivna utföringsexemplen, utan kan varieras inom ramen för uppfinningstanken.The invention is not limited to the stated exemplary embodiments, but can be varied within the scope of the inventive idea.
Claims (6)