RU96114197A - METHOD FOR CONNECTING ENAMELED PIPES - Google Patents

METHOD FOR CONNECTING ENAMELED PIPES

Info

Publication number
RU96114197A
RU96114197A RU96114197/06A RU96114197A RU96114197A RU 96114197 A RU96114197 A RU 96114197A RU 96114197/06 A RU96114197/06 A RU 96114197/06A RU 96114197 A RU96114197 A RU 96114197A RU 96114197 A RU96114197 A RU 96114197A
Authority
RU
Russia
Prior art keywords
pipes
coating
welding
root
connecting enameled
Prior art date
Application number
RU96114197/06A
Other languages
Russian (ru)
Other versions
RU2109197C1 (en
Inventor
Н.П. Кармазинов
В.Б. Потапов
А.Т. Санжировский
О.И. Стеклов
В.Б. Уразов
Original Assignee
Государственная академия нефти и газа им.И.М.Губкина
Filing date
Publication date
Application filed by Государственная академия нефти и газа им.И.М.Губкина filed Critical Государственная академия нефти и газа им.И.М.Губкина
Priority to RU96114197A priority Critical patent/RU2109197C1/en
Priority claimed from RU96114197A external-priority patent/RU2109197C1/en
Application granted granted Critical
Publication of RU2109197C1 publication Critical patent/RU2109197C1/en
Publication of RU96114197A publication Critical patent/RU96114197A/en

Links

Claims (2)

1. Способ соединения эмалированных труб с кислым типом покрытия, включающий одностороннюю сварку корневого шва, отличающийся тем, что в процессе сварки используют высоколегированные электроды с покрытием основного типа с образованием на внутренней поверхности шва коррозионностойкого покрытия сплавлением шлака с околошовной эмалью.1. The method of connecting enameled pipes with an acid type of coating, including one-sided welding of the root seam, characterized in that the welding process uses highly alloyed electrodes with a coating of the main type with the formation on the inner surface of the weld of a corrosion-resistant coating by alloying slag with heat-treated enamel. 2. Способ по п.1, отличающийся тем, что осуществляют сварку труб с притуплением 1,5-2,0 мм в корне стыка и поддерживают погонную энергию сварки 600-700 Дж/см. 2. The method according to claim 1, characterized in that the pipes are welded with a blunting of 1.5-2.0 mm at the root of the joint and the linear energy of welding is maintained at 600-700 J / cm.
RU96114197A 1996-07-10 1996-07-10 Method of connection of enamelled pipes RU2109197C1 (en)