RU98117295A - METHOD FOR WELDING PIPES FROM STEELS WITH ANTI-CORROSION COATING IN A PIPELINE - Google Patents

METHOD FOR WELDING PIPES FROM STEELS WITH ANTI-CORROSION COATING IN A PIPELINE

Info

Publication number
RU98117295A
RU98117295A RU98117295/02A RU98117295A RU98117295A RU 98117295 A RU98117295 A RU 98117295A RU 98117295/02 A RU98117295/02 A RU 98117295/02A RU 98117295 A RU98117295 A RU 98117295A RU 98117295 A RU98117295 A RU 98117295A
Authority
RU
Russia
Prior art keywords
welding
corrosion coating
pipes
pipeline
steels
Prior art date
Application number
RU98117295/02A
Other languages
Russian (ru)
Other versions
RU2155655C2 (en
Inventor
Е.Н. Галиченко
А.П. Медведев
Н.Н. Прохоров
М.Ю. Мухин
А.О. Малашенко
Original Assignee
Предприятие "Белозерное"
Filing date
Publication date
Application filed by Предприятие "Белозерное" filed Critical Предприятие "Белозерное"
Priority to RU98117295A priority Critical patent/RU2155655C2/en
Priority claimed from RU98117295A external-priority patent/RU2155655C2/en
Publication of RU98117295A publication Critical patent/RU98117295A/en
Application granted granted Critical
Publication of RU2155655C2 publication Critical patent/RU2155655C2/en

Links

Claims (1)

Способ сварки труб из сталей с антикоррозионным покрытием в трубопровод, включающий обработку торцов труб механическим способом, сборку стыка и комбинированную сварку стыка с выполнением корневого шва ручной аргонодуговой сваркой в среде защитного газа и заваркой оставшегося сечения ручной дуговой сваркой покрытыми электродами, отличающийся тем, что обработку торцов труб под сварку производят по прямой линейной образующей с углом раскрытия 35-37o, ручную аргонодуговую сварку корневого шва по внутреннему антикоррозионному покрытию из сталей аустенитного класса производят с подачей аргона (защитного газа) только с внешней стороны шва при сварочном токе 180 - 210 А.A method of welding pipes from steel with an anti-corrosion coating into a pipeline, including machining the ends of the pipes mechanically, assembling the joint and combined welding of the joint with the root weld by manual argon-arc welding in a protective gas medium and welding of the remaining cross section by manual arc welding with coated electrodes, characterized in that the processing the ends of the pipes for welding are produced in a straight linear generatrix with an opening angle of 35-37 o , manual argon-arc welding of the root seam along the internal anti-corrosion coating of austenitic class steels are produced with argon supply (shielding gas) only from the outside of the weld at a welding current of 180 - 210 A.
RU98117295A 1998-09-09 1998-09-09 Method for welding steel tubes with corrosion-resistant coating RU2155655C2 (en)