RU2009035C1 - Method of marking out pipe joining line - Google Patents

Method of marking out pipe joining line Download PDF

Info

Publication number
RU2009035C1
RU2009035C1 SU4937276A RU2009035C1 RU 2009035 C1 RU2009035 C1 RU 2009035C1 SU 4937276 A SU4937276 A SU 4937276A RU 2009035 C1 RU2009035 C1 RU 2009035C1
Authority
RU
Russia
Prior art keywords
marking
pipe
light
line
light source
Prior art date
Application number
Other languages
Russian (ru)
Inventor
Е.М. Кирин
П.А. Емельянов
Г.П. Ветлугина
С.В. Рожков
Original Assignee
Пензенский Политехнический Институт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Пензенский Политехнический Институт filed Critical Пензенский Политехнический Институт
Priority to SU4937276 priority Critical patent/RU2009035C1/en
Application granted granted Critical
Publication of RU2009035C1 publication Critical patent/RU2009035C1/en

Abstract

FIELD: mechanical engineering. SUBSTANCE: during marking-out process source of light is moved along exterior faces of prismatic pipe being joint and is positioned in the center of the faces in such a way that its center coincides with the planes of the aforementioned faces. The line of intersection of each face is marked along the boundary between light and shade formed by the source of light and the body of the pipe being joint. EFFECT: higher accuracy of marking out. 2 dwg

Description

Изобретение относится к трубным соединениям, точнее - к способам разметки стыковки труб перед сваркой. Изобретение предназначено для разметки стыков труб, а также стыков труб с другими поверхностями (сфера, тор, конус и т. д. ). The invention relates to pipe joints, more precisely, to methods for marking the joining of pipes before welding. The invention is intended for marking pipe joints, as well as pipe joints with other surfaces (sphere, torus, cone, etc.).

Наиболее близким по технической сущности к предлагаемому изобретению является способ разметки стыков труб, который заключается в том, что разметку линии пересечения и обрезку труб перед стыковкой ведут с помощью разметочной зоны, которую получают на основной трубе путем направления через стыкуемую трубу светового пучка от источника света и образования на основной трубе засвеченной зоны, образуемой на светочувствительной зоне. Способ осуществляется следующим образом. На основную трубу пропускают пучок света, в результате чего образуется засвеченная разметочная зона. Далее зону размечают с припуском на толщину стыкуемой трубы, вырезают в основной трубе отверстие по разметочной зоне, вставляют стыкуемую трубу, размечают ее по отверстию, обрезают, после чего трубы сваривают. Способ позволяет в 3-5 раз увеличить производительность разметки, значительно снизить трудоемкость, упростить разметку, увеличить точность стыковки трубных соединений. The closest in technical essence to the present invention is a method for marking pipe joints, which consists in marking the intersection line and cutting the pipes before joining using a marking zone, which is obtained on the main pipe by directing the light beam from the light source through the pipe to be joined and the formation on the main pipe of the illuminated zone formed on the photosensitive zone. The method is as follows. A beam of light is transmitted to the main pipe, as a result of which an illuminated marking zone is formed. Next, the zone is marked with an allowance for the thickness of the joined pipe, a hole is cut out in the main pipe along the marking zone, the joined pipe is inserted, it is marked along the hole, cut, and then the pipes are welded. The method allows to increase the marking productivity by 3-5 times, significantly reduce the complexity, simplify the marking, increase the accuracy of the joining of pipe joints.

Однако, резервы известного способа еще далеко не исчерпаны. Имеется резерв и необходимость в повышении точности разметки для особо ответственных соединений. However, the reserves of this method are far from exhausted. There is a reserve and the need to improve the accuracy of the marking for critical connections.

Целью изобретения является увеличение точности разметки за счет образования разметочной зоны непосредственно по внешнему контуру стыкуемой трубы и устранения необходимости построения линии припуска. The aim of the invention is to increase the accuracy of the marking due to the formation of the marking zone directly along the external contour of the joined pipe and eliminate the need to build an allowance line.

На фиг. 1 изображена схема реализации способа, вид спереди; на фиг. 2 - вид сверху, где 1 - основная труба, 2 - стыкуемая труба, 3 - источник света. In FIG. 1 shows a diagram of the implementation of the method, front view; in FIG. 2 is a top view, where 1 is the main pipe, 2 is the joint pipe, 3 is the light source.

Способ осуществляется следующим образом. The method is as follows.

Сначала трубы устанавливают по чертежу в соответствии с которым выдерживают положение осей труб относительно друг друга. Трубы располагают на некотором расстоянии друг от друга или непосредственно стыкуют их. First, the pipes are installed according to the drawing in accordance with which they maintain the position of the axes of the pipes relative to each other. Pipes are placed at some distance from each other or directly join them.

Далее подготавливают источник света (параболическая лампа, обычная маломощная лампа с отражателем или любой другой компактный источник света) и разметочную чертилку. После этого устанавливают источник света на верхнем торце стыкуемой трубы и монтируют его, например, на грани AF. Источник света устанавливают так, чтобы он находился примерно на середине грани (для получения четкой границы света и тени по всей длине линии пересечения) и совпадал с плоскостью грани (для увеличения точности разметки). После установки источника света на основной детали образуется четкая полоса разделяющая область света и тени. По этой полосе с помощью чертилки размечают линию пересечения грани AF призматической стыкуемой трубы с основной трубой. Затем аналогичные действия производят по всем граням и размечают соответствующие участки линии стыковки. Next, prepare a light source (parabolic lamp, ordinary low-power lamp with a reflector or any other compact light source) and a marking pen. After that, a light source is installed on the upper end of the abutting pipe and mounted, for example, on the face AF. The light source is set so that it is located approximately in the middle of the face (to obtain a clear border of light and shadow along the entire length of the intersection line) and coincides with the plane of the face (to increase the marking accuracy). After installing the light source on the main part, a clear band forms separating the area of light and shadow. In this strip, with the help of a scriber, mark the line of intersection of the face AF of the prismatic butt pipe with the main pipe. Then, similar actions are performed on all faces and mark the corresponding sections of the docking line.

Разметка производится с высокой точностью. Это обусловлено тем, что способ позволяет получать непосредственно линию пересечения по внешнему контуру стыкуемой детали в отличие от способа-прототипа, в котором линия пересечения получается дополнительной разметкой линии пересечения по разметочной зоне, полученной по внутреннему контуру стыкуемой трубы. Учитывая то обстоятельство, что разметка с припуском всегда приводит к ошибкам (толщина стыкуемой трубы никогда не проецируется в истинную величину на поверхность основной трубы), предлагаемый способ позволяет устранить необходимость использования припуска. Это безусловно, способствует увеличению точности разметки. The marking is made with high accuracy. This is due to the fact that the method allows you to get directly the intersection line along the external contour of the jointed part, in contrast to the prototype method, in which the intersection line is obtained by additional marking of the intersection line along the marking zone obtained along the inner contour of the jointed pipe. Given the fact that the marking with allowance always leads to errors (the thickness of the joined pipe is never projected into the true value on the surface of the main pipe), the proposed method eliminates the need to use an allowance. This, of course, helps to increase the accuracy of the markup.

Положительный эффект обеспечивается за счет следующего:
1. Перемещение источника света и установка его по граням стыкуемой трубы описанным в заявке образом позволяет последовательно, по участкам, получить линию стыковки труб непосредственно по внешнему контуру стыкуемой трубы без применения припуска.
A positive effect is ensured by the following:
1. Moving the light source and installing it along the edges of the joined pipe in the manner described in the application allows sequentially, in sections, to obtain a pipe docking line directly along the external contour of the joined pipe without using an allowance.

2. Разметка линии стыковки на границе света и тени, образуемой от источника света и тела стыкуемой трубы, позволяет повысить точность разметки без использования фоточувствительного слоя, без создания особых условий для работоспособности упомянутого слоя. Как правило, граница света и тени - четкая, ясная, что позволяет с помощью чертилки обозначать линию стыковки с высокой точностью разметки. 2. The marking of the docking line at the border of light and shadow formed from the light source and the body of the joined pipe allows to increase the marking accuracy without using a photosensitive layer, without creating special conditions for the operability of the mentioned layer. As a rule, the border of light and shadow is clear, clear, which allows you to use the scriber to indicate the line of connection with high marking accuracy.

По сравнению с прототипом предлагаемый способ обеспечивает следующий положительный эффект:
1. Обеспечивается разметка линии пересечения без дополнительной разметки линии припуска (линии обрезки) с учетом толщины стенки стыкуемой трубы, что повышает точность разметки и снижает трудоемкость разметки.
Compared with the prototype of the proposed method provides the following positive effect:
1. The marking of the intersection line is provided without additional marking of the allowance line (cutting line) taking into account the wall thickness of the joined pipe, which increases the accuracy of the marking and reduces the complexity of the marking.

2. Повышается точность разметки. Проведенные сравнительные испытания на моделях труб из пластмасс позволили установить, что точность линии стыка повышается (по контуру) до ± 0,2-0,5 мм, что очень важно для ответственных соединений. 2. Increases the accuracy of the markup. The comparative tests on plastic pipe models made it possible to establish that the accuracy of the joint line increases (along the contour) to ± 0.2-0.5 mm, which is very important for critical joints.

Снижается трудоемкость разметки за счет устранения операции по разметки линии стыковки основной трубы по припуску на толщину стыкуемой трубы. В предлагаемом изобретении линия обрезки получается автоматически. Трудоемкость снижается в 1,2-1,5 раза. The complexity of the marking is reduced by eliminating the operation of marking the line of docking of the main pipe according to the allowance for the thickness of the joined pipe. In the present invention, the cropping line is obtained automatically. The complexity is reduced by 1.2-1.5 times.

Изобретение найдет применение в машиностроении, судостроении, самолетостроении химическом машиностроении и других областях, где требуется обеспечить быструю и точную разметку трубных соединений. (56) Авторское свидетельство СССР N 1165564, кл. B 25 H 7/02, 1984. The invention will find application in mechanical engineering, shipbuilding, aircraft manufacturing, chemical engineering and other areas where it is required to provide fast and accurate marking of pipe joints. (56) Copyright certificate of the USSR N 1165564, cl. B 25 H 7/02, 1984.

Авторское свидетельство СССР N 1458201, кл. B 25 H 7/02, 1989. USSR copyright certificate N 1458201, cl. B 25 H 7/02, 1989.

Claims (1)

СПОСОБ РАЗМЕТКИ ЛИНИИ СТЫКОВКИ ТРУБ, заключающийся в том, что устанавливают на одну из стыкуемых труб источник света, наносят на вторую трубу разметочную зону и вырезают отверстие, совпадающее с этой зоной, наносят линию разметки на первую трубу и обрезают эту трубу по линии разметки, отличающийся тем, что, с целью повышения точности разметки за счет образования разметочной зоны по внешнему контуру стыкуемой трубы призматической формы, источник света последовательно устанавливают на внешних гранях стыкуемой трубы в середине каждой грани так, чтобы центр источника света совпадал с осью симметрии соответстующей грани, а линию разметки каждой грани наносят по границе света и тени. METHOD FOR PIPING THE LINK OF THE PIPE JOINING, which consists in installing a light source on one of the joined pipes, applying a marking zone to the second pipe and cutting a hole coinciding with this zone, marking the mark on the first pipe and cutting this pipe along the marking line, different in order to increase the accuracy of the marking due to the formation of a marking zone along the outer contour of the jointed pipe of a prismatic shape, the light source is sequentially installed on the outer faces of the jointed pipe in the middle of each face so that the center of the light source coincides with the axis of symmetry of the corresponding face, and the marking line of each face is drawn along the border of light and shadow.
SU4937276 1991-05-20 1991-05-20 Method of marking out pipe joining line RU2009035C1 (en)