PL62937B1 - - Google Patents

Download PDF

Info

Publication number
PL62937B1
PL62937B1 PL120867A PL12086767A PL62937B1 PL 62937 B1 PL62937 B1 PL 62937B1 PL 120867 A PL120867 A PL 120867A PL 12086767 A PL12086767 A PL 12086767A PL 62937 B1 PL62937 B1 PL 62937B1
Authority
PL
Poland
Prior art keywords
loosening
fur
skins
amount
trypsin
Prior art date
Application number
PL120867A
Other languages
Polish (pl)
Inventor
Janicki Józef
Dzieza Remigiusz
Original Assignee
Instytut Przemyslu Skórzanego
Filing date
Publication date
Application filed by Instytut Przemyslu Skórzanego filed Critical Instytut Przemyslu Skórzanego
Publication of PL62937B1 publication Critical patent/PL62937B1/pl

Description

Pierwszenstwo: Opublikowano: 01.VI.1967 (P 120 867) 25.VI.1971 62937 KI. 28 a, 2 MKP C 14 c, 1/08 UKD Wspóltwórcy wynalazku: Józef Janicki, Remigiusz Dzieza Wlasciciel patentu: Instytut Przemyslu Skórzanego, Lódz (Polska), Sposób rozluzniania skór futerkowych Przedmiotem wynalazku jest sposób rozluzniania skór futerkowych -polegajacy na zastosowaniu do rozluznia¬ nia tkanki skórnej skór surowych i rozmoczonych en¬ zymów proteolitycznych w roztworach soli kuchennej.Znane sa rózne sposoby rozluzniania tkanki skórnej 5 skór futerkowych. Dotychczas rozluznianie tkanki skór¬ nej skór futerkowych przeprowadza sie przed ich gar¬ bowaniem.Rozluznienie tkanki skórnej skór futerkowych zwia¬ zane jest z rozwlóknieniem zwartej struktury splotów 10 wlókien kolagenowych oraz z wylugowaniem z dermy bialek bezpostaciowych oraz tluszczu naturalnego. Wy¬ lugowanie z dermy bialek bezpostaciowych nastepuje w czasie rozmaczania, prania, piklowania, kwaszenia oraz traktowania skór futerkowych w kapielach o pH 15 2—4,5 lub 5,5—7,2, zawierajacych enzymy proteolitycz¬ ne otrzymane z wyciagów z plesni lub bakterii. Lugo¬ wanie z dermy tluszczu naturalnego nastepuje w czasie prania skór futerkowych. Rozwarstwienie zwartej struk¬ tury splotów wlókien kolagenowych uzyskuje sie dotych- 20 czas w czasie piklowania, kwaszenia lub traktowania skór futerkowych w kapielach zawierajacych enzymy proteolityczne otrzymane z wyciagów z plesni i bakte¬ rii.Rozluznianie skór futerkowych w kapielach kwasza- 25 cych, otrzymywanych w wyniku sfermentowania otrab i maki, zwiazane jest z dzialaniem na tkanke skórna mieszaniny nizszych kwasów organicznych oraz enzy¬ mów proteolitycznych pochodzenia roslinnego, typu pa- painy. Mankamentem metody kwaszenia jest koniecz- 30 nosc rozluzniania skór futerkowych przez dlugi okres czasu (2 — 14 dni) oraz trudny do kontrolowania prze¬ bieg procesów natury biochemicznej. Skóry rozluznione ta metoda ulegaja czesto uszkodzeniu, jak na przyklad odwloszeniu.Rozwarstwianie tkanki skórnej skór futerkowych w kapielach zawierajacych enzymy proteolityczne — otrzy¬ manych z wyciagów z plesni i bakterii — wymaga sto¬ sowania drogich, importowanych preparatów enzyma¬ tycznych oraz odpowiedniego przygotowania skór do rozluznienia.Stosowany z powodzeniem w garbarstwie sposób roz¬ luzniania odwapnionej dermy skór bydlecych, oparty na traktowaniu skór w kapieli o pH okolo 8,2 i tempera¬ turze 38°C, zawierajacej preparat enzymatyczny, jak na przyklad garbon, zastosowany do rozluzniania skór fu¬ terkowych powoduje wyrazne oslabienie sily osadzenia cebulek wlosowych w tkance skórnej oraz czesciowe od¬ wloszenie skór.Wszystkie te wady eliminuje sposób rozluzniania skór futerkowych wedlug wynalazku, który umozliwia wylu¬ gowanie z tkanki skórnej znacznej ilosci bialek bezpo¬ staciowych i tluszczu naturalnego, rozwarstwienie zwar¬ tej struktury splotów wlókien kolagenowych, przy jed¬ noczesnym zabezpieczeniu skór przed ich odwloszeniem, a jednoczesnie pozwala podwyzszyc wydajnosc po¬ wierzchniowa skór po wyprawie o 2—12%.Sposób rozluzniania skór futerkowych wedlug wyna¬ lazku polega na tym, ze rozmoczone, surowe skóry fu¬ terkowe rozluznia sie przez okres od 30 minut do 18 6293762937 3 4 godzin w kapieli o pH 7,5—8,8 i temperaturze 20—40°C, zawierajacej sól kuchenna w ilosci 30—80 g/l oraz pre¬ parat enzymatyczny na przyklad garbon, zawierajacy en¬ zymy proteolityczne typu trypsyny lub katepsyn oraz li¬ pazy w ilosci 0,01—0,15 g/l w przeliczeniu na czysta trypsyne.Po rozluznieniu enzymatycznym skóry wiruje sie, po czym sie je pierze, plucze, pikluje, garbuje, natluszcza i wykoncza w sposób stosowany w przemysle futrzar¬ skim, badz pierze w podwyzszonej temperaturze wedlug technologii zastrzezonej w patencie nr 56097 oraz piklu¬ je, garbuje, natluszcza i wykoncza wedlug zasad stoso¬ wanych w przemysle futrzarskim.Przyklad I. Surowe skóry owcze, o grubej tkance skórnej, rozmoczone w sposób stosowany w przemysle futrzarskim, po mizdrowaniu i mechanicznym oczysz¬ czeniu okrywy wlosowej, zarzuca sie do kapieli rozluz¬ niajacej. Rozluznianie tkanki skórnej skór owczych przeprowadza sie przez okres 18 godzin w kapieli o pH 7,5 i temperaturze 20°C, zawierajacej chlorek sodowy w ilosci 80 g/l oraz preparat enzymatyczny garbon w ilo¬ sci 0,15 g/l w przeliczeniu na czysta trypsyne. Nastepnie skóry wiruje sie, po czym garbuje formalinowo i pierze w kapielach o podwyzszonej temperaturze w sposób po¬ dany w patencie nr 56097, pikluje, garbuje i wykoncza w sposób stosowany w przemysle futrzarskim.Przyklad II. Rozmoczone i mizdrowane skóry królicze rozluznia sie przez okres 30 minut w kapieli o temperaturze 40°C i pH 8,8, zawierajacej chlorek so¬ dowy w ilosci 30 g/l oraz preparat enzymatyczny na przyklad garbon, zawierajacy lipazy oraz enzymy pro¬ teolityczne typu trypsyny lub katepsyn w ilosci 0,01 g/l w przeliczeniu na czysta trypsyne. Po rozluznianiu skóry wiruje sie, pikluje, garbuje i wykoncza w sposób stosowany w przemysle futrzarskim. PLPriority: Published: 01.VI.1967 (P 120 867) 25.VI.1971 62937 IC. 28 a, 2 MKP C 14 c, 1/08 UKD Inventors of the invention: Józef Janicki, Remigiusz Dzieza Patent owner: Institute of the Leather Industry, Lodz (Poland), The method of loosening fur skins The subject of the invention is a method of loosening fur skins - based on the use of loosening The skin tissue of hides and the soaked proteolytic enzymes in common salt solutions. Various methods of loosening the skin tissue of fur skins are known. Hitherto, the loosening of the dermal tissue of the fur skins is performed prior to their tanning. The loosening of the dermal tissue of the fur skins is associated with the fibering of the dense structure of the strands of collagen fibers and the leaching of amorphous proteins and natural fat from the dermis. Leaching out of the amorphous proteins from the skin takes place during soaking, washing, pickling, souring and treating the fur in baths with a pH of 2-4.5 or 5.5-7.2, containing proteolytic enzymes obtained from extracts from mold or bacteria. The lengthening of the natural fat leather occurs during the washing of the fur skins. The delamination of the dense structure of the strands of collagen fibers has so far been obtained during pickling, souring or treatment of furskins in baths containing proteolytic enzymes obtained from extracts from mold and bacterias. Loosening the furskins in sour baths obtained in sour baths. As a result of the fermentation of ottomans and flour, it is associated with the action of a mixture of lower organic acids and proteolytic enzymes of plant origin, such as papaya, on the skin tissue. The drawback of the leavening method is the necessity to loosen the fur for a long period of time (2 - 14 days) and the difficult to control course of biochemical processes. Skin loosened by this method is often damaged, such as dehinning. The disintegration of the skin tissue of fur skins in baths containing proteolytic enzymes - obtained from extracts of mold and bacteria - requires the use of expensive, imported enzyme preparations and appropriate preparation of the skins for A successfully used tanning process for loosening decalcified cowhide leather, based on the treatment of the leather in a bath with a pH of about 8.2 and a temperature of 38 ° C, containing an enzyme preparation, such as a tannin, used to loosen the leather. The mycelium causes a marked weakening of the strength of embedding the hair follicles in the skin tissue and a partial de-hair removal of the skin. ¬ this structure of weaves of collagen fibers, at the same time protecting the skins against their dehidification, and at the same time it allows to increase the surface efficiency of the skins after the trip by 2-12%. The method of loosening fur skins according to the invention consists in the fact that soggy, raw furskins are loosened by period from 30 minutes to 18 6293762937 3-4 hours in a bath of pH 7.5-8.8 and temperature 20-40 ° C, containing 30-80 g / l of table salt and an enzyme preparation, for example proteolytic enzymes such as trypsin or cathepsin and lypase in the amount of 0.01-0.15 g / l in terms of pure trypsin. After enzymatic loosening of the skin, it is swirled, then it is washed, rinsed, pickled, tanned, oily and it performs in a manner used in the fur industry, or washes at an elevated temperature according to the technology claimed in the patent No. 56097, and pickles, tans, greases and finishes according to the principles used in the fur industry. Example I. Raw sheepskin, thick vol the skin rim, soaked in the way used in the fur industry, after fleshing and mechanical cleaning of the hair coat, it is thrown into a relaxing bath. Skin tissue loosening of sheepskins is carried out for 18 hours in a bath at pH 7.5 and temperature 20 ° C, containing sodium chloride in the amount of 80 g / l and the enzyme preparation garbon in the amount of 0.15 g / l in terms of pure trypsin. The skins are then spun, formalin tanned and washed in elevated temperature baths as described in Patent No. 56097, pickled, tanned, and finished in the manner used in the fur industry. Example II. Soggy and fleshed rabbit skins are loosened for 30 minutes in a bath at 40 ° C and pH 8.8, containing sodium chloride in the amount of 30 g / l and an enzymatic preparation, for example, hump, containing lipases and pro-theolytic enzymes such as trypsin or cathepsin in an amount of 0.01 g / l based on pure trypsin. After loosening the leather, it is twirled, pickled, tanned and finished in the manner used in the fur industry. PL

Claims (1)

1. Zastrzezenie patentowe 15 Sposób rozluzniania skór futerkowych, znamienny tym, ze rozmoczone, surowe skóry futerkowe poddaje sie rozluznianiu przez okres od 30 minut do 18 godzin w kapieli o pH 7,5—8,8 i temperaturze 20—40°C, za- 20 wierajacej chlorek sodowy w ilosci 30—80 g/l oraz pre¬ parat enzymatyczny na przyklad garbon, zawierajacy enzymy proteolityczne typu trypsyny lub katepsyn oraz lipazy w ilosci 0,01—0,15 g/l w przeliczeniu na czysta trypsyne. 10 20 WDA-1. Zam. 649, naklad 250 cgz. PL1. Claim 15 A method of loosening fur skins, characterized in that soggy, raw fur skins are loosened for a period of 30 minutes to 18 hours in a bath at pH 7.5-8.8 and temperature 20-40 ° C, - 20 containing sodium chloride in an amount of 30-80 g / l and an enzyme preparation, for example a hump, containing proteolytic enzymes of the trypsin or cathepsin type and lipase in an amount of 0.01-0.15 g / l in terms of pure trypsin. 10 20 WDA-1. Order 649, mintage 250 cg. PL
PL120867A 1967-06-01 PL62937B1 (en)