PL404270A1 - Process for preparing a polymer mixture of sulfur from waste flotation of copper ore reducing agent and the amount of hydrogen sulphide fumes of asphalt used, especially as a supplement for the road asphalt mixtures - Google Patents

Process for preparing a polymer mixture of sulfur from waste flotation of copper ore reducing agent and the amount of hydrogen sulphide fumes of asphalt used, especially as a supplement for the road asphalt mixtures

Info

Publication number
PL404270A1
PL404270A1 PL404270A PL40427013A PL404270A1 PL 404270 A1 PL404270 A1 PL 404270A1 PL 404270 A PL404270 A PL 404270A PL 40427013 A PL40427013 A PL 40427013A PL 404270 A1 PL404270 A1 PL 404270A1
Authority
PL
Poland
Prior art keywords
asphalt
road
amount
copper ore
fumes
Prior art date
Application number
PL404270A
Other languages
Polish (pl)
Other versions
PL226608B1 (en
Inventor
Andrzej Janiczek
Włodzimierz Mysłowski
Original Assignee
Andrzej Janiczek
Włodzimierz Mysłowski
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Andrzej Janiczek, Włodzimierz Mysłowski filed Critical Andrzej Janiczek
Priority to PL404270A priority Critical patent/PL226608B1/en
Publication of PL404270A1 publication Critical patent/PL404270A1/en
Publication of PL226608B1 publication Critical patent/PL226608B1/en

Abstract

Sposób otrzymywania mieszaniny polimeru siarki z odpadem po flotacji rudy miedzi, jako środkiem zmniejszającym emisję siarkowodoru i zmniejszającym zużycie asfaltu zwłaszcza jako dodatek do asfaltowych mieszanek drogowych, polega na mieszaniu w mieszalniku poziomym 80-90% wagowych ciekłego polimeru siarki z 10-20% wagowych wysuszonego odpadu po flotacji rudy miedzi w temperaturze 140°C z prędkością obrotową mieszadła 100 obr/min w czasie 30 minut, by następnie po tym czasie ciekłą zawartość mieszalnika po schłodzeniu na płatkownicy uformować w formie drobnych płatków lub granulek jeśli uformowanie przebiega na granulatorze bębnowym, tak sporządzony dodatek do asfaltów jest dozowany w wytwórni mieszanek drogowych do mieszalnika, do którego to dozujemy ogrzany wypełniacz mineralny, asfalt drogowy i dodatek do asfaltu, który nie tylko, że zmniejsza ilość wyziewu siarkowodoru z około 100 ppm do 10 ppm, ale również obniża w składzie asfaltowej mieszanki drogowej ilość zużytego asfaltu drogowego z 6 do 2% wagowych w zależności od ilości dozowanego dodatku do asfaltu do sporządzanej asfaltowej mieszanki drogowej.The method of obtaining a mixture of sulfur polymer with waste from copper ore flotation as a means of reducing hydrogen sulfide emission and reducing asphalt consumption, especially as an addition to asphalt road mixtures, consists in mixing in a horizontal mixer 80-90% by weight of liquid sulfur polymer with 10-20% by weight of dried waste from copper ore flotation at a temperature of 140 ° C with a rotational speed of 100 rpm for 30 minutes, then after that time the liquid contents of the mixer after cooling on the flaker to be formed in the form of small flakes or granules if the formation takes place on a drum granulator, yes prepared bitumen additive is dosed in the road mixes plant to the mixer, to which we dispense heated mineral filler, road asphalt and asphalt additive, which not only reduces the amount of hydrogen sulfide fumes from about 100 ppm to 10 ppm, but also reduces the composition asphalt mixture amount of used asphalt road from 6 to 2% by weight depending on the amount of bitumen additive added to the asphalt road mix.

PL404270A 2013-06-10 2013-06-10 Process for preparing a polymer mixture of sulfur from waste flotation of copper ore reducing agent and the amount of hydrogen sulphide fumes of asphalt used, especially as a supplement for the road asphalt mixtures PL226608B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
PL404270A PL226608B1 (en) 2013-06-10 2013-06-10 Process for preparing a polymer mixture of sulfur from waste flotation of copper ore reducing agent and the amount of hydrogen sulphide fumes of asphalt used, especially as a supplement for the road asphalt mixtures

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PL404270A PL226608B1 (en) 2013-06-10 2013-06-10 Process for preparing a polymer mixture of sulfur from waste flotation of copper ore reducing agent and the amount of hydrogen sulphide fumes of asphalt used, especially as a supplement for the road asphalt mixtures

Publications (2)

Publication Number Publication Date
PL404270A1 true PL404270A1 (en) 2014-12-22
PL226608B1 PL226608B1 (en) 2017-08-31

Family

ID=52106817

Family Applications (1)

Application Number Title Priority Date Filing Date
PL404270A PL226608B1 (en) 2013-06-10 2013-06-10 Process for preparing a polymer mixture of sulfur from waste flotation of copper ore reducing agent and the amount of hydrogen sulphide fumes of asphalt used, especially as a supplement for the road asphalt mixtures

Country Status (1)

Country Link
PL (1) PL226608B1 (en)

Also Published As

Publication number Publication date
PL226608B1 (en) 2017-08-31

Similar Documents

Publication Publication Date Title
ES2610954T3 (en) Method for producing agglomerates having rubber and wax, agglomerates produced according to said method, and use of said agglomerates in asphalts or bituminous compounds
MY173339A (en) The method of production of granulated polymer-asphalt binder and sulfur concrete with participation of sulfur polymer obtained in waste sulfur solvent-borne modification
EP3978456A3 (en) Additive for asphalt mixes containing reclaimed bituminous products
EA201190245A1 (en) COMPOSITION FOR IMPROVED STABILITY AND OPERATIONAL CHARACTERISTICS OF ASPHALT-CONCRETE MIXTURES AND REDUCTION OF THEIR ENVIRONMENT
MX2016009254A (en) Asphalt mixture, method for producing same and paving method using same.
UA111094C2 (en) Compound for realization of modified bitumen for asphalts
EA201301325A1 (en) ASPHALT COMPOSITION
MX2019008522A (en) Asphalt composition for road paving.
RU2014110043A (en) TECHNOLOGICAL SYSTEM OF MODIFICATION OF ASPHALT AND METHOD OF INTRODUCING ASPHALT ADDITIVES
WO2011146735A3 (en) Mixtures of zeolite and rap/ras
HRP20200291T1 (en) Anti-icing additive composition for bituminous conglomerates
PL404270A1 (en) Process for preparing a polymer mixture of sulfur from waste flotation of copper ore reducing agent and the amount of hydrogen sulphide fumes of asphalt used, especially as a supplement for the road asphalt mixtures
Gul et al. Evaluation of various factors affecting mix design of sulfur-extended asphalt mixes
CA2914206C (en) Recycled hot asphalt mixture production method
RU2010110798A (en) ASPHALT MIX
RU2543838C1 (en) Method to produce asphalt-concrete mix
RU2494059C1 (en) Crude mixture for making aggloporite
Butz et al. Innovative method for producing crumbed rubber modified asphalt
PL420254A1 (en) Method for obtaining sulfur granules with addition of hydrogen sulfide releasing inhibitor
CN106147249B (en) A kind of warm mix type Rut resistance composite modifier and preparation method thereof
RU2009103715A (en) METHOD FOR PRODUCING CRUSHED MACHINE ASPHALT-CONCRETE MIX WITH ADDITION OF DEDICATIONS OF CRUSHING OF LIMESTONS OF BRAND 400
PL389668A1 (en) Sulphur polymer obtained from the sulphur solvent modification and method for production thereof
RU2012114263A (en) ASPHALT MIX
BE1018787A4 (en) BOUILLIE DELEGATION.
PL403882A1 (en) Method for producing the mineral and asphalt mix