KR970062202A - Non-slip jaw contained by waste tire shredder - Google Patents
Non-slip jaw contained by waste tire shredder Download PDFInfo
- Publication number
- KR970062202A KR970062202A KR1019970024378A KR19970024378A KR970062202A KR 970062202 A KR970062202 A KR 970062202A KR 1019970024378 A KR1019970024378 A KR 1019970024378A KR 19970024378 A KR19970024378 A KR 19970024378A KR 970062202 A KR970062202 A KR 970062202A
- Authority
- KR
- South Korea
- Prior art keywords
- slip jaw
- waste tire
- roller
- mixed
- slip
- Prior art date
Abstract
목적purpose
겨울철에도 미끄럼 방지턱의 기능을 상실하지 않는 미끄럼 방지턱을 제공함을 목적으로 한다.It is an object of the present invention to provide a non-slip jaw that does not lose the function of the non-slip jaw even in winter.
규사, 또는 제철 슬래그, 폐타이어파쇄체, 아스팔트를 약 100°~170℃로 가열 혼합하여 이를 미끄럼 방지턱을 포설할 곳에 포설한 후 이를 롤러로 다짐하여서된 미끄럼 방지턱을 만들거나 또는 규사, 제철 슬래그, 폐타이어파쇄체를 혼합하여 혼합골재를 만드는 한편, 미끄럼 방지턱을 포설한 곳에 에폭시수지를 약 5mm 두께로 도포하고, 즉시 그 위에 상기 혼합골재를 살포 후 이를 롤러로 다짐하여서된 미끄럼 방지턱.Silica sand or steel slag, waste tire crushed body, and asphalt are heated and mixed at about 100 ° to 170 ° C., which is then placed in a place where a non-slip jaw is to be installed, and then the roller is compacted with a roller to make a non-slip jaw or silica sand, steel slag, A non-slip jaw is made by mixing waste tire crushed body to make a mixed aggregate, while applying an epoxy resin to a thickness of about 5 mm where a non-slip jaw is installed, and immediately spraying the mixed aggregate thereon and then compacting it with a roller.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
Claims (3)