KR970062097A - 저수축 폴리에스테르 섬유의 제조방법 - Google Patents

저수축 폴리에스테르 섬유의 제조방법 Download PDF

Info

Publication number
KR970062097A
KR970062097A KR1019950050704A KR19950050704A KR970062097A KR 970062097 A KR970062097 A KR 970062097A KR 1019950050704 A KR1019950050704 A KR 1019950050704A KR 19950050704 A KR19950050704 A KR 19950050704A KR 970062097 A KR970062097 A KR 970062097A
Authority
KR
South Korea
Prior art keywords
relaxation
polyester fiber
manufacturing
zone
roller
Prior art date
Application number
KR1019950050704A
Other languages
English (en)
Inventor
한재성
Original Assignee
이웅열
주식회사 코오롱
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이웅열, 주식회사 코오롱 filed Critical 이웅열
Priority to KR1019950050704A priority Critical patent/KR970062097A/ko
Publication of KR970062097A publication Critical patent/KR970062097A/ko

Abstract

본 발명은 고뎃롤러를 이용하여 다단계 연신 및 이완열처리하는 폴리에스테르 연신사이 제조방법에 있어서 제1차 이완영역과 제2차 이완영역에서 300~500℃의 비접촉열판을 사용하여 열처리하고, 상기 1차 및 2차 이완 영역의 2번째 고뎃롤러의 온도를 260~280℃로 하여서 이완열고정이 충분하게 이루어지도록 하는 방법임.
본발명으로 제조된 연신사는 이완열고정을 충분히 받았기때문에 건열수축율이 3.2~3.8%의 저수축성이 발현됨.

Description

저수축 폴리에스테르 섬유의 제조방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 본 발명의 제조공정 개략도.

Claims (2)

  1. 폴리에스테르폴리머를 용융방사하고 다단연신후 이완처리하여 저수축 폴리에스테르섬유를 제조함에 있어서 이완처리를 2개의 고뎃롤러를 가진 1차 이완영역 및 2개의 고뎃롤러를 가진 2차 이완영역에서 행하며, 1차 이완영역 및 2차 이완영역 사이에서 300~500℃의 비접촉열판으로 열처리함을 특징으로 하는 저수축 폴리에스테르섬유의 제조방법.
  2. 제1항에 있어서, 1차 이완영역 및 2차 이완영역의 2번째 고뎃롤러의 온도가 260~280℃임을 특징으로 하는 저수축 폴리에스테르섬유의 제조방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019950050704A 1995-12-15 1995-12-15 저수축 폴리에스테르 섬유의 제조방법 KR970062097A (ko)