KR970010980A - 토페도의 내부 응구용선 용해방법 - Google Patents

토페도의 내부 응구용선 용해방법 Download PDF

Info

Publication number
KR970010980A
KR970010980A KR1019950023954A KR19950023954A KR970010980A KR 970010980 A KR970010980 A KR 970010980A KR 1019950023954 A KR1019950023954 A KR 1019950023954A KR 19950023954 A KR19950023954 A KR 19950023954A KR 970010980 A KR970010980 A KR 970010980A
Authority
KR
South Korea
Prior art keywords
molten iron
topedo
slag
blowing
molten
Prior art date
Application number
KR1019950023954A
Other languages
English (en)
Other versions
KR0146800B1 (ko
Inventor
김현근
권영식
정효철
Original Assignee
김종진
포항종합제철 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김종진, 포항종합제철 주식회사 filed Critical 김종진
Priority to KR1019950023954A priority Critical patent/KR0146800B1/ko
Publication of KR970010980A publication Critical patent/KR970010980A/ko
Application granted granted Critical
Publication of KR0146800B1 publication Critical patent/KR0146800B1/ko

Abstract

본 발명은 제강설비의 하나인 토페도(torpedo)의 내부에 응고되어 있는 용선을 효율적으로 용해할 수 있는 방법을 제공함에 그 목적이 있다. 상기 목적달성을 위해 본 발명은 토페도내에 응고되어 있는 용선을 폐목, 코크스의 투입과 사소취입으로 발화시킨 후 발열재를 투입하여 용선을 승온시킨 다음, 질소가스에 의해 슬래그를 배재시키고, 이러한 과정을 반복실시한 후에 용해된 용선을 출선시키는 토페도의 내부 응고용선 용해방법에 관한 것을 그 기술적 요지로 한다.

Description

토페도의 내부 응고용선 용해방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 통상적인 토페도의 내부단면도,
제2도는 토페도의 내부에 부착된 지금을 제거하는 종래의 방법을 나타내는 모식도,
제3도는 토페도의 내부에 완전 응고된 용선의 모습을 나타내는 모식도,
제4도는 토페도의 내부에 완전 응고된 용선을 본 발명에 의해 용해하는 모습을 나타내는 모식도.

Claims (2)

  1. 고로로부터 수선되어 그 일부 또는 전부가 완전 응고된 용선이 존재하에 토페도의 내부에 폐목을 투입하고, 상기 폐목이 점화되면 코크스를 투입하고, 랜스를 통해 산소를 취입하는 단계; 상기 산소취입과 함께 발열재를 투입하여 응고된 용선을 일부 용해시키는 단계; 상기 취입 대신 질소가스를 취입하여 용해된 용선의 상부에 있는 슬래그를 포밍(forming)시켜 토페도의 개구부로 슬래그를 배재시키는 단계; 및 슬래그가 배재된 용선이 완전히 용해될 때까지 상기와 같은 용선의 용해단계와 슬래그가 배재단계를 반복실시한 후, 용선을 출선시키는 단계를 포함하여 구성됨을 특징으로 하는 토페도의 내부응고 용선 용해방법.
  2. 제1항에 있어서, 상기 발열재가 알루미늄 합금 및 실리콘 합금임을 특징으로 하는 방법.
    ※ 참고 사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019950023954A 1995-08-03 1995-08-03 토페도의 내부 응고용선 용해방법 KR0146800B1 (ko)