KR960017515A - 입자특성이 우수한 침상형 알파 산화철의 제조방법 - Google Patents

입자특성이 우수한 침상형 알파 산화철의 제조방법 Download PDF

Info

Publication number
KR960017515A
KR960017515A KR1019940029117A KR19940029117A KR960017515A KR 960017515 A KR960017515 A KR 960017515A KR 1019940029117 A KR1019940029117 A KR 1019940029117A KR 19940029117 A KR19940029117 A KR 19940029117A KR 960017515 A KR960017515 A KR 960017515A
Authority
KR
South Korea
Prior art keywords
solution
iron oxide
ferric hydroxide
aqueous
slurry
Prior art date
Application number
KR1019940029117A
Other languages
English (en)
Other versions
KR0136167B1 (ko
Inventor
변태봉
김대영
손진군
Original Assignee
김만제
포항종합제철 주식회사
신창식
재단법인 산업과학기술연구소
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김만제, 포항종합제철 주식회사, 신창식, 재단법인 산업과학기술연구소 filed Critical 김만제
Priority to KR1019940029117A priority Critical patent/KR0136167B1/ko
Publication of KR960017515A publication Critical patent/KR960017515A/ko
Application granted granted Critical
Publication of KR0136167B1 publication Critical patent/KR0136167B1/ko

Abstract

본 발명은 출발원료로 제이철염을 사용하고 이로부터 제조된 수산화제이철 수용액에 적정량의 타타르산을 첨가하여 수열반응시키므로서 고밀도 기록재료에 적합한 입자특성, 특히 입자크기가 미세하고 침상비가 큰 침상형 α산화철의 제조방법을 제공하고자 하는데, 그 목적이 있다.
본 발명은 침상형 α산화철의 제조방법에 있어서, 출발원료인 제이철염 수용액에 알카리 중화반응에 의해 수산화제이철 수용액을 제조하는 단계; 상기 수산화제이철 수용액에 타타르산을 상기 수산화제이철의 철원자에 대한 몰양 환산 값으로 1×10-5-1×10-4몰양의 범위로 첨가하여 슬러리를 제조하는 단계; 상기 슬러리용액의 염기도를 9.0~12.0의 범위로 조절하는 단계; 및 상기 슬러리용액을 100~160℃의 온도범위에서 수열반응시키는 단계를 포함하여 구성됨을 특징으로 하는 입자특성이 우수한 침상형 α산화철의 제조방법에 관한 것을 그 요지로 한다.

Description

입자특성이 우수한 침상형 알파 산화철의 제조방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (1)

  1. 침상형 α산화철의 제조방법에 있어서, 출발원료인 제이철염 수용액에 알카리 중화반응에 의해 수산화제이철 수용액을 제조하는 단계; 상기 수산화제이철 수용액에 타타르산을 상기 수산화제이철의 철원자에 대한 몰양 환산 값으로 1×10-5-1×10-4몰양의 범위로 첨가하여 슬러리를 제조하는 단계; 상기 슬러리용액의 염기도를 9.0~12.0의 범위로 조절하는 단계; 및 상기 슬러리용액을 100~160℃의 온도범위에서 수열반응시키는 단계를 포함하여 구성됨을 특징으로 하는 입자특성이 우수한 침상형 α산화철의 제조방법
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019940029117A 1994-11-08 1994-11-08 입자특성이 우수한 침상형 알파 산화철의 제조방법 KR0136167B1 (ko)