KR940003894A - Water repellent glazing and its manufacturing method - Google Patents
Water repellent glazing and its manufacturing method Download PDFInfo
- Publication number
- KR940003894A KR940003894A KR1019930015237A KR930015237A KR940003894A KR 940003894 A KR940003894 A KR 940003894A KR 1019930015237 A KR1019930015237 A KR 1019930015237A KR 930015237 A KR930015237 A KR 930015237A KR 940003894 A KR940003894 A KR 940003894A
- Authority
- KR
- South Korea
- Prior art keywords
- fluorine compound
- sol
- ceramic
- water
- mixture
- Prior art date
Abstract
본 발명은 유리 기본체와 유기 기본체의 표면에 형성된 세라믹층(세라믹층은 세라믹 졸과 불소 화합물을 혼합하여 열처리함으로써 수득된다)으로 구성되는 발수성 창유리에 관한 것이다.The present invention relates to a water repellent glazing composed of a ceramic layer formed on the surface of a glass base and an organic base (ceramic layer is obtained by mixing and heat treating a ceramic sol and a fluorine compound).
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
제1도는 불소화합물 농도와 담가(曇價)의 관계를 나타낸 불소화합물 농도-담가 특성 그래프이며,1 is a fluorine compound concentration-load characteristic graph showing the relationship between fluorine compound concentration and solubility.
제2도는 인양 속도와 발수성 및 인양 속도와 투과율의 관계를 나타내는 인양속도-발수성·투과율 특성 그래프이며,2 is a graph of the lifting speed-water repellency and transmittance characteristics showing the relationship between the lifting speed and the water repellency and the lifting speed and the transmittance,
제3도는 가열온도와 발수성 및 가열온도와 내수성의 관계를 나타내는 가열온도-발수성·내수성 특성 그래프이며,3 is a graph of heating temperature-water repellency and water resistance characteristics showing the relationship between heating temperature and water repellency and heating temperature and water resistance,
제4도는 지르코니아의 자외선 차궤율을 나타낸 차폐율-파장 특성 그래프이다4 is a graph of shielding rate-wavelength characteristics showing the ultraviolet ray shielding rate of zirconia
Claims (11)