KR920005210A - 저장형 음극의 제조방법 - Google Patents

저장형 음극의 제조방법 Download PDF

Info

Publication number
KR920005210A
KR920005210A KR1019900013423A KR900013423A KR920005210A KR 920005210 A KR920005210 A KR 920005210A KR 1019900013423 A KR1019900013423 A KR 1019900013423A KR 900013423 A KR900013423 A KR 900013423A KR 920005210 A KR920005210 A KR 920005210A
Authority
KR
South Korea
Prior art keywords
porous metal
aqueous solution
scandium nitrate
metal gas
nitrate aqueous
Prior art date
Application number
KR1019900013423A
Other languages
English (en)
Other versions
KR920007414B1 (ko
Inventor
이안섭
Original Assignee
김정배
삼성전관 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김정배, 삼성전관 주식회사 filed Critical 김정배
Priority to KR1019900013423A priority Critical patent/KR920007414B1/ko
Publication of KR920005210A publication Critical patent/KR920005210A/ko
Application granted granted Critical
Publication of KR920007414B1 publication Critical patent/KR920007414B1/ko

Abstract

내용 없음.

Description

저장형 음극의 제조방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 종래의 저장형 음극의 부분 개략 단면도.
제2도는 제1도에서의 A부분의 확대도.
제3도는 이 발명에 따른 저장형 음극의 확대 상세도이다.
* 도면의 주요 부분에 대한 부호의 설명
1 : 다공질 금속기체 2 : 전자 방출물질
3 : 저장조 4 : 슬리이브
5 : 히터 6 : 기공
7 : 텅스텐과 스칸듐 옥사이드가 혼합된 다공질 금속기체
8 : 텅스텐입자에 스칸듐옥사이드가 코팅된 다공질 금속기체

Claims (2)

  1. 오목형상의 저장조내에 바륨 칼슘 알루미네이트를 저장 시키고, 상기 저장조 상부에 다공질 금속분말의 압축성형체를 장착시킨 저장형 음극의 제조방법에 있어서, 다공질 금속기체를 질산 스칸듐 수용액에 넣어 진공상태에서 다공질 사이로 상기 질산 스칸듐 수용액을 침투시키는 단계와 질산 스칸듐 수용액이 침투된 상기 다공질 금속기체를 환원분위기 또는 진공중에서 가열시키는 단계와로 구성되어 상기 다공질 금속기체의 입자에 박막층을 형성시키는 저장형 음극의 제조방법.
  2. 제1항에 있어서, 상기 질산 스칸듐 수용액의 농도가 0.01% 내지 5%이며, 상기 질산 스칸듐 수용액이 침투된 다공질 금속기체를 가열시키는 온도가 300℃ 내지 400℃인 저장형 음극의 제조방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019900013423A 1990-08-29 1990-08-29 저장형 음극의 제조방법 KR920007414B1 (ko)