KR830001408A KR1019790002773A KR790002773A KR830001408A KR 830001408 A KR830001408 A KR 830001408A KR 1019790002773 A KR1019790002773 A KR 1019790002773A KR 790002773 A KR790002773 A KR 790002773A KR 830001408 A KR830001408 A KR 830001408A
Authority
KR
South Korea
Prior art keywords
lower alkyl
water
soluble
moiety
structural formula
Prior art date
Application number
KR1019790002773A
Other languages
English (en)
Other versions
KR850000599B1 (ko
Inventor
이. 가이거 게리
씨. 메이 로서
Original Assignee
알렉산더 디. 릿치
베쯔 레보라토리스 인코포레이티드
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 알렉산더 디. 릿치, 베쯔 레보라토리스 인코포레이티드 filed Critical 알렉산더 디. 릿치
Publication of KR830001408A publication Critical patent/KR830001408A/ko
Application granted granted Critical
Publication of KR850000599B1 publication Critical patent/KR850000599B1/ko

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C23COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
    • C23FNON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
    • C23F11/00Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
    • C23F11/08Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Mechanical Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Preventing Corrosion Or Incrustation Of Metals (AREA)
  • Compositions Of Macromolecular Compounds (AREA)

Abstract

내용 없음

Description

수성 매체 내 부식방지 방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도~2도 용해성 아연의 양을 그 조건과 비교하여 도표화한 것.

Claims (1)

  1. 수성매체에 수용성 아연 화합물과 아크릴산 또는 그 수용성염으로부터 유도된 부위와 수산기치환 저급알킬 아크릴에이트의 부위를 함유하는 다음 구조식을 가진 상기 폴리머의 부위 즉,
    상기 구조식에서 R은 수소 또는 1 내지 3탄소원의 저급아킬
    R1은 OH,NH2혹은 OM여기에서 M은 수용성양이온
    R2는 약 2 내지 6탄소원자의 저급알킬
    R3는 H 또는 1 내지 3탄소원자의 저급알킬이며, x:y의 몰비는 1:4 내지 36:1인 수용성 폴리머를 가하여 함유하는 효과적인 양의 수성매체성 아연침전과 접촉하는 금속표면의 부식량을 감소시키는 부식방지 방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR7902773A 1979-04-05 1979-08-14 부식방지 조성물 KR850000599B1 (ko)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
US2734679A 1979-04-05 1979-04-05
US27346 1979-04-05

Publications (2)

Publication Number Publication Date
KR830001408A true KR830001408A (ko) 1983-04-30
KR850000599B1 KR850000599B1 (ko) 1985-04-30

Family

ID=21837185

Family Applications (1)

Application Number Title Priority Date Filing Date
KR7902773A KR850000599B1 (ko) 1979-04-05 1979-08-14 부식방지 조성물

Country Status (3)

Country Link
JP (1) JPS55139446A (ko)
KR (1) KR850000599B1 (ko)
CA (1) CA1118589A (ko)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2012206044A (ja) * 2011-03-30 2012-10-25 Kurita Water Ind Ltd 冷却水系のスケール防止方法

Family Cites Families (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS51146341A (en) * 1975-06-12 1976-12-15 Sanyo Chemical Ind Ltd Agent for preventing corrosion*generation of scale and contamination in water circulation system

Also Published As

Publication number Publication date
CA1118589A (en) 1982-02-23
JPS55139446A (en) 1980-10-31
KR850000599B1 (ko) 1985-04-30

Similar Documents

Publication Publication Date Title
GB1455343A (en) Corrosion inhibition
KR840004460A (ko) 금속 표면처리 수용액
KR840004425A (ko) N-알킬-노스코핀의 제조방법
EP0188884A1 (en) Method of controlling iron induced fouling in water systems
DE3568568D1 (en) Carboxylic/sulfonic/quaternary ammonium polymers for use as scale and corrosion inhibitors
KR860001766A (ko) 용수계통에 있어서 스케일 형성 억제방법
CA2013461A1 (en) Gellable aqueous composition and its use in enhanced petroleum recovery
KR850000406A (ko) 4-클로로-2-페닐이미다졸-5-아세트산유도체의 제조방법
GB1474362A (en) Process for inhibiting the corrosion and deposition of boiler scale in water-conveying systems
EP0101230A3 (en) Ferrous sulfide dissolution in acid with lowered gas formation
KR830010404A (ko) 방사선에 의한 중합성 조성물
KR830009348A (ko) 수-분산 수소성 중점화 조성물
CA2036539A1 (en) Biocide activator
ATE38820T1 (de) Karbonsaeure-sulfonsaeure-polyalkylenoxidkopolymerisate und ihre verwendung als korrosions- und kesselsteininhibitoren.
CA2052732A1 (en) Method for inhibiting scale formation
JPS56125345A (en) Acylation of aminocarboxylic acid
KR870004909A (ko) 수용성계에서 철의 안정화
GB1533782A (en) Use of n-acyl-1-aminoalkane-1,1-diphosphonic acids as complexing agents
KR830001408A (ko) 수성 매체 내 부식방지 방법
KR860000416A (ko) 비철금속의 방식제 및 방식방법
KR830005325A (ko) 수용성 화학 발광 시스템
KR890000621A (ko) 부동액 조성물
JPS57185988A (en) Anticorrosive for metal
MX169858B (es) Procedimiento para producir pintura
JPH0357195B2 (ko)

Legal Events

Date Code Title Description
E902 Notification of reason for refusal
E902 Notification of reason for refusal
E902 Notification of reason for refusal
G160 Decision to publish patent application
E701 Decision to grant or registration of patent right
GRNT Written decision to grant
FPAY Annual fee payment

Payment date: 19930319

Year of fee payment: 9

LAPS Lapse due to unpaid annual fee