KR20090009727U - A lining tape used for gypsum board joint - Google Patents

A lining tape used for gypsum board joint

Info

Publication number
KR20090009727U
KR20090009727U KR2020080003794U KR20080003794U KR20090009727U KR 20090009727 U KR20090009727 U KR 20090009727U KR 2020080003794 U KR2020080003794 U KR 2020080003794U KR 20080003794 U KR20080003794 U KR 20080003794U KR 20090009727 U KR20090009727 U KR 20090009727U
Authority
KR
South Korea
Prior art keywords
gypsum board
medium
super
super medium
tape
Prior art date
Application number
KR2020080003794U
Other languages
Korean (ko)
Inventor
이정기
김명옥
Original Assignee
이정기
김명옥
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이정기, 김명옥 filed Critical 이정기
Priority to KR2020080003794U priority Critical patent/KR20090009727U/en
Publication of KR20090009727U publication Critical patent/KR20090009727U/en

Abstract

본 고안은 석고보드 이음매용 초배지 테이프에 관한 것으로, 특히 3겹으로 제조되어 석고보드 이음매 및 흠집을 보완하고 수축 및 이완에 의한 이음매 파단을 방지할 수 있는 초배지 테이프에 관한 것이다. 본 고안에서는 (a) 120㎜내외의 폭으로 제조된 바깥쪽 제1초배지; (b) 60㎜ 내외의 폭으로 제조된 중간 제2초배지; 및 (c) 90㎜ 내외의 폭으로 제조된 안쪽 제3초배지로 구성되며, 초배지 사이에 비접착 공간부가 형성되도록 접착되어 제조된다. 또한, 각 초배지의 가장자리 두께를 중앙부의 두께보다 얇게 제조함으로써 이들 상부에 마감지 도배시 가장자리 라인이 드러나지 않도록 하고, 접착제를 도포하여 롤 형태로 공급함으로써 시공을 편리하게 하는 효과가 있다.The present invention relates to a super medium tape for gypsum board joints, and more particularly, to a super medium tape that can be manufactured in three layers to compensate for gypsum board joints and scratches and to prevent joint breakage due to shrinkage and relaxation. In the present invention (a) the outer first super medium manufactured to a width of about 120mm; (b) an intermediate second super medium prepared in a width of about 60 mm; And (c) an inner third super medium prepared in a width of about 90 mm, and is bonded and manufactured to form a non-bonded space between the super mediums. In addition, by making the edge thickness of each super medium thinner than the thickness of the center portion, the edge line is not exposed when the finish paper is applied to the upper portion thereof, and an adhesive is applied to supply the roll in the form of a roll to facilitate the construction.

Description

석고보드 이음매용 초배지 테이프 {A lining tape used for gypsum board joint}Super medium tape for gypsum board seam {A lining tape used for gypsum board joint}

본 고안은 건축 내장용 석고보드 이음매에 사용되는 초배지 테이프에 관한 것으로, 특히 석고보드 이음매에 접착하여 이음매 부분의 표면을 매끄럽게 하고, 석고보드의 수축 및 이완에 의한 이음매의 파단을 방지할 수 있는 석고보드 이음매용 초배지 테이프에 관한 것이다.The present invention relates to a super-badge tape used for gypsum board joints for building interiors, in particular, it is adhered to gypsum board joints to smooth the surface of the joints, and prevents the breakage of the joints due to shrinkage and relaxation of the gypsum board. It is related with the board | substrate super medium tape.

건축물 내부 벽체 및 천장마감재로 방음 및 방열을 위하여 불연성 소재인 석고보드를 가장 일반적으로 사용하고 있는 실정이다. 상기 석고보드를 고정함에 있어서, 못 또는 나사못으로 가장자리를 고정하기 때문에 함몰되거나 볼록하게 되어 표면이 울퉁불퉁하게 되고, 매끄럽지 못한 시멘트 벽면으로 인하여 이웃하는 석고보드와의 높이차가 발생하게 된다. 또한, 이렇게 울퉁불퉁한 표면 상부에 마감지를 곧바로 시공하게 되면 표면이 매끄럽지 못하고, 석고보드 경계면이 드러나게 되어 미관상 좋지 않게 된다. 또한, 석고보드 이음매를 충분하게 보완하지 않으면 마감지가 이음매 부분으로 함몰되는 불량이 발생되고, 심할 경우에는 재시공을 필요로 하여 경제적, 시간적 손실을 입게 된다.As a wall and ceiling finishing material inside buildings, gypsum board, which is a non-combustible material, is most commonly used for sound insulation and heat dissipation. In fixing the gypsum board, it is recessed or convex because the edges are fixed by nails or screws, and the surface becomes rugged, and a height difference with neighboring gypsum boards occurs due to the uneven cement wall surface. In addition, if the finishing paper is immediately installed on the uneven surface, the surface is not smooth, and the gypsum board boundary surface is exposed, resulting in poor aesthetics. In addition, if the gypsum board joints are not sufficiently complemented, defects in which the finishing paper is recessed into the joint parts may occur, and in severe cases, reconstruction may be required, resulting in economic and time loss.

상기와 같은 시공불량을 보완하기 위하여, 흠집 및 이음매 상부에 석고보드 이음매용 초배지 테이프를 필수적으로 시공하고 있다. 국내특허 공개번호 제0001741호, 국내실용 공고번호 제0209313호 및 국내실용 등록번호 제0321861호에는 석고보드 이음매에 사용하는 홑겹 초배지와 접착제가 도포된 홑겹 초배지가 공지되어있다. 그러나 상기 석고보드 이음부 틈새용 초배지는 홑겹으로 제작되어 강도가 약하여 시공시 주의를 필요로 하며, 시공 후에도 마감지를 접착시키는 압력 또는 석고보드의 수축 및 이완에 의해 쉽게 찢어지는 문제점이 발생한다. In order to compensate for such a poor construction, it is necessary to construct a super medium tape for gypsum board joints on the scratches and joints. Korean Patent Publication No. 0001741, Domestic Application Publication No. 0203313 and Domestic Application Registration No. 0321861 are known as single layered media used for gypsum board seams and single layered media coated with adhesive. However, the super medium for the gap between the gypsum board joints is made of a single layer, so the strength is weak and requires attention during construction, and there is a problem of easy tearing due to the pressure or the contraction and relaxation of the gypsum board after the construction.

국내특허 등록번호 제0398626호에 공지된 이음매용 초배지는 상기 홑겹 이음매용 초배지의 인장 및 파단 강도를 높이기 위하여 제1웨브(안쪽 초배지)와 이보다 폭이 더 넓은 제2웨브(바깥쪽 초배지)를 접착하여 2겹으로 제조하였다. 또한, 상기 시공된 이음매용 초배지 상부에 실크벽지 및 합지벽지 등과 같은 고급 마감지를 도배하는 경우 이음매용 초배지의 가장자리 라인이 드러나지 않도록 하기 위하여 가장자리 부분을 샌드페이퍼 등을 이용하여 완만하도록 제작하였다. 그러나 상기 이음매용 초배지는 바깥쪽 초배지에 안쪽 초배지의 전면이 접착되어 있어, 석고보드의 수축 및 이완에 의해 동시에 파단될 수 있으며, 석고보드 표면의 흠집을 보완할 수 없다는 단점이 있다.A joint super medium known in Korean Patent Registration No. 0398626 bonds a first web (inner super medium) and a wider second web (outer super medium) to increase the tensile and breaking strength of the single-ply super medium. It was prepared in two layers. In addition, when the high-quality finishing paper such as silk wallpaper and laminated wallpaper on the construction of the joint super medium, the edge portion of the joint super medium is made to be gentle using sandpaper to prevent the edge line from being exposed. However, the seam super badge is attached to the outer super medium to the front of the inner super medium, can be broken at the same time by shrinkage and relaxation of the gypsum board, there is a disadvantage that can not compensate for scratches on the surface of the gypsum board.

또한, 국내실용신안 등록번호 제0283081호에는 석고보드 이음매용 4겹 또는 5겹으로 제조되는 석고보드 이음매용 초배지가 공지되어있다. 그러나 상기 이음매용 초배지는 두꺼워서 이들 상부에 마감지를 도배하게 되면 이음매 부분이 돌출될 우려가 있다. 또한, 바깥쪽 제1초배지에 비해 점차 폭이 좁아지는 제2, 3, 4초배지를 사용함으로써 석고보드 이음매 접착되는 제4초배지의 폭이 매우 좁아지게 된다. 때문에 시공시 이음매의 틈새가 넓은 경우 이음매용 초배지의 안쪽 제4초배지가 이음매에 정확히 위치하도록 맞춰주지 않으면 이음매용 초배지의 높이차로 인한 시공 불량이 발생하는 단점이 있다.In addition, the domestic utility model registration No. 0283081 is known for the gypsum board seam super medium produced in four or five ply gypsum board seam. However, the jointed super medium is thick so that when the finish paper on the upper portion there is a fear that the joint portion protrudes. In addition, by using the second, third, fourth second medium that is gradually narrower than the outer first second medium, the width of the fourth second medium to be bonded to the gypsum board is very narrow. Therefore, when the gap of the joint is wide during construction, there is a disadvantage in that the construction failure due to the difference in the height of the joint medium for the seam if the inner 4 second medium of the seam medium for the seam is not exactly aligned to the seam.

본 고안에서는 종래 석고보드 이음매용 홑겹 초배지 및 2겹 초배지가 흠집 및 이음매를 충분히 보완하지 못하여 마감지 시공시 함몰되는 불량이 발생되는 문제점을 개선하고자 한다. 또한, 본 고안에서는 가장자리 두께가 중앙부 두께보다 얇은 초배지를 사용함으로써 고급 마감지 시공시에도 샌드페이퍼 공정을 생략할 수 있으며, 접착제를 도포하여 롤 형태로 제공함으로써 시공을 용이하여 공사 기간을 단축시키고자 한다.The present invention is to improve the problem that the conventional single gypsum board and two-ply super-badge for gypsum board joints do not sufficiently compensate for scratches and joints, so that a defect that is engulfed during construction of the finishing paper is generated. In addition, in the present invention, by using an ultra-thin media having a thickness smaller than the thickness of the center portion, the sandpaper process can be omitted even in the construction of high-quality finishing papers, and the construction period is shortened by facilitating the construction by providing an adhesive in roll form. .

상기와 같은 목적을 달성하기 위해 본 고안에서는,In the present invention to achieve the above object,

(a) 120㎜내외의 폭으로 제조된 바깥쪽 제1초배지; (b) 60㎜ 내외의 폭으로 제조된 중간 제2초배지; 및 (c) 90㎜ 내외의 폭으로 제조된 안쪽 제3초배지로 구성되며, 초배지 사이에 비접착 공간이 형성되도록 접착하여 석고보드 흡집 및 이음매를 보완하고 석고보드 수축 및 이완에 의해 찢어지지 않는 석고보드 이음매용 초배지 테이프가 제공된다. 또한, 가장자리 두께가 중앙부 두께보다 얇은 초배지를 사용함으로써 이들 상부에 고급 마감지 시공시 샌드페이퍼 공정을 생략하여도 초배지 가장자리 라인이 드러나지 않는 석고보드 이음매용 초배지 테이프가 제공된다.(a) an outer first sheath medium produced with a width of about 120 mm; (b) an intermediate second super medium prepared in a width of about 60 mm; And (c) an inner third super medium prepared in a width of about 90 mm, and bonded to form a non-adhesive space between the super mediums to compensate for gypsum board absorption and seam, and not torn by gypsum board shrinkage and relaxation. Super medium tape for board joints is provided. In addition, the use of ultra-thin media having an edge thickness thinner than the thickness of the center portion provides a gypsum board joint super-bad tape that does not reveal the edges of the super-paper media even if the sandpaper process is omitted during the construction of high-quality finishing papers.

본 고안에 의해 제조된 석고보드 이음매용 초배지 테이프는, 3겹으로 제조되어 석고보드 흠집 및 이음매를 보완할 수 있으며, 인장 강도 및 파단 강도가 우수하여 석고보드 수축 및 이완에 의해 쉽게 찢어지지 않으면서도 미관상 우수한 마감지 표면을 얻을 수 있게 된다.The gypsum board joint super medium tape manufactured by the present invention is manufactured in three layers to compensate for gypsum board scratches and joints, and is excellent in tensile strength and breaking strength without being easily torn by gypsum board shrinkage and relaxation. Aesthetically superior finish paper surfaces can be obtained.

또한, 석고보드 이음매에 접착되는 가장 폭이 좁은 제2초배지가 제1초배지와 제3초배지 사이에 위치하도록 하고, 두 번째로 폭이 넓은 제3초배지가 석고보드 이음매에 접착되도록 하여 넓은 이음매 틈새에 접착할 때도 용이하게 접착할 수 있으며, 가장자리 두께가 중앙부 두께보다 얇은 초배지를 사용하여 고급 마감지 시공시 샌드페이퍼 공정을 생략할 수 있어 공사 기간을 단축시키는 효과가 있다.In addition, the second narrowest medium that is bonded to the gypsum board seam is positioned between the first and third second medium, and the second widest third medium is adhered to the gypsum board seam so that the widest gap It can be easily bonded when bonding, and it is possible to omit the sandpaper process when constructing a high-quality finishing paper by using super medium with thinner edges than the thickness of the center part, thereby shortening the construction period.

도 1은 본 고안에 의해 접착제가 도포부(50)가 형성된 롤 형태의 석고보드 이음매용 초배지 테이프(100). Figure 1 is a gypsum board seam super badge tape 100 in the form of a roll is formed by the adhesive coating portion 50 by the present invention.

도 2는 본 고안에 의한 석고보드 이음매용 초배지 테이프(100)의 분해 사시도.Figure 2 is an exploded perspective view of the gypsum board joint super medium tape 100 according to the present invention.

도 3은 본 고안에 의한 석고보드 이음매용 초배지 테이프(100)의 결합된 상태를 확대 도시한 종단면도.Figure 3 is an enlarged longitudinal cross-sectional view showing a combined state of the gypsum board joint super medium tape 100 according to the present invention.

도 4는 본 고안에 의한 석고보드 이음매용 초배지 테이프(100)를 석고보드(200) 이음매에 시공된 상태도.Figure 4 is a state in which the gypsum board seam super medium tape 100 according to the present invention constructed on the gypsum board 200 seam.

<도면의 주요부분에 대한 부호의 설명><Description of the symbols for the main parts of the drawings>

10: 제1초배지10: first candle medium

20: 제2초배지20: second candle badge

30: 제3초배지30: Third Candle Badge

40: 비접착 공간부40: non-stick space

50: 접착제 도포부50: adhesive coating

100: 석고보드 이음매용 초배지 테이프100: Gypsum board joint super medium tape

200: 석고보드200: gypsum board

300: 석고보드 이음매300: gypsum board seam

본 고안에서는, In this invention,

상기 목적을 달성하기 위하여 도2에 도시된 바와 같이 폭 90㎜ 내외의 제3초배지(30) 상부 중앙부에 60㎜ 내외의 제2초배지(20)를 위치시키고, 상기 2겹 초배지를 120㎜ 내외의 제1초배지(10) 중앙부에 제2초배지(20)가 안쪽에 위치하도록 한다. 또한, 도 3에 도시된 바와 같이 상기 제1초배지(20) 가장자리부터 제3초배지(30)의 가장자리 2㎜ 내외가 포함되는 폭으로 접착제를 도포하여 접착제 도포부(50)를 형성하여 롤 형태로 권취한다. 상기 본 고안에 의한 3중 초배지 테이프는 마감지를 시공할 때 강한 압력을 가하더라도 쉽게 찢어지지 않는 강도를 갖게 된다. In order to achieve the above object, as shown in FIG. 2, a second super medium 20 of about 60 mm is placed in the upper central portion of the third super medium 30 of about 90 mm in width, and the double ply medium of about 120 mm is placed. The second super medium 20 is located in the central portion of the first super medium 10. In addition, as shown in Figure 3 by applying an adhesive in a width including the inner and outer edges of the edge of the first second medium 20, the edge of the third second medium 30, 2mm to form an adhesive coating portion 50 to form a roll Wind up. Triple super medium tape according to the present invention has a strength that is not easily torn even when a strong pressure is applied when constructing the finishing paper.

본 고안에서는, 샌드페이퍼 공정을 생략할 수 있도록 제1초배지, 제2초배지 및 제3초배지는 가장자리의 두께가 중앙부 두께보다 얇은 초배지를 제작 사용하였기 때문에 곧바로 이들 상부에 고급 마감지를 도배하더라도 초배지 테이프의 가장자리 라인이 드러나지 않는다.In the present invention, the first, second, and third medium badges are used to make the sandpaper process so that the edge paper thickness is thinner than the center thickness. The line is not visible.

또한, 도 3에 도시된 바와 같이 접착제가 도포되지 않은 초배지 내부에 비접착 공간부(40)가 형성되도록 제조한다. 상기 제1초배지(10)와 제2초배지(20) 사이 및 제2초배지(20)와 제3초배지(30) 사이에 형성되는 비접착 공간부(40)는 천장 및 벽체에 시공된 석고보드(200) 표면이 울퉁불퉁하더라도 이를 보완하는 효과가 있어 상부에 시공되는 마감지 표면이 매끄럽게 된다. 도3에 도시된 본 고안에 의한 석고보드 이음매용 초배지 테이프(100)의 종단면에서 비접착 공간부(40)는 설명을 위하여 크게 도시된 것이며, 실제로는 공간부(40)의 두께는 매우 얇다.In addition, as shown in FIG. 3, the non-adhesive space portion 40 is formed inside the super medium to which the adhesive is not applied. The non-adhesive space 40 formed between the first and second second medium 10 and 20 and the second second medium 20 and 30 is a gypsum board installed on the ceiling and wall ( 200) Even if the surface is uneven, there is an effect of compensating for it so that the surface of the finishing paper constructed on the top is smooth. The non-adhesive space portion 40 in the longitudinal section of the gypsum board joint super medium tape 100 according to the present invention shown in FIG. 3 is shown for explanatory purposes, and in reality, the thickness of the space portion 40 is very thin.

상기 본 고안의 제조방법에 의해 제조된 석고보드 이음매용 초배지 테이프(100)의 제3초배지(30)가 접착되어 있는 측면의 가장자리에 접착제를 도포하여 도1에 도시된 바와 같이 롤 형태로 제공된다. 롤 형태로 제공된 초배지 테이프(100)는 도4에 도시된 바와 같이 제1초배지(10)가 바깥쪽이 되도록 석고보드 이음매(300)에 부착하여 시공한다. 또한, 틈새가 넓은 석고보드 이음매(300)에 시공하더라도 본 고안에 의한 초배지 테이프(100)는 석고보드 이음매(300)에 접착되는 제3초배지(30)의 폭이 넓어 용이하게 접착할 수 있어 빠르게 시공할 수 있다.The adhesive is applied to the edge of the side surface of the gypsum board joint super medium tape 100 manufactured by the manufacturing method of the present invention to which the third super medium 30 is bonded, and is provided in roll form as shown in FIG. 1. . The super badge tape 100 provided in roll form is attached to the gypsum board seam 300 so that the first super medium 10 is outward as shown in FIG. 4. In addition, even if the construction is wide gypsum board seam 300, the super medium tape 100 according to the present invention can be easily bonded because the width of the third super medium 30 is bonded to the gypsum board seam 300 is wide Can be installed.

상기 시공된 석고보드 이음매용 초배지 테이프(100)는 3중으로 제조되어 석고보드 표면의 흠집 및 이음매(300)가 드러나지 않도록 보완할 수 있으며, 충분한 강도를 갖고 있어 석고보드(200)의 수축 및 이완에 의해서 쉽게 찢어지지 않으며, 마감지가 함몰되는 불량이 발생하지 않으며, 고급 마감지 사용시에도 샌드페이퍼 공정을 생략할 수 있다.The constructed gypsum board joint super medium tape 100 may be manufactured in three layers to supplement the scratches and the seams 300 on the gypsum board surface, and have sufficient strength to shrink and relax the gypsum board 200. It is not easily torn by, the defect that the finishing paper is not generated, the sandpaper process can be omitted even when using a high-quality finish paper.

상기 본 고안은 동일한 기술분야에서 통상의 지식을 가진 자에 의해 본 고안의 기술사상과 아래에 기재될 실용신안등록청구범위의 균등범위 내에서 다양한 수정 및 변형이 가능한 것은 물론이다.The present invention is of course possible various modifications and variations within the equivalent range of the technical concept and the utility model registration claims to be described below by those skilled in the art.

Claims (3)

(a) 120㎜내외의 폭으로 제조된 바깥쪽 제1초배지(10);(a) an outer first super medium (10) made to a width of about 120 mm; (b) 60㎜ 내외의 폭으로 제조된 중간 제2초배지(20);(b) an intermediate second medium medium 20 having a width of about 60 mm; (c) 90㎜ 내외의 폭으로 제조된 안쪽 제3초배지(30)로 구성되며,(c) a third inner medium (30) made of a width of about 90mm, 초배지 사이에 비접착 공간(40)이 형성되도록 접착되는 것을 특징으로 하는 석고보드 이음매용 초배지 테이프(100).Non-adhesive space 40 between the super-badge, gypsum board seam super-badge tape 100, characterized in that bonded to form. 제1항에 있어서,The method of claim 1, 상기 제1초배지 내지 제3초배지 중 하나 이상의 초배지(10, 20, 30)는 양측 가장자리의 두께가 중앙측의 두께보다 얇은 것을 특징으로 하는 석고보드 이음매용 초배지 테이프(100).At least one of the first medium to the third medium medium (10, 20, 30) is the gypsum board joint super medium tape 100, characterized in that the thickness of both edges is thinner than the thickness of the center side. 제1항 또는 제2항의 상기 초배지 테이프에 접착제가 도포(50)되어 롤 형태로 제조되는 것을 특징으로 하는 석고보드 이음매용 초배지 테이프(100).Adhesive tape is applied to the super medium tape of claim 1 or claim 2 to produce a gypsum board seam super medium tape (100), characterized in that it is manufactured in a roll form.
KR2020080003794U 2008-03-24 2008-03-24 A lining tape used for gypsum board joint KR20090009727U (en)