KR102517737B1 - Lining paper for joint of plaster board and its manufacturing method - Google Patents

Lining paper for joint of plaster board and its manufacturing method Download PDF

Info

Publication number
KR102517737B1
KR102517737B1 KR1020220103992A KR20220103992A KR102517737B1 KR 102517737 B1 KR102517737 B1 KR 102517737B1 KR 1020220103992 A KR1020220103992 A KR 1020220103992A KR 20220103992 A KR20220103992 A KR 20220103992A KR 102517737 B1 KR102517737 B1 KR 102517737B1
Authority
KR
South Korea
Prior art keywords
paper
reinforcing net
inclined surface
oil
super medium
Prior art date
Application number
KR1020220103992A
Other languages
Korean (ko)
Inventor
김의경
Original Assignee
김의경
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김의경 filed Critical 김의경
Priority to KR1020220103992A priority Critical patent/KR102517737B1/en
Application granted granted Critical
Publication of KR102517737B1 publication Critical patent/KR102517737B1/en

Abstract

The present invention relates to lining paper which is attached to joints of a gypsum board or a cement wall before wallpapering, and lining paper for gypsum board joints which prevents sagging and sinking due to changes in temperature and humidity, and tearing and deformation due to shrinkage and relaxation and a manufacturing method thereof. According to the present invention, an adhesive portion is formed by applying an oil-soluble adhesive to the center of one side of the lining paper having a certain width and length. In addition, a reinforcing net woven with a synthetic resin yarn is placed on an upper side of the oil-soluble adhesive applied to the center of the lining paper to be fixed. The lining paper exposed to a side of the reinforcing net forms an inclined surface whose thickness becomes thinner toward the outside. After wetting an upper side of the reinforcing net with water, inner paper used as a non-adhesive part is attached, and wallpaper paste is applied to the inclined surface of the lining paper. Moreover, the inclined surface is attached to a gypsum board, wherein inner paper covers joints of the gypsum board. Accordingly, high quality wallpapering can be provided.

Description

석고보드 이음새용 초배지 및 그 제조방법{Lining paper for joint of plaster board and its manufacturing method}Super medium for gypsum board joints and its manufacturing method {Lining paper for joint of plaster board and its manufacturing method}

본 발명은 도배를 하기 전에 석고보드 또는 시멘트 벽면의 이음새에 부착되는 초배지에 관한 것으로, 초배지가 온,습도의 변화에 의한 쳐짐과 함몰현상을 방지하는 한편 수축, 이완에 따른 찢김이나 변형을 방지하는 석고보드 이음새용 초배지 및 그 제조방법에 관한 것이다.The present invention relates to a paperboard attached to a joint of a gypsum board or cement wall before papering, which prevents the paperboard from sagging and sinking due to changes in temperature and humidity, while preventing tearing or deformation due to shrinkage and relaxation It relates to a super medium for gypsum board joints and a manufacturing method thereof.

실내의 천정이나 벽면의 마감을 위하여 도배를 할 때 도 1에 도시된 바와 같이 석고보드(1)(2)나 시멘트 벽면에 그대로 도배지(5)를 바르게 되면, 석고보드(1)(2)의 이음새 부분이나 시멘트의 울퉁불퉁한 부분이 도배지(5)에 그대로 노출되는 문제와 함께 도배지(5)가 석고보드(1)(2)의 이음새 부분에서 함몰되는 현상이 발생하기 때문에 이를 방지하기 위하여 도 2에 도시된 바와 같이 도배를 하기 전에 석고보드(1)(2)의 이음새 부분이나 높낮이가 차이가 발생하는 부분은 초배지(3)를 바른 다음 도배지(5)를 바르고 있으나, 이 경우에도 온,습도의 심한 변환에 따라 석고보드(1)(2)의 이음새 부분에 붙여진 초배지(3)가 습기를 많이 머금게 되고, 이로 인하여 석고보드(1)(2)의 이음새 부분이 늘어나 쳐지거나 함몰되는 현상이 발생하기 때문에 초배지(3)에 발라진 도배지(5)도 쳐지거나 함몰되는 문제가 발생하게 된다.When wallpapering is applied to finish the ceiling or wall of an indoor room, as shown in FIG. In addition to the problem that the seam or the uneven part of the cement is exposed to the paper 5 as it is, the paper 5 is depressed at the seam of the gypsum board (1) (2), so to prevent this, Fig. 2 As shown in, the joints of the gypsum boards (1) and (2) or the parts where the height is different before the papering is applied with the paper (3) and then the paper (5), but even in this case, the temperature and humidity According to the severe transformation of the gypsum board (1) (2), the supernatant (3) attached to the seam part contains a lot of moisture, which causes the seam part of the gypsum board (1) (2) to stretch or sink. Because of this, a problem arises in that the paper (5) applied to the second medium (3) is also sagging or sunken.

이러한 문제를 해결하기 위하여 실용신안 등록 20-0321861호에는 도 3에 도시된 바와 같이 초배지(3)의 한쪽으로 접착제(4a)를 도포한 다음 초배지(3)의 양쪽으로 접착제(4a)가 일부 노출되게 초배지(3)의 중앙으로 보강지(4)를 접착시킴으로써, 초배지(3)를 바를 때 석고보드(1)(2)의 이음새 부분에 보강지(4)를 위치시켜 온,습도의 변화가 발생할 때 보강지(4)로 인하여 쳐지거나 찢어지는 문제를 해결하고 있으나, 기본적으로 초배지(3)가 쳐지고 찢어지거나 틀어지게 되는 문제는 초배지(3)가 종이 성분이라서 접착제를 도포할 때 습기를 너무 많이 흡수하기 때문에 발생되는 현상으로, 보강지(4)도 종이로 이루어져 있기 때문에 보강지(4)도 과도한 습기를 머금을 수밖에 없는 것이어서, 초배지(3)의 일측면에 보강지(4)를 부착하더라도 초배지(3)나 도배지(5)의 건조 과정에서 석고보드(1)(2)의 이음새 부분에서 쳐지거나, 터지고, 틀어지는 문제가 발생할 수밖에 없다.In order to solve this problem, in Utility Model Registration No. 20-0321861, as shown in FIG. 3, the adhesive 4a is applied to one side of the super medium (3), and then the adhesive (4a) is partially exposed on both sides of the super medium (3). By adhering the reinforcing paper (4) to the center of the superbattery (3) so that the reinforcing paper (4) is placed at the seam of the gypsum board (1) (2) when applying the superbattery (3), the change in humidity When it occurs, we are solving the problem of sagging or tearing due to the reinforcing paper (4), but basically, the problem that the first paper (3) is sagging, torn or twisted is that the second paper (3) is a paper component, so it absorbs moisture when applying the adhesive. This is a phenomenon that occurs because it absorbs too much. Since the reinforcing paper 4 is also made of paper, the reinforcing paper 4 has no choice but to contain excessive moisture, so the reinforcing paper 4 is placed on one side of the paper background 3. Even if it is attached, problems such as sagging, bursting, or twisting at the seams of the gypsum boards (1) (2) in the drying process of the paper (3) or the paper (5) inevitably occur.

그리고, 초배지의 상측으로 도배지를 바르기 때문에 초배지의 선단에서 초배지와 도배지가 겹치는 부위에서 도배지가 외측으로 돌출되는 편차가 발생하여 미관을 해치는 문제가 있고, 이러한 문제는 초배지의 외측 선단을 샌드페이퍼 등으로 갈아주어 해결할 수 있으나, 초배지를 붙이는 작업 후 경사면을 이루게 갈아주기 때문에 작업시간이 오래 걸리는 한편 도배 현장에서의 작업이 사실상 어려운 단점이 있다.In addition, since the paper is applied to the upper side of the paper, there is a problem in that the paper is protruded outward at the tip of the paper and the paper is overlapped with the paper, thereby damaging the aesthetics. It can be solved by giving it, but it takes a long time to work because it is ground to form a slope after the work of attaching the paper, while the work on the papering site is virtually difficult.

이러한, 문제를 해결하기 위하여 등록특허 10-1656688호에는 도 4에 도시된 바와 같이 초배지(3)의 중앙에 일정 폭의 코팅부(3a)를 형성하여 습기는 적게 머금으면서 접착이 이루어지지 않는 비접착 부분을 형성함으로써, 도 5에 도시된 바와 같이 초배지(3)를 바를 때 코팅부(3a)의 양쪽으로 접착제를 도포한 후 코팅부(3a)가 석고보드(1)(2)의 이음새 부분을 가려주는 형태로 붙이게 되면, 초배지(3)와 석고보드(1)(2) 사이에 코팅부(3a)로 비접착이 이루어지면서 습기를 머금지 않는 부분인 공간을 만들기 때문에 석고보드(1)(2)의 이음새가 도배지(5)의 외측에서 보이지 않게 하는 한편 코팅부(3a)에서 코팅액의 도포로 인하여 습기를 적게 머금기 때문에 초배지(3)의 쳐짐이 적게 발생하면서도 습도의 변화에 따른 일정한 탄력성을 유지하여 초배지(3) 및 도배지(5)의 늘어짐과 터짐 및 변형을 방지하고 있다.In order to solve this problem, in Registration Patent No. 10-1656688, as shown in Figure 4, a coating portion (3a) of a certain width is formed in the center of the chobaeji (3) to prevent adhesion while holding less moisture. By forming the adhesive portion, as shown in FIG. 5, when the super medium (3) is applied, the adhesive is applied to both sides of the coating portion (3a), and then the coating portion (3a) is the seam portion of the gypsum board (1) (2). When attached in the form of covering the gypsum board (1) because it creates a space that does not contain moisture while non-adhesion is made with the coating part (3a) between the super paper (3) and the gypsum board (1) (2). Since the seam of (2) is not visible from the outside of the paper (5), and the coating part (3a) retains less moisture due to the application of the coating liquid, the sagging of the paper (3) occurs less, while maintaining a constant level according to the change in humidity By maintaining elasticity, sagging, bursting, and deformation of the super medium (3) and the coated medium (5) are prevented.

상기 초배지(3)의 일측면에 코팅부(3a)를 형성하는 코팅액은 아크릴 수지(Acrylic resin)를 포함하기 때문에 습기를 머금지 않게 되고, 이로 인하여 초배지(3)를 바를 때 코팅부(3a)로 비접착 부분을 확보하면서 석고보드(1)(2)의 이완과 수축에 따라 초배지(3)의 찢김이나 변형이 발생하는 것을 방지하는 한편 비접착 부분으로 인하여 초배지(3)와 도배지(5)의 단차가 보이지 않도록 하고 있다.Since the coating liquid forming the coating part (3a) on one side of the super medium (3) contains an acrylic resin, it does not retain moisture, and therefore, when the super medium (3) is applied, the coating part (3a) While securing the non-adhesive part, preventing tearing or deformation of the paper (3) due to the relaxation and contraction of the gypsum board (1) (2), while the non-adhesive part prevents the paper (3) and paper (5) The step difference is not visible.

그러나, 초배지(3)의 중앙에 아크릴 수지를 주재로 하는 코팅부(3a)의 비접착 부분을 형성하는 방식은 코팅부(3a)를 형성하는 코팅액이 아크릴 수비를 포함한다 하더라도 코팅부(3a)가 형성된 부위에서 습기를 머금을 수밖에 없고, 이로 인하여 습도가 높은 계절에는 쳐짐이 발생하게 되고, 코팅부(3a)에서 비접착이 이루어짐에도 불구하고 습기에 의한 쳐짐을 방지할 정도로 힘을 받쳐주지 못하게 되고, 이로 인하여 도배지(5)의 쳐짐이 발생하거나, 초배지(3)와 도배지(5)의 겹치는 부위에서 단차가 발생할 수밖에 없는 문제를 해결하지 못하고 있다.However, the method of forming the non-adhesive portion of the coating portion (3a) mainly made of acrylic resin in the center of the super medium (3), even if the coating liquid forming the coating portion (3a) contains acrylic water, the coating portion (3a) Inevitably, moisture is contained in the formed area, and due to this, sagging occurs in the season with high humidity, and even though non-adhesion is made in the coating part 3a, it is impossible to support the force enough to prevent sagging due to moisture. As a result, it is not possible to solve the problem of sagging of the paper (5) or a step in the overlapping area of the paper (3) and the paper (5).

특히, 코팅부(3a)를 이루는 코팅액의 도포에도 불구하고 습기를 머금을 수밖에 없음은 물론 코팅부(3a)에서 쳐짐을 방지할 정도의 힘을 주지 못하게 되고, 이로 인하여 습기가 많을 때 도배지(5)의 늘어짐에 의한 하중을 완벽히 잡아주지 못하여 쳐짐이나 변형이 발생하는 문제를 완전히 해결하지 못함은 물론 건조가 이루어지는 경우에도 도배지(5)가 당겨지면서 틀어지거나 찢어지게 되는 경우가 발생하게 된다.In particular, despite the application of the coating liquid constituting the coating portion (3a), it is inevitable to retain moisture, as well as to prevent the coating portion (3a) from sagging. ), it does not completely solve the problem of sagging or deformation due to the sagging of the load, and even when drying occurs, the paper 5 is pulled and twisted or torn.

실용신안 등록 20-0321861호(2003.07.22 등록)Utility model registration No. 20-0321861 (registered on July 22, 2003) 특허등록 10-1656688호(2016.09.06 등록)Patent Registration No. 10-1656688 (registered on September 6, 2016) 실용신안 등록 20-2009-0009727호(2009.09.29 등록)Utility model registration No. 20-2009-0009727 (registered on September 29, 2009) 특허등록 10-1516932호(2015.04.25 등록)Patent Registration No. 10-1516932 (registered on 2015.04.25)

본 발명은 초배지의 중앙으로 아크릴 수지를 포함하는 코팅액으로 코팅부를 형성하되 코팅부를 비접착 부위로 사용하여 초배지를 석고보드의 이음새 부분에 부착함으로써 도배지가 온,습도의 변화에 따른 이완과 수축으로 인한 문제와 쳐짐이나 찢어짐이 발생하는 문제를 해결함에 있어서, 아크릴 수지를 주재로 하여 형성되는 코팅부에서 습기를 머금을 수밖에 없는 한편 코팅부의 강도가 낮아서 습기를 머금을 때 쉽게 쳐지는 현상이 발생하는 문제와 함께 초배지의 양쪽 선단에 단차가 존재하기 때문에 도배지에서 단차가 나타나는 문제를 해결하기 위한 것으로, 초배지의 중앙 부위에 습기를 머금지 않는 지용성 접착제로 강도를 보강하는 폴리프로필렌의 보강망을 접착시킨 후 초배지의 측면을 갈아서 경사면을 형성함으로써 석고보드의 이음새 부분에서 쳐짐이나 찢어짐이 발생하지 않도록 하는 한편 초배지 위에 도배지를 바를 때 단차가 나타나지 않도록 하는 것이다.The present invention forms a coating part with a coating solution containing acrylic resin in the center of the paper medium, but uses the coating part as a non-adhesive part to attach the paper medium to the seam of the gypsum board, resulting in relaxation and contraction of the paper medium due to changes in temperature and humidity. In solving the problem and the problem of sagging or tearing, the coating part formed mainly of acrylic resin has no choice but to contain moisture, while the strength of the coating part is low, so it easily sag when it contains moisture. This is to solve the problem of the level difference in the paper because there is a level difference at both ends of the first paper, and after bonding a polypropylene reinforcing net that reinforces the strength with an oil-soluble adhesive that does not hold moisture in the center of the second paper By grinding the side of the paper to form an inclined surface, sagging or tearing does not occur at the seam of the gypsum board, while a step does not appear when the paper is applied on the paper.

본 발명은 일정 폭과 길이를 갖는 초배지의 일측면 중앙에 지용성 접착제를 도포하여 접착부를 형성하고, 상기 초배지의 중앙에 발라진 지용성 접착제의 상측에 합성수지사로 직조되는 보강망을 배치하여 고정되게 하고, 상기 보강망의 측면으로 노출되는 초배지는 외측으로 갈수록 두께가 얇아지게 경사면을 형성함으로써 이루어진다.The present invention forms an adhesive by applying an oil-soluble adhesive to the center of one side of a chobae having a certain width and length, and placing a reinforcing net woven with synthetic resin yarn on the upper side of the oil-soluble adhesive applied to the center of the chobae to be fixed, The super medium exposed to the side of the reinforcing net is made by forming an inclined surface so that the thickness becomes thinner toward the outside.

본 발명은 초배지의 일측면에 초배지의 폭보다 적은 보강망을 물과 섞이지 않아 습기를 머금지 않는 지용성 접착제로 고정시키되 상기 보강망은 합성수지사로 이루어져 습기를 머금지 않음은 물론 높은 강도를 갖도록 하고, 상기 보강망은 직경 0.02~0.05mm의 굵기를 갖는 폴리프로필렌, 폴리에틸렌 등의 합성수지 재질로 이루어지고, 망목의 직경은 5-10mm의 길이를 갖게 형성되며, 망목은 일정한 형태로 이루어지지 않고, 인접된 망목의 크기가 서로 다른 자유로운 형태로 이루어진다.In the present invention, a reinforcing network smaller than the width of the chobae is fixed with an oil-soluble adhesive that does not mix with water and does not contain moisture, but the reinforcing network is made of synthetic resin yarn and does not contain moisture, as well as having high strength, The reinforcing net is made of a synthetic resin material such as polypropylene or polyethylene having a thickness of 0.02 to 0.05 mm in diameter, and the diameter of the mesh is formed to have a length of 5 to 10 mm. The size of the mesh is made in a free form with different sizes.

본 발명은 양쪽으로 경사면이 형성되고, 일측면에 지용성 접착제로 보강망을 부착시킨 초배지를 사용할 때 보강망의 상측에 물을 적신 후 비접착 부위로 사용되는 속지를 부착하고, 상기 초배지의 경사면에는 도배용 풀이 도포되게 한 후 경사면을 석고보드에 부착시키되 속지가 석고보드의 이음새를 덮어주는 형태로 부착되게 한다.In the present invention, when using a paper medium in which inclined surfaces are formed on both sides and a reinforcing net attached to one side with an oil-soluble adhesive, water is moistened on the upper side of the reinforcing net and then an inlay used as a non-adhesive portion is attached, and on the inclined surface of the second medium After applying the glue for wallpapering, attach the inclined surface to the gypsum board so that the inlay is attached in such a way as to cover the seams of the gypsum board.

삭제delete

본 발명은 일정 폭과 길이를 갖는 초배지의 일측면 중앙 부위에 지용성 접착제를 도포하여 접착부를 형성하는 과정을 수행하고, 상기 초배지의 중앙 부위에 발라진 지용성 접착제의 상측에 합성수지사로 직조되는 보강망을 배치하여 접착시키는 과정을 수행하고, 상기 보강망의 측면으로 노출되는 초배지는 외측으로 갈수록 두께가 얇아지게 경사면을 형성하는 과정을 수행하고, 상기 초배지는 일정 길이 단위로 말아주는 과정을 수행하여 제조하고, In the present invention, a process of forming an adhesive portion by applying an oil-soluble adhesive to the central portion of one side of a chobat having a certain width and length, and placing a reinforcing net woven with synthetic resin yarn on the upper side of the oil-soluble adhesive applied to the central portion of the chobaji and performing the bonding process, and the super medium exposed to the side of the reinforcing net performs the process of forming an inclined surface so that the thickness becomes thinner as it goes outward, and the super medium is prepared by performing a rolling process in units of a certain length,

제조된 초배지는 보강망의 상측에 물을 적신 후 속지를 부착하는 과정을 수행하고, 상기 초배지의 경사면에는 도배용 풀을 도포하는 과정을 수행하고, 상기 초배지를 석고보드의 이음새를 덮어주게 접착시키는 과정을 수행함으로써 초배지의 도포가 이루어지게 된다.The prepared paper medium is subjected to a process of soaking water on the upper side of the reinforcing net and then attaching the inlay, applying a paste for wallpapering to the inclined surface of the paper medium, and adhering the paper medium to cover the seams of the gypsum board By performing the process, the coating of the super medium is made.

삭제delete

본 발명은 초배지의 일측에 보강망이 지용성 접착제로 접착된 상태로 공장에서의 제조가 완료되어 롤 형태로 작업 현장에 공급되고, 작업 현장에서는 보강망의 상측에 물을 뿌리며 비접촉 부위를 형성하는 속지를 고정시키는 작업을 한 후 초배지의 양쪽으로 도배용 풀을 발라 초배지를 붙이게 되는 것으로, 초배지의 건조가 이루어진 후 초배지의 상측으로 도배지를 바르게 된다.In the present invention, manufacturing in a factory is completed with a reinforcing net attached to one side of the super medium with an oil-soluble adhesive, and supplied to the work site in the form of a roll, and at the work site, water is sprayed on the upper side of the reinforcing net to form a non-contact area. After the fixing work is done, glue for papering is applied to both sides of the paper and the paper is attached. After the paper is dried, the paper is applied to the top of the paper.

본 발명은 초배지의 중앙에서 석고보드의 이음새를 가리는 그물망 형태의 보강망을 물과 섞이지 않는 지용성 접착제로 고정시킴으로써 초배지가 습도를 머금어 쳐지게 되는 현상을 방지하는 한편 온,습도에 따라 이완되거나 늘어질 때 변형이나 찢어짐이 발생하지 않도록 하고, 또한, 초배지의 양쪽으로 두께가 얇아지게 경사면을 형성시킴으로써 초배지에 도배지를 바르더라도 겹치는 부위에서 단차가 나타나지 않도록 하여, 고품질의 도배를 제공할 수 있는 것이다.The present invention prevents the phenomenon that the paper is soaked in moisture by fixing the reinforcing net in the form of a mesh covering the joints of the gypsum board with a water-immiscible oil-soluble adhesive in the center of the paper, while relaxing or sagging depending on the temperature and humidity. It is possible to provide high-quality papering by preventing deformation or tearing from occurring, and by forming inclined surfaces with a thin thickness on both sides of the paper, so that no steps appear in the overlapping area even if the paper is applied to the paper.

특히, 본 발명은 초배지에 습기를 머금지 않고 높은 강도를 갖는 보강망을 일측에 부착시킴으로써 강도와 견고함을 보장하고, 늘어짐을 방지하는 한편 초배지에 형성된 경사면에 의해 도배지를 바를 때 단차가 나타나지 않는 것이다.In particular, the present invention guarantees strength and sturdiness by attaching a reinforcing net having high strength to one side without holding moisture in the paper, preventing sagging and preventing a step from appearing when the paper is applied by the inclined surface formed on the paper. will be.

삭제delete

본 발명은 석고보드의 이음새를 메꾸거나 흠집을 메꾼 후 페인트 작업을 할 때 퍼티 작업을 하지 않고, 본 발명의 초배지를 이용하여 이음새나 흠집을 막아준 후 페인트칠을 할 수 있으며, 이 경우도 초배지가 지용성 접착제를 사용하여 강도를 높이는 보강망을 접착시킴으로써, 페인트의 무게를 충분히 견디기 때문에 크랙이 발생하거나 쳐지는 것을 방지할 수 있다.In the present invention, when painting after filling in the seams or scratches of the gypsum board, it is possible to paint after sealing the seams or scratches using the paper of the present invention without putting putty, and in this case also By attaching a reinforcing net that increases strength using a fat-soluble adhesive, cracks or sagging can be prevented because it can sufficiently withstand the weight of the paint.

도 1은 초배지 없이 도배지를 바른 단면도
도 2는 초배지로 석고보드 이음새를 바른 후 도배지를 바른 단면도
도 3은 보강지를 사용하는 기존 초배지의 사용상태 단면도
도 4는 코팅부가 형성된 기존 초배지의 사시도
도 5는 코팅부가 형성된 기존 초배지의 사용상태 단면도
도 6은 본 발명의 보강망 사시도
도 7은 본 발명의 초배지에 지용성 접착제를 도포한 상태의 사시도
도 8은 본 발명의 초배지에 보강망을 지용성 접착제로 고정시킨 상태의 사시도
도 9는 본 발명의 초배지 측면에 경사면을 형성한 상태의 사시도
도 10은 본 발명의 초배지 단면도
도 11은 본 발명의 초배지 사용상태를 위한 설명도
도 12는 본 발명 초배지의 사시도
도 13은 본 발명의 초배지 실시예 사용상태 단면도
도 14는 본 발명의 보강망 실시예 사진
1 is a cross-sectional view of applying the paper without the second paper
Figure 2 is a cross-sectional view of applying the paper after applying the gypsum board seam with the first paper
Figure 3 is a cross-sectional view of the state of use of the existing super medium using reinforced paper
Figure 4 is a perspective view of the existing super medium formed with a coating portion
Figure 5 is a cross-sectional view of the state of use of the existing super medium with a coating portion formed
6 is a perspective view of the reinforcing net of the present invention
Figure 7 is a perspective view of a state in which the fat-soluble adhesive is applied to the super medium of the present invention
Figure 8 is a perspective view of a state in which the reinforcing net is fixed to the paper medium of the present invention with an oil-soluble adhesive
Figure 9 is a perspective view of a state in which an inclined surface is formed on the side of the super medium of the present invention
10 is a cross-sectional view of the super medium of the present invention
11 is an explanatory diagram for the state of using super medium of the present invention
12 is a perspective view of the super medium of the present invention
Figure 13 is a cross-sectional view of the use state of the super medium embodiment of the present invention
14 is a photograph of an embodiment of the reinforcing network of the present invention

본 발명은 석고보드의 이음새를 막아주는 초배지에 관한 것으로, 초배지의 중앙에 강도 보강을 위하여 합성수지사로 직조되고 그물망 형태를 갖는 보강망을 습기를 머금지 않게 지용성 접착제로 고정하고, 상기 보강망이 고정된 초배지의 양쪽에는 외측으로 갈수록 두께가 얇아지게 경사면을 형성한 후 경사면에 도배용 풀을 발라주는 것이다.The present invention relates to a paper sheet that prevents the seam of a gypsum board, in which a reinforcing net woven with synthetic resin yarn and having a mesh shape is fixed with an oil-soluble adhesive so as not to retain moisture in the center of the paper sheet to reinforce strength, and the reinforcing net is fixed. On both sides of the first paper, a slope is formed so that the thickness becomes thinner toward the outside, and then glue for wallpapering is applied to the slope.

본 발명은 보강망이 석고보드 이음새를 가리는 형태로 초배지를 붙이는 것으로, 초배지를 붙일 때 물을 뿌려서 속지가 보강망을 덮어주게 고정시키는 동시에 초배지의 경사면에 도배용 풀을 발라 초배지를 접착시킴으로써, 속지가 비접촉 부위를 형성하여 석고보드에서 분리된 상태로 고정되는 한편 지용성 접착제의 사용으로 초배지가 습기를 머금는 것을 줄이며, 또한, 강도 보강용 보강망의 사용으로 초배지가 늘어지고 쳐지는 현상을 방지하는 것이다.The present invention is to attach the paper badge in the form of a reinforcing net covering the gypsum board seam, and when attaching the paper badge, water is sprayed to fix the inlay to cover the reinforcing net, and at the same time, by applying glue for papering to the slope of the paper badge to adhere the paper badge, Forms a non-contact area and is fixed in a separated state from the gypsum board, while the use of an oil-soluble adhesive reduces the moisture retention of the paper, and also, the use of a reinforcing net for strength reinforcement prevents the paper from stretching and sagging. .

본 발명은 습기를 머금지 않음은 물론 강도를 보강하는 보강망이 지용성 접착제에 의해 접착이 이루어지되 속지의 내측에 위치하는 형태로 초배지가 붙여지고, 초배지의 양측면으로만 풀칠에 의해 접착되는 것이어서, 초배지가 습기에 강하여 온,습도에 의해 초배지가 늘어지거나 쳐지는 현상이 발생할 때 보강망에 의해 쳐짐이나 늘어짐이 방지되기 때문에 도배지를 바르더라도 초배지 부분에서 늘어짐과 쳐짐 등의 현상이 발생하지 않으며, 또한, 초배지의 측면은 외측으로 갈수록 두께가 얇아지게 형성되어 있기 때문에 초배지를 바른 후 도배지를 바를 때 서로 겹치는 부위에서 단차가 나타나지 않아, 고품격의 도배를 하게 된다.In the present invention, a reinforcing net that does not contain moisture as well as reinforcing strength is bonded by an oil-soluble adhesive, but the paper is attached in a form located on the inside of the inlay, and only both sides of the paper are glued by gluing, Since the paper is strong against moisture, when the paper is stretched or sagging due to temperature and humidity, the reinforcing net prevents sagging or sagging, so even if the paper is applied, the phenomenon of sagging and sagging does not occur in the part of the paper. , Since the thickness of the side of the paper is thinner toward the outer side, when the paper is applied after applying the paper, there is no step difference in the overlapping area, resulting in a high-quality paper.

삭제delete

이하, 본 발명을 첨부된 도면에 의거 상세히 설명한다.Hereinafter, the present invention will be described in detail based on the accompanying drawings.

본 발명은 일정 폭과 길이를 갖는 공지의 초배지(10)를 구비하되 상기 초배지(10)의 중앙에는 도 7과 같이 좌우측으로 일정 간격을 두고 물과 섞이지 않는 지용성 접착제(20)를 도포하여 초배지(10)가 습기를 머금지 않도록 한 다음 도 6과 같이 지용성 접착제(20)를 도포한 폭과 같은 폭을 갖고 합성수지로 이루어지는 그물 형태의 보강망(30)을 덮어준 후 압착시킴으로써 도 8과 같이 초배지(10)의 중앙 부위에 보강망(30)을 지용성 접착제(20)로 고정시키게 된다.The present invention is provided with a known chobat 10 having a certain width and length, but the oil-soluble adhesive 20 immiscible with water is applied at regular intervals to the left and right as shown in FIG. 10) is covered with a reinforcing net 30 in the form of a net made of synthetic resin having the same width as the width of the oil-soluble adhesive 20 applied as shown in FIG. The reinforcing net 30 is fixed to the central portion of (10) with the oil-soluble adhesive 20.

여기서, 초배지(10)는 도배할 때 사용되는 공지의 제품이고, 지용성 접착제(20)는 물과 섞이지 않는 성질을 이용하여 보강망(30)을 초배지(10)에 접착시킬 때 초배지(10)가 습기를 머금지 않도록 하고, 상기 보강망(30)은 중앙 부위에 접착하되 초배지(10)의 양쪽으로 초배지(10)의 측면이 일부 노출되는 형태로 고정되게 하며, 상기 초배지(10)의 양측면에 보강망(30)으로 씌워지지 않고 노출되는 공간은 도배용 풀을 발라 초배지(10)를 접착시키기 위함이고, 이러한 공간은 경사면(11)을 형성하여 단차가 발생하지 않도록 한다.Here, the second medium 10 is a known product used when papering, and the oil-soluble adhesive 20 uses a water immiscible property to adhere the reinforcing net 30 to the second medium 10. To prevent moisture, the reinforcing net 30 is adhered to the central portion, but fixed in such a way that the side surfaces of the first medium 10 are partially exposed on both sides of the first medium 10, and on both sides of the second medium 10 The space exposed without being covered with the reinforcing net 30 is to apply glue for papering to adhere the paper background 10, and this space forms an inclined surface 11 to prevent a step from occurring.

본 발명은 초배지(10)의 중앙 부위에 길이 방향으로 보강망(30)을 지용성 접착제(20)로 접착시킴에 있어서, 상기 보강망(30)은 폴리프로필렌, 폴리에틸렌 등의 0.02~0.05mm의 굵기를 갖는 합성수지사를 이용하여 망목이 5~10mm를 갖게 그물망 형태로 직조된 것을 사용하며, 상기 보강망(30)의 망목은 규칙적이지 않고 불규칙적으로 형성되게 하고, 필요에 따라 망목이 규칙적으로 이루어진 그물망을 사용하여도 무관하다.In the present invention, in attaching the reinforcing net 30 in the longitudinal direction to the central portion of the super medium 10 with the oil-soluble adhesive 20, the reinforcing net 30 has a thickness of 0.02 to 0.05 mm, such as polypropylene and polyethylene. Using a synthetic resin yarn having a mesh woven in the form of a mesh having a size of 5 to 10 mm, the mesh of the reinforcing net 30 is not regular but irregularly formed, and the mesh is regularly formed as needed. It doesn't matter if you use

여기서, 보강망(30)은 합성수지사로 제작되어 습기를 머금지 않음은 물론 높은 강도를 갖는 한편 그물망 형태를 이루어져 적은 중량으로 제작하여도 폭 넓은 부위를 커버할 수 있으며, 물과 섞이지 않는 지용성 접착제의 사용으로 초배지(10)가 습기를 머금는 것을 방지하게 된다.Here, the reinforcing net 30 is made of synthetic resin yarn, which does not absorb moisture and has high strength, while being made in the form of a net to cover a wide area even when manufactured with a small weight, and is a water-immiscible oil-soluble adhesive. The use prevents the super medium 10 from retaining moisture.

이 같이 초배지(10)의 표면에 지용성 접착제(20)로 보강망(30)을 고정시킨 후에는 도 9와 같이 초배지(10)의 측면 두께를 외측으로 갈수록 얇아지게 갈아서 경사면(11)을 형성함으로써 도 10과 같은 단면을 갖도록 한 후 도 11과 같이 보강망(30)의 상측에 물을 뿌리며 속지(50)를 씌워서 보강망(30)의 상측에 붙어있게 하는 동시에 경사면(11)에 도배용 풀(40)을 발라준 다음 석고보드(1)(2)의 이음새를 속지(50)로 덮어주는 형태로 초배지(10)를 붙여주게 된다.In this way, after fixing the reinforcing net 30 with the oil-soluble adhesive 20 on the surface of the chobaeji 10, as shown in FIG. 9, by grinding the side thickness of the chobaeji 10 to become thinner toward the outside to form an inclined surface 11 After having a cross section as shown in FIG. 10, as shown in FIG. 11, water is sprayed on the upper side of the reinforcing net 30 and the inlay 50 is covered so that it is attached to the upper side of the reinforcing net 30, and at the same time, glue for wallpapering on the inclined surface 11 (40) is applied, and then the super medium (10) is attached in the form of covering the seams of the gypsum boards (1) (2) with the inlay (50).

본 발명은 보강망(30)을 초배지(10)의 표면에 지용성 접착제(20)로 접착시킨 상태에서 보강망(30)의 상부를 속지(50)로 씌워준 후 초배지(10)의 경사면(11)에 도배용 풀(40)을 발라 석고보드(1)(2)의 이음새를 속지(50)로 가려주게 도배용 풀(40)로 경사면을 부착시키는 것으로, 석고보드(1)(2)의 이음새 부위에서 속지(50)로 비접착이 이루어진 상태로 초배지(10)가 온,습도의 영향으로 처짐이나 늘어짐이 발생하지 않도록 하는 한편 과도하게 습도가 높더라도 습기를 먹지 않은 합성수지사로 이루어지고 지용성 접착제로 초배지(10)에 접착된 보강망(30)이 초배지(10)가 습기를 먹어 늘어지거나 쳐지게 되는 것을 잡아주기 때문에 온,습도의 영향으로 인하여 석고보드(1)(2)의 이음새 부분에서 초배지(10)가 늘어지거나 쳐지는 것이 방지되는 한편 초배지(10)의 과도한 수축으로 인한 찢어짐이나 변형이 발생하지 않는 효과가 있다.In the present invention, the upper portion of the reinforcing net 30 is covered with the inlay 50 in a state in which the reinforcing net 30 is adhered to the surface of the super medium 10 with the oil-soluble adhesive 20, and then the inclined surface 11 of the super medium 10 By applying the wallpapering glue 40 to the gypsum board (1) (2) and attaching the inclined surface with the wallpapering glue (40) to cover the joints of the gypsum board (1) (2) with the inlay (50), the joints of the gypsum board (1) (2) In the state where the inlay 50 is non-adhesive at the site, the super medium 10 does not sag or sag under the influence of temperature and humidity, while it is made of synthetic resin yarn that does not eat moisture even if the humidity is excessively high, and is made of oil-soluble adhesive. Since the reinforcing net 30 adhered to the chobaeji 10 catches the chobaeji 10 from being sagged or drooped by eating moisture, the chobatae (10) is prevented from sagging or drooping, while tearing or deformation due to excessive shrinkage of the super medium (10) does not occur.

또한, 본 발명은 초배지(10)의 경사면(11)에 통상적인 도배용 풀(40)을 도포하여 접착이 이루어지게 하는 것으로, 초배지(10)를 접착할 때 경사면(11)으로 인하여 도배지(60)가 초배지(10)와 겹치는 부위에는 높이에 대한 편차가 발생하는 것을 방지하게 된다.In addition, the present invention is to apply a conventional wallpapering glue (40) to the inclined surface (11) of the second paper (10) to achieve adhesion, and when the second paper (10) is adhered to the inclined surface (11) due to the paper (60) ) is prevented from occurring in the region where the super medium 10 overlaps with the deviation in height.

삭제delete

여기서, 초배지(10a)를 제지할 때 다양한 길이를 갖는 폴리프로필렌사를 넣고 제지를 하여도 무방하다.Here, when making the super medium (10a), it is okay to put polypropylene yarns having various lengths into the paper.

이러한 본 발명은 일정 폭과 길이를 갖는 초배지(10)의 일측면 중앙 부위에 지용성 접착제(20)를 도포하여 접착부를 형성하는 과정을 수행하고, 상기 초배지(10)의 중앙 부위에 발라진 지용성 접착제(20)의 상측에 합성수지사로 직조되는 보강망(30)을 배치하여 접착시키는 과정을 수행하고, 상기 보강망(30)의 측면으로 노출되는 초배지(10)는 외측으로 갈수록 두께가 얇아지게 경사면(11)을 형성하는 과정을 수행하고, 상기 초배지(10)는 일정 길이 단위로 말아주는 과정을 수행함으로써 제조가 이루어진다.The present invention performs a process of forming an adhesive portion by applying the oil-soluble adhesive 20 to the central portion of one side of the super medium 10 having a certain width and length, and the oil-soluble adhesive applied to the central portion of the super medium 10 ( 20), a reinforcing net 30 woven with synthetic resin yarn is placed on the upper side of the bonding process, and the super badge 10 exposed to the side of the reinforcing net 30 becomes thinner toward the outer side of the inclined surface 11 ) Performing a process of forming, and the super medium 10 is manufactured by performing a process of rolling in units of a certain length.

이렇게 제조된 초배지는 도배지(60)를 바르게 되는 작업현장으로 옮긴 후 초배지(10)의 보강망(30) 상측에 물을 적신 후 속지(50)를 부착하는 과정을 수행하고, 상기 초배지(10)의 경사면(11)에는 도배용 풀(40)을 도포하는 과정을 수행한 후 상기 초배지(10)의 속지(10)가 석고보드(1)(2)의 이음새를 덮어주게 초배지(10)를 접착시키는 과정을 수행한 다음 상측으로 도배지(60)를 접착시킴으로써 작업이 완료된다.The chobae prepared in this way is moved to the work site where the paper 60 is applied, and then the upper side of the reinforcing net 30 of the chobae 10 is wetted with water, and then the inlay 50 is attached. After performing the process of applying the wallpapering glue 40 to the inclined surface 11 of the, the inlay 10 of the second paper 10 covers the seams of the gypsum boards 1 and 2, and then the second paper 10 is adhered. The work is completed by adhering the paper 60 to the upper side after performing the process of doing so.

삭제delete

한편, 본 발명은 석고보드의 이음새를 메꾸거나 흠집을 메꾼 후 페인트 작업을 할 때 사용할 수 있는 것으로, 통상 퍼티 작업에 의해 이음새나 흠집을 메꾸게 되나, 본 발명에서는 초배지(10)를 이용하여 이음새나 흠집을 막아준 후 페인트칠을 할 수 있으며, 이 경우도 초배지(10)가 페인트의 무게를 충분히 견디기 때문에 크랙이 발생하거나 쳐지는 것을 방지할 수 있다.On the other hand, the present invention can be used when painting after filling the seams or flaws of the gypsum board, and usually fills the seams or flaws by putty work, but in the present invention, the seams are It is possible to paint after preventing scratches, and in this case, cracks can be prevented from occurring or sagging because the first paper 10 sufficiently withstands the weight of the paint.

이러한, 본 발명은 도배를 할 때 석고보드(1)(2)의 이음새 부분에서 도배지(60)가 함몰되거나 늘어지는 현상 또는 찢어지고 변형이 일어나는 현상을 방지하기 위한 것으로, 초배지(10)의 일측면에 합성수지사로 이루어지고 강도를 보강하는 보강망(30)을 물과 섞이지 않는 지용성 접착제(20)로 접착시킴으로써 초배지(10)가 최소한의 습기를 머금게 한 상태로 공장에서 생산한 다음 보강망(30)이 부착된 초배지(10)를 도배가 이루어지는 작업 현장으로 공급하게 되고, 도배 현장에서는 초배지(10)를 바를 때 경사면(11)에 도배용 풀(40)을 칠하는 한편 보강망(30)의 상측에 물을 뿌려 속지(50)를 붙여준 상태로 만든 다음 초배지(10)를 바르게 된다.Such, the present invention is to prevent the phenomenon that the paper 60 is sunken or stretched or torn and deformed at the seam of the gypsum board (1) (2) when papering, one of the first paper (10) By adhering a reinforcing net (30) made of synthetic resin yarn on the side and reinforcing strength with a water-immiscible oil-soluble adhesive (20), the super-paper (10) is produced in a factory with minimal moisture, and then the reinforcing net (30 ) is supplied to the work site where the paper is attached (10) to which paper is applied, and at the papering site, when applying the paper (10), the paper paste (40) is painted on the slope (11) while the reinforcing net (30) Water is sprayed on the upper side to make the inlay 50 attached, and then the second medium 10 is applied.

즉, 현장에서는 초배지(10)의 일측면에 보강망(30)이 고정된 상태로 공급받게 되면, 초배지(10)의 양측면으로 형성된 경사면(11)에 도배용 풀(40)을 바르는 한편 보강망(30)의 상측에 물을 뿌리면서 속지(50)를 붙인 다음 초배지(10)를 석고보드(1)(2)의 이음새에 붙이는 것으로, 석고보드(1)(2)의 이음새 부분을 가리는 초배지(10)를 바를 때, 초배지(10)의 중앙에 지용성 접착제(20)로 고정된 보강망(30)이 석고보드(1)(2)의 이음새를 가리게 하되 보강망(30)의 상측은 속지(50)로 덮어줌으로써, 초배지(10)를 바를 때 속지(50)가 석고보드(1)(2)의 이음새를 가리는 형태로 접착되며, 이때, 속지(50)는 석고보드(1)(2)와 비접착이 이루어지게 한다.That is, in the field, when the reinforcing net 30 is supplied in a fixed state on one side of the grass medium 10, the paper paste 40 is applied to the inclined surface 11 formed on both sides of the grass medium 10 while the reinforcing net By attaching the inlay (50) while spraying water on the upper side of (30), and then attaching the paper (10) to the seam of the gypsum board (1) (2), the paper paper covering the seam of the gypsum board (1) (2) When (10) is applied, the reinforcing net 30 fixed with the oil-soluble adhesive 20 in the center of the super medium 10 covers the seams of the gypsum boards 1 and 2, but the upper side of the reinforcing net 30 is inlayed. By covering with (50), when the super medium (10) is applied, the inlay (50) is adhered in the form of covering the seam of the gypsum board (1) (2), and at this time, the inlay (50) is the gypsum board (1) (2). ) and non-adhesion.

본 발명의 초배지(10)는 경사면(11)에 바른 도배용 풀(40)로 접착이 이루어지면서 속지(50)는 비접착 부위를 형성하게 되므로, 기존 방식의 초배지(3)를 사용하는 것에 비하여 강도를 보강하기 위한 보강망(30)에 의해 현저히 높은 강도와 인장력 등을 갖추는 한편 지용성 접착제(20)의 사용으로 초배지(10)가 머금게 되는 습도를 낮춤으로써, 초배지(10)를 붙이는 작업 후 습도로 인하여 초배지(10)가 이완되더라도 과도한 이완을 보강망(30)으로 잡아주어 늘어짐이나 쳐짐이 발생하지 않으며, 건조함으로 인하여 초배지(10)가 수축되더라도 보강망(30)이 잡아주기 때문에 초배지(10)가 찢어지거나 변형이 발생되지 않는다.Since the inlay 50 forms a non-adhesive area while the inlay 50 is adhered to the wallpapering paste 40 applied to the inclined surface 11, compared to using the conventional super medium 3 By the reinforcing net 30 for reinforcing strength, it has significantly high strength and tensile strength, while lowering the humidity in which the paper medium 10 is held by the use of the oil-soluble adhesive 20, the humidity after the work of attaching the paper medium 10 Even if the super medium 10 relaxes due to this, excessive relaxation is caught by the reinforcing net 30 so that sagging or sagging does not occur, and even if the super medium 10 shrinks due to dryness, the reinforcing net 30 catches the super medium 10 ) is not torn or deformed.

본 발명의 보강망(30)은 폴리프로필렌, 폴리에스터 등의 합성수지사로 그물망 형태를 갖추게 되고, 이러한 보강망(30)은 물과 섞이지 않는 지용성 접착제(20)에 의해 초배지(10)에 고정되는 것이어서 초배지(10)가 보강망(30)의 접촉으로 인하여 습기를 머금지 않도록 하는 한편 마치 콘크리트 타공시 철근을 배근하는 것과 같이 초배지(10)의 강도를 현저히 높이게 되고, 이로 인하여 초배지(10)의 늘어짐이나 쳐짐 또는 찢어짐이나 변형이 발생하는 것을 효과적으로 방지하게 된다.The reinforcing net 30 of the present invention is equipped with a net shape of synthetic resin yarns such as polypropylene and polyester, and this reinforcing net 30 is fixed to the first medium 10 by a water-immiscible oil-soluble adhesive 20 On the other hand, the strength of the chobaeji (10) is remarkably increased, such as placing reinforcing bars during perforation of concrete, so that the chobaeji (10) does not contain moisture due to the contact of the reinforcing net (30), and this causes the sagging of the chobaegeji (10). It effectively prevents sagging, tearing or deformation from occurring.

삭제delete

한편, 본 발명은 초배지(10)의 외측으로 도배지(60)를 바를 때 초배지(10)와 겹쳐지는 부위에서 도배지(60)가 단차를 보이는 현상을 방지하기 위한 것으로, 초배지(10)에 도배용 풀(40)을 바르기 이전에 초배지(10)의 측면을 갈아서 경사면(11)을 형성하되 상기 경사면(11)은 외측으로 갈수록 얇아지게 갈아준 다음 작업 현장에서 경사면(11)에 도배용 풀(40)을 발라 접착이 이루어지는 것으로, 초배지(10)의 측면이 얇은 상태에서 서서히 두꺼워지며 접착되기 때문에 초배지(10)의 외측에 부착되는 도배지(60)에서는 외측으로 단차가 나타나지 않게 된다.On the other hand, the present invention is to prevent the phenomenon in which the paper 60 shows a step in the area where the paper 60 overlaps with the paper 10 when the paper 60 is applied to the outside of the paper 10, for papering the paper 10 Before applying the glue 40, grind the side of the grass paper 10 to form an inclined surface 11, but the inclined surface 11 is ground thinner toward the outside, and then glue 40 for wallpapering on the inclined surface 11 at the work site ) is applied and the adhesion is made, and since the side of the super medium 10 gradually becomes thicker and adhered in a thin state, no step appears to the outside in the paper 60 attached to the outside of the super medium 10.

본 발명에서 초배지(10)를 갈아서 경사면(11)을 형성시키는 이유는 도배지(60)와 겹쳐질 때 도배지(60)에서 단차가 나타나지 않도록 하기 위함으로, 경사면(11)에는 도배용 풀(40)을 발라 사용하며, 도배용 풀(40)을 사용하는 이유는 초배지(10)를 바른 후 건조할 때 초배지(10)를 팽팽하게 당겨주기 때문에 도배용 풀(40)을 사용하게 된다.In the present invention, the reason for forming the inclined surface 11 by grinding the grass paper 10 is to prevent the step from appearing in the paper paper 60 when overlapped with the paper paper 60. It is used by applying, and the reason for using the paper paste 40 is to use the paper paste 40 because the paper paper 10 is pulled tight when drying after applying the paper paper 10.

10,10a : 초배지 11 : 경사면
20 : 접착제 30 : 보강망
40 : 풀 50 : 속지
60 : 도배지
10,10a: super medium 11: slope
20: adhesive 30: reinforcing net
40: Full 50: Fooled
60: Paper

Claims (6)

일정 폭과 길이를 갖는 초배지(10)의 일측면 중앙 부위에 지용성 접착제(20)를 도포하여 접착부를 형성하고;
상기 초배지(10)의 중앙 부위에 발라진 지용성 접착제(20)의 상측에 합성수지사로 직조되는 보강망(30)을 배치하여 고정되게 하되 상기 보강망(30)은 직경 0.02~0.05mm의 굵기를 갖는 폴리프로필렌, 폴리에틸렌의 합성수지로 제작하는 한편 상기 보강망(30)의 망목은 길이가 5~10mm로 불규칙적으로 형성하고;
상기 보강망(30)의 측면으로 노출되는 초배지(10)는 외측으로 갈수록 두께가 얇아지게 경사면(11)을 형성하고;
상기 초배지(10)의 일측면에 지용성 접착제(20)로 접착시킨 보강망(30)의 상측에 물을 적셔 속지(50)를 부착하고;
상기 초배지(10)의 경사면(11)에는 도배용 풀(40)을 도포한 후 속지(50)가 석고보드(1)(2)의 이음새를 가리게 경사면(11)을 부착하여 이루어지는 것을 특징으로 하는 석고보드 이음새용 초배지.
Forming an adhesive portion by applying a fat-soluble adhesive 20 to the central portion of one side of the super medium 10 having a certain width and length;
A reinforcing net 30 woven with synthetic resin yarn is placed on the upper side of the oil-soluble adhesive 20 applied to the central portion of the super medium 10 to be fixed, but the reinforcing net 30 is poly having a thickness of 0.02 to 0.05 mm in diameter Made of synthetic resin of propylene and polyethylene, while the mesh of the reinforcing net 30 is irregularly formed with a length of 5 to 10 mm;
Chobaeji 10 exposed to the side of the reinforcing net 30 forms an inclined surface 11 so that the thickness becomes thinner toward the outside;
Moisten water and attach the inlay 50 to the upper side of the reinforcing net 30 bonded to one side of the super medium 10 with the oil-soluble adhesive 20;
After applying the wallpapering glue (40) to the inclined surface (11) of the super medium (10), the inlay (50) is attached to the inclined surface (11) to cover the joints of the gypsum boards (1) (2), characterized in that Super paper for gypsum board joints.
삭제delete 삭제delete 일정 폭과 길이를 갖는 초배지(10)의 일측면 중앙 부위에 지용성 접착제(20)를 도포하여 접착부를 형성하는 과정을 수행하고,
상기 초배지(10)의 중앙 부위에 발라진 지용성 접착제(20)의 상측에 합성수지사로 직조되는 보강망(30)을 배치하여 접착시키는 과정을 수행하되 상기 보강망(30)은 직경 0.02~0.05mm의 굵기를 갖는 폴리프로필렌, 폴리에틸렌의 합성수지로 제작하는 한편 상기 보강망(30)의 망목은 길이가 5~10mm로 불규칙적으로 형성하고,
상기 보강망(30)의 측면으로 노출되는 초배지(10)는 외측으로 갈수록 두께가 얇아지게 경사면(11)을 형성하는 과정을 수행하고,
상기 초배지(10)의 일측면에 지용성 접착제(20)로 접착시킨 보강망(30)의 상측에 물을 적셔 속지(50)를 부착하는 과정을 수행하고,
상기 초배지(10)의 경사면(11)에는 도배용 풀(40)을 도포한 후 속지(50)가 석고보드(1)(2)의 이음새를 가리게 경사면(11)을 부착하는 과정을 수행하는 것을 특징으로 하는 석고보드 이음새용 초배지 제조방법.

A process of forming an adhesive portion by applying the oil-soluble adhesive 20 to the central portion of one side of the super medium 10 having a certain width and length,
A reinforcing net 30 woven with synthetic resin yarn is placed on the upper side of the oil-soluble adhesive 20 applied to the central portion of the super medium 10 to perform a bonding process, but the reinforcing net 30 has a diameter of 0.02 to 0.05 mm in thickness On the other hand, the mesh of the reinforcing net 30 is irregularly formed with a length of 5 to 10 mm,
The super medium 10 exposed to the side of the reinforcing net 30 performs a process of forming an inclined surface 11 so that the thickness becomes thinner toward the outside,
A process of attaching the inlay 50 by soaking water on the upper side of the reinforcing net 30 bonded to one side of the super medium 10 with the oil-soluble adhesive 20,
After applying the wallpapering glue 40 to the inclined surface 11 of the super medium 10, the process of attaching the inclined surface 11 so that the inlay 50 covers the seams of the gypsum boards 1 and 2 Method for manufacturing super medium for gypsum board joints, characterized in that

삭제delete 삭제delete
KR1020220103992A 2022-08-19 2022-08-19 Lining paper for joint of plaster board and its manufacturing method KR102517737B1 (en)