KR20040098893A KR1020030031210A KR20030031210A KR20040098893A KR 20040098893 A KR20040098893 A KR 20040098893A KR 1020030031210 A KR1020030031210 A KR 1020030031210A KR 20030031210 A KR20030031210 A KR 20030031210A KR 20040098893 A KR20040098893 A KR 20040098893A
Authority
KR
South Korea
Prior art keywords
panel
laminated
door
synthetic resin
toilet
Prior art date
Application number
KR1020030031210A
Other languages
Korean (ko)
Other versions
KR100522315B1 (en
Inventor
김영식
Original Assignee
주식회사 영화산업
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 영화산업 filed Critical 주식회사 영화산업
Priority to KR10-2003-0031210A priority Critical patent/KR100522315B1/en
Publication of KR20040098893A publication Critical patent/KR20040098893A/en
Application granted granted Critical
Publication of KR100522315B1 publication Critical patent/KR100522315B1/en

Links

Classifications

    • EFIXED CONSTRUCTIONS
    • E06DOORS, WINDOWS, SHUTTERS, OR ROLLER BLINDS IN GENERAL; LADDERS
    • E06BFIXED OR MOVABLE CLOSURES FOR OPENINGS IN BUILDINGS, VEHICLES, FENCES OR LIKE ENCLOSURES IN GENERAL, e.g. DOORS, WINDOWS, BLINDS, GATES
    • E06B3/00Window sashes, door leaves, or like elements for closing wall or like openings; Layout of fixed or moving closures, e.g. windows in wall or like openings; Features of rigidly-mounted outer frames relating to the mounting of wing frames
    • E06B3/70Door leaves
    • E06B3/82Flush doors, i.e. with completely flat surface
    • E06B3/86Flush doors, i.e. with completely flat surface of plastics without an internal frame, e.g. with exterior panels substantially of plastics
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B32LAYERED PRODUCTS
    • B32BLAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
    • B32B37/00Methods or apparatus for laminating, e.g. by curing or by ultrasonic bonding
    • B32B37/06Methods or apparatus for laminating, e.g. by curing or by ultrasonic bonding characterised by the heating method
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B32LAYERED PRODUCTS
    • B32BLAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
    • B32B37/00Methods or apparatus for laminating, e.g. by curing or by ultrasonic bonding
    • B32B37/10Methods or apparatus for laminating, e.g. by curing or by ultrasonic bonding characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
    • EFIXED CONSTRUCTIONS
    • E05LOCKS; KEYS; WINDOW OR DOOR FITTINGS; SAFES
    • E05YINDEXING SCHEME RELATING TO HINGES OR OTHER SUSPENSION DEVICES FOR DOORS, WINDOWS OR WINGS AND DEVICES FOR MOVING WINGS INTO OPEN OR CLOSED POSITION, CHECKS FOR WINGS AND WING FITTINGS NOT OTHERWISE PROVIDED FOR, CONCERNED WITH THE FUNCTIONING OF THE WING
    • E05Y2900/00Application of doors, windows, wings or fittings thereof
    • E05Y2900/10Application of doors, windows, wings or fittings thereof for buildings or parts thereof
    • E05Y2900/112Application of doors, windows, wings or fittings thereof for buildings or parts thereof for restrooms

Abstract

PURPOSE: A toilet door producing method is provided to prevent figures from being decolored by making a panel for a door using synthetic resin, to restrict the figures from damaging, and to secure a beautiful appearance by integrally molding the figures of the door with the panel. CONSTITUTION: A toilet door producing method is composed of steps for aligning to contact one side of a synthetic resin panel with 0.9t thickness and one side of a decor sheet with 0.15t¯0.2t thickness; laying, pressing, and laminating the aligned synthetic resin panel and the decor sheet on a hot plate by a heat pressurizing press; placing a laminated panel(10) in a mold and then forming figures on the laminated panel by vacuum pressure; arranging the laminated panels with the figures at both sides and combining a honeycomb-type core material(50) between the laminated panels; and joining the laminated panels to both sides of the core material and then finishing the edge.

Description

화장실 도어의 제조방법{MANUFACTURE METHOD OF RESTROOM DOOR}Manufacturing Method of Toilet Door {MANUFACTURE METHOD OF RESTROOM DOOR}

본 발명은 일정한 공간의 출입을 개폐하는 수단인 도어 특히 휴게실 등에 설치된 화장실 도어의 제조방법에 관한 것으로, 더욱 상세하게는 작업공정의 단순화를 꾀하고, 화장실 문화의 고급화를 유도할 수 있는 화장실도어의 제조방법에 관한 것이다.The present invention relates to a method of manufacturing a bathroom door installed in a door, especially a rest room, which is a means for opening and closing a fixed space, and more particularly, to a process of simplifying a work process and inducing a high quality toilet culture. It relates to a manufacturing method.

일반적으로 사람들이 많이 드나드는 휴게실의 공동 화장실에 설치된 화장실 도어는, 목재로 이루어진 심재부와, 이 심재부의 양측면에 합판 등과 같은 합성목이 접합된 것이 대부분으로서, 상기 목재도어의 외부면에 페인트 등을 이용하여 페인팅하여 외관이 깔끔하도록 하고 있다.In general, a toilet door installed in a common restroom of a common room where a lot of people come and go is formed by joining a core member made of wood and a synthetic wood such as plywood to both sides of the core member. The painting is used to make the exterior look neat.

그러나, 이와 같은 목재로 이루어진 화장실 도어는, 그 재질의 특성상 습기에 약해질 수 밖에는 없기 때문에, 쉽게 썩거나 하는 등의 문제점이 있과 함께 깔끔한 외관이 유지되도록 하기 위해 페인팅한 페인트가 떨어져 나감에 따라 기간이 경과될수록 도어의 외관에 좋지 않은 결과를 가져온다.However, the toilet door made of wood is weak to moisture due to its material properties, so it is easy to rot, and as the painted paint falls off to maintain a clean appearance. Over time, the appearance of the door is bad.

근자들어서는, 상기와 같이 목재로 이루어진 화장실 도어가 지닌 문제점을해결하고자, 합성수지재로 성형된 플라스틱 도어가 제안되고 있다.In recent years, in order to solve the problem of the toilet door made of wood as described above, a plastic door molded of a synthetic resin material has been proposed.

도 1은 이와 같은 플라스틱 도어의 구성을 나타낸 단면도로서, 도시된 바와 같이 소정의 형상으로 사출성형된 전면판(1)과 배면판(2) 사이에 간격을 유지하기 위한 다수의 간격유지부재(3)를 삽입하여 부착시키고, 상기 전면판(1) 및 배면판(2)의 양측면 및 상하단에는 마감부재(4)를 부착하는 방식으로 제조된다.1 is a cross-sectional view showing the configuration of such a plastic door, a plurality of gap holding member (3) for maintaining a gap between the front plate 1 and the back plate (2) injection molded in a predetermined shape as shown The insert is attached to, and is prepared by attaching the finishing member (4) on both sides and the upper and lower ends of the front plate (1) and the back plate (2).

상기와 같이 제조된 플라스틱도어는, 종래 목재로 이루어진 도어에 비해 습기에 강하기 때문에 도어가 부식되거나 하는 문제점이 해결되는 반면, 외관이 사출성형된 전면판과 배면판에 의해 고급스럽지 못하고 내구성이 현저하게 저하됨에 따라 자주 파손되는 문제점이 있다.The plastic door manufactured as described above has a problem that the door is corroded because it is more resistant to moisture than a door made of wood, but the exterior is not luxurious and durable due to the injection molded front and back plates. There is a problem that often breaks down.

더욱이 근자들어서는 보다 깨끗하고 청결한 화장실 문화를 정착하기 위한 노력을 하고 있는 실정임을 감안할 때, 상기와 같은 플라스틱도어는 화장실의 전체적인 미관을 해치는 결과를 가져온다.Moreover, in view of the fact that in recent years, efforts have been made to establish a cleaner and cleaner toilet culture, such plastic doors result in a deterioration of the overall beauty of the toilet.

따라서, 내구성이 강하고 외관이 미려한 화장실 도어가 절실하게 요구되는 실정이다.Therefore, a situation in which a toilet door with strong durability and a beautiful appearance is urgently required.

본 발명은 상기와 같은 종래 휴게실 등에 설치되는 화장실 도어가 지닌 문제점을 해결하기 위해 안출된 것으로, 견고한 내구성은 물론 미려한 외관에 의해 화장실 전체의 인테리어에 기여할 수 있는 화장실 도어의 제조방법을 제공함에 그 목적이 있다.The present invention has been made to solve the problems that the toilet door is installed in the conventional rest room, such as the above, to provide a method of manufacturing a toilet door that can contribute to the entire interior of the toilet by a solid durability as well as a beautiful appearance. There is this.

도 1은 종래 화장실 도어의 일예를 도시한 구성단면도이다.1 is a cross-sectional view showing an example of a conventional toilet door.

도 2는 본 발명인 화장실도어의 제조방법의 제조공정을 간략적으로 나타낸 공정도이다.Figure 2 is a process diagram briefly showing the manufacturing process of the manufacturing method of the present invention toilet door.

도 3은 본 발명인 화장실도어의 제조방법에 의해 합성수지패널과 데코시트가 정렬되는 정렬단계를 나타낸 분해사시도이다.Figure 3 is an exploded perspective view showing the alignment step of the synthetic resin panel and the decoration sheet by the manufacturing method of the present invention toilet door.

도 4는 본 발명인 화장실도어의 제조방법에 의해 합성수지패널과 데코시트가 정렬되는 정렬단계의 다른 실시예를 나타낸 분해사시도이다.Figure 4 is an exploded perspective view showing another embodiment of the alignment step of the synthetic resin panel and the decoration sheet by the manufacturing method of the present invention toilet door.

도 5는 본 발명인 화장실도어의 제조방법에 의해 정렬된 합성수지패널과 데코시트를 열가압하여 접합하는 합지단계를 나타낸 간략도이다.Figure 5 is a simplified diagram showing a lamination step of bonding by pressing the synthetic resin panel and the decor sheet aligned by the manufacturing method of the present invention toilet door.

도 6은 본 발명인 화장실도어의 제조방법에 의해 합지된 합지패널에 무늬를 성형하는 성형단계를 나타낸 간략도이다.Figure 6 is a simplified diagram showing a molding step of forming a pattern on the laminated panel laminated by the method of the present invention toilet door.

도 7은 본 발명인 화장실도어의 제조방법에 의해 합지패널과 심재부의 결합단계를 나타낸 분해사시도이다.Figure 7 is an exploded perspective view showing the bonding step of the laminated panel and the core material by the method of manufacturing the toilet door of the present invention.

<도면의 주요부분에 대한 부호의 설명><Description of the symbols for the main parts of the drawings>

10 : 합지패널 11 : 합성수지패널10: laminated panel 11: synthetic resin panel

12 : 데코시트 20 : 열가압프레스12: decor sheet 20: heat press

21 : 열판 30 : 성형기21: hot plate 30: molding machine

31 : 무늬부 32 : 파지구31: pattern 32: grip

33 : 공기배출구 40 : 가열기33: air outlet 40: heater

41 : 라미네이팅 히터 50 : 심재부41: laminating heater 50: core material

상기 목적을 이루기 위해 본 발명인 화장실도어의 제조방법은,In order to achieve the above object, the present invention provides a method of manufacturing a bathroom door,

합성수지패널의 일면과 데코시트의 일면이 접하도록 정렬하는 정렬단계와,An alignment step of aligning one surface of the synthetic resin panel with one surface of the decorative sheet,

상기 정렬된 합성수지패널과 데코시트를 열판의 상부에 적층한 후, 열가압프레스로 가압하여 합지하는 합지단계와,The laminated step of laminating the aligned synthetic resin panel and the decor sheet on the upper portion of the hot plate, and then press the laminated by pressing the heat press;

상기 합지단계에 의해 합지된 합지패널을 성형틀에 안착한 후, 진공압착에 의해 합지패널에 무늬를 성형하는 성형단계와,A molding step of seating the laminated panel laminated by the laminating step in a molding frame, and then forming a pattern on the laminated panel by vacuum pressing;

상기 성형단계에 의해 무늬가 성형된 합지패널을 양측에 구비하고 내측에 하니콤방식으로 이루어진 심재부를 결합하는 심재결합단계와,A core material joining step of providing a laminated panel molded on the pattern by the molding step on both sides and joining a core part made of a honeycomb method to the inside;

상기 심재결합단계에 의해 심재부의 양측면에 합지패널을 접한 후, 테두리를 마감하는 마감단계가 포함되어 이루어진 것을 특징으로 한다.After contacting the laminated panel on both sides of the core member by the core recombination step, characterized in that it comprises a finishing step of closing the rim.

상기와 같은 특징으로 이루어진 본 발명인 화장실도어의 제조방법은, 합성수지패널과 데코시트가 합지된 합지패널이 도어의 양측에 구비되어 있음에 따라, 습기 등에 강하고 다양한 무늬가 진공압착에 의해 이루어짐에 따라 견고성이 뛰어나고, 미려한 외관에 의해 화장실 전체의 인테리어에 효과를 기대할 수 있다.According to the present invention, the manufacturing method of the bathroom door having the above characteristics is provided with both sides of the door, the laminated panel in which the synthetic resin panel and the decor sheet are laminated, which is strong due to moisture and various patterns made by vacuum pressing. This excellent and beautiful appearance can expect an effect on the interior of the entire bathroom.

이하, 본 발명인 화장실도어의 제조방법에 대해 첨부된 도면을 참조하여 좀 더 구체적으로 설명한다.Hereinafter, with reference to the accompanying drawings for the manufacturing method of the present invention toilet door will be described in more detail.

도 2는 본 발명인 화장실도어의 제조방법의 제조공정을 나타낸 공정도이고, 도 3은 본 발명인 화장실도어의 제조방법에 의해 합성수지패널(11)의 일면과 데코시트(12)의 일면을 서로 접하여 정렬하는 정렬단계를 나타낸다.2 is a process chart showing a manufacturing process of the manufacturing method of the toilet door of the present invention, Figure 3 is to align one surface of the synthetic resin panel 11 and one surface of the decor sheet 12 by the manufacturing method of the toilet door of the present invention in contact with each other. Indicates an alignment step.

상기 합성수지패널(11)의 두께는 0.9t 정도이고 재질은 한정하는 것은 아니나 ABS재질로 형성되는 것이 좋다.The thickness of the synthetic resin panel 11 is about 0.9t and the material is not limited but is preferably formed of ABS material.

또한, 상기 데코시트의 두께는 0.15t ~ 0.2t 정도로 형성된다.In addition, the thickness of the decor sheet is formed about 0.15t ~ 0.2t.

도 4는 본 발명인 화장실도어의 제조방법 중 합성수지패널과 데코시트를 정렬하는 정렬단계에서 상기 합성수지패널과 데코시트를 다르게 구성하여 정렬하는 것으로, 이 경우 완성된 화장실도어의 또 다른 심미감을 기대할 수 있다.4 is to arrange the synthetic resin panel and the decor sheet differently in the alignment step of arranging the synthetic resin panel and the decor sheet in the manufacturing method of the present invention toilet door, in this case, you can expect another aesthetic of the finished toilet door. .

상기와 같이 합성수지패널(11)의 일면과 데코시트(12)의 일면이 서로 접하도록 한 다음, 도 5에 도시된 바와 같이 열가압프레스(20)를 이용하여 정렬된 합성수지패널과 데코시트를 열가압합지하는 합지단계과정을 거친다.As described above, one surface of the synthetic resin panel 11 and one surface of the decorative sheet 12 are in contact with each other, and then the synthetic resin panel and the decorative sheet are opened using the thermopress press 20 as shown in FIG. 5. Pressurized lamination goes through the lamination process.

즉, 상기 열가압프레스(20)의 열판(21)들 사이에 합성수지패널(11)과 데코시트(12)의 일면이 서로 접하여 이루어진 합지패널(10)을 적당량 적층한 후, 상기 열판(21)에 소정의 열을 가함과 동시에 가압함으로써, 열판(21)들 사이에 적층된 합지패널(10)의 합지가 이루어진다.That is, after laminating an appropriate amount of the laminated panel 10 formed on one surface of the synthetic resin panel 11 and the decor sheet 12 between the hot plates 21 of the hot pressing press 20, the hot plate 21 By applying a predetermined heat to and simultaneously pressurizing, the lamination of the laminated panel 10 laminated between the hot plates 21 is made.

상기와 같이 열가압프레스(20)에 의해 합지된 합지패널(10)을, 도 6에 도시된 바와 같이 성형기(30)의 상부에 안착시킨 후, 진공에 의해 무늬를 성형하는 성형단계를 진행한다.As described above, the laminated panel 10 laminated by the hot pressing press 20 is seated on the upper part of the molding machine 30 as shown in FIG. 6, and then a molding step of forming a pattern by vacuum is performed. .

상기 성형단계는, 합성수지패널(11)과 데코시트(12)가 접하여진 합지패널(10)을, 상단에 무늬부(31)가 형성된 성형기(30)의 상단에 안착시킨 후 안착된 합지패널(10)의 테두리부를 상기 성형기(30)의 측면에 구성된 파지구(32)로 파지한 다음, 상기 성형기(30)를 가열기(40)에 넣어 상기 가열기(40)의 하부에 다수개 구성된 라미네이팅 히터(41)를 이용하여 성형기(30)의 상단에 안착된 합지패널(10)을 1분정도 가열한다.In the molding step, the laminated panel 10 in which the synthetic resin panel 11 and the decor sheet 12 are in contact with each other, is seated on the upper end of the molding machine 30 in which the pattern part 31 is formed, and then the laminated panel ( 10, the edge portion of the molding machine 30 is gripped by the holding hole 32 formed on the side of the molding machine 30, and then put the molding machine 30 in the heater 40, a plurality of laminating heaters configured in the lower portion of the heater 40 41) to heat the laminated panel 10 seated on the upper end of the molding machine 30 for about 1 minute.

이와 같이 합지패널(10)을 1분 정도 가열한 다음, 상기 가열기(40)에 장입된 성형기(30)를 꺼낸 후, 상기 성형기(30)의 양측에 구성된 공기배출구(33)를 이용하여 합지패널(10)과 성형기(30)의 무늬부(31) 사이에 잔류하고 있는 공기를 순간적으로 배출하게 되면, 라미네이팅히터의 가열에 의해 물러진 합지패널(10)은, 이 합지패널(10)이 안착된 성형기(30)의 무늬부(31)에 밀착됨으로써, 무늬부(31)의 형성된 무늬와 동일한 무늬가 형성된다.After heating the lamination panel 10 for 1 minute as described above, the molding machine 30 loaded in the heater 40 is taken out, and then the lamination panel is formed by using air outlets 33 formed at both sides of the molding machine 30. When the air remaining between the pattern part 31 of the molding machine 30 and 10 is discharged instantaneously, the laminated panel 10 which has fallen by heating of the laminating heater is seated by the laminated panel 10. By contact | adhering to the pattern part 31 of the formed molding machine 30, the same pattern as the pattern formed in the pattern part 31 is formed.

상기와 같이 성형단계에 의해 표면에 무늬가 형성된 합지패널(10)을 심재의 양측면에 결합하는 심재결합단계에 의해 화장실도어의 제조가 완성된다.Manufacturing of the bathroom door is completed by the core material joining step of coupling the laminated panel 10 having a pattern formed on the surface by the molding step to both sides of the core material as described above.

즉, 도 7에 도시된 바와 같이 하니콤 방식으로 형성된 심재부(50)의 양측에 상기 무늬가 형성된 합지패널(10)(10)을 위치시킨 후, 접합제 등과 같은 접합수단을 이용하여 상기 심재부(50)의 양측면에 합지패널(10)(10)을 각각 접합한다.That is, after placing the patterned laminated panel 10, 10 on both sides of the core portion 50 formed in a honeycomb manner as shown in Figure 7, the core material using a bonding means such as a binder The laminated panels 10 and 10 are joined to both sides of the section 50, respectively.

이와 같이 심재부(50)와 합지패널(10)(10)과를 접합한 후, 테두리부에 별도의 마감부재(미도시)를 이용하여 마감하는 마감단계를 거침으로써 본 발명인 화장실도어의 제조방법에 의해 화장실도어가 제조된다.After joining the core member 50 and the laminated panel 10 and 10 in this way, the manufacturing method of the present invention toilet door by going through the finishing step of finishing using a separate finishing member (not shown) in the rim. The toilet door is manufactured by.

상기와 같은 단계들을 거쳐 제조된 화장실도어는 그 두께가 얇기 때문에, 화장실도어로 사용되는 데 전혀 무리가 따르지 않는다.Since the toilet door manufactured through the above steps is thin in thickness, it is not difficult to use the toilet door at all.

뿐만 아니라, 상기와 같이 제조된 화장실도어는 외관의 미려함에 의해 화장실 전체의 인테리어에 기여할 수 있고, 재질이 합성수지로 이루어짐에 따라 장기간 동안 사용하여도 도어에 형성된 무늬가 탈색되거나 훼손되지 않는다.In addition, the toilet door manufactured as described above may contribute to the entire interior of the bathroom by the beauty of the exterior, and the material formed of the synthetic resin does not discolor or damage the pattern formed on the door even for a long time.

따라서, 미려한 화장실 문화의 정책에 크게 기여할 수 있음과 동시에, 종래 휴게실 화장실 등과 같은 공용화장실이 지닌 불쾌한 느낌을 해결할 수 있다.Therefore, it is possible to greatly contribute to the policy of the beautiful toilet culture, and at the same time, it is possible to solve the unpleasant feeling of the common toilet such as the rest room toilet.

상술한 바와 같이 본 발명인 화장실도어의 제조방법에 의하면, 도어를 이루는 패널이 합성수지재질로 이루어짐에 따라 형성된 무늬가 탈색되지 않고, 도어의 무늬가 패널과 일체로 성형됨으로써, 무늬가 훼손되지 않을 뿐만 아니라, 미려한 외관에 의해 화장실의 인테리어에 크게 기여할 수 있는 효과가 기대된다.According to the manufacturing method of the toilet door of the present invention as described above, the pattern formed as the panel forming the door is made of synthetic resin material is not discolored, the pattern of the door is molded integrally with the panel, not only does not damage the pattern. In addition, the beautiful appearance is expected to contribute significantly to the interior of the bathroom.

Claims (1)

휴게실 등과 같은 장소에 설치되는 공용화장실의 도어를 제조함에 있어서,In manufacturing a door of a common toilet installed in a place such as a rest room, 0.9t 두께의 합성수지패널의 일면과 0.15t ~ 0.2t 두께의 데코시트의 일면이 접하도록 정렬하는 정렬단계와;An alignment step of aligning one surface of the 0.9t thick synthetic resin panel and one surface of the 0.15t to 0.2t thick decorative sheet; 상기 정렬된 합성수지패널과 데코시트를 열판의 상부에 적층한 후, 열가압프레스로 가압하여 합지하는 합지단계와;A laminating step of laminating the aligned synthetic resin panel and the decor sheet on the upper part of the hot plate, and then pressing the laminated resin panel by pressing with a heat press; 상기 합지단계에 의해 합지된 합지패널을 성형틀에 안착한 후, 진공압착에 의해 합지패널에 무늬를 성형하는 성형단계와;A molding step of seating the laminated panel laminated by the laminating step in a molding frame and then molding a pattern on the laminated panel by vacuum pressing; 상기 성형단계에 의해 무늬가 성형된 합지패널을 양측에 구비하고 내측에 하니콤방식으로 이루어진 심재부를 결합하는 심재결합단계와;A core material joining step of providing a laminated panel formed with a pattern by the molding step on both sides and joining a core part made of a honeycomb method to an inside thereof; 상기 심재결합단계에 의해 심재부의 양측면에 합지패널을 접한 후, 테두리를 마감하는 마감단계가 포함되어 이루어진 것을 특징으로 하는 화장실도어의 제조방법.After contacting the laminated panel on both sides of the core member by the core re-joining step, the manufacturing method of the toilet door characterized in that it comprises a finishing step of closing the rim.
KR10-2003-0031210A 2003-05-16 2003-05-16 Manufacture method of restroom door KR100522315B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
KR10-2003-0031210A KR100522315B1 (en) 2003-05-16 2003-05-16 Manufacture method of restroom door

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
KR10-2003-0031210A KR100522315B1 (en) 2003-05-16 2003-05-16 Manufacture method of restroom door

Publications (2)

Publication Number Publication Date
KR20040098893A true KR20040098893A (en) 2004-11-26
KR100522315B1 KR100522315B1 (en) 2005-10-18

Family

ID=37376588

Family Applications (1)

Application Number Title Priority Date Filing Date
KR10-2003-0031210A KR100522315B1 (en) 2003-05-16 2003-05-16 Manufacture method of restroom door

Country Status (1)

Country Link
KR (1) KR100522315B1 (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100747638B1 (en) * 2006-08-30 2007-08-08 주식회사 시민테크건설 The door for a bathroom, and, the manufacturing method
KR102564358B1 (en) * 2022-12-28 2023-08-08 공원동 Abs door manufacturing apparatus

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100747638B1 (en) * 2006-08-30 2007-08-08 주식회사 시민테크건설 The door for a bathroom, and, the manufacturing method
KR102564358B1 (en) * 2022-12-28 2023-08-08 공원동 Abs door manufacturing apparatus

Also Published As

Publication number Publication date
KR100522315B1 (en) 2005-10-18

Similar Documents

Publication Publication Date Title
US8677707B2 (en) Door skin, method of manufacturing a door produced therewith, and door produced therefrom
US7370454B2 (en) Door skin, method of manufacturing a door produced therewith, and door produced therefrom
KR100858965B1 (en) Reverse molded panel
US7823353B2 (en) Door, method of making door, and stack of doors
CA2520654C (en) Reverse molded plant-on panel component, method of manufacture, and method of decorating a door therewith
JP2003236994A (en) Composite-moldable cosmetic laminated plate
US7481900B1 (en) Method of manufacturing a molded door skin
KR100522315B1 (en) Manufacture method of restroom door
US8226788B1 (en) Method of manufacturing a molded door
JP3574642B2 (en) Manufacturing method of decorative board
KR200266839Y1 (en) Plastic pannel having imprinted pattern for door
JPH06226943A (en) Production of decorative plate used for furniture
KR200291566Y1 (en) Finely attired plywood of the forming solid body design
KR20210091530A (en) How to make furniture doors to improve productivity
KR200291496Y1 (en) The door for furniture
KR200352973Y1 (en) Cubicle
KR100691104B1 (en) Door panel with wood sheet
KR200434763Y1 (en) A column of frame for bed
KR19990068729A (en) Furniture door
JPH08197699A (en) Decorative panel for integral molding with resin and production thereof
ITTO981005A1 (en) PROCEDURE FOR THE MANUFACTURE OF AN INTERIOR DOOR.

Legal Events

Date Code Title Description
A201 Request for examination
E701 Decision to grant or registration of patent right
GRNT Written decision to grant
FPAY Annual fee payment

Payment date: 20121008

Year of fee payment: 8

FPAY Annual fee payment

Payment date: 20131111

Year of fee payment: 9

LAPS Lapse due to unpaid annual fee