KR200389700Y1 - Door frame for coke oven door - Google Patents

Door frame for coke oven door Download PDF

Info

Publication number
KR200389700Y1
KR200389700Y1 KR20-2005-0009977U KR20050009977U KR200389700Y1 KR 200389700 Y1 KR200389700 Y1 KR 200389700Y1 KR 20050009977 U KR20050009977 U KR 20050009977U KR 200389700 Y1 KR200389700 Y1 KR 200389700Y1
Authority
KR
South Korea
Prior art keywords
door frame
coke oven
door
carbonization chamber
carbon
Prior art date
Application number
KR20-2005-0009977U
Other languages
Korean (ko)
Inventor
백광일
Original Assignee
동양주공주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 동양주공주식회사 filed Critical 동양주공주식회사
Priority to KR20-2005-0009977U priority Critical patent/KR200389700Y1/en
Application granted granted Critical
Publication of KR200389700Y1 publication Critical patent/KR200389700Y1/en

Abstract

본 고안은 코크스오븐 도어용 도어프레임에 관한 것으로, 코크스오븐의 탄화실 입구에 설치되어 코크스오븐 도어가 장탈착되는 것에 의해 상기 탄화실을 밀폐하여 기밀을 유지하도록 하는 도어프레임에 있어서; 상기 도어프레임중 열변형 혹은 접촉 충격에 의한 균열, 파손, 변형이 쉽게 유발될 수 있는 국부에 그 일부를 절삭하고, 그 절삭된 부위에 탄소함량이 적어도 0.35% 함유된 구조용강인 S45C로 된 다수의 보강편을 볼트고정하여 보강한 코크스오븐 도어용 도어프레임을 제공한다.The present invention relates to a door frame for a coke oven door, the door frame is installed at the entrance to the carbonization chamber of the coke oven to close the carbonization chamber to be kept tight by the coke oven door is detachable; A portion of the door frame is made of S45C, which is a structural steel containing at least 0.35% of carbon in the cut part of the door frame, the part of which is easily cracked, broken or deformed by thermal deformation or contact impact, and which contains at least 0.35% of carbon. Provides a door frame for the coke oven door reinforced by bolts reinforcement.

본 고안에 따르면 고열환경속에서 잦은 접촉 충격을 받으면서 작업되는 코크스오븐 도어용 도어프레임의 취약 부분을 내열성, 내마모성의 보강편으로 보강함으로써 도어프레임의 수명을 연장하고, 가스 누출을 미리 예방할 수 있어 가스에 의한 중독사고, 환경오염 등을 방지하는 효과를 제공하게 된다.According to the present invention, by reinforcing the vulnerable part of the door frame for the coke oven door that is operated under frequent contact shock in a high temperature environment with a heat resistant and abrasion reinforcing piece, the life of the door frame can be extended and gas leakage can be prevented in advance. It will provide an effect of preventing poisoning accidents, environmental pollution and the like.

Description

코크스오븐 도어용 도어프레임{DOOR FRAME FOR COKE OVEN DOOR}Door frame for coke oven door {DOOR FRAME FOR COKE OVEN DOOR}

본 고안은 코크스오븐 도어용 도어프레임에 관한 것으로, 보다 상세하게는 코크스오븐 도어에 사용되는 도어프레임의 요부를 내열성 및 내충격성을 재질로 보강함으로써 도어의 수명을 연장하고 기밀을 유지하여 환경오염을 예방할 수 있도록 한 코크스오븐 도어용 도어프레임에 관한 것이다.The present invention relates to a door frame for a coke oven door, and more particularly, by reinforcing the main portion of the door frame used for the coke oven door with heat and impact resistance material to extend the life of the door and to maintain airtightness to prevent environmental pollution It relates to a door frame for a coke oven door that can be prevented.

일반적으로, 코크스오븐은 용광로로 투입되는 원료인 코크스를 제조하는 데에 사용되는 연료건류장치로서, 132개의 개별 탄화실을 가지며, 각 탄화실마다 구비된 도어를 이용하여 이를 밀폐한 후 장입된 유연탄을 대략 18시간 이상 건류하여 코크스를 만들게 된다.Generally, coke oven is a fuel distillation apparatus used to manufacture coke, which is a raw material input to a blast furnace. The coke oven has 132 individual carbonization chambers and is sealed by using doors provided in each carbonization chamber and then charged with coal. Coke is made by coking for about 18 hours or more.

이와 같이 탄화실 밀폐를 위해 중요한 요소인 코크스오븐 도어는 매우 무거운 중량물이기 때문에 유압실린더를 갖춘 도어인출기를 통해 도어프레임에 장탈착되게 된다.As such, the coke oven door, which is an important element for sealing the carbonization chamber, is very heavy and is mounted on the door frame through a door extractor equipped with a hydraulic cylinder.

그런데, 도 1의 도시와 같이, 종래 도어프레임(10)은 대부분 주철이 적용되어 사용되고 있기 때문에 코크스 제조공정이 반복적으로 이루어짐에 따라 코크스오븐 도어(12)를 포함한 도어프레임(10)이 가열과 냉각되는 과정을 반복하게 되고, 이로 인해 이들의 국부가 고온 열충격에 의한 조직 변화를 일으켜 열간균열 혹은 열변형을 유발시키게 된다.By the way, as shown in Figure 1, the conventional door frame 10 is used because most of the cast iron is used as the coke manufacturing process is repeatedly made, the door frame 10 including the coke oven door 12 is heated and cooled The process is repeated, which causes the localization of the tissue changes due to high temperature thermal shock, causing hot cracking or thermal deformation.

또한, 이러한 열변형은 도어프레임(10)의 수명을 단축시킴은 물론 도어(12)와의 틈새를 유발시켜 코크스오븐가스(COG)의 누출을 가져와 작업자의 가스중독, 환경오염 등 커다란 문제를 파생시키게 된다.In addition, such thermal deformation not only shortens the life of the door frame 10 but also causes a gap with the door 12, resulting in leakage of coke oven gas (COG), leading to a great problem such as gas poisoning and environmental pollution of the worker. do.

뿐만 아니라, 중량물인 도어(12)의 장탈착시 잦은 접촉 충격을 받게 되어 국부적인 손상, 균열 등의 문제가 야기되고, 이또한 상술한 바와 동일한 문제를 야기시키게 된다.In addition, when the heavy load or detachment of the door 12 is subjected to frequent contact shocks cause problems such as local damage, cracks, and this also causes the same problem as described above.

아울러, 도면중 미설명 부호 16은 도어(12)를 도어프레임(10)에 고정하기 위한 래치바(14)가 걸림고정되도록 도어프레임(10)상에 형성된 후크형 걸이이다.In addition, reference numeral 16 in the drawings is a hook-type hook formed on the door frame 10 to lock the latch bar 14 for fixing the door 12 to the door frame 10.

본 고안은 상술한 바와 같은 종래 기술이 갖는 제반 문제점을 감안하여 이를 해결하고자 창출한 것으로, 고온 환경속에서 코크스오븐 도어와 잦은 접촉 충격을 받는 도어프레임의 요부를 신속하게 교체가능한 구조로 만들어 필요에 따라 교체 사용토록 함으로써 그 사용수명을 연장시킴은 물론 열변형에 따른 코크스오븐가스의 누출을 막아 작업의 안정성을 확보하고 환경오염을 예방할 수 있도록 한 코크스오븐 도어용 도어프레임을 제공함에 그 목적이 있다.The present invention was created in view of the above-mentioned problems of the prior art, and has been created to solve this problem, and the main part of the door frame which is frequently touched with the coke oven door in a high temperature environment can be quickly replaced with a necessary structure. Its purpose is to provide a door frame for the coke oven door that can extend its service life and prevent the leakage of coke oven gas due to thermal deformation, thereby ensuring the safety of work and preventing environmental pollution. .

본 고안은 상기한 기술적 과제를 달성하기 위하여, 코크스오븐의 탄화실 입구에 설치되어 코크스오븐 도어가 장탈착되는 것에 의해 상기 탄화실을 밀폐하여 기밀을 유지하도록 하는 도어프레임에 있어서; 상기 도어프레임중 열변형 혹은 접촉 충격에 의한 균열, 파손, 변형이 쉽게 유발될 수 있는 국부에 그 일부를 절삭하고, 그 절삭된 부위에 탄소함량이 적어도 0.35% 함유된 구조용강인 S45C로 된 다수의 보강편을 볼트고정하여 보강한 코크스오븐 도어용 도어프레임을 제공함에 그 기술적 특징이 있다.In order to achieve the above technical problem, the present invention is to provide a door frame for maintaining the airtight to seal the carbonization chamber by the coke oven door is installed at the entrance to the carbonization chamber of the coke oven; A portion of the door frame is made of S45C, which is a structural steel containing at least 0.35% of carbon in the cut part of the door frame, the part of which is easily cracked, broken or deformed by thermal deformation or contact impact, and which contains at least 0.35% of carbon. The technical feature is to provide a door frame for the coke oven door reinforced by bolts reinforcement.

이하에서는, 첨부도면을 참고하여 본 고안에 따른 바람직한 실시예를 보다 상세하게 설명하기로 한다.Hereinafter, with reference to the accompanying drawings will be described in detail a preferred embodiment according to the present invention.

도 2는 본 고안에 따른 도어프레임의 외관 사시도이고, 도 3 및 도 4는 본 고안에 따른 요부 단면도로서 각각 도 2의 'A'부와 'B'부를 확대도시한 것이다.2 is an external perspective view of the door frame according to the present invention, and FIGS. 3 and 4 are enlarged views of the 'A' part and 'B' part of FIG.

도 2에 도시된 바와 같이, 코크스오븐 도어를 지지하는 도어프레임(100)이 구비되는데 상기 도어프레임(100)은 기존과 같이 도어를 장탈착하기 위한 중공부(110)가 형성된 구조이다.As shown in FIG. 2, a door frame 100 supporting the coke oven door is provided, and the door frame 100 has a structure in which a hollow part 110 for mounting and detaching the door is formed.

즉, 상기 도어프레임(100)은 도어가 장착될 공간이 제거된 대략 사각테두리 형태를 이룬다.That is, the door frame 100 forms a substantially rectangular frame in which the space in which the door is to be mounted is removed.

그리고, 상기 도어프레임(100)의 일측면 상하 길이 적소에는 고정부(120)가 형성된다.In addition, the fixing part 120 is formed at one side up and down length of the door frame 100.

또한, 상기 고정부(120)에는 후크형 걸이(122)가 고정 설치된다.In addition, the hook-type hook 122 is fixed to the fixing part 120.

이때, 상기 고정부(120)의 일부, 이를테면 후크형 걸이(122)가 고정설치되는 부분 혹은 그 주변 부분에 이의 열변형 내지 충격변형, 파손, 균열 등을 방지하도록 일정크기의 절삭면(124)이 형성되고, 상기 절삭면(124)에는 그 절삭된 크기와 대응되는 제1보강편(200)이 교체가능하게 부착 고정된다.At this time, a part of the fixing part 120, for example, the cutting surface 124 of a predetermined size to prevent the thermal deformation, impact deformation, breakage, cracking, etc. in the portion or the peripheral portion of the hook-shaped hook 122 is fixed installation Is formed, the first reinforcing piece 200 corresponding to the cut size is fixed to the cutting surface 124 is replaceable.

여기에서, 상기 제1보강편(200)은 내마모성(내충격성), 내열성(내열변형성)이 우수한 구조용강 재질인 S45C(탄소함량 0.35%)가 바람직하며, 고정볼트(220)에 의해 교체가능하게 고정됨이 바람직하다.Here, the first reinforcing piece 200 is preferably a structural steel material S45C (carbon content 0.35%) excellent in wear resistance (impact resistance), heat resistance (heat deformation), and is replaceable by a fixing bolt 220 It is preferred to be fixed.

이를 위해, 상기 절삭면(124)에는 적어도 두개 이상의 볼트체결홈(126)이 절삭면(124)의 내부를 향해 요입형성되고, 상기 제1보강편(200)에는 상기 볼트체결홈(126)과 대응되는 개수의 볼트공(210)이 관통형성된다.To this end, at least two bolting grooves 126 are recessed in the cutting surface 124 toward the inside of the cutting surface 124, and the bolt coupling grooves 126 and the first reinforcing pieces 200 are formed. A corresponding number of bolt holes 210 are formed through.

이때, 상기 볼트공(210)은 상기 고정볼트(220)를 완전히 수납할 수 있도록 탄턱(212)을 갖는 구조로 이루어지는데 상기 탄턱(212)을 중심으로 그 상부에는 고정볼트(220)의 볼트머리가 완전히 내장되게 배치되고 그 하부에는 고정볼트(220)의 몸체가 삽입관통되게 배치된다.At this time, the bolt hole 210 is made of a structure having a jaw 212 to completely accommodate the fixing bolt 220, the bolt head of the fixing bolt 220 in the upper portion around the tan jaw 212 Is disposed to be completely embedded and the body of the fixing bolt 220 is inserted through the lower portion is disposed.

따라서, 상기 제1보강편(200)은 상기 고정부(120)에 교체가능하게 부착되게 되는데, 그 부착 위치는 예시된 부위에 국한되지 않고 고온환경속에서 국부적인 변형이 쉽게 유발될 수 있는 도어프레임(100)의 다수 개소에 적의 선택되어 설치될 수 있음은 물론이다.Therefore, the first reinforcing piece 200 is to be attached to the fixing portion 120 replaceably, the attachment position is not limited to the illustrated portion and the door that can be easily localized deformation in a high temperature environment Of course, the enemy can be selected and installed in a plurality of places of the frame 100.

한편, 도 2 및 도 4에서와 같이, 도어프레임(100)의 상단부 및 하단부에도 상기 고정부(120)와 유사한 형태의 제2보강편(300)이 교체가능하게 부착된다.On the other hand, as shown in Figures 2 and 4, the second reinforcing piece 300 of a similar shape to the fixing part 120 is also replaceably attached to the upper end and the lower end of the door frame 100.

여기에서는 설명의 편의상 도어프레임(100)의 상단부(130)를 예시적으로 설명하기로 한다.Here, for convenience of description, the upper end 130 of the door frame 100 will be described as an example.

도시된 도 4에서, 본 고안 제2보강편(300)은 상술한 제1보강편(200)과 동일한 재질인 S45C로 형성됨이 바람직하다.In FIG. 4, the second reinforcement piece 300 of the present invention is preferably formed of S45C having the same material as the first reinforcement piece 200 described above.

또한, 상기 제2보강편(300)에는 상기 제1보강편(200)의 구조와 대동소이한 형태를 갖는 적어도 2개 이상의 볼트공(310)이 형성된다.In addition, at least two bolt holes 310 having a shape substantially similar to that of the first reinforcing piece 200 are formed in the second reinforcing piece 300.

나아가, 상기 제2보강편(300)이 부착될 도어프레임(100)의 상단부(130)에는 그 면 일부가 절삭제거된 절삭홈(134)이 형성되고, 상기 절삭홈(134)에는 상기 볼트공(310)과 대응되는 볼트체결홈(136)이 형성되며, 상기 볼트공(310)을 관통하여 상기 볼트체결홈(136)에 볼트결합되는 고정볼트(320)가 구비됨으로써 상기 제2보강편(300)과 도어프레임(100)의 상단부(130) 간의 결합이 완료되게 된다.Furthermore, a cutting groove 134 is formed in the upper end 130 of the door frame 100 to which the second reinforcing piece 300 is to be attached, and a portion of the surface thereof is cut off, and the bolt hole is formed in the cutting groove 134. A bolt fastening groove 136 corresponding to the 310 is formed, and the fixing bolt 320 is bolted to the bolt fastening groove 136 by penetrating the bolt hole 310 to provide the second reinforcing piece ( The coupling between the upper portion 130 of the 300 and the door frame 100 is completed.

따라서, 도어프레임(100)상의 열변형 및 충격변형이 쉽게 일어나는 국부를 간단히 보강할 수 있게 된다.Therefore, it is possible to simply reinforce the portion where heat deformation and impact deformation easily occur on the door frame 100.

이러한 구성으로 이루어진 본 고안의 작동관계는 다음과 같다.The working relationship of the present invention made of such a configuration is as follows.

도어프레임(100)상의 취약 부분에 상술한 바와 같은 제1,2보강편(200,300)을 볼트 체결방식으로 교체가능하게 체결고정하여 코크스오븐 탄화실 밀폐용 부재로 사용하게 된다.The first and second reinforcement pieces 200 and 300 as described above are fixed to the weak part on the door frame 100 so as to be replaceable by bolt fastening and used as a member for sealing the coke oven carbonization chamber.

즉, 원료탄인 점결성 석탄(유연탄)을 탄화실에 장입한 다음 코크스오븐 도어(도 1의 '12')를 도어프레임(100)에 장착한 후 압축스프링(미도시)의 힘으로 핫페이스(hot face)를 탄화실 내부로 밀착시킨 상태에서 래치바(도 1의 '14')로 도어프레임(100)의 고정부(120)에 구비된 후크형 걸이(122)를 걸어 고정함으로써 탄화실을 밀폐시키게 된다.That is, after charging the coking coal (soft coal), which is raw coal, into a carbonization chamber, the coke oven door ('12' of FIG. 1) is mounted on the door frame 100, and then a hot face is applied by the force of the compression spring (not shown). The carbonization chamber is sealed by hooking and fixing the hook type hook 122 provided on the fixing part 120 of the door frame 100 with the latch bar ('14' in FIG. 1) while keeping the face closely in the carbonization chamber. Let's go.

그런 다음, 대략 1000℃ 내외로 가열하여 소정시간이 경과하면 수분이나 휘발분이 가스화되어 방출되고, 나중에 대부분의 탄소와 회분으로 이루어진 코크스가 제조되게 된다.Then, after heating to about 1000 ° C. and a predetermined time elapses, moisture or volatile matter is gasified and released, and coke made of most carbon and ash is produced later.

이와 같은 과정을 거쳐 코크스가 제조되면 상기 도어(12)를 개방하고 제조된 코크스를 인출하여 냉각한 다음 후공정으로 이송시키게 된다.When the coke is manufactured through such a process, the door 12 is opened, the manufactured coke is taken out, cooled, and then transferred to a later process.

이러한 과정을 반복적으로 수행하던 중에 만약 도어프레임(100)의 국부, 즉 열변형이 쉽게 일어날 수 있는 도어프레임(100)의 상단부나 하단부 혹은 접촉 충격을 많이 받는 후크형 걸이(122) 설치부 등의 균열, 파손 내지 열변형에 의한 틈새유발로 탄화실 내부의 가스가 누출되게 되면 작업자는 해당 작업이 완료된 후 변형이 유발된 부위의 제1,2보강편(200,300)을 교체함으로써 문제 발생에 대한 신속한 후속조치를 간단 용이하게 취할 수 있게 된다.While repeatedly performing such a process, if the local part of the door frame 100, that is, the upper part or the lower part of the door frame 100, which can easily undergo thermal deformation, or the hook-type hook 122 installation part which receives a lot of contact shocks, etc. If gas inside the carbonization chamber is leaked due to cracking, breakage, or crevice caused by thermal deformation, the operator can promptly solve the problem by replacing the first and second reinforcing pieces (200,300) of the deformed part after the work is completed. Follow-up actions can be taken simply and easily.

즉, 과거 작업 경험에 비추어 변형이 쉽게 유발되는 부위를 미리 잘 알고 있으므로 그 부위 및 주변을 제1,2보강편(200,300)으로 보강함으로써 상술한 교체 작업을 통한 신속한 조치가 가능하며, 교체 작업은 단순히 작업공구를 이용하여 고정볼트(220,320)를 풀거나 조이는 것을 통해 간단 용이하게 할 수 있다.That is, in the light of past work experience, it is well known in advance that a part easily deforms, and thus, the first and second reinforcement pieces 200 and 300 are reinforced, and thus the quick action through the above-described replacement work is possible. It can be easily done simply by loosening or tightening the fixing bolts 220 and 320 using a work tool.

따라서, 도어프레임(100)의 수명이 연장됨은 물론 가스 누출에 의한 중독사고나 환경오염을 미연에 예방할 수 있게 된다.Therefore, the life of the door frame 100 is extended, as well as it is possible to prevent poisoning accidents or environmental pollution due to gas leakage in advance.

이상에서 상세히 설명한 바와 같이, 본 고안에 따르면 고열환경속에서 잦은 접촉 충격을 받으면서 작업되는 코크스오븐 도어용 도어프레임의 취약 부분을 내열성, 내마모성의 보강편으로 보강함으로써 도어프레임의 수명을 연장하고, 가스 누출을 미리 예방할 수 있어 가스에 의한 중독사고, 환경오염 등을 방지하는 효과를 제공하게 된다.As described in detail above, according to the present invention, by reinforcing the vulnerable portion of the door frame for the coke oven door that is operated under frequent contact shock in a high temperature environment with a heat-resistant, wear-resistant reinforcing piece to extend the life of the door frame, gas Leakage can be prevented in advance, thereby providing an effect of preventing gas poisoning accidents and environmental pollution.

도 1은 종래 코크스오븐에 설치되는 도어프레임을 보인 예시적인 사시도,1 is an exemplary perspective view showing a door frame installed in a conventional coke oven,

도 2는 본 고안에 따른 도어프레임의 외관 사시도,2 is an external perspective view of a door frame according to the present invention;

도 3 및 도 4는 본 고안에 따른 요부 단면도.3 and 4 is a sectional view of the main part according to the present invention.

♧ 도면의 주요 부분에 대한 부호의 설명 ♧♧ description of the symbols for the main parts of the drawing ♧

100....도어프레임 120....고정부100 .... door frame 120 ....

122....후크형 걸이 124....절삭면122 .... hook hook 124 .... cutting surface

126,136....볼트체결홈 130....상단부126,136 .... Bolted groove 130 .... Top

134....절삭홈 200....제1보강편134 .... cutting groove 200 .... 1st reinforcement

210,310....볼트공 220,320....고정볼트210,310 ... bolts 220,320 bolts

300....제2보강편300 .... 2 Reinforcement

Claims (1)

코크스오븐의 탄화실 입구에 설치되어 코크스오븐 도어가 장탈착되는 것에 의해 상기 탄화실을 밀폐하여 기밀을 유지하도록 하는 도어프레임에 있어서;A door frame installed at a carbonization chamber inlet of a coke oven to seal the carbonization chamber and maintain airtightness by the coke oven door being detachable; 상기 도어프레임중 열변형 혹은 접촉 충격에 의한 균열, 파손, 변형이 쉽게 유발될 수 있는 국부에 그 일부를 절삭하고, 그 절삭된 부위에 탄소함량이 적어도 0.35% 함유된 구조용강인 S45C로 된 다수의 보강편을 볼트고정하여 보강한 것을 특징으로 하는 코크스오븐 도어용 도어프레임.A portion of the door frame is made of S45C, which is a structural steel containing at least 0.35% of carbon in the cut part of the door frame, the part of which is easily cracked, broken or deformed by thermal deformation or contact impact, and which contains at least 0.35% of carbon. Door frame for coke oven door, characterized in that the reinforcing piece bolted to reinforcement.
KR20-2005-0009977U 2005-04-12 2005-04-12 Door frame for coke oven door KR200389700Y1 (en)