KR19990081885A - 제빙(除氷) 조성물 및 제빙 방법 - Google Patents

제빙(除氷) 조성물 및 제빙 방법 Download PDF

Info

Publication number
KR19990081885A
KR19990081885A KR1019980705597A KR19980705597A KR19990081885A KR 19990081885 A KR19990081885 A KR 19990081885A KR 1019980705597 A KR1019980705597 A KR 1019980705597A KR 19980705597 A KR19980705597 A KR 19980705597A KR 19990081885 A KR19990081885 A KR 19990081885A
Authority
KR
South Korea
Prior art keywords
composition
immersion
ice
weight
chloride
Prior art date
Application number
KR1019980705597A
Other languages
English (en)
Inventor
조지 에이. 잰크
워렌 디. 쥬니어 존슨
Original Assignee
잰크조지에이.
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 잰크조지에이. filed Critical 잰크조지에이.
Publication of KR19990081885A publication Critical patent/KR19990081885A/ko

Abstract

본 발명은 옥수수의 습식 밀링 공정에서 나온 부산물을 포함하는 신규하고 개선된 환경적 허용성을 지니며 무시할 정도의 부식성을 지닌 제빙 조성물에 관한 것으로, 상기 부산물은 생분해성 물질이다. 또한, 본 발명은 이 제빙 조성물을 사용하여 도로, 교량 및 기타 옥외 노면에 존재하는 눈이나 얼음 침적물을 제거하는 방법에 관한 것이다.

Description

제빙(除氷) 조성물 및 제빙 방법
도로 및 교량에 존재하는 얼음 및 눈 때문에 차량 통행이 매우 느려지고, 일반 대중에 위험이 증가하게 된다는 것은 잘 알려진 사실이다. 교통 문제를 어느 정도 완화시키기 위하여 기계적으로 눈을 제거하는 방법이 종종 사용된다. 또한, 차로에 있는 눈 및 얼음을 녹이기 위하여 염화물 염(chloride salts)과 같은 화학적 화합물도 종종 사용되며, 이 때 염화물 염의 유형은 고체형이건 용액형이건 또는 모래 및 기타 물질과의 혼합물이건 상관이 없다. 그러나, 대부분의 제빙 화합물은 환경적으로 유해하므로, 지방 행정 당국에서는 눈 및 얼음 침적물을 제거하기 위하여 사용되는 화학 물질의 양 및 유형을 제한하는 일이 흔히 있다.
차로를 처리하는데 사용되는 대부분의 화학 물질은 다음과 같은 이유에서 해롭다. 이들 화학 물질인 염은 토양을 알칼리성으로 변하게 하고, 또 식물들의 뿌리 계통으로 흡수되기 때문에 토양 및 주변 초목을 손상시킨다. 이들은 민물, 강물 및 호수를 오염시키며, 지하수로 흡수되는 일이 흔히 있다. 또, 염은 부식 효과를 지니기 때문에 차량에 큰 손상을 미칠 뿐만 아니라, 도로의 콘크리트 및 금속계 구조물들에도 나쁜 영향을 미친다. 대부분의 염이 콘크리트 구조물의 파괴를 유발한다는 사실은 잘 알려져 있으며, 상기 염은 상기 구조물의 강도와 수명을 현저히 저하시킨다. 이러한 이유들로 인하여, 대부분의 주에서는 염의 사용을 금지해 왔고, 다른 주에서도 염의 사용을 크게 제한하였다.
부식성 염류를 비부식성 물질, 예컨대 알콜류 및 글리콜류로 대체하는 것이 바람직하다는 것은 잘 알려져 있으나, 이들의 인화성, 독성 및 가격 때문에 이들 다른 물질들은 지금까지 효과적으로 그리고 경제적으로 사용되지 못하였다.
본 발명은 옥수수의 습식 밀링 공정의 부산물로 이루어진 환경적으로 허용가능하며 무시할 정도의 부식성을 지닌 제빙(deicing) 조성물에 관한 것으로, 상기 부산물은 생분해성 물질이다. 또한, 본 발명은 상기 제빙 조성물을 도로, 교량, 활주로, 유도로(誘導路) 및 기타 옥외 노면에 존재하는 눈 및 얼음 침적물을 제거하는 데 사용하는 방법에 관한 것이다.
본 발명은 산업 분야에서 침지수(steepwater)로 알려진 옥수수의 습식 밀링 공정의 부산물을 활성 성분으로서 함유하는, 환경적으로 허용가능한 동결 방지(anti-freeze) 및 제빙 조성물에 관한 것이다. 상기 조성물은 수용성이고, 부식성은 무시할 만 하며, 가격이 저렴하고, 대량으로 널리 이용가능하다. 또한, 본 발명은 상기 제빙 조성물을 사용하여 도로, 교량, 할주로, 유도로 및 기타 옥외 노면에 눈 및 얼음 침적물이 존재하지 않도록 하는 방법에 관한 것이다.
통상 제빙제로 사용되는 물질은 적당한 수 용해성, 용액의 낮은 빙점, 저렴한 비용으로 산업적 규모로의 이용 가능성, 비부식성, 환경적 허용성 및 통상의 공지된 수단 및 입수가능한 수단으로 도포할 수 있는 성능 등의 특징을 가진다.
전술한 내용의 측면에서, 본 발명의 제1 목적은 눈과 얼음이 없는 노면을 만들기에 적합한 동결 방지 및 제빙 조성물로서, 수용성이고, 빙점이 낮고, 전세계에서 산업적 대량으로 입수 용이하고, 부식성이 무시할 정도이며, 환경 친화적이고, 기존의 처리 대원들이 현재 사용되고 있는 장치로 도포할 수 있는 동결 방지 및 제빙 조성물을 제공하는 것이다.
본 발명의 제2 목적은 환경 친화성이 있고, 부식성이 무시할 정도이며, 가격 경쟁력이 있는 제빙 조성물을 제공하는 것이다.
본 발명의 제3 목적은 모래, 강의 자갈, 탄 재(cinder), 톱밥 또는 기타 미끄럼 방지제(skid-reducing), 가공 자갈(manufactured grit)과 배합하여 사용할 수 있고, 차후에 눈과 얼음이 없는 노면 상태를 유지하고자 하는 도로, 교량, 활주로, 유도로 및 기타 노면에 도포할 수 있는 환경 친화성이 있고, 부식성이 무시할 정도인 제빙 조성물을 제공하는 것이다.
본 발명의 제4 목적은 눈 및 얼음이 도로, 교량 및 기타 옥외 노면에 부착되는 것을 예방하기 위하여 눈이나 얼음이 쌓이기 전에 이들 노면을 예비처리하는 데 사용할 수 있는 환경 친화성 제빙 조성물을 제공하는 것이다.
본 발명의 제5 목적은 기타 화학적 제빙제 및/또는 미끄럼 방지 화학 시약과 배합 또는 혼합하여 사용할 수 있고, 차후에 눈과 얼음이 없는 노면 상태를 유지하고자 하는 도로, 교량, 활주로, 유도로 및 기타 노면에 도포할 수 있는 환경 친화성이 있고, 부식성이 무시할 정도인 제빙 조성물을 제공하는 것이다.
본 발명의 제6 목적은, 도로, 교량, 활주로, 유도로 및 기타 옥외 노면에 얼음과 눈이 존재하지 않도록 하는 방법으로서, 얼음이 얼거나 눈이 오기 전에 상기 노면에 본 발명의 제빙 조성물을 그자체로 도포하거나, 또는 화학적 제빙제 또는 기타 미끄럼 방지 첨가제와의 배합물 또는 혼합물로서 도포하는 단계를 포함하는 방법을 제공하는 것이다.
바람직한 실시 형태의 상세한 설명
본 발명의 제빙 조성물은 껍질을 벗긴 옥수수의 습식 밀링 공정의 부산물이다. 이 습식 밀링 공정은 옥수수유, 덱스트로스, 옥수수 시럽, 과당이 높은 옥수수 시럽, 덱스트린, 건조 전분 및 동물용 사료 등의 스테이플 제품을 생성하기 위하여 흔히 이용된다. 옥수수의 습식 밀링 공정의 주요 단계는 침지 단계, 밀링 단계, 회수 단계 및 가공 처리 단계를 포함한다. 침지 공정 중에, 옥수수 낟알을 극소량의 아황산을 포함하는 고온 용액에 적시므로써 연화시킨다. 이어서, 연화된 낟알을 침지수로부터 분리시킨 다음, 소망하는 최종 생성물에 따라 추가로 가공 처리한다. 잔존 침지수는 가용성 물질을 함유하며, 이 침지수는 증발 및/또는 건조시킨 후에 통상적으로 가금용 사료의 영양 첨가제로서 사용하기 위해 회수한다.
습식 밀링 공정 부산물은 본 발명 조성물의 활성 물질로서 사용된다. 따라서, 본 발명의 제빙 조성물은 배합물 중에 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하고, 상기 조성물은 임의의 첨가제를 더 포함할 수 있다. 임의의 첨가제 물질로는 모래, 강의 자갈, 탄 재, 톱밥 또는 기타 미끄럼 방지제, 가공 자갈 및 기타 화학적 제빙제를 들 수 있다. 본 발명의 조성물은 눈이나 얼음이 없는 도로, 교량 및 기타 노면을 만들고 유지하는데 특히 적합한 동결 방지제 및 제빙제이다. 본 발명의 제빙 조성물은 눈이나 얼음이 노면에 쌓이기 전에 노면을 도포하는 것이 가장 바람직하며, 이러한 도포 공정에 의해 눈과 얼음이 노면에 부착되는 것을 예방할 수 있다. 눈과 얼음이 쌓인 후에는, 본 발명의 제빙 조성물을 다시 도포하되, 이때에는 쌓인 눈 및 얼음에 도포한다. 이러한 2-단계 도포에 의해 제설기 및 기타 기계적 수단을 사용하여 쌓인 눈 및 얼음을 제거하는 것이 용이해진다.
대부분의 지방 행정 당국이 통상 염화물 염과 기타 화학적 결빙 방지제를 대량으로 구입함을 감안하면, 본 발명의 조성물은 염화물 염, 예를 들면 칼슘 마그네슘 아세테이트와 혼합 또는 배합할 수 있음을 예견할 수 있다(염화물 염의 첨가는, 이들 농도에 따라 좌우되기는 하지만, 본 발명의 낮은 부식성 및 환경적 친화성을 열화시킬 수 있음). 지방 행정 당국에서는 이미 대량의 기타 화학 물질을 구입한 이상, 이들을 본 발명의 더욱 효과적이고 더욱 허용성이 있는 조성물과 단지 소량만을 혼합해야 하고, 또 이러한 배합이 환경적 측면에서 바람직하지 못하다는 것이 명백하다 할지라도, 대부분의 지방 행정 당국에서는 이들 화학 물질을 그대로 사용하려 할 것이다.
본 발명의 제빙 조성물은 또한 부식성 염과 혼합될 때 부식 억제제로서 작용한 다. 본 발명 조성물과 염화물 염 5 중량%의 배합물의 부식 효과가 물 95%와 염 5%의 배합물보다 현저히 낮다는 것을 실험을 통해 알 수 있었다. 따라서, 본 발명의 조성물은 이 조성물의 다른 특성에 큰 영향을 미치지 않는 소량의 염과 효과적으로 혼합될 수 있다.
또, 본 발명은 눈과 얼음이 없는 노면을 만드는 방법을 제공하는데, 이 방법은 결빙 또는 눈이 쌓이기 전에 본 발명의 조성물을 노면에 도포하는 것으로 이루어진다. 상기 조성물은 차선 1 마일당 20~60 갤론(GPLM), 즉 차선 1 마일당 200~600 파운드의 함량(평방 야드당 0.48~1.44 온스에 해당함)으로 차량이 이동하는 노면에 도포하는 것이 바람직하다. 또, 상기 조성물은 눈이나 얼음이 쌓인 후에 상기 눈과 얼음을 녹이기 위하여 도포할 수도 있다.
침지수 농축물을 취급, 보관 또는 사용하는 것이 사람, 동물 또는 환경에 위험하다는 것은 알려지지도 확인되지도 않았다. 진한 침지수는 최근에 등급이 낮은 동물용 사료 첨가제로 사용되거나 또는 기타 저가 용도에 사용된다.
또한, 본 발명의 조성물은 눈과 얼음이 활주로 및 유도로에 쌓이는 것을 예방하기 위하여 공항에서 저렴한 비용으로 효과적으로 사용될 수 있다. 요즘 대부분의 공항은 비행기의 날개를 제빙하기 위하여 글리콜과 안정화제를 사용하고, 공항에서는 유거수를 처리하기 위하여 하수 처리 비용을 지불해야만 한다. 이러한 비용은 글리콜로 오염된 물 1 갤론당 최소 3.00 달러가 든다. 이러한 목적에 글리콜 대신 본 발명의 조성물을 사용할 수 있다는 실험 결과를 얻었다. 글리콜을 생략함으로써 글리콜로 오염된 물을 처리하는 최고의 품질 관리 기술을 요하는 공정이 필요없게 되었고, 환경 측면에서도 이롭다.
본 발명에 의한 옥수수 습식 밀링 공정의 침지수 농축물의 대표적인 조성은 하기 표 1에 기재된 바와 같다.
성분 건조 기준(수분 없음) 농축(48% 고형물/52% 수분)
미정제 단백질 33.0% 16.0%
미정제 지방 0.2% 0.1%
산 세척 섬유 0.66% 0.32%
2.31% 1.12%
칼슘 0.02% 0.01%
0.56% 0.27%
칼륨 2.74% 1.32%
마그네슘 1.08% 0.52%
나트륨 0.13% 0.06%
145 ppm 70 ppm
알루미늄 22 ppm 10 ppm
망간 34 ppm 17 ppm
구리 8 ppm 4 ppm
아연 140 ppm 68 ppm
총 재(ash) 27% 5.4~21.68%
본 발명의 조성물의 주 장점을 하기 1) 내지 10)에 요약 제시하였다.
1) 본 발명의 조성물은 허용되지 않을 정도의 부식성을 지니지도 않았고, 환경에 손상을 미치지도 않는다. 이러한 특성은 차량, 도로 및 주변 환경에 손상을 주는 공지의 조성물에 비해 큰 장점이다.
2) 본 발명의 조성물은 빙점이 0℉ 미만이다. 상기 조성물은 +10℉에서 액체 상태이며 자유롭게 유동하고, 주위 온도에서 쌓인 얼음이나 눈 또는 노면에 쉽게 분무 도포될 수 있다. 또한, 상기 조성물은 이들을 도포하기 전에 가열시킬 수 있다.
3) 본 발명의 조성물은 노면에 이미 도포되었기 때문에, 비교적 소량으로 도포될 수 있고, 본 발명의 조성물은 그 자리에 잔존하는 경향이 있으며, 바람이나 차량 통과와 같은 작용에 의해 쉽게 날라가 버리지 않으며, 상기 조성물은 이것이 도포되는 노면에 눈 및 얼음이 부착되는 것을 방지하는 경향이 있다.
4) 본 발명의 조성물은 임의의 통상의 온도에서 및/또는 눈 및 얼음 폭풍우가 임박하기 전에 도포할 수 있다.
5) 본 발명의 조성물은 도포 대원을 특별히 훈련시키지 않고도 통상 사용되는 설비를 이용하여 도로에 용이하게 도포할 수 있다.
6) 본 발명의 조성물은 용액의 형태로 도포할 수 있는데, 용액은 빠르게 도포되며, 심지어 차량으로 35 mph 이상의 속도로 도포할 수 있다.
7) 본 발명의 조성물은 스노우 벨트에 위치한 대부분의 주에서 대량으로 입수할 수 있는 등급이 낮고 가격이 저렴한 산업용 부산물이다. 상기 문제 지역과 근접하다는 이유로 수송 비용이 감소되기 때문에 가격이 낮아져서 잠재 시장에서의 이용가능성에 도움을 준다.
8) 본 발명의 조성물은 재생가능한 농업용 부산물이며, 이것의 시판물의 사용은 미국 농부 및 농업 산업 분야에 도움을 준다.
9) 본 발명의 조성물은 생분해성 물질이며, 생물학적 산소 요구량(BOD)이 낮다. 물질의 BOD는 상기 물질 1 파운드당 필요한 산소의 비율(파운드 단위)을 나타내는 무(無)단위의 숫자이다. 사실상 BOD는 유기체가 풍부한 물질의 호기성 미생물의 대사 요구량을 나타낸다. 대부분의 공지의 제빙제는 생분해성이 아니며(따라서, BOD가 0임), 실지로 이들은 축적되어 환경을 유독하게 만든다. 생분해성인 공지의 한 제빙제는 칼슘 마그네슘 아세테이트(CMA)이지만, 본 발명의 조성물은 CMA보다 실질적으로 낮은 BOD를 가진다.
10) 본 발명의 조성물은 눈 및 얼음이 활주로 및 유도로에 쌓이는 것을 예방하기 위하여 공항에서 저렴한 비용으로 사용할 수 있어서, 환경적으로 친화성이 없다고 알려진 다른 화학 물질 제빙제를 사용할 필요성을 없애거나 또는 더욱 감소시킨다.
시험 개요
본 발명은 하기의 시험 결과를 통해 더욱 상세히 예시하고자 하며, 이들 시험에 사용된 본 발명 조성물의 특정 혼합물에 의해 본 발명의 범위가 국한되는 것은 아니다. 건조 물질 함량 약 50 중량%로 농축시킨 시험용의 밀 작업 침지수를 14℉의 외부 온도에서 임의의 첨가제 없이 약 20 평방 야드의 눈 시이트에 3.5 인치 두께로 도포하였다. 비교용으로, 산업용 염류와 모래의 혼합물을 근처의 약 20 평방 야드의 눈 시이트에 3.5 인치 두께로 제2 도포하였다. 건조 물질의 함량이 50 중량%인 조성물의 용융 효과가 염과 모래의 혼합물의 용융 효과보다 우수하다는 것이 확인되었고, 효과의 지속성과 활성 강도 두가지도 같은 결과를 얻었다. 건조 물질 함량이 50 중량%인 본 발명의 조성물은 염과 모래의 혼합물보다 1 시간 내지 30분 일찍 용융 효과를 나타내었다. 더욱이, 50% 농도의 본 발명 조성물은 7.5℉ 정도의 낮은 온도에서도 활성을 나타내는 반면, 염과 모래 혼합물의 용융 효과는 느렸고, 약 20℉에서는 완전히 중단되었다.
다양한 주위 온도에서 침지수의 농도를 건조 물질 함량 30 중량% 내지 60 중량%로 달리하는 시험을 수행하였다. 이 시험은 결빙되기 전에 결빙 방지용과 결빙 후 제빙용으로 실시하였다. 모든 경우에서 침지수 생성물의 결과는 최근에 사용되는 다른 공지의 제빙제와 같거나 우수하다는 결과를 얻었다.
본 발명의 조성물을 부식, 생물학적 분해 요구 및 다양한 온도에서의 효능에 대하여 평가하기 위하여 추가의 시험을 실시하였다.
부식 시험
마일드(mild) 강철 볼트를 다양한 농도의 침지수에 침지시켰다. 침지한 지 4 개월 후에, 상기 볼트를 육안으로 검사한 결과 녹 또는 산화 흔적이 발견되지 않았다. 실험실 부식 시험으로 부식 효과가 1년당 0.53 mil로 측정되었고, 이 수치는 다른 화학적 제빙제에 비해 매우 낮은 수치이며, 순수한 물의 부식도보다 작았다.
다양한 농도의 침지수로 마일드 강철 볼트를 정규적으로 분무하였다. 정규적인 분무를 행한지 4 개월 후에, 볼트를 육안 검사한 결과 녹 또는 산화의 흔적을 발견하지 못하였다. 부식이 일어나는 대신, 상기 볼트는 건조된 침지수의 층으로 밀봉된 것으로 보이며, 이 막에 의해 분해되기 보다는 오히려 보호되는 것으로 보인다.
이 시험 결과를 하기 표 2에 나타내었다.
시험 재료 부식량 (mil/년-MPY)
마일드 강철 0.50
스텐레스 강철 검출되지 않음
알루미늄 검출되지 않음
비교용으로, 마일드 강철 볼트를 전술한 것과 유사한 시험 조건으로 처리하되, 물과 5% 농도의 각종 염화물 염의 혼합물을 사용하였다. 그 결과 극심한 부식, 녹 및 불량화가 관찰되었다.
환경 시험
본 발명 조성물의 각종 혼합물 1 파운드당 생물학적 산소 요구량(파운드 단위)을 측정하기 위하여 본 시험을 실시하였다. BOD는 유기체의 호기성 미생물의 대사 요구량을 나타낸다. 결과는 하기 표 3에 나타내었다.
농도(중량) BOD 요구량(물질 1 파운드당 O2의 파운드)
25% (고체 함량) 0.13~0.15
48% (고체 함량) 0.21~0.26
본 발명의 조성물은 현재 등급이 낮은 동물 사료 첨가제로 사용된다. 이들이 가금 산업 분야에서 널리 받아들여지고 있고, 사육되는 동물에 임의의 유해량의 유해 물질을 남기는 것으로 알려지지 않았기 때문에, 상기 조성물은 환경적 측면에서 완전히 안전하고, 취급에 있어서도 안전한 것으로 간주된다.
동결, 제빙 및 결빙 방지 시험
하기 표 4에는 48%(고체 함량)로 농축된 본 발명 혼합물의 점성(consistency)을 나타내었다.
온도(℉) 상태
+20 자유 유동하는 액체
+10 묽은 시럽
0 진한 당밀(molasses)
-20 진한 퍼티형(putty-like)
하기 표 5에는 약 50%의 가용성 물질을 포함하는 통상의 밀 작업 침지수 용액에 대한 빙점과 많은 정보를 나타내었다.
상기 표에서 나타낸 바와 같이, 염화물 염의 용융 효과는 제한되었고(약 20℉ 이하에서 효과 없음), 본 발명 조성물의 용융 효과는 7.5℉ 정도의 낮은 온도에서도 유효하였다.

Claims (24)

  1. 생분해성의 침지수 가용성 물질을 포함하는 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 조성물.
  2. 제1항에 있어서, 염화나트륨, 염화칼슘, 염화칼륨, 염화마그네슘, 칼슘 마그네슘 아세테이트 및 우레아로 이루어진 군에서 선택되는 1종 이상의 성분을 더 포함하는 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 조성물.
  3. 제1항에 있어서, 상기 침지수 가용성 물질이 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 조성물.
  4. 침지수 가용성 물질을 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 조성물.
  5. 제4항에 있어서, 미끄럼 방지용 골재를 더 포함하는 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 조성물.
  6. 제4항에 있어서, 염화나트륨, 염화칼슘, 염화칼륨, 염화마그네슘, 칼슘 마그네슘 아세테이트 및 우레아로 이루어진 군에서 선택되는 1종 이상의 성분을 더 포함하는 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 조성물.
  7. 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 동결 방지 및 제빙(除氷) 조성물.
  8. 침지수 가용성 물질을 포함하는 조성물을 옥외 노면 또는 그 위에 쌓인 눈 및 얼음에 차선 1 마일당 20 내지 60 갤론의 비율로 도포하는 단계를 포함하는 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 방법.
  9. 제8항에 있어서, 상기 조성물이 염화나트륨, 염화칼슘, 염화칼륨, 염화마그네슘, 칼슘 마그네슘 아세테이트 및 우레아로 이루어진 군에서 선택되는 1종 이상의 성분을 더 포함하는 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 방법.
  10. 제8항에 있어서, 상기 조성물이 모래, 강의 자갈, 탄 재(cinder), 톱밥 및 가공 자갈(manufactured grit)로 이루어진 군에서 선택되는 1종 이상의 성분을 포함하는 미끄럼 방지용 골재를 더 포함하는 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 방법.
  11. (1) 미끄럼 방지용 골재와, (2) 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%의 배합물과의 혼합물을 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 동결 방지 및 제빙 조성물.
  12. 제11항에 있어서, 미끄럼 방지용 골재가 모래, 강의 자갈, 탄 재, 톱밥 및 가공 자갈로 이루어진 군에서 선택되는 1종 이상의 성분을 포함하는 것이 특징인 동결 방지 및 제빙 조성물.
  13. (1) 염화나트륨, 염화칼슘, 염화칼륨, 염화마그네슘, 칼슘 마그네슘 아세테이트 및 우레아로 이루어진 군에서 선택되는 1종 이상의 성분과, (2) 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%의 배합물과의 혼합물을 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 도로에 눈 및 얼음이 쌓이는 것을 방지하기 위한 동결 방지 및 제빙 조성물.
  14. 제13항에 있어서, 상기 1종 이상의 성분이 염화나트륨인 것이 특징인 동결 방지 및 제빙 조성물.
  15. 제13항에 있어서, 상기 1종 이상의 성분이 칼슘 마그네슘 아세테이트인 것이 특징인 동결 방지 및 제빙 조성물.
  16. 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하는 조성물을 옥외 노면 또는 그 위에 쌓인 눈 및 얼음에 차선 1 마일당 20 내지 60 갤론의 비율로 도포하는 단계를 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 방법.
  17. 제16항에 있어서, 상기 조성물이 염화나트륨, 염화칼슘, 염화칼륨, 염화마그네슘, 칼슘 마그네슘 아세테이트 및 우레아로 이루어진 군에서 선택되는 1종 이상의 성분을 더 포함하는 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 방법.
  18. 제16항에 있어서, 상기 조성물이 모래, 강의 자갈, 탄 재, 톱밥 및 가공 자갈로 이루어진 군에서 선택되는 1종 이상의 성분을 포함하는 미끄럼 방지용 골재를 더 포함하는 것이 특징인, 옥외 노면에 눈 및 얼음이 쌓이는 것을 방지하기 위한 방법.
  19. 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 부식 억제 조성물.
  20. 염화물 염의 부식 효과를 억제하기 위한 부식 억제 조성물로서, 상기 조성물은 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하며, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 부식 억제 조성물.
  21. 제20항에 있어서, 상기 염화물 염이 염화나트륨, 염화칼슘, 염화칼륨 및 염화마그네슘으로 이루어진 군에서 선택되는 것이 특징인 부식 억제 조성물.
  22. 염화나트륨의 부식 효과를 억제하기 위한 부식 억제 조성물로서, 상기 조성물은 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하며, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 부식 억제 조성물.
  23. 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 동결 방지 조성물.
  24. 침지수 가용성 물질 14~80 중량%와 물 20~86 중량%를 포함하고, 상기 침지수 가용성 물질은 옥수수의 습식 밀링 공정 중에 형성된 물질인 것이 특징인, 눈 및 얼음이 쌓이는 것을 방지하기 위한 제빙 조성물.
KR1019980705597A 1996-01-22 1997-01-21 제빙(除氷) 조성물 및 제빙 방법 KR19990081885A (ko)