KR101256010B1 - Method for remodeling inner wall or outer wall of building using three-dimensional pattern board - Google Patents

Method for remodeling inner wall or outer wall of building using three-dimensional pattern board Download PDF

Info

Publication number
KR101256010B1
KR101256010B1 KR1020120048389A KR20120048389A KR101256010B1 KR 101256010 B1 KR101256010 B1 KR 101256010B1 KR 1020120048389 A KR1020120048389 A KR 1020120048389A KR 20120048389 A KR20120048389 A KR 20120048389A KR 101256010 B1 KR101256010 B1 KR 101256010B1
Authority
KR
South Korea
Prior art keywords
board
weight
building
dimensional
dimensional pattern
Prior art date
Application number
KR1020120048389A
Other languages
Korean (ko)
Inventor
신경환
이상현
Original Assignee
주식회사 이파엘지종합특수방수
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 이파엘지종합특수방수 filed Critical 주식회사 이파엘지종합특수방수
Priority to KR1020120048389A priority Critical patent/KR101256010B1/en
Application granted granted Critical
Publication of KR101256010B1 publication Critical patent/KR101256010B1/en

Abstract

PURPOSE: A method for remodeling the inner or outer walls of a building using a three-dimensional patterned board are provided to improve the construction environment of a building, to reduce the time and cost for remodeling construction, and to improve the external appearance of the building by attaching three-dimensional patterned boards on the outer wall when remodeling the deteriorated building. CONSTITUTION: A method for remodeling the inner or outer walls of a building using a three-dimensional patterned board comprise the following steps of: directly applying a primer on a board and forming a three-dimensional pattern on the board by free falling a pattern source with an artistic intent of the manufacturer(S121); and attaching the board on the outer wall of a building using epoxy putty(S122). [Reference numerals] (S121) Freely dropping three-dimensional pattern materials on a board by a manufacturer with an artistic intent to form a three-dimensional pattern; (S122) Attaching the board formed with the three-dimensional pattern to a building wall;

Description

입체문양보드를 이용한 건물 내외벽 리모델링 공법{Method for remodeling inner wall or outer wall of building using three-dimensional pattern board}Method for remodeling inner wall or outer wall of building using three-dimensional pattern board}

본 발명은 입체문양보드를 이용한 건물 내외벽 리모델링 공법에 관한 것으로, 보다 상세하게는 소비자의 취향에 따라 보드에 전통문양이나 캐릭터와 같이 다양한 입체문양을 성형하여 건물 내외벽에 시공함으로써 리모델링 건물의 미관이 미려하고 리모델링으로 인한 건물의 가치를 상승시킬 수 있는 입체문양보드를 이용한 건물 내외벽 리모델링 공법에 관한 것이다.The present invention relates to a building interior and exterior wall remodeling method using a three-dimensional glyph board, and more specifically, by forming a variety of three-dimensional patterns like traditional patterns or characters on the board according to the taste of the consumer to construct the interior and exterior walls of the building remodeling The interior and exterior wall remodeling method using a three-dimensional glyph board that can increase the value of the building due to this beautiful and remodeling.

최근 건물이 노후화됨에 따라 기존의 건물을 해체한 후 다시 새로운 건물을 짓거나 건물의 일정 부분만을 해체하여 보수하는 작업이 많이 행해지고 있다. 일반적으로, 리모델링이라 함은 신축에 대비되는 개념으로 기존 건축물의 유지, 보수나 증축, 개축 등을 포함하는 광의의 개념으로서, 건축분야의 재활용 프로젝트를 뜻하는 신축에 대비되는 개념으로서 기존의 건축물을 새롭게 디자인하는 개보수의 모든 작업을 일컫는다. 즉, 기존의 건축물을 손봐서 새 건물처럼 사용할 수 있도록 하는 모든 작업을 의미하는 것으로, 신축이나 재건축과 구별되며 현행 건축법에 따르면 증축, 개축, 대수선으로 정의할 수 있다.Recently, as the building is getting older, there is a lot of work to rebuild a new building after dismantling the existing building or dismantle only a part of the building. In general, remodeling is a concept in preparation for new construction. It is a broad concept including maintenance, repair, extension, and reconstruction of an existing building. It refers to all the work of renovation. In other words, it means all works that can use existing buildings as new buildings, and are distinguished from new construction or reconstruction, and can be defined as extension, reconstruction, and algebra according to the current building law.

건물을 리모델링하는 공법에는 여러 가지가 있으나, 리모델링 작업시에 건물의 벽면을 철거한다거나 페인트 칠을 하는 등의 공정이 이루어지는 것이 대부분이기 때문에 필연적으로 소음을 유발하고 분진 등이 발생된다. 특히 리모델링의 대상이 되는 건물이 도심지나 주택가 등에 위치하는 경우 건물의 리모델링 과정에서 발생되는 소음 및 분진으로 인하여 주변 건물에 피해를 주며, 이에 대한 민원이 발생하여 공사 소요기간의 지연 원인으로 작용할 수 있다.There are many methods for remodeling a building, but most of the processes such as dismantling or painting walls of buildings during remodeling work inevitably generate noise and generate dust. Especially, if the building to be remodeled is located in downtown area or residential area, it causes damages to nearby buildings due to noise and dust generated in the remodeling process of the building, .

또한 건물의 리모델링 시에 발생하는 콘크리트 파편이 건물의 외부로 튈 경우 주변 건물이나 행인, 차량 등에 피해를 줄 수 있으므로 리모델링 작업은 매우 세심한 주의를 요한다. 이에 사람들이 주거문화에 대한 기대치가 증감함에 따라 리모델링에 대한 수요가 증가하고 있고, 동시에 타인의 삶이나 주변 환경에 영향을 주지 않으면서 리모델링 공사를 진행할 수 있는 공법이나 구조물에 대한 필요가 대두되고 있다.In addition, the remodeling work requires very careful attention as concrete debris generated during the remodeling of the building may damage the surrounding buildings, pedestrians, and vehicles. As people's expectations about residential culture increase, the demand for remodeling increases, and at the same time, there is a need for construction methods and structures that can be remodeled without affecting the lives of others or the surrounding environment. .

이러한 점들을 개선하기 위하여 리모델링 방법으로 최근에 벽체에 직접 보드나 시트를 설치하여 공사의 간편화, 공사의 환경개선화, 공사비용 절감, 공사기간 단축되어 시공되고 있는 장점이 있으나 이러한 시공법은 너무 밋밋하고 획일적인 리모델링 공법으로 미관이 좋지 않다.In order to improve these points, the remodeling method has recently installed boards or sheets directly on the walls to simplify construction, improve the environment, reduce construction costs, and shorten the construction period. However, these construction methods are too flat. The uniform remodeling method does not look good.

한편, 특허등록공보 제10-0950040호에서 섬유시트를 제작하는 공정이 복잡하여 제작기간이 많이 걸리고, 문양을 정형화할 수 없고 시공하려면 숙련된 기술이 요구되고, 입체문양 성형재료가 단순하여 다양한 종류의 재료가 요구되며, 시트를 벽체에 부착하기 어려운 문제점이 있었다.On the other hand, in the Patent Registration Publication No. 10-0950040, the process of manufacturing the fiber sheet is complicated, it takes a lot of production period, the pattern can not be standardized, it requires skilled skills to construct, the three-dimensional pattern molding material is simple and various kinds The material is required, there was a problem that is difficult to attach the sheet to the wall.

한국등록특허공보 제10-0950040호(등록일: 2010.03.22)Korea Patent Publication No. 10-0950040 (Registration Date: 2010.03.22)

본 발명은 상기와 같은 문제점을 해결하고자 제안된 것으로, 본 발명의 목적은 소비자의 취향에 따라 보드에 전통문양이나 캐릭터와 같이 다양한 입체문양을 성형하여 건물 내외벽에 시공함으로써 리모델링 건물의 미관이 미려하고 리모델링으로 인한 건물의 가치를 상승시킬 수 있는 입체문양보드를 이용한 건물 내외벽 리모델링 방법을 제공하는 것이다. The present invention has been proposed to solve the above problems, the object of the present invention is to form a variety of three-dimensional patterns, such as traditional patterns or characters on the board according to the taste of the consumer by constructing on the interior and exterior walls of the building beautiful beauty And it is to provide a remodeling method of the interior and exterior walls using a three-dimensional glyph board that can increase the value of the building due to the remodeling.

본 발명의 다른 목적은 건축물의 리모델링시 공사기간 단축, 공사환경 개선, 공사비용 최소화하고 외적인 미관을 향상시켜 건물의 개성미를 부여할 수 있는 입체문양보드를 이용한 건물 내외벽 리모델링 방법을 제공하는 것이다.Another object of the present invention is to provide a remodeling method of the interior and exterior walls using a three-dimensional glyph board that can give a personality of the building by shortening the construction period, improving the construction environment, minimizing the construction cost and improving the external aesthetics.

상기와 같은 목적을 달성하기 위하여, 본 발명의 일 양상에 따른 입체문양보드를 이용한 건물 내외벽 리모델링 공법은, 제작자의 예술적인 기법을 살려서 직접 프라이머를 보드에 도포하고 입체문양재료를 낙하하여 보드에 입체문양을 형성하는 단계, 및 입체문양이 형성된 보드를 건물 벽체에 부착하는 단계를 포함한다.In order to achieve the above object, the building interior and exterior wall remodeling method using a three-dimensional pattern board according to an aspect of the present invention, by applying the manufacturer's artistic techniques directly onto the board and drop the three-dimensional pattern material on the board Forming a three-dimensional pattern, and attaching the three-dimensional patterned board to the building wall.

본 발명의 다른 양상에 따른 입체문양보드를 이용한 건물 내외벽 리모델링 공법은, 점착시트지에 디지털 프린팅 기계를 이용하여 고객이 주문한 문양을 프린팅하고, 문양이 프린팅된 점착시트지를 보드에 접합한 후에, 보드와 접착된 점착시트지의 문양에 프라이머를 도포하고 입체문양재료를 시공하는 단계, 입체문양이 형성된 보드를 건물 벽체에 부착하는 단계를 포함한다.Building interior and exterior wall remodeling method using a three-dimensional pattern board according to another aspect of the present invention, after printing the pattern ordered by the customer using a digital printing machine on the adhesive sheet, and bonded the adhesive sheet of the pattern printed on the board, And applying a primer to a pattern of the adhesive sheet attached to the sheet and constructing a three-dimensional pattern material, and attaching the board on which the three-dimensional pattern is formed to the building wall.

상기 입체문양재료는 무광택용인 무기아크릴도막제 또는 광택용인 무용제우레탄도막제로 구현되며, 무광택용인 무기아크릴도막제는 유리전이온도(Tg) -5℃, 고형분45중량%, 점도 3000cps인 수용성아크릴에멀젼 30∼40중량%, 빠른건조와 도막경화를 위해 알루미나시멘트 18∼25중량%, 색소 3∼5중량%, 규사6∼8호사 23∼30중량%, 옥분말 15∼20중량%, 유동화제 0.4∼1중량%, 분산제 0.4∼1중량%, 소포제 0.1∼0.3중량%, 증점제0.1∼0.5중량%이며 이때 점도는 7000cps이고,The three-dimensional pattern material is embodied as an inorganic acrylic coating agent for matting or a solvent-free urethane coating agent for gloss, and the inorganic acrylic coating agent for matting is a glass transition temperature (Tg) -5 ° C, a solid content of 45% by weight, and a viscosity of 3000 cps. -40% by weight, 18-25% by weight of alumina cement, 3-5% by weight of dye, 3-30% by weight of silica sand, 23-30% by weight of silica sand 6-8, 15-20% by weight of jade powder, 0.4 ~ 1% by weight, dispersant 0.4-1% by weight, antifoam 0.1-0.3% by weight, thickener 0.1-0.5% by weight, with a viscosity of 7000 cps,

상기 광택용인 무용제우레탄도막제는 가지화 폴리에테르-폴리에스테르 폴리올(branched polyether-polyester polyol) 30∼40중량%, 경화제 헥사메틸렌디이소시아네이트(HMDI) 11∼20중량%, 색소 3.4∼5중량%, 희석제 5.5∼10중량%, 필러는 옥분말 20∼30중량%, 규사6∼8호사 20∼30중량%, 소포제 0.1∼0.3 중량%로 구성되며 이때 점도는 8500cps인 것을 특징으로 한다.The solvent-free urethane coating agent for the gloss is 30-40% by weight of branched polyether-polyester polyol, 11-20% by weight of a curing agent hexamethylene diisocyanate (HMDI), 3.4-5% by weight of a pigment, Diluent 5.5 to 10% by weight, filler is composed of 20 to 30% by weight of jade powder, 20 to 30% by weight of silica sand 6-8, antifoaming agent 0.1 to 0.3% by weight, the viscosity is characterized in that 8500cps.

상기 보드는 CRC보드, 마그네슘 보드, 규산 칼슘 보드, FC 보드(화이바 시멘트 보드), 금속보드, 플라스틱보드, 유리보드, 합판 및 시멘트 보드 중 어느 하나인 것을 특징으로 한다. The board is characterized in that any one of the CRC board, magnesium board, calcium silicate board, FC board (fiber cement board), metal board, plastic board, glass board, plywood and cement board.

상기와 같은 구성에 따르면 노후화된 건물의 리모델링을 위하여 벽체에 입체문양보드를 부착시킴으로서 미려한 외관을 나타낼 수 있는 유용한 효과가 있다. According to the above configuration, by attaching a three-dimensional pattern board to the wall for the remodeling of the aging building has a useful effect that can exhibit a beautiful appearance.

또한, 건축물의 리모델링시 공사기간 단축, 공사비용 절감, 공사환경개선 및 미관을 향상시켜 건물에 가치를 증가 할 수 있는 효과가 있다. In addition, there is an effect that can increase the value of the building by shortening the construction period, reducing construction costs, improving the construction environment and aesthetics when remodeling the building.

도 1 은 본 발명에 따른 입체문양보드를 제조하는 과정을 설명하기 위한 예시도,
도 2 는 본 발명에 따른 입체문양보드를 제조하는 과정을 설명하기 위한 다른 예시도,
도 3 은 본 발명의 일 실시예에 따른 입체문양보드 일예,
도 4 는 본 발명의 작업 순서 흐름도,
도 5 는 건물 외벽에 입체문양보드를 시공하기 전과 시공 후의 모습을 나타낸 참조도,
도 5 는 건물 내벽에 입체문양보드를 시공한 후의 모습을 나타낸 참조도이다.
1 is an exemplary view for explaining a process of manufacturing a three-dimensional pattern board according to the present invention,
Figure 2 is another exemplary view for explaining the process of manufacturing a three-dimensional pattern board according to the present invention,
Figure 3 is an example of a three-dimensional pattern board according to an embodiment of the present invention,
4 is a flowchart of a work flow of the present invention;
5 is a reference diagram showing the state before and after the construction of the three-dimensional pattern board on the building exterior wall,
5 is a reference diagram showing the state after the construction of the three-dimensional pattern board on the inner wall of the building.

이하, 첨부된 도면을 참조하여 전술한, 그리고 추가적인 양상을 기술되는 바람직한 실시예를 통하여 본 발명을 당업자가 용이하게 이해하고 재현할 수 있도록 상세히 설명하기로 한다. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Reference will now be made in detail to the present embodiments of the present invention, examples of which are illustrated in the accompanying drawings, wherein like reference numerals refer to the like elements throughout.

도 1, 2는 본 발명의 작업 순서에 따라 입체문양보드를 제조하는 과정을 설명하기 위한 예시도이고, 도 3 은 본 발명의 일 실시예에 따른 입체문양보드이다.1 and 2 is an exemplary view for explaining a process of manufacturing a three-dimensional pattern board according to the working order of the present invention, Figure 3 is a three-dimensional pattern board according to an embodiment of the present invention.

먼저, 단계 S111은 점착시트지에 디지털 프린팅 기계를 이용하여 고객이 주문한 문양을 프린팅하고 문양부분에 시트를 제거하는 단계이다. 문양은 소비자의 취향에 따라 전통문양이나 캐릭터와 같이 다양한 입체문양이 가능하다. 단계 S112는 문양이 프린팅된 점착시트지를 보드에 접합하는 단계이다. First, step S111 is a step of printing a pattern ordered by the customer using a digital printing machine on the adhesive sheet and removing the sheet on the pattern portion. The pattern can be a variety of three-dimensional patterns, such as traditional patterns or characters, depending on the taste of the consumer. Step S112 is a step of bonding the printed adhesive sheet paper on the board.

단계 S113은 보드에 접합된 점착시트지의 문양에, 프라이머를 도포하여 건조되면 입체문양재료를 문양에 떨어뜨려 시공하고 점착시트지를 제거하는 단계이다. 이때 시공 두께는 0.3∼3mm이다.Step S113 is a step of applying the primer to the pattern of the adhesive sheet paper bonded to the board, and drying the three-dimensional pattern material on the pattern to dry and remove the adhesive sheet paper. At this time, the construction thickness is 0.3 to 3 mm.

본 발명에서 사용되는 프라이머는 보드와 입체문양재료의 부착성을 증가시키주는 기능을 하며 프라이머의 성분은 수성아크릴에멀젼이며, 수성아크릴에멀젼은 유리전이온도(Tg)가 -5℃이고, 점도가 300cps, 고형분 12.5중량%인 것을 특징으로 한다.The primer used in the present invention functions to increase the adhesion between the board and the three-dimensional pattern material, the component of the primer is an aqueous acrylic emulsion, the aqueous acrylic emulsion has a glass transition temperature (Tg) of -5 ℃, viscosity of 300cps And 12.5% by weight of solid content.

그리고 본 발명에 사용되는 입체문양재료는 친환경적 제품이고, 건조가 빠르고, 도막이 형성되면 갈라짐이 없어야 하며, 도막이 빨리 경화되어 보드에 setting되어야 하며, 도막을 시공하기에 적당한 점도를 갖는 것이 바람직하다. 일례로, 본 발명에 사용되는 입체문양재료는 무광택용 무기아크릴도막제와 광택용 무용제우레탄도막제를 사용할 수 있다.And the three-dimensional pattern material used in the present invention is an environmentally friendly product, fast drying, there should be no cracks when the coating film is formed, the coating film should be cured quickly and set on the board, it is preferable to have a suitable viscosity for the coating film. As an example, the three-dimensional pattern material used for this invention can use the inorganic acrylic coating agent for matte and the solvent-free urethane coating agent for glossiness.

무광택용인 무기아크릴도막제는 유리전이온도(Tg) -5℃, 고형분45중량%, 점도3000cps인 수용성아크릴에멀젼 30∼40중량%, 빠른건조와 도막경화를 위해 알루미나시멘트 18∼25중량%, 색 소3∼5중량%, 규사6∼8호사 23∼30중량%, 옥분말 15∼20중량%, 유동화제 0.4∼1중량%, 분산제 0.4∼1중량%, 소포제 0.1∼0.3중량%, 증점제0.1∼0.5중량%이며 이때 점도는 7000cps이다.Inorganic acrylic coating film for matting is glass transition temperature (Tg) -5 ℃, solid content 45% by weight, water soluble acrylic emulsion with viscosity 3000cps 30-40% by weight, alumina cement 18-25% by weight for quick drying and coating hardening, color Small 3-5 weight%, silica sand 6-8 No. 23-30 weight%, jade powder 15-20 weight%, glidant 0.4-1 weight%, dispersant 0.4-1 weight%, defoaming agent 0.1-0.3 weight%, thickener 0.1 0.5 wt% with a viscosity of 7000 cps.

그리고 광택용인 무용제우레탄도막제는 가지화 폴리에테르-폴리에스테르 폴리올(branched polyether-polyester polyol) 30∼40중량%, 경화제 헥사메틸렌디이소시아네이트(HMDI) 11∼20중량%, 색소 3.4∼5중량%, 희석제 5.5∼10중량%, 필러는 옥분말 20∼30중량%, 규사6∼8호사 20∼30중량%, 소포제 0.1∼0.3 중량%로 구성되며 이때 점도는 8500cps이다. Solvent-free urethane coating agent for gloss is 30-40% by weight of branched polyether-polyester polyol, 11-20% by weight of hardener hexamethylene diisocyanate (HMDI), 3.4-5% by weight of pigment, The diluent is 5.5 to 10% by weight, the filler is composed of 20 to 30% by weight of jade powder, 20 to 30% by weight of silica sand 6-8, and 0.1 to 0.3% by weight of an antifoaming agent with a viscosity of 8500 cps.

상기 입체문양재료의 도막 두께는 0.3∼3mm이며 규사의 크기에 따라 0.3∼1mm는 규사 8호사, 1∼2mm는 규사 7호사, 2∼3mm는 규사 6호사를 사용하는 것을 특징으로 한다.The film thickness of the three-dimensional pattern material is 0.3 to 3mm, depending on the size of the silica sand is characterized in that the use of silica sand 8 yarn, 1 to 2 mm silica sand 7 yarn, 2 to 3 mm silica sand 6 yarn.

단계 S114는 입체문양이 형성된 보드를 건물 벽체에 에폭시 퍼티를 사용하여 부착하는 단계이다. 일례로, 보드는 CRC보드, 마그네슘 보드, 규산 칼슘 보드, FC 보드 (화이바 시멘트 보드), 금속보드, 플라스틱보드, 유리보드 및 시멘트 보드 중 어느 하나로 구현될 수 있다. Step S114 is a step of attaching the three-dimensional patterned board to the building wall using an epoxy putty. For example, the board may be implemented as any one of a CRC board, magnesium board, calcium silicate board, FC board (fiber cement board), metal board, plastic board, glass board and cement board.

도 2 는 도 1의 단계 S111, S112, S113 단계를 생략하고 보드에 직접 프라이머를 도포하고 입체문양재료를 낙하하는 단계이다. 단계 S121은 보드에 제작자가 예술적인 의도를 가지고 입체문양재료를 자유롭게 낙하시켜서 입체문양을 형성하는 단계이다. 문양은 소비자의 취향에 따라 전통문양이나 캐릭터와 같이 다양한 입체문양이 가능하다. 2 is a step of applying a primer directly to the board and dropping the three-dimensional pattern material omitting the steps S111, S112, S113 of FIG. Step S121 is a step for forming a three-dimensional pattern by freely dropping the three-dimensional pattern material with the artistic intention on the board. The pattern can be a variety of three-dimensional patterns, such as traditional patterns or characters, depending on the taste of the consumer.

단계 S122는 입체문양이 형성된 보드를 건물 벽체에 에폭시 퍼티를 사용하여 부착하는 단계이다. 일례로, 보드는 CRC보드, 마그네슘 보드, 규산 칼슘 보드, FC 보드 (화이바 시멘트 보드), 금속보드, 플라스틱보드, 유리보드 및 시멘트 보드 중 어느 하나로 구현될 수 있다. Step S122 is a step of attaching the three-dimensional patterned board to the building wall using an epoxy putty. For example, the board may be implemented as any one of a CRC board, magnesium board, calcium silicate board, FC board (fiber cement board), metal board, plastic board, glass board and cement board.

도 4 는 건물 외벽에 입체문양보드를 시공하기 전과 시공 후의 모습을 나타낸 참조도이고, 도 5 는 건물 내벽에 입체문양보드를 시공한 후의 모습을 나타낸 참조도이다. 4 is a reference diagram showing the state before and after the construction of the three-dimensional pattern board on the building outer wall, Figure 5 is a reference diagram showing the state after the construction of the three-dimensional pattern board on the building inner wall.

도 1 과 같이 본 실시예에 따라 도 4와 도 5를 통하여 알 수 있듯이 크랙이 발생하고 오염이 심하게 된 건물 외벽과 내벽에 간단한 공정으로 짧은 기간 안에 저렴한 비용으로 시공할 수 있으며 이렇게 시공된 건물 외벽은 방수, 방오 및 광택이 매우 뛰어난 것을 알 수 있다.As can be seen from Figures 4 and 5 according to the present embodiment as shown in Figure 1 can be installed at a low cost in a short period of time by a simple process to the building outer wall and inner wall cracking and severely polluted building outer wall thus constructed It can be seen that silver is very waterproof, antifouling and gloss.

본 실시예에 따라 시공된 건물 외벽과 내벽은 미술작품과 같은 입체문양이 표현되어짐으로서, 각각의 건물에 대한 다양한 개성미를 넣어줄 뿐만 아니라 미관을 향상시켜줄 수 있게 된다.
The outer wall and the inner wall of the building constructed in accordance with the present embodiment is represented by a three-dimensional pattern, such as a work of art, it is possible to not only put a variety of personality for each building, but also improve the aesthetics.

지금까지, 본 명세서에는 본 발명이 속하는 기술 분야에서 통상의 지식을 지닌 자가 본 발명을 용이하게 이해하고 재현할 수 있도록 도면에 도시한 실시예들을 참고로 설명되었으나 이는 예시적인 것에 불과하며, 당해 기술분야에 통상의 지식을 지닌 자라면 본 발명의 실시예들로부터 다양한 변형 및 균등한 타 실시예가 가능하다는 점을 이해할 것이다. 따라서 본 발명의 진정한 기술적 보호범위는 첨부된 특허청구범위에 의해서만 정해져야 할 것이다.
Thus far, the present specification has been described with reference to the embodiments shown in the drawings so that those skilled in the art to which the present invention pertains can easily understand and reproduce the present invention. Those skilled in the art will understand that various modifications and equivalent other embodiments are possible from the embodiments of the present invention. Therefore, the true technical protection scope of the present invention should be defined only by the appended claims.

Claims (6)

점착시트지에 디지털 프린팅 기계를 이용하여 문양을 프린팅하는 단계;
상기 문양이 프린팅된 점착시트지를 보드에 접합하는 단계;
상기 보드와 접착된 점착시트지의 문양에 프라이머를 도포하고 입체문양재료를 시공하여 상기 보드에 입체문양을 형성하는 단계; 및
상기 입체문양이 형성된 보드를 건물 벽체에 부착하는 단계;를 포함하되,
상기 입체문양재료는 무광택용인 무기아크릴도막제 또는 광택용인 무용제우레탄도막제로 구현되는 입체문양보드를 이용한 건물 내외벽 리모델링 공법.
Printing a pattern on a pressure sensitive adhesive sheet using a digital printing machine;
Bonding the patterned adhesive sheet to a board;
Forming a three-dimensional pattern on the board by applying a primer to the pattern of the adhesive sheet paper bonded to the board and constructing a three-dimensional pattern material; And
And attaching the board on which the three-dimensional pattern is formed to a building wall.
The three-dimensional glyph material is a building interior and exterior wall remodeling method using a three-dimensional glyph board implemented with a matt inorganic inorganic acrylic coating or a solvent-free urethane coating.
청구항 1에 있어서,
상기 프라이머는 보드와 입체문양재료의 부착성을 증가시키며, 상기 프라이머의 성분은 수성아크릴에멀젼이며, 상기 수성아크릴에멀젼은 유리전이온도(Tg)가 -5℃이고, 점도가 300cps, 고형분 12.5중량%인 것을 특징으로 하는 입체문양보드를 이용한 건물 내외벽 리모델링 공법.
The method according to claim 1,
The primer increases the adhesion between the board and the three-dimensional pattern material, the component of the primer is an aqueous acrylic emulsion, the aqueous acrylic emulsion has a glass transition temperature (Tg) of -5 ℃, viscosity of 300cps, solids 12.5% by weight Building interior and exterior walls remodeling method using a three-dimensional pattern board, characterized in that.
청구항 1에 있어서,
상기 보드는 CRC보드, 마그네슘 보드, 규산칼슘 보드, FC 보드, 금속보드, 플라스틱보드, 유리보드, 합판 및 시멘트 보드 중 어느 하나인 것을 특징으로 하는 입체문양보드를 이용한 건물 내외벽 리모델링 공법.
The method according to claim 1,
Wherein the board is a CRC board, magnesium board, calcium silicate board, FC board, metal board, plastic board, glass board, plywood and cement board any one of the interior and exterior wall remodeling method using a three-dimensional pattern board.
청구항 1에 있어서,
상기 무광택용인 무기아크릴도막제는 유리전이온도(Tg) -5℃, 고형분45중량%, 점도3000cps인 수용성아크릴에멀젼 30∼40중량%, 빠른건조와 도막경화를 위해 알루미나시멘트 18∼25중량%, 색소 3∼5중량%, 규사6∼8호사 23∼30중량%, 옥분말 15∼20중량%, 유동화제 0.4∼1중량%, 분산제 0.4∼1중량%, 소포제 0.1∼0.3중량%, 증점제 0.1∼0.5중량%이며 이때 점도는 7000cps이고,
상기 광택용인 무용제우레탄도막제는 가지화 폴리에테르-폴리에스테르 폴리올(branched polyether-polyester polyol) 30∼40중량%, 경화제 헥사메틸렌디이소시아네이트(HMDI) 11∼20중량%, 색소 3.4∼5중량%, 희석제 5.5∼10중량%, 필러는 옥분말 20∼30중량%, 규사6∼8호사 20∼30중량%, 소포제 0.1∼0.3 중량%로 구성되며 이때 점도는 8500cps인 것을 특징으로 하는 입체문양보드를 이용한 건물 내외벽 리모델링 공법.
The method according to claim 1,
The inorganic acrylic coating agent for the matte glass transition temperature (Tg) -5 ℃, solid content 45% by weight, water soluble acrylic emulsion 30-40% by weight of viscosity 3000cps, alumina cement 18-25% by weight for fast drying and coating film curing, 3 to 5% by weight of dye, 3 to 5% by weight of silica sand 6 to 8, 15 to 20% by weight of jade powder, 0.4 to 1% by weight of fluidizing agent, 0.4 to 1% by weight of dispersant, 0.1 to 0.3% by weight of antifoaming agent, thickener 0.1 -0.5 wt% with a viscosity of 7000 cps,
The solvent-free urethane coating agent for the gloss is 30-40% by weight of branched polyether-polyester polyol, 11-20% by weight of a curing agent hexamethylene diisocyanate (HMDI), 3.4-5% by weight of a pigment, 5.5-10% by weight of diluent, filler is composed of 20-30% by weight of jade powder, 20-30% by weight of silica sand 6-8, and 0.1-0.3% by weight of antifoaming agent, wherein the viscosity is 8500 cps. Remodeling method of interior and exterior walls using
청구항 1에 있어서,
상기 입체문양재료의 도막 두께는 규사의 크기에 따라 0.3∼1mm는 규사 8호사, 1∼2mm는 규사 7호사, 2∼3mm는 규사 6호사를 사용하는 것을 특징으로 하는 입체문양보드를 이용한 건물 내외벽 리모델링 공법.
The method according to claim 1,
The thickness of the three-dimensional glyph material in the building using a three-dimensional glyph board, characterized in that the 0.3 to 1mm silica sand 8, 1 to 2 mm silica sand 7, 2 to 3 mm silica sand 6 depending on the size of the silica sand Exterior wall remodeling method.
삭제delete
KR1020120048389A 2012-05-08 2012-05-08 Method for remodeling inner wall or outer wall of building using three-dimensional pattern board KR101256010B1 (en)