KR100795949B1 - Adhesive-tape be easy to cut and manufacturing method the same - Google Patents

Adhesive-tape be easy to cut and manufacturing method the same Download PDF

Info

Publication number
KR100795949B1
KR100795949B1 KR1020070081093A KR20070081093A KR100795949B1 KR 100795949 B1 KR100795949 B1 KR 100795949B1 KR 1020070081093 A KR1020070081093 A KR 1020070081093A KR 20070081093 A KR20070081093 A KR 20070081093A KR 100795949 B1 KR100795949 B1 KR 100795949B1
Authority
KR
South Korea
Prior art keywords
adhesive tape
cutting
fine
cut
pressure
Prior art date
Application number
KR1020070081093A
Other languages
Korean (ko)
Inventor
이병석
손성호
Original Assignee
(주)에버텍
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by (주)에버텍 filed Critical (주)에버텍
Priority to KR1020070081093A priority Critical patent/KR100795949B1/en
Application granted granted Critical
Publication of KR100795949B1 publication Critical patent/KR100795949B1/en

Abstract

A method for manufacturing a cleavable adhesive tape is provided to produce the cleavable adhesive tape by forming micro cutting grooves at both side ends of the adhesive tape, to lower a production cost, and to obtain a simple production process. A method for manufacturing a cleavable adhesive tape(1) includes the steps of: charging natural or synthetic rubbers and resins, an antioxidant, an organic solvent, etc, into a blending tank and blending and aging the mixture to obtain an adhesive(20); transferring wound film(10) to an adhesive coating position; coating one surface of the film with the adhesive, and back-treating the other surface; hot-air drying the adhesive applied on the film, and winding the adhesive-coated film around a pipe(30) to form an adhesive tape roll; cutting the adhesive tape roll into an adhesive tape having a predetermined width using a tape cutter, wherein the tape cutter comprises ring knives having micro protrusions formed to a side direction of an end part thereof and cuts the adhesive tape by the ring knives with forming micro-cutting grooves(40) on the side ends of the tape; and packaging the cut adhesive tape by the unit. Cutting is easily achieved by the micro cut grooves formed at the side ends of the adhesive tape.

Description

절단이 자유로운 점착테이프와 그 제조방법{Adhesive-tape be easy to cut and manufacturing method the same}Adhesive tape with easy cutting and its manufacturing method {Adhesive-tape be easy to cut and manufacturing method the same}

본 발명은 포장용 점착테이프에 관한 것으로, 보다 상세하게는 점착테이프의 양측단에 절단장치의 링나이프를 이용하여 다수개의 미세절단홈을 형성함으로써 별도의 절단수단을 이용하지 않아도 사용자의 임의에 따라 길이조절과 절단이 자유로운 점착테이프와 그 제조방법에 관한 것이다. The present invention relates to a pressure-sensitive adhesive tape for packaging, and more particularly, by forming a plurality of fine cutting grooves using ring knives of the cutting device on both sides of the pressure-sensitive adhesive tape without the need for a separate cutting means length The present invention relates to a pressure-sensitive adhesive tape free of adjustment and cutting and a method of manufacturing the same.

일반적으로 각종 포장용 테이프로 사용하고 있는 점착테이프는 테이프의 일면에 점착제를 도포하여 지관에 롤 타입으로 권취된 구성을 가진다. In general, the adhesive tape used as various packaging tapes has a structure in which a pressure-sensitive adhesive is applied to one surface of the tape and wound in a roll type on a branch pipe.

보다 상세하게, 상기 점착테이프는 합성수지 원단필름의 일면 전체에 점착제를 도포하여 상기 점착제에 의해 부착될 수 있도록 제조된 것으로, 통상 이러한 합성수지 원단필름은, 셀로판, 셀룰로우즈와 그 유도체, 폴리에틸렌(PE), 폴리프로필렌(PP), 폴리비닐 클로라이드(PVC), 폴리에스테르(PET), 폴리이미드(PI) 등이 사용된다. More specifically, the pressure-sensitive adhesive tape is manufactured to be attached to the entire surface of the synthetic resin fabric film to be attached by the pressure-sensitive adhesive, such synthetic resin fabric film, cellophane, cellulose and its derivatives, polyethylene (PE) ), Polypropylene (PP), polyvinyl chloride (PVC), polyester (PET), polyimide (PI) and the like are used.

이러한 원단필름 중, 상기 폴리프로필렌(PP)을 일축 또는 이축으로 연신하여 제조한 OPP(Oriented poly propylene) 필름은 투명하며 광택이 있고 우수한 방습성 을 가지기 때문에 각종 박스 포장용 투명 점착테이프로서 널리 사용되고 있다. Among these fabric films, OPP (Oriented poly propylene) film prepared by stretching the polypropylene (PP) uniaxially or biaxially is widely used as a transparent adhesive tape for various box packaging because of its transparency, gloss and excellent moisture resistance.

그러나, 이와 같은 원단필름에 점착제를 도포하여 만든 점착테이프는, 원단필름 자체가 쉽게 끊어지지 않는 특성을 가지기 때문에 점착테이프를 사용하는 사용자가 포장 등의 용도로 사용한 다음 그 길이에 따라 절단하고자 할 때 쉽게 종 또는 횡방향으로 절단되지 않으며 힘을 가했을 때 늘어나는 현상이 발생한다.However, since the adhesive tape made by applying the adhesive to such fabric film has the property that the fabric film itself is not easily broken, when the user using the adhesive tape is used for packaging, etc., and then cuts it according to its length It is not easily cut in the longitudinal or transverse direction and stretches when a force is applied.

따라서, 점착테이프를 사용한 다음에는 이를 사용자의 임의 길이대로 절단하기 위해서 가위나 칼과 같은 별도의 절단도구를 사용하거나, 플라스틱·금속재질의 톱니형 절단날을 장착한 테이프 디스펜서를 사용하여 절단·사용하고 있다. Therefore, after using the adhesive tape, use a separate cutting tool such as scissors or a knife to cut it to an arbitrary length of the user, or use a tape dispenser equipped with a plastic or metal serrated cutting blade. Doing.

이와 같이, 상기의 모든 방법들은 점착테이프를 절단하는 데 있어 절단 장치나 도구를 필요로 한다. 특히 상기 가위등의 절단도구를 사용하는 방법에 있어서는 테이프의 절단을 위해서는 항상 절단도구를 휴대해야 하는 불편함과, 점착테이프를 많이 사용해야 하는 작업에서는 가위를 사용해서 점착테이프를 일일이 절단해야 함으로써 작업시간이 지연되는 문제점을 가지고 있었다. As such, all of the above methods require a cutting device or tool to cut the adhesive tape. In particular, in the method of using a cutting tool such as scissors, the inconvenience of having to carry the cutting tool at all times to cut the tape, and in the task of using a large number of adhesive tapes, the adhesive tape must be cut by using a pair of scissors. I had this delayed issue.

그리고, 많이 사용되고 있는 상기 절단날을 장착한 디스펜서가 구성된 점착테이프는 그 절단날의 홈 부분이 뾰족하고 날카로운 금속이나 단단한 재질로 되어 있어 어린이나 사용법에 미숙한 사람에게 상처를 입힐 수 있으며, 점착테이프를 둘러싸는 케이스 때문에 전체적으로 부피가 커짐으로써, 주머니에 휴대할 때나 작업시에 불편함을 주며 그 생산비도 올라가게 되어 소비자들에게 부담을 줄 수 있다. In addition, the adhesive tape composed of the dispenser equipped with the cutting blades, which are widely used, may be injured in children or inexperienced people, since the groove portion of the cutting blade is made of sharp and sharp metal or hard material. Due to the bulky case surrounding the case, it is inconvenient when carrying it in a pocket or at work, and the production cost goes up, which can burden consumers.

이와 같은 절단도구의 불편함을 해소하기 위해, 상기 점착테이프 자체만으로도 절단이 용이하게 하는 방법들이 다양하게 고안되고 있다. 도 1을 참조하면, 이 러한 종래의 고안들 일실시예로, 점착테이프(100)의 표면에 복수개의 홀(101)을 천공하여 일정한 간격으로 구비된 천공선(102)을 테이프의 폭방향으로 형성하였다. 이에 따라, 상기 천공선(102)은 일반적인 절취선의 역할을 하게 되어 점착테이프 사용자는 상기 천공선(102)을 따라 쉽게 길이 절단이 가능하였다. In order to alleviate the inconvenience of such a cutting tool, various methods for facilitating the cutting with the adhesive tape itself have been devised. Referring to FIG. 1, in one embodiment of such conventional designs, a plurality of holes 101 are drilled on the surface of the adhesive tape 100 so that a perforated line 102 provided at regular intervals in the width direction of the tape. Formed. Accordingly, the perforated wire 102 serves as a general cut line, so that the adhesive tape user can easily cut the length along the perforated wire 102.

그러나, 이러한 구조를 가지는 점착테이프(100)는, 상기 천공선(102)이 일정한 간격으로 점착테이프(100)의 표면상에 존재하기 때문에 포장작업에 사용 중 옆으로 당기는 장력을 견디지 못해 원치 않는 길이에서 절단되는 문제점이 발생한다. 또한, 테이프 사용자는 반드시 상기 천공선(102)이 존재하는 위치에서만 절단해야 하는 불편함이 있어서 그 길이를 조절하는데 어려움이 있었다. However, the adhesive tape 100 having such a structure has an undesired length because the perforated wire 102 is present on the surface of the adhesive tape 100 at regular intervals so that the adhesive tape 100 cannot withstand the tension pulled sideways during use in packaging work. There is a problem that is cut off. In addition, the user of the tape must be cut only at the position where the perforation line 102 is present, and there was a difficulty in adjusting the length.

더불어, 이러한 천공선(102)이 존재하는 점착테이프(100)를 제조하기 위해서는, 상기 천공선(102)을 형성하기 위한 천공장치 등 별도의 기계장치가 필요하여, 제조단가의 상승 및 제조시간이 길어지는 등의 문제점이 발생한다. In addition, in order to manufacture the adhesive tape 100 in which the perforated wire 102 exists, a separate mechanical device such as a perforation device for forming the perforated wire 102 is required, so that the manufacturing cost is increased and the manufacturing time is increased. Problems such as lengthening occur.

또다른 방법으로, 도 1(b)를 참조하면, 점착테이프(100)의 양측단에 길이방향으로 절취선(113)을 일정한 간격으로 형성하였다. 이러한 절취선(113)을 점착제가 도포된 테이프에 형성하기는 어렵기 때문에 양 측부 일측에 점착제가 도포되지 않은 비도포면(112)과 부분도포면(111)을 형성하고, 상기 비도포면(112) 구역내에 절취선(113)을 형성하였다. As another method, referring to FIG. 1 (b), the cutting lines 113 were formed at both ends of the adhesive tape 100 in the longitudinal direction at regular intervals. Since it is difficult to form such a perforated line 113 on the adhesive-coated tape, the non-coating surface 112 and the partial coating surface 111, which are not coated with the adhesive, are formed on one side of both sides, and within the non-coating surface 112 region. A cutout line 113 was formed.

그러나, 이와 같이 비도포면(112)을 가지는 점착테이프(100)는 늘어짐이 약한 원단필름의 경우 도포면(110)과 비도포면(112)의 두께 차이로 굴곡현상이 나타나며, 박스 포장시 비도포구간으로 인해 좌우 뒤틀림이 발생하거나 전체 밀림현상 이 발생하는 문제점이 있었다. However, the adhesive tape 100 having the uncoated surface 112 as described above has a bending phenomenon due to the difference in thickness between the coated surface 110 and the non-coated surface 112 in the case of a weak film fabric, and the uncoated section when packaging the box. Due to this, there was a problem that the left and right warpage occurs or the entire jungle phenomenon.

또한, 도 1(a)와 마찬가지로, 그 제조방법에 있어 상기 비도포면(112), 부분도포면(111), 절취선(113), 접착제 도포면(110)을 형성하기 위한 많은 공정이 필요하고 별도 제조장치나 제조장치의 정밀한 조작이 필요한 문제점이 있다. In addition, as in Fig. 1 (a), in the manufacturing method, a number of steps for forming the non-coated surface 112, the partial coating surface 111, the cutout line 113, the adhesive coating surface 110 is required and a separate manufacturing apparatus There is a problem that requires precise manipulation of the manufacturing apparatus.

한편, 도 1(c)를 참조하면, 비도포면을 형성하지 않고 점착테이프(100)의 양측에 다수개의 절개홈(120)을 형성하는 방법이 있다. 그러나, 이와 같이 절개홈(120)을 점착테이프(100)상에 일정한 간격으로 형성하기 위해서는 천공장치(미도시)와 같이 별도의 기계장치가 필요하였고, 제조시간도 상당히 오랜 시간이 걸릴 뿐만 아니라 상기 절개홈(120)의 간격에 따라 기계장치의 간격 또한 조정해야 하는 등 생산성 효율이 굉장히 떨어지는 문제점이 있었다. 또한, 이에 따라 제조단가 또한 급상승하는 문제점이 있다. 그리고, 상기 절개홈(120)은 대부분 육안으로 확인할 수 있는 크기를 가져 제품의 미관상 보기 좋지 않으며 사용중 상기 절개홈(120)에 의해 원하지 않는 위치에서 절단되는 경우가 발생한다. On the other hand, referring to Figure 1 (c), there is a method of forming a plurality of cut grooves 120 on both sides of the adhesive tape 100 without forming an uncoated surface. However, in order to form the incision groove 120 at regular intervals on the adhesive tape 100 as described above, a separate mechanical device such as a drilling device (not shown) was required, and the manufacturing time was not only very long. According to the spacing of the incision groove 120, there is a problem in that the productivity efficiency is very poor, such as the interval of the mechanical device must also be adjusted. In addition, there is a problem that the manufacturing unit price also rises accordingly. In addition, the incision groove 120 has a size that can be confirmed mostly with the naked eye, the appearance of the product does not look good and is cut at an undesired position by the incision groove 120 during use.

그리고, 도 2를 참조하면, 점착테이프(100)의 양측단에 절취선 등을 형성하기 위한 종래의 장치를 설명하면 다음과 같다. 2, a conventional apparatus for forming a perforation line and the like at both ends of the adhesive tape 100 is as follows.

도시한 바와 같이, 몸체의 상부에 방사상으로 다수개의 홈 절단날(133)이 배치된 절단날 상판(131)과 하판(132)을 구비하여, 일정폭의 롤 형상으로 절단된 낱개의 점착테이프(100)를 상기 상,하판(131, 132) 사이에 올리고 가압판인 상판(131)으로 상기 점착테이프(100)를 눌러 일시에 점착테이프(100)의 측단에 절취선(미도시)을 형성시킨다. As shown in the drawing, the adhesive tape having a cutting blade upper plate 131 and a lower plate 132 in which a plurality of groove cutting edges 133 are disposed radially on the upper body is cut into a roll of a predetermined width ( 100 is placed between the upper and lower plates 131 and 132 to form a cutting line (not shown) at the side end of the adhesive tape 100 at a time by pressing the adhesive tape 100 with the upper plate 131 which is a pressing plate.

그러나, 이와 같은 장치를 이용한 점착테이프(100)는 도 1(c)와 같이 별도의 기계장치에 따른 제조단가의 상승 및 생산성 효율이 떨어지며, 압착에 의해 점착테이프(100)의 모양이 변질되거나 그 성능이 떨어지는 문제점이 있다. 또한, 상기 절단날(133)은 그대로 상부에서 누르기만 하는 것으로 시간의 경과에 따라 점착테이프의 점착제에 의해 날이 무뎌져 그 성능이 떨어지는 문제점 또한 발생한다. However, the pressure-sensitive adhesive tape 100 using such a device increases the manufacturing cost and productivity efficiency of the separate machine as shown in Figure 1 (c), the shape of the pressure-sensitive adhesive tape 100 is deteriorated by the compression or the There is a problem of poor performance. In addition, the cutting blade 133 is only pressed from the top as it is, as the time passes by the pressure-sensitive adhesive of the pressure-sensitive adhesive tape also causes a problem that its performance is lowered.

한편, 상기에 기술된 방법과 달리, 점착테이프의 절단이 용이하도록 원단필름을 제조할 때 절단이 잘되는 특성을 가지도록 제조하는 방법이 있다. On the other hand, unlike the method described above, there is a method for producing a characteristic that is well cut when manufacturing the original film to facilitate the cutting of the adhesive tape.

그러나, 이와 같은 원단필름을 제조하기 위해서는 다양한 첨가제가 들어갈 뿐만 아니라 원단필름 구조자체에 변형을 가하는 것이기 때문에 단가가 굉장이 높은 문제점이 있다. 따라서, 이를 사용하는 점착테이프의 단가 또한 일반적인 점착테이프에 비해 높을 수 밖에 없으며, 절단이 용이한 이점에도 불구하고 고객의 소비욕구를 저해시키는 문제점이 발생한다. However, in order to manufacture such a fabric film there is a problem that the unit price is very high because it is not only to add a variety of additives but also to modify the fabric film structure itself. Therefore, the unit cost of the adhesive tape using the same can also be higher than the general adhesive tape, and despite the advantages of easy cutting, there is a problem that inhibits the customer's desire to consume.

이에 따라, 사용자의 임의에 따라 절단이 용이하면서도 그 길이를 마음대로 조절가능하게 하고, 그 제조방법이 간단하여 단가가 낮으면서도 사용자의 사용욕구를 충분히 만족시킬 수 있는 점착테이프와 그 제조방법의 발명이 요구되고 있다. Accordingly, the invention of the pressure-sensitive adhesive tape and its manufacturing method can be easily cut according to the user's arbitrarily, and the length thereof can be arbitrarily adjusted, and the manufacturing method is simple to satisfy the user's needs even though the unit price is low. It is required.

본 발명은 전술한 문제점들을 해결하고자 안출된 것으로서, 양측단에 미세절단홈이 형성되어 사용자가 임의의 길이로 절단이 자유로운 점착테이프를 제공하는 것을 목적으로 한다. The present invention has been made to solve the above problems, an object of the present invention is to provide a pressure-sensitive adhesive tape freely cut to any length by the minute cutting grooves are formed at both ends.

또한, 미세절단홈을 형성하기 위한 그 제조방법이 간단하여 제조단가가 낮으면서도 사용자의 소비욕구를 충분히 만족시킬 수 있는 절단이 자유로운 점착테이프와 그 제조방법을 제공하는 것을 목적으로 한다. In addition, it is an object of the present invention to provide a pressure-sensitive adhesive tape and a method for manufacturing the same, which can be easily cut to satisfy the user's consumption needs while having a low manufacturing cost due to its simple manufacturing method for forming a fine cutting groove.

더불어, 권취된 점착테이프롤을 생산 길이에 맞게 절단함에 있어서, 절단장치의 링나이프에 다수개의 미세돌기를 형성하여 롤에서 절단되어 생산되는 점착테이프의 일측 또는 양측단에 미세절단홈이 형성되는 절단이 자유로운 점착테이프 제조방법을 제공하는 것을 목적으로 한다. In addition, in cutting the wound adhesive tape roll to the production length, the cutting is formed by forming a plurality of fine projections on the ring knife of the cutting device to form a fine cutting groove on one side or both ends of the adhesive tape produced by cutting from the roll It is an object of the present invention to provide a method for producing this free adhesive tape.

본 발명에 따른 절단이 자유로운 점착테이프는, 합성수지를 일축 또는 이축 연신하여 길이를 늘린 원단필름과, 상기 원단 필름의 일면에 완전 도포된 점착제를 포함하여 구성되고, 이를 지관에 두께를 가지는 롤형태로 권취하여 링나이프를 이용해 일정 폭을 가지도록 절단하여 이루어지는 점착테이프에 있어서, 상기 점착테이프는 권취된 롤형태의 측단에 두께방향으로 다수개의 미세절단홈이 육안으로 구분되지 않을 정도의 깊이로 형성되되; Adhesive tape free cutting according to the present invention comprises a fabric film uniaxially or biaxially stretched to increase the length, and a pressure-sensitive adhesive completely coated on one side of the fabric film, it is in the form of a roll having a thickness on the branch pipe In the adhesive tape is wound and cut to have a predetermined width by using a ring knife, the adhesive tape is formed to a depth such that a plurality of micro-cut grooves in the thickness direction in the thickness direction on the side of the wound roll shape is not visible to the naked eye. ;

상기 링나이프는 측방향으로 돌출된 다수개의 미세돌기가 형성되어, 상기 미 세돌기에 의해 상기 미세절단홈은 이웃하는 미세절단홈과 간격이 일정하지 않고 불규칙하게 형성되는 것을 특징으로 한다. The ring knife is formed with a plurality of minute protrusions protruding in the lateral direction, the micro-cut grooves are characterized in that the micro-cut grooves are irregular and irregular intervals with the neighboring micro-cut grooves.

이때, 상기 링나이프의 미세돌기의 움직임에 따라 상기 미세절단홈은, 권취된 점착테이프의 두께와 동일한 길이를 가진다. At this time, the micro-cutting groove has the same length as the thickness of the wound adhesive tape according to the movement of the fine protrusion of the ring knife.

그리고, 바람직하게 상기 링나이프의 미세돌기는 3∼5 마이크론(micron)의 크기를 가지며, 상기 미세절단홈은 3∼5 마이크론(micron)의 깊이를 가진다. And, preferably, the ring protrusion fine protrusion has a size of 3 to 5 microns, and the fine cutting groove has a depth of 3 to 5 microns.

한편, 상기 원단필름은, 폴리프로필렌(PP)을 이축으로 연신하여 제조한 BOPP필름인 것을 특징으로 한다. On the other hand, the raw film is characterized in that the BOPP film produced by stretching polypropylene (PP) biaxially.

그리고, 이러한 절단이 자유로운 점착테이프를 제조하는 제조방법은, 합성수지를 일축 또는 이축 연신하여 길이를 늘린 원단필름과, 상기 원단 필름의 일면에 도포된 점착제를 포함하고, 이를 지관에 두께를 가지는 롤형태로 권취하여 구성되는 점착테이프를 제조하는 제조방법에 있어서,In addition, the manufacturing method for manufacturing such a free-cut adhesive tape comprises a fabric film uniaxially or biaxially stretched to increase the length, and a pressure-sensitive adhesive applied to one surface of the fabric film, a roll shape having a thickness on the paper tube In the production method for producing a pressure-sensitive adhesive tape wound by

천연 또는 합성 고무계와 수지, 노화방지제, 유기용제 등을 배합탱크에 넣어 점착제로 배합·숙성시키는 점착제 배합단계와; 권취된 상태의 원단필름을 상기 점착제를 도포하기 위한 위치로 이송시키는 원단필름 공급단계와; 상기 원단필름의 일측면에 상기 점착제를 완전히 도포하고, 타측면은 배면처리하여 코팅하는 점착제 도포단계와; 상기 원단필름에 도포된 점착제를 열풍건조시키고, 점착제가 도포된 원단필름을 지관에 감아 점착테이프롤을 형성하는 건조 및 권취단계와; 상기 점착테이프롤을 테이프 재단기를 이용하여 일정폭을 가지는 점착테이프로 절단하되, 상기 테이프 재단기는 단부의 측방향으로 미세돌기가 형성된 링나이프가 구비되어 상 기 링나이프에 의해 상기 점착테이프는 측단에 미세절단홈이 형성되면서 절단되는 절단단계와; 상기 절단된 점착테이프를 단위별로 포장하고 출고하는 포장·완료단계를 포함하여 이루어지며; 상기 점착테이프의 측단에 형성된 미세절단홈에 의해 제조되는 점착테이프는 절단이 용이한 것을 특징으로 한다. A pressure-sensitive adhesive compounding step of blending and maturing a natural or synthetic rubber system with a resin, an anti-aging agent, an organic solvent, etc. in a mixing tank; A raw film supplying step of transferring the rolled film to a position for applying the pressure-sensitive adhesive; A pressure-sensitive adhesive coating step of completely applying the pressure-sensitive adhesive on one side of the fabric film, and coating the other side by treating the back surface; A drying and winding step of drying the pressure-sensitive adhesive applied to the fabric film and winding the fabric-coated film to which the pressure-sensitive adhesive is applied to a paper tube to form an adhesive tape roll; The adhesive tape roll is cut into an adhesive tape having a predetermined width by using a tape cutting machine, and the tape cutting machine is provided with a ring knife formed with fine protrusions in a lateral direction of the end. A cutting step of cutting while forming a fine cutting groove; It comprises a packing and completion step of packing and shipping the cut adhesive tape for each unit; The adhesive tape manufactured by the micro cutting groove formed at the side end of the adhesive tape is characterized in that the cutting is easy.

이때, 상기 원단필름은, 상기 원단필름은, 폴리프로필렌(PP)을 이축으로 연신하여 제조한 BOPP필름인 것을 특징으로 한다. In this case, the raw film is characterized in that the raw film is a BOPP film produced by stretching polypropylene (PP) biaxially.

그리고, 상기 절단단계는, 점착테이프롤을 테이프 재단기의 고정장치 회전축에 끼워 삽입하는 권취된 점착테이프롤 고정과정과, 상기 회전축을 회전시켜 점착테이프롤이 일정한 회전속도를 가지며 회전하는 점착테이프롤 회전과정과, 상기 회전하는 점착테이프롤을 상기 테이프 재단기의 절단장치 링나이프를 이용하여 폭을 가지도록 절단하여 단일 점착테이프로 생산하는 링나이프에 의한 점착테이프롤 절단과정과, 상기 절단과정에서 링나이프의 미세돌기에 의해 절단되는 점착테이프의 절단면에 두께방향으로 미세절단홈을 형성시키는 링나이프 돌기에 의한 미세절단홈 형성과정과, 상기 미세절단홈이 형성된 다수개의 점착테이프로 절단된 점착테이프롤을 회전축에서 제거하는 완료 점착테이프 회수과정을 포함하여 이루어지진다. And, the cutting step, the pressure-sensitive adhesive tape roll fixing process for inserting the pressure-sensitive adhesive tape roll inserted into the rotary shaft of the fixing device of the tape cutting machine, and the pressure-sensitive adhesive tape roll rotates by rotating the rotary shaft to have a constant rotation speed Process, cutting the rotating adhesive tape roll to have a width using a cutting device ring knife of the tape cutting machine to produce a single adhesive tape, and cutting the adhesive tape roll by the ring knife, and the ring knife in the cutting process. The process of forming a fine cutting groove by the ring knife protrusion to form a fine cutting groove in the thickness direction on the cutting surface of the adhesive tape cut by the fine projection of the, and the adhesive tape roll cut by a plurality of adhesive tape formed with the fine cutting groove It includes the process of recovering the completed adhesive tape removed from the rotating shaft.

그리고, 상기 절단단계에서 사용되는 테이프 재단기는, 점착테이프롤이 끼워져 삽입되는 회전축이 구비된 본체와, 상기 본체의 일측에 구비되어 상기 회전축의 회전속도와 점착테이프롤의 절단폭을 제어하는 자동제어반이 형성된 고정장치와; 상기 점착테이프롤의 개수에 대응되는 수의 링나이프와, 상기 링나이프를 지지하는 회동축이 구비된 몸체가 형성된 절단장치를 포함하여 구성된다. The tape cutting machine used in the cutting step includes a main body having a rotating shaft into which the adhesive tape roll is inserted and inserted into one side of the main body to control a rotation speed of the rotating shaft and a cutting width of the adhesive tape roll. A formed fixing device; And a cutting device having a number of ring knives corresponding to the number of the adhesive tape rolls, and a body having a rotating shaft supporting the ring knives.

한편, 상기 링나이프는, 원형몸체부와, 상기 원형몸체부의 외주면을 형성하는 원형칼날부와, 상기 원형칼날부의 단부를 따라 등간격으로 측방향 돌출된 미세돌기를 포함하여 구성된다. On the other hand, the ring knife is configured to include a circular body portion, a circular blade portion forming the outer circumferential surface of the circular body portion, and fine projections protruding laterally at equal intervals along the ends of the circular blade portion.

그리고, 상기 링나이프는, 상기 원형칼날부의 단부를 따라 등간격으로 형성된 요홈을 더 포함하며, 상기 미세돌기는 상기 요홈을 형성하기 위한 외부충격에 의해 상기 원형칼날부가 밀려나면서 측방향으로 돌출되어 형성된다. The ring knife further includes grooves formed at equal intervals along an end portion of the circular blade portion, and the fine protrusion protrudes laterally while the circular blade portion is pushed out by an external impact to form the groove. do.

또한, 상기 미세돌기는, 3∼5 마이크론(micron)의 크기로 원형칼날부의 일측방향으로 이웃하는 미세돌기와 10㎜의 간격을 가지고 돌출되게 형성된다. 또한, 상기 미세돌기는, 3∼5 마이크론(micron)의 크기로 원형칼날부의 양측방향으로 이웃하는 미세돌기와 10㎜의 간격을 가지고 돌출되게 형성된다. In addition, the micro-projections are formed to protrude at a distance of 10 mm from the neighboring micro-projections in one direction of the circular blade portion in the size of 3 to 5 microns (micron). In addition, the micro-projections are formed to protrude at intervals of 10 mm from neighboring micro-projections in both lateral directions of a size of 3 to 5 microns.

이와 같이 본 발명에 따른 절단이 자유로운 점착테이프와 그 제조방법에 따르면, 사용되는 점착테이프의 일측단 또는 양측단에 미세절단홈이 점착테이프의 두께방향으로 형성되기 때문에 사용자는 임의대로 필요로 하는 길이만큼 그 길이를 조절하여 사용할 수 있는 효과가 있다. Thus, according to the adhesive tape and the method of manufacturing the free cutting according to the present invention, since the fine cutting groove is formed in the thickness direction of the adhesive tape at one end or both ends of the adhesive tape to be used, the user may arbitrarily require As long as the length can be adjusted to use the effect.

또한, 사용하고자 하는 곳에 점착테이프를 부착하는 과정과 동시에 미세절단홈을 이용한 절단과정을 할 수 있어 가위와 같은 별도의 절단수단을 구비하지 않아도 되기 때문에 절단을 위한 시간을 단축할 수 있고, 절단수단으로 인해 상처를 입을 수 있는 위험을 줄이는 효과가 있다. In addition, the process of attaching the adhesive tape to the place to be used can be cut at the same time using the micro-cutting grooves, so it is not necessary to provide a separate cutting means such as scissors, thereby reducing the time for cutting and cutting means. This has the effect of reducing the risk of injury.

더불어, 단일 점착테이프를 생산하기 위한 절단장치의 링나이프 원형칼날에 미세돌기를 형성함으로써, 점착테이프의 측단에 미세절단홈을 형성하기 위한 별도의 제조장치가 필요하지 않고, 기존 점착테이프의 상품성과 성질을 유지하면서 제조할 수 있기 때문에 생산 공정에 어려움이 없으며 추가적인 재료가 들어가지 않아 종래 상품화된 점착테이프의 생산성과 단가는 동일하고 편이성은 극대화시키는 효과가 있다. In addition, by forming a fine protrusion on the ring knife circular blade of the cutting device for producing a single adhesive tape, there is no need for a separate manufacturing device for forming a fine cutting groove on the side end of the adhesive tape, Since it can be manufactured while maintaining the properties, there is no difficulty in the production process and no additional materials are included, so the productivity and cost of the commercialized adhesive tape are the same, and the convenience is maximized.

이하에는 첨부한 도면을 참조하여 본 발명에 따른 절단이 자유로운 점착테이프와 그 제조방법의 바람직한 실시예에 대해 상세하게 설명한다. Hereinafter, with reference to the accompanying drawings will be described in detail a preferred embodiment of the adhesive tape and the manufacturing method of the free cutting according to the present invention.

도 3은 본 발명에 따른 절단이 자유로운 점착테이프를 보여주는 사시도 및 부분 확대도이고, 도 4는 본 발명에 따른 절단이 자유로운 점착테이프의 일부를 보여주는 평면도 및 부분 확대도이다. 3 is a perspective view and a partially enlarged view showing a free cut adhesive tape according to the present invention, Figure 4 is a plan view and a partially enlarged view showing a portion of a free cut adhesive tape according to the present invention.

도시한 바와 같이, 본 발명에 따른 절단이 자유로운 점착테이프(1)는, 합성수지를 일축 또는 이축 연신(延伸)하여 길이를 늘린 원단필름(10)과, 상기 원단 필름(10)의 일면에 완전하게 도포된 점착제(20)를 포함하여 이루어지는데, 상기 점착제(20)가 도포된 원단필름(10)은 종이로 만든 지관(30)에 권취되어 일정한 두께(A)를 가지는 롤형태로 형성된다. 이때, 상기 롤은 아직 절단되지 않은 점착테이프(1)가 일체형으로 형성된 점착테이프롤로서, 이를 링나이프를 이용해 일정폭을 가지도록 절단하여 단일 점착테이프(1)를 생산하게 된다. As shown, the free-cut adhesive tape 1 according to the present invention, the uniaxial or biaxially stretched synthetic resin to extend the length of the original film 10, and one surface of the original film 10 completely It comprises a pressure-sensitive adhesive 20 is applied, the fabric film 10 is applied to the pressure-sensitive adhesive 20 is wound in a paper tube 30 made of paper is formed in a roll shape having a constant thickness (A). At this time, the roll is an adhesive tape roll in which the adhesive tape 1, which is not yet cut, is integrally formed. The roll is cut to have a predetermined width using a ring knife to produce a single adhesive tape 1.

이때, 상기 점착테이프(1)는 점착테이프롤과 같이 지관에 권취된 롤형태를 가지며, 측단에 두께방향으로 다수개의 미세절단홈(40)이 형성된 것을 특징으로 한 다. At this time, the adhesive tape (1) has a roll shape wound on the branch pipe like the adhesive tape roll, characterized in that a plurality of fine cutting grooves 40 are formed in the thickness direction at the side end.

한편, 바람직하게 상기 미세절단홈(40)은 이웃하는 미세절단홈(40)과 그 간격이 일정하지 않고 불규칙하게 형성되는데, 이는 상기 점착테이프(1)을 제조할 때 링나이프(미도시)의 측방향으로 돌출된 미세돌기의 회전에 따라 미세절단홈(40)이 형성되면서 절단면, 즉 단부가 긁히듯이 형성되기 때문에, 회전속도에 따라 상기 미세절단홈(40)은 불규칙한 간격을 가지고 형성된다. On the other hand, preferably the fine cutting groove 40 is adjacent to the fine cutting groove 40 and the gap is not formed irregularly, which is when the adhesive tape (1) of the ring knife (not shown) Since the cutting surface, that is, the end is formed as if the fine cutting groove 40 is formed in accordance with the rotation of the fine protrusion protruding in the lateral direction, the fine cutting groove 40 is formed at irregular intervals in accordance with the rotational speed.

이와 같이 형성된 미세절단홈(40)은, 상기 링나이프 미세돌기의 크기에 의해 바람직하게 육안으로 구분되지 않을 정도의 깊이와 크기를 가지면서 형성되며, 점착테이프(1)의 측단에 형성되는 이웃하는 미세절단홈(40)과의 간격이 매우 조밀하기 때문에 상기 점착테이프(1)를 이용하여 포장 등의 용도로 사용하는 사용자는 전혀 불편함이 없이 필요한 길이로 절단하여 사용할 수 있는 것을 특징으로 한다.The fine cutting groove 40 formed as described above is formed while having a depth and a size such that it is not easily distinguished by the naked eye by the size of the ring knife fine protrusion, and is formed at the side end of the adhesive tape 1. Since the gap with the fine cutting groove 40 is very dense, the user using the adhesive tape 1 for packaging or the like can cut and use the required length without any inconvenience.

이때, 상기 링나이프의 미세돌기가 일측방향으로 돌출되었다면 이에 따라 점착테이프 또한 일측단에만 미세절단홈(40)이 형성되며, 상기 링나이프의 미세돌기가 양측방향으로 돌출되었다면 이에 따라 점착테이프 또한 양측단에 미세절단홈(40)이 형성된다. At this time, if the fine protrusion of the ring knife is protruded in one direction, the adhesive tape also has a fine cutting groove 40 is formed only at one side, and if the fine protrusion of the ring knife is protruded in both directions, the adhesive tape is also both sides accordingly. The micro cutting groove 40 is formed at the end.

그리고, 상기 미세절단홈(40)은 그 공정에 따라 롤형태로 권취된 점착테이프(1)의 두께(A)와 동일한 길이를 가지며, 상기 두께 방향으로 다수개 형성될 수 있다. In addition, the fine cutting groove 40 has the same length as the thickness (A) of the pressure-sensitive adhesive tape 1 wound in a roll shape according to the process, it may be formed in plurality in the thickness direction.

또한, 상기 점착테이프(1)를 제조하는 공정에서 절단장치(미도시)에 구비된 링나이프에 의해 일정폭(B)으로 절단된 점착테이프(1)가 생산될 때, 상기 링나이프 의 미세돌기의 크기에 따라 미세절단홈(40)이 형성되는데, 상기 미세돌기의 크기는 육안으로 확인하기 쉽지 않은 크기를 가지기 때문에 이에 의해 형성되는 상기 미세절단홈(40) 매우 작은 크기를 가진다. In addition, when the adhesive tape 1 cut to a predetermined width B is produced by a ring knife provided in a cutting device (not shown) in the process of manufacturing the adhesive tape 1, the fine projection of the ring knife According to the size of the fine cutting groove 40 is formed, because the size of the micro-protrusion has a size that is not easy to see with the naked eye, the fine cutting groove 40 formed by it has a very small size.

보다 상세하게, 도 4를 참조하면, 상기 점착테이프(1)의 일측 또는 양측단에 형성되는 미세절단홈(40)은 그 크기가 매우 작기 때문에 일반적으로 사용되는 점착테이프와 외관상 크게 다르지 않으며, 종래 점착테이프의 사용성능 및 접착성능과 동일한 효과를 가지면서도, 상기 미세절단홈(40)에 의해 자유롭게 절단가능한 편이성이 특징적으로 포함되어 상품성과 사용자의 사용편이성을 극대화시킨다. In more detail, referring to FIG. 4, since the micro cutting grooves 40 formed at one or both ends of the adhesive tape 1 are very small in size, they are not significantly different in appearance from the adhesive tapes generally used. While having the same effects as the use performance and adhesive performance of the adhesive tape, the ease of freely cut by the micro-cut groove 40 is characterized by maximizing the ease of use and user convenience.

바람직하게, 상기 미세절단홈(40)을 형성하는 링나이프의 미세돌기의 크기는 3∼5 마이크론(micron)의 크기를 가지며, 이에 따라 상기 미세절단홈(40)은 바람직하게 이와 동일하게 3∼5 마이크론(micron)의 깊이를 가지면서 형성된다. Preferably, the size of the micro projections of the ring knife forming the micro cutting groove 40 has a size of 3 to 5 microns, and thus the micro cutting groove 40 is preferably the same as 3 to 5 micron. It is formed with a depth of 5 microns.

한편, 일반적으로 점착테이프에 사용되는 상기 원단필름(10)은 다양한 합성수지가 사용되는데, 상기 합성수지는 쉽게 끊어지지 않는 특성을 가지며, 본 발명에 따른 점착테이프(1)는 이러한 합성수지 중 폴리프로필렌(PP)을 종 또는 횡방향, 종·횡방향, 즉 일축 또는 이축으로 연신하여 제조한 OPP(Oriented poly propylene) 필름을 사용한다. On the other hand, the fabric film 10 generally used for the adhesive tape is used a variety of synthetic resin, the synthetic resin has a characteristic that is not easily broken, the adhesive tape 1 according to the present invention is a polypropylene (PP) of such a synthetic resin ) OPP (Oriented poly propylene) film manufactured by stretching longitudinally or transversely, longitudinally and transversely, ie, uniaxially or biaxially.

보다 상세하게는, 상기 OPP필름 중 이축연신(biaxial orientation) 공정을 통해 더 한층 물성을 향상시킨 BOPP(biaxial Oriented poly propylene)필름이 사용되는데, 이와 같이 폴리프로필렌(PP)을 이축으로 연신하여 제조한 BOPP필름은 인체에 무해하며 무독, 무취, 무미하고, 탄성률과 투명도 및 광택도가 우수하여 점착테 이프(1)의 원단필름(10)으로 사용하기 적합하다. More specifically, a biaxial oriented poly propylene (BOPP) film, which further improves physical properties through a biaxial orientation process, is used in the OPP film. BOPP film is harmless to the human body, non-toxic, odorless, tasteless, excellent in elastic modulus, transparency and glossiness, suitable for use as the raw film 10 of the adhesive tape (1).

또한, 상기 점착제(20)는 천연 또는 합성고무계, 아크릴계, 실리콘계 등의 감압성 점착제(20)를 사용한다. In addition, the pressure-sensitive adhesive 20 uses a pressure-sensitive adhesive 20, such as natural or synthetic rubber, acrylic, silicone.

이와 같이, 사용자의 임의에 따라 잘 절단되지 않는 합성수지를 원단필름(10)으로 하는 점착테이프(1)의 일측 또는 양측단에 제조단계에서 다수개의 미세절단홈(40)을 형성함으로써, 사용자는 임의대로 필요로 하는 길이만큼 그 길이를 조절하여 사용할 수 있으며, 사용하고자 하는 곳에 점착테이프(1)를 부착하는 과정과 동시에 미세절단홈(40)을 이용한 절단과정을 할 수 있어 가위와 같은 별도의 절단수단을 구비하지 않아도 되기 때문에 절단을 위한 시간을 단축할 수 있고, 절단수단으로 인해 상처를 입을 수 있는 위험을 줄일 수 있다. Thus, by forming a plurality of fine cutting grooves 40 in the manufacturing step on one side or both ends of the adhesive tape (1) to the synthetic film 10, which is not cut well according to the user's arbitrary, the user It can be used by adjusting the length as needed, and the process of attaching the adhesive tape (1) to the desired place and the cutting process using the micro-cutting groove 40 can be performed at the same time. Since it is not necessary to provide a means, it is possible to shorten the time for cutting and to reduce the risk of being injured by the cutting means.

도 5는 본 발명에 따른 절단이 자유로운 점착테이프의 제조방법을 보여주는 공정도이고, 도 6은 본 발명의 절단이 자유로운 점착테이프의 제조방법에 따른 절단단계를 보여주는 과정도이며, 도 7(a)(b)는 도 6에 따른 점착테이프롤의 절단과정과 미세절단홈의 형성을 보여주는 개략적인 도면이다. 5 is a process chart showing a method of manufacturing a free cutting adhesive tape according to the present invention, Figure 6 is a process chart showing a cutting step according to the manufacturing method of a free cutting adhesive tape of the present invention, Figure 7 (a) ( b) is a schematic diagram showing the process of cutting the adhesive tape roll according to Figure 6 and the formation of a fine cutting groove.

또한, 도 8은 본 발명의 절단이 자유로운 점착테이프의 제조방법에 따른 절단장치에 적용되는 링나이프를 보여주는 사시도이고, 도 9(a)(b)는 도 8에 따른 링나이프의 일예를 보여주는 평면도이다. 8 is a perspective view showing a ring knife applied to a cutting device according to a method of manufacturing a pressure-sensitive adhesive tape free cutting of the present invention, Figure 9 (a) (b) is a plan view showing an example of the ring knife according to FIG. to be.

도시한 바와 같이, 본 발명에 따른 절단이 자유로운 점착테이프(1)를 제조하는 제조방법(1a)은, 합성수지를 일축 또는 이축 연신하여 길이를 늘린 원단필름과, 상기 원단필름의 일면에 도포된 점착제를 포함하고, 이를 지관에 두께를 가지는 롤 형태로 권취하여 점착테이프를 생산하되, 상기 점착테이프의 일측단 또는 양측단에 두께방향으로 다수개의 미세절단홈을 형성하기 위해, 점착제 배합단계(S1)와, 원단필름 공급단계(S2), 점착제 도포단계(S3), 건조 및 권취단계(S4), 절단단계(S5), 그리고 포장·완료 단계(S6)를 포함하여 이루어진다. As shown, the manufacturing method (1a) for producing the adhesive tape (1) free cutting according to the present invention, the uniaxial or biaxial stretching of the synthetic film to increase the length, and the adhesive applied to one surface of the fabric film To include, and to produce a pressure-sensitive adhesive tape by winding it in the form of a roll having a thickness on the paper tube, to form a plurality of micro-cut grooves in the thickness direction on one side or both ends of the pressure-sensitive adhesive, pressure-sensitive adhesive compounding step (S1) And, including the raw film supply step (S2), pressure-sensitive adhesive coating step (S3), drying and winding step (S4), cutting step (S5), and packaging and completion step (S6).

이때, 상기 점착제 배합단계(S1)는, BOPP필름과 같은 원단필름(10)의 일면 전체에 도포되는 점착제(20)를 배합하는 과정으로, 상기 점착제(20)로 사용되는 천연 또는 합성 고무계, 수지, 첨가제로 노화방지제, 유기용제 등을 배합실의 배합탱크내에 넣고 12시간에 걸쳐 배합, 숙성시킨다. 이와 같이 배합된 점착제는 원단필름에 도포되기 위해 이어지는 코팅처리실로 이송된다. At this time, the pressure-sensitive adhesive compounding step (S1) is a process of compounding the pressure-sensitive adhesive 20 to be applied to the entire surface of the original film 10, such as BOPP film, natural or synthetic rubber, resin used as the pressure-sensitive adhesive 20 As an additive, an anti-aging agent, an organic solvent, and the like are put in a mixing tank of the mixing chamber and mixed and aged for 12 hours. The pressure-sensitive adhesive blended in this way is transferred to the subsequent coating treatment chamber to be applied to the original film.

한편, 상기 원단필름 공급단계(S2)는, 상기 BOPP 원단필름이 권취된 상태로 상기 점착제를 도포하기 위한 코팅처리실로 이송하는 단계로, 상기 코팅처리실로 이송된 원단필름은 이송벨트에 의한 이송장치 또는 롤러에 의해 점착제를 도포하기 위한 위치로 이송된다. On the other hand, the raw film supply step (S2), the BOPP raw film is transported to the coating processing chamber for applying the pressure-sensitive adhesive in the wound state, the raw film transported to the coating processing chamber is conveyed by a transfer belt Or it transfers to the position for apply | coating an adhesive by a roller.

그리고, 상기 점착제 도포단계(S3)는, 상기 원단필름의 일면에 상기 배합된 점착제를 도포하는 과정으로, 상기 점착제를 도포하기 전에 상기 원단필름은 일측면에 상기 점착제를 완전히 도포하고, 타측면을 이형제 등에 의한 배면처리, 즉 코팅처리 된다. 이와 같은 배면처리에 의해 생산되는 점착테이프(1)는 권취된 롤형태로 존재할 때 다른 점착테이프 면과 잘 떨어져 사용이 편리하게 된다. In addition, the pressure-sensitive adhesive coating step (S3) is a process of applying the compounded pressure-sensitive adhesive on one surface of the original film, the original film is completely coated with the pressure-sensitive adhesive on one side, before applying the pressure-sensitive adhesive, Back treatment with a release agent or the like is coated. The adhesive tape 1 produced by such a back treatment is easily separated from other adhesive tape faces when present in the form of a rolled roll, which is convenient to use.

이때, 필요에 따라 상기 원단필름에 색상이 들어가는 인쇄처리가 포함될 수 있으며, 점착제는 점착제가 담긴 통 또는 롤러 등에 의해 원단필름의 일면에 전체 적으로 도포된다. In this case, a color printing may be included in the fabric film as needed, and the pressure-sensitive adhesive is entirely applied to one surface of the fabric film by a container or a roller containing an adhesive.

그리고, 상기 건조 및 권취단계(S4)에서, 상기 점착제가 도포된 원단필름은 보일러에 의해 열풍건조되며, 일정한 길이로 종이 지관에 감겨 권취되어 점착테이프롤(도 7a, 50)로 형성된다. And, in the drying and winding step (S4), the pressure-sensitive adhesive coated fabric film is hot air dried by a boiler, wound around a paper paper tube with a predetermined length is formed of an adhesive tape roll (Fig. 7a, 50).

이때, 바람직하게 상기 점착테이프롤(50)의 폭은 1040∼1240㎜ 길이를 가진다. At this time, preferably the width of the adhesive tape roll 50 has a length of 1040 ~ 1240mm.

그리고, 상기 점착테이프롤(50)은 절단실로 이송되어 절단단계(S5)에 따라 테이프 재단기(2)에 의해 생산·출고되는 폭을 가지며 절단된다. Then, the adhesive tape roll 50 is transferred to the cutting chamber is cut with a width produced and released by the tape cutting machine 2 according to the cutting step (S5).

바람직하게, 상기 절단단계(S5)에서 점착테이프롤(50)을 상기 테이프 재단기(2)를 이용하여 일정폭을 가지는 점착테이프(1)로 절단하되, 이때 상기 테이프 재단기(2)는 상기 점착테이프롤(50)을 일정폭으로 자르기 위한 링나이프(80)를 포함하여 구성되는데, 이때 상기 링나이프(80)의 원형칼날부(83)의 단부 외측을 따라 측방향으로 미세돌기가 형성되어 상기 점착테이프롤(50)을 절단할 때 완성되는 점착테이프(1)의 측단에 다수개의 미세절단홈(40)을 형성한다. Preferably, in the cutting step (S5), the adhesive tape roll 50 is cut into an adhesive tape 1 having a predetermined width by using the tape cutter 2, wherein the tape cutter 2 is the adhesive tape It comprises a ring knife 80 for cutting the roll 50 to a predetermined width, wherein the fine projection is formed laterally along the outside of the end of the circular blade portion 83 of the ring knife 80 When cutting the tape roll 50 to form a plurality of fine cutting grooves 40 on the side end of the adhesive tape (1) completed.

이어서, 이와 같이 측단에 미세절단홈(40)이 형성된 점착테이프(1)는 포장·완료단계(S6)에 따라 단위별로 포장되어 출고된다. Subsequently, the adhesive tape 1 having the fine cutting grooves 40 formed at the side ends in this way is packed and shipped from the unit according to the packing and completion step S6.

이와 같이 이루어지는 절단이 자유로운 점착테이프의 제조방법(1a)은, 그 공정흐름이 간단하고, 별도의 미세절단홈(40)을 만들기 위한 복잡한 기계장치가 필요하지 않기 때문에 생산단가가 종래의 점착테이프 제조단가와 동일한 가격을 가지는 절단이 자유로운 점착테이프(1)을 제조할 수 있으며, 일반 사용자의 편이성은 상기 미세절단홈(40)에 의해 절단이 자유로워 극대화된다. The production method (1a) of the free-cutting adhesive tape made in this way is simple in its process flow and does not require a complicated mechanical device for making a separate fine cutting groove (40). It is possible to manufacture a pressure-sensitive adhesive tape 1 having the same price as the unit price, and the convenience of the general user is maximized by the free cutting by the fine cutting groove 40.

그리고, 바람직하게 상기 원단필름은 폴리프로필렌(PP)을 이축으로 연신하여 제조한 BOPP필름인 것을 특징으로 한다. Preferably, the raw film is a BOPP film produced by stretching polypropylene (PP) biaxially.

한편, 도 6과 도 7(a)(b)을 참조하여, 상기 미세절단홈(40)이 형성된 점착테이프(1)를 완성하기 위해 점착테이프롤(50)을 절단하는 절단단계(S5)를 보다 상세하게 살펴보면 다음과 같다. Meanwhile, referring to FIGS. 6 and 7 (a) and (b), a cutting step S5 of cutting the adhesive tape roll 50 to complete the adhesive tape 1 on which the micro cutting grooves 40 are formed is performed. Looking in more detail as follows.

상기 절단단계(S5)는, 권취된 점착테이프롤 고정과정(S51), 점착테이프롤 회전과정(S52), 링나이프에 의한 점착테이프롤 절단과정(S53), 링나이프 돌기에 의한 미세절단홈 형성과정(S54), 그리고 완료 점착테이프 회수과정(S55)을 따라 원단필름에 점착제가 도포되어 종이 지관에 일정한 길이로 권취된 점착테이프롤(50)을 절단하여 일측단 또는 양측단에 절단미세홈(40)이 형성된 절단이 자유로운 점착테이프(1)를 생산한다. The cutting step (S5), the wound adhesive tape roll fixing process (S51), the adhesive tape roll rotation process (S52), the adhesive tape roll cutting process (S53) by the ring knife, the ring knife protrusion to form a fine cut groove In accordance with the process (S54), and the completion of the adhesive tape recovery process (S55), the adhesive is applied to the fabric film to cut the adhesive tape roll 50 wound to a certain length on the paper tube to cut the fine groove (one side or both ends) 40 is formed to produce a free cutting adhesive tape (1).

우선, 건조 및 권취단계(도 5, S4)에 따라 권취된 점착테이프롤(50)은 테이프 재단기(2)가 구비된 절단실로 이송벨트 등에 의해 이송되어, 권취된 점착테이프롤 고정과정(S51)에 따라 상기 테이프 재단기(2)의 고정장치(60) 회전축(62)에 삽입되어 고정된다. First, the adhesive tape roll 50 wound according to the drying and winding step (FIG. 5, S4) is transferred to a cutting chamber equipped with a tape cutter 2, such as by a conveying belt, and the fixed adhesive tape roll fixing process (S51). In accordance with the tape cutting machine 2 of the fixing device 60 is inserted into the rotating shaft 62 is fixed.

그리고, 상기 위치가 고정된 점착테이프롤(50)은 점착테이프 회전과정(S52)에 따라, 상기 테이프 재단기(2)의 고정장치(60) 회전축(62)이 일측에 구비된 구동모터(미도시.)에 의해 회전하면서 일정한 회전속도를 가지며 회전하게 된다.In addition, the adhesive tape roll 50 having the fixed position is a driving motor (not shown) provided with a rotating shaft 62 of the fixing device 60 of the tape cutting machine 2 according to the adhesive tape rotation process S52. Rotate by.) And rotate with constant rotation speed.

한편, 상기 테이프 재단기(2)는 상기 점착테이프롤(50)을 절단하기 위한 원 형의 칼날구조를 가지는 링나이프(80)가 구비된 절단장치(70)를 포함하며, 링나이프에 의한 점착테이프롤 절단과정(S53)에 따라 상기 링나이프(80)는 절단장치(70)의 움직임에 의해 상기 점착테이프롤(50)을 일정한 폭으로 절단하여 단일 점착테이프로 구분시킨다. On the other hand, the tape cutting machine 2 includes a cutting device 70 provided with a ring knife 80 having a circular blade structure for cutting the adhesive tape roll 50, the adhesive tape by the ring knife According to the roll cutting process (S53), the ring knife 80 cuts the adhesive tape roll 50 to a predetermined width by the movement of the cutting device 70, and divides the adhesive tape roll 50 into a single adhesive tape.

그리고, 링나이프 돌기에 의한 미세절단홈 형성과정(S54)에 따라, 상기 절단과정(S53)에서 링나이프의 미세돌기에 의해 절단되는 점착테이프의 절단면, 즉 측단에 두께방향으로 미세절단홈(40)이 형성된다. 다시 말하면, 상기 링나이프는 점착테이프롤 측으로 이동하면서 회전하는 상기 점착테이프롤(50)을 가압하게 되고 그 가압력과 회전력에 의해 점착테이프롤(50)은 절단되는데, 이때 절단되어 구분되는 점착테이프(1)에는 링나이프의 측방향으로 돌출되게 형성된 미세돌기(81)에 의해 측단에 미세절단홈(40)이 형성된다. Then, according to the micro-cut groove forming process (S54) by the ring knife protrusion, the cutting surface of the adhesive tape is cut by the fine protrusion of the ring knife in the cutting process (S53), that is, the fine cutting groove 40 in the thickness direction on the side end (40) ) Is formed. In other words, the ring knife presses the rotating adhesive tape roll 50 while moving toward the adhesive tape roll side, and the adhesive tape roll 50 is cut by the pressing force and the rotational force. In 1), the fine cutting groove 40 is formed at the side end by the fine protrusion 81 formed to protrude in the lateral direction of the ring knife.

한편, 상기 링나이프(80)에 형성된 미세돌기(81)가 일측면에 형성되어 있다면 상기 점착테이프(1)는 일측단에 미세절단홈(40)이 형성되고, 상기 링나이프(80)에 형성된 미세돌기(81)가 양측면에 형성되어 있다면 상기 점착테이프(1)는 양측단에 미세절단홈(40)이 형성된다.On the other hand, if the fine protrusions 81 formed on the ring knife 80 is formed on one side, the adhesive tape 1 is formed with a fine cutting groove 40 on one side end, formed in the ring knife 80 If the fine protrusions 81 are formed on both sides, the adhesive tape 1 has fine cutting grooves 40 formed at both ends thereof.

그리고, 상기 미세절단홈(40)이 형성된 다수개의 점착테이프(1)로 구분되어 절단된 점착테이프롤(50)은 완료 점착테이프 회수과정(S55)에 따라, 상기 테이프 재단기(2)의 고정장치 회전축(62)에서 회수되어 제거되고 단일 점착테이프(1)로 생산된다. Then, the adhesive tape roll 50 is divided into a plurality of adhesive tape (1) formed with the fine cutting groove 40 is cut according to the completed adhesive tape recovery process (S55), the fixing device of the tape cutting machine (2) Recovered from the rotating shaft 62 is removed and produced as a single adhesive tape (1).

도 7(a)를 참조하여, 상기 테이프 재단기(2)를 보다 상세하게 살펴보면 다음 과 같다. Referring to Figure 7 (a), looking at the tape cutting machine 2 in more detail as follows.

상기 테이프 재단기(2)는, 크게 점착테이프롤(50)이 고정되어 일정한 회전속도로 구동모터(미도시.)에 의해 회전할 수 있게 하는 자동제어반(61)이 구비된 고정장치(60)와, 상기 고정장치(60)에 고정되어 회전하는 점착테이프롤(50)을 상기 자동제어반(61)에 저장된 입력값에 따라 일정한 폭을 가지도록 절단하는 링나이프(80)가 구비된 절단장치(70)로 구성된다. The tape cutting machine 2 is a fixing device 60 is provided with an automatic control panel 61 to allow the adhesive tape roll 50 is largely fixed to rotate by a drive motor (not shown) at a constant rotational speed; The cutting device 70 is provided with a ring knife 80 for cutting the adhesive tape roll 50 fixed and fixed to the fixing device 60 to have a predetermined width according to an input value stored in the automatic control panel 61. It is composed of

보다 상세하게, 상기 고정장치(60)는, 점착테이프롤(50)이 끼워져 삽입되는 회전축(62)이 구비된 본체(63)와, 상기 본체(63)의 일측에 구비되어 회전속도와 생산되는 점착테이프의 폭을 조절하는 자동제어반(61)으로 구성된다. In more detail, the fixing device 60 is provided with a main body 63 having a rotating shaft 62 into which the adhesive tape roll 50 is inserted and inserted into one side of the main body 63 to produce a rotational speed. It consists of an automatic control panel 61 for adjusting the width of the adhesive tape.

이에 따라, 상기 자동제어반(61)에 의해 회전축(62)의 회전속도와 생산되는 점착테이프의 절단폭이 결정되고, 상기 점착테이프롤(50)은 상기 회전축의 회전에 따라 회전하게 된다. Accordingly, the rotation speed of the rotary shaft 62 and the cutting width of the adhesive tape produced by the automatic control panel 61 are determined, and the adhesive tape roll 50 is rotated according to the rotation of the rotary shaft.

그리고, 상기 절단장치(70)는, 바람직하게 상기 고정장치(60)와 베이스 테이블(미도시)에 의해 연결되어 단일 공정을 수행할 수 있게 형성되는데, 상기 고정장치(60)의 회전축에 고정된 점착테이프롤(50)의 개수에 대응되는 수의 링나이프(80)와, 상기 링나이프(80)을 지지하는 회동축(72)이 형성된 몸체(71)로 구성된다. In addition, the cutting device 70 is preferably connected by the fixing device 60 and the base table (not shown) to perform a single process, which is fixed to the rotating shaft of the fixing device 60. It consists of a number of ring knives 80 corresponding to the number of the adhesive tape roll 50, the body 71 is formed with a rotating shaft 72 for supporting the ring knife 80.

이에 따라, 상기 링나이프(80)는 장치조작에 따른 몸체(71)의 이동에 따라 회전하는 점착테이프롤(50) 측으로 이동하여 접촉하면서, 상기 점착테이프롤(50)의 회전력에 따라 회동축(72)을 중심으로 상기 점착테이프롤(50)과 대응되는 방향으로 동일하게 회전하게 된다. 그리고, 상기 점착테이프롤(50) 방향으로 절단장치(70)의 몸체(71)가 이동하면서 상기 링나이프(80) 또한 이동하여 상기 점착테이프롤(50)을 가압력과 회전력에 의해 정해진 크기, 즉 일정폭 대로 절단하게 된다. Accordingly, the ring knife 80 moves to the side of the adhesive tape roll 50 which rotates in accordance with the movement of the body 71 according to the device operation, while contacting the ring knife 80 according to the rotational force of the adhesive tape roll 50. 72 is rotated the same in the direction corresponding to the adhesive tape roll (50). Then, while the body 71 of the cutting device 70 moves in the direction of the adhesive tape roll 50, the ring knife 80 also moves to move the adhesive tape roll 50 to a size determined by pressing force and rotational force. It cuts to a certain width.

한편, 도 8을 참조하면, 상기 링나이프(80)는 원형의 칼날을 가지기 때문에 점착테이프롤(50)의 절단시 가압력이 높게 되고, 강성(剛性)이 높은 점착테이프라도 확실하게 절단하는 것이 가능하다. Meanwhile, referring to FIG. 8, since the ring knife 80 has a circular blade, the pressing force is high when the adhesive tape roll 50 is cut, and the adhesive tape having high rigidity can be reliably cut. Do.

보다 상세하게, 상기 링나이프(80)는 원형몸체부(82)와, 상기 원형몸체부(82)의 외주면을 형성하는 원형칼날부(83)로 구성되고, 필요에 따라 상기 원형몸체부(82)의 중심에는 상기 절단장치(도7a, 70)의 회동축(도7a, 72)이 끼워져 위치될 수 있도록 관통된 축공(84)이 형성된다. More specifically, the ring knife 80 is composed of a circular body portion 82 and a circular blade portion 83 forming the outer circumferential surface of the circular body portion 82, the circular body portion 82 as necessary In the center of the) is formed a shaft hole 84 through which the rotating shafts (Figs. 7A and 72) of the cutting devices (Figs. 7A and 70) are fitted.

그리고, 상기 원형칼날부(83)의 단부를 따라 등간격으로 돌출된 미세돌기(81)가 형성된 것을 특징으로 한다. 이때, 상기 미세돌기(81)는 상기 원형칼날부(83)의 측방향으로 돌출되게 형성된다.Then, it characterized in that the micro-projections 81 protruding at equal intervals along the end of the circular blade portion 83 is formed. At this time, the fine protrusions 81 are formed to protrude in the lateral direction of the circular blade portion (83).

도 9(a)(b)를 참조하면, 바람직하게, 상기 미세돌기(81)는 원형칼날부의 측방향으로 돌출된 크기(b)가 3∼5 마이크론(micron)의 크기를 가지며, 원형칼날부(83)의 이웃하는 미세돌기(81)와 등간격(a), 바람직하게는 10㎜의 간격을 가지고 돌출되게 형성된 것을 특징으로 한다. Referring to Figure 9 (a) (b), preferably, the micro-projection 81 has a size (b) protruding laterally of the circular blade portion has a size of 3 to 5 microns, circular blade portion It is characterized in that it is formed to protrude at an interval (a), preferably 10 mm, and the adjacent minute protrusions 81 of (83).

그리고, 도 9(a)와 같이, 필요에 따라 상기 미세돌기(81)는 링나이프(80)의 원형칼날부의 일측방향으로 돌출되게 형성되거나, 도 9(b)와 같이 링나이프(80)의 원형칼날부의 양측방향으로 돌출되게 형성될 수 있다. And, as shown in Figure 9 (a), if necessary, the fine projection 81 is formed to protrude in one direction of the circular blade portion of the ring knife 80, or as shown in Figure 9 (b) of the ring knife 80 The circular blade portion may be formed to protrude in both directions.

일측방향으로 돌출되게 형성된 미세돌기(도9a, 81)가 형성된 링나이프(80)를 사용할 때 생산되는 점착테이프(1)은 일측단에만 미세절단홈(40)이 형성되고, 양측방향으로 돌출되게 형성된 미세돌기(도9b, 81)가 형성된 링나이프(80)를 사용할 때 생산되는 점착테이프(1)는 양측단에 미세절단홈(40)이 형성된다.The adhesive tape 1 produced when using the ring knife 80 formed with the fine protrusions (FIGS. 9A and 81) formed to protrude in one direction is formed with fine cutting grooves 40 formed only at one end thereof, and protrudes in both directions. The adhesive tape 1 produced when using the ring knife 80 formed with the formed fine protrusions (Figs. 9B and 81) has fine cutting grooves 40 formed at both ends thereof.

재차, 도 8을 참조하면, 이와 같은, 링나이프의 측방향으로 돌출된 미세돌기(81)를 형성하기 위해, 상기 링나이프(80)는 등간격으로 요홈(85)을 형성하면서 미세돌기(81)를 형성한다. Referring again to FIG. 8, in order to form the micro-projections 81 protruding in the lateral direction of the ring knife, the ring-knifes 80 form the grooves 85 at equal intervals while the micro-projections 81 are formed. ).

다시 말하면, 상기 링나이프(80)는, 상기 원형칼날부(83)의 단부를 따라 등간격으로 형성된 요홈(85)을 더 포함하며, 상기 미세돌기(81)는 상기 요홈을 형성하기 위한 외부충격에 의해 상기 원형칼날부(83)가 밀려나면서 측방향으로 돌출되어 형성된다. In other words, the ring knife 80 further includes grooves 85 formed at equal intervals along the ends of the circular blade portion 83, and the fine protrusions 81 have an external impact for forming the grooves. The circular blade portion 83 is protruded in the lateral direction by being pushed out by.

일예로, 상기 요홈(85)은 일정한 등간격으로 정과 망치와 같은 도구를 이용하여 수공으로 형성할 수 있다. 이때 상기 요홈(85)을 형성하기 위해 충격을 가할 때 밀려나는 원형칼날부(83)의 일측에 의해 상기 미세돌기(81)는 측방향으로 밀려 형성된다. For example, the groove 85 may be formed by hand using a tool such as a chisel and a hammer at regular equal intervals. At this time, the micro-projections 81 are pushed in the lateral direction by one side of the circular blade portion 83 that is pushed out when an impact is applied to form the grooves 85.

또다른 예로, 상기 요홈(85)은 상기 요홈(85)과 이웃하는 요홈(85)의 간격과 동일하게 돌출된 절단날을 가지는 원형의 장치를 이용한다. 이에 따라, 링나이프(80)을 상기 원형 장치를 따라 회전시키면서 상기 원형장치의 절단날이 링나이프(80)의 원형칼날부(83)를 쪼아 요홈(85)을 형성하면서 일측이 측방향으로 밀리게 되고 미세돌기(81)가 형성된다. As another example, the groove 85 uses a circular device having a cutting blade that protrudes to be equal to the distance between the groove 85 and the adjacent groove 85. Accordingly, while rotating the ring knife 80 along the circular device, one side is pushed laterally while the cutting blade of the circular device peckes the circular blade portion 83 of the ring knife 80 to form the groove 85. And fine protrusions 81 are formed.

다시, 도 7(b)를 참조하면, 이와 같이 등간격으로 다수개의 미세돌기(81)가 형성된 링나이프(80)는, 회전하는 점착테이프롤(50)의 회전에 따라 이와 접촉하면서 회전력에 의해 동일하게 회전하게 된다. 그리고, 절단장치의 움직임에 따라 상기 점착테이프롤(50)에 가압력을 가해 그 힘과 회전력에 의해 상기 점착테이프롤(50)을 절단하게 된다. Referring again to FIG. 7B, the ring knife 80 having the plurality of fine protrusions 81 formed at equal intervals in this manner is contacted with the rotation of the rotating adhesive tape roll 50 by the rotational force. Will rotate the same. Then, the pressure is applied to the pressure-sensitive adhesive tape roll 50 in accordance with the movement of the cutting device to cut the pressure-sensitive adhesive tape roll 50 by the force and rotational force.

이때, 상기 링나이프(80)에 돌출되게 형성된 미세돌기(81)는 링나이프의 회전에 따라 상기 점착테이프롤(50)을 파고들면서 절단되는 면상, 즉 완성된 점착테이프(1)의 측단면을 따라 미세절단홈(40)을 롤형태의 두께방향으로 형성하게 된다. At this time, the minute projections 81 formed to protrude from the ring knife 80 are cut into the adhesive tape roll 50 as the ring knife rotates, that is, the side cross-section of the completed adhesive tape 1. Accordingly, the fine cutting groove 40 is formed in the thickness direction of the roll shape.

그리고, 상기 링나이프(80)의 회전하게 되는 속도와 점착테이프롤(50)의 두께에 따라, 그리고 원단필름에 도포된 점착제의 저항력에 따라 점착테이프(1)에 형성되는 상기 미세절단홈(40)은 이웃하는 미세절단홈(40)과 등간격이 아닌 불규칙한 간격을 가지며 형성된다. The micro-cut groove 40 is formed in the adhesive tape 1 according to the speed at which the ring knife 80 rotates and the thickness of the adhesive tape roll 50 and the resistance of the adhesive applied to the fabric film. ) Is formed at irregular intervals and not at equal intervals with the neighboring micro cutting groove 40.

그러나, 이와 같이 형성되는 미세절단홈(40)은 육안으로 쉽게 확인되지 않을 정도의 크기와 길이로 그리고 이웃하는 미세절단홈(40)과는 사용자의 사용에 불편함이 없을 정도로 밀접하게 형성되기 때문에, 사용자는 포장 등의 용도로 상기 절단이 자유로운 점착테이프(1)를 사용할 때 전혀 불편함이 없이 원하는 길이로 상기 점착테이프(1)를 사용하고 쉽게 미세절단홈(40)을 이용하여 절단할 수 있다. However, since the fine cutting groove 40 is formed in such a size and length that it is not easily identified with the naked eye and the neighboring micro cutting groove 40 is so close that there is no inconvenience for the user. , The user can use the adhesive tape (1) to the desired length without any inconvenience when using the adhesive tape (1) free cutting for the purpose of packaging and can be easily cut using the fine cutting groove (40) have.

이상에서 기술한 바와 같이, 본 발명에 따른 절단이 자유로운 점착테이프(1)는 사무실, 학교 등에서 일상적으로 사용되는 부착용, 문서의 수정용, 박스 포장 등 여러 용도와 목적을 같는 점착테이프의 성능을 만족시키고, 날카로운 절단도구없이 테이프를 쉽게 사용자 임의 길이대로 절단 할 수 있는 특징으로, 도구의 사용 이 미숙한 어린이들이 사용해도 위험성이 없는 점착테이프를 제공한다.As described above, the free-cutting adhesive tape 1 according to the present invention satisfies the performance of the adhesive tape having the same purpose and purpose as for various applications such as attachment, document modification, and box packaging, which are used in offices and schools. It can be cut easily to user's arbitrary length without sharp cutting tool, and it provides adhesive tape without risk even for children who are inexperienced in using the tool.

이상에서 설명한 본 발명은 발명이 속하는 기술분야에서 통상의 지식을 가진 자에 있어 본 발명의 기술적 사상을 벗어나지 않는 범위 내에서 여러 가지 치환 변형 및 변경이 가능하므로 전술한 실시예 및 첨부된 도면에 한정되는 것은 아니다.The present invention described above is limited to the above-described embodiment and the accompanying drawings as various substitutions and modifications can be made within a range without departing from the technical spirit of the present invention for those skilled in the art. It doesn't happen.

도 1(a)(b)(c)는 종래 기술에 따른 절단이 용이한 점착테이프를 보여주는 사시도 및 부분 평면도. Figure 1 (a) (b) (c) is a perspective view and a partial plan view showing an easy-to-cut adhesive tape according to the prior art.

도 2는 종래 기술에 따른 절단이 용이한 점착테이프를 제조하기 위한 장치를 보여주는 개략적인 도면. Figure 2 is a schematic view showing an apparatus for producing a tape for easy cutting according to the prior art.

도 3은 본 발명에 따른 절단이 자유로운 점착테이프를 보여주는 사시도 및 부분 확대도. Figure 3 is a perspective view and a partially enlarged view showing a free cutting adhesive tape according to the present invention.

도 4는 본 발명에 따른 절단이 자유로운 점착테이프의 일부를 보여주는 평면도 및 부분 확대도. Figure 4 is a plan view and a partial enlarged view showing a part of the adhesive tape free cutting according to the present invention.

도 5는 본 발명에 따른 절단이 자유로운 점착테이프의 제조방법을 보여주는 공정도. 5 is a process chart showing a method of manufacturing a free cutting adhesive tape according to the present invention.

도 6은 본 발명의 절단이 자유로운 점착테이프의 제조방법에 따른 절단단계를 보여주는 과정도.Figure 6 is a process showing a cutting step according to the method of manufacturing a free cutting adhesive tape of the present invention.

도 7(a)(b)는 도 6에 따른 점착테이프롤의 절단과정과 미세절단홈의 형성을 보여주는 개략적인 도면. Figure 7 (a) (b) is a schematic diagram showing the process of cutting the adhesive tape roll according to Figure 6 and the formation of micro-cut grooves.

도 8은 본 발명의 절단이 자유로운 점착테이프의 제조방법에 따른 절단장치에 적용되는 링나이프를 보여주는 사시도. Figure 8 is a perspective view showing a ring knife applied to the cutting device according to the method of manufacturing a free cutting adhesive tape of the present invention.

도 9(a)(b)는 도 8에 따른 링나이프의 일예를 보여주는 평면도. 9 (a) and 9 (b) are plan views illustrating one example of a ring knife according to FIG. 8.

***도면의 주요 부분에 대한 부호 설명****** Explanation of symbols for main parts of drawings ***

1 : 절단이 자유로운 점착테이프1: Free adhesive tape

1a : 절단이 자유로운 점착테이프 제조방법1a: Method of manufacturing adhesive tape with free cutting

10 : 원단필름 20 : 점착제10: fabric film 20: adhesive

30 : 종이 지관 40 : 미세절단홈30: paper branch 40: fine cutting groove

50 : 점착테이프롤 80 : 링나이프50: adhesive tape roll 80: ring knife

81 : 미세돌기81: fine protrusion

Claims (12)

삭제delete 삭제delete 삭제delete 삭제delete 합성수지를 일축 또는 이축 연신하여 길이를 늘린 원단필름과, 상기 원단 필름의 일면에 도포된 점착제를 포함하고, 이를 지관에 두께를 가지는 롤형태로 권취하여 구성되는 점착테이프를 제조하는 제조방법에 있어서,In the manufacturing method for producing a pressure-sensitive adhesive tape comprising a fabric film extending the length by uniaxially or biaxially stretched a synthetic resin, and a pressure-sensitive adhesive applied to one surface of the fabric film, and wound in a roll shape having a thickness on the branch pipe, 천연 또는 합성 고무계와 수지, 노화방지제, 유기용제 등을 배합탱크에 넣어 점착제로 배합·숙성시키는 점착제 배합단계와;A pressure-sensitive adhesive compounding step of blending and maturing a natural or synthetic rubber system with a resin, an anti-aging agent, an organic solvent, etc. in a mixing tank; 권취된 상태의 원단필름을 상기 점착제를 도포하기 위한 위치로 이송시키는 원단필름 공급단계와;A raw film supplying step of transferring the rolled film to a position for applying the pressure-sensitive adhesive; 상기 원단필름의 일측면에 상기 점착제를 완전히 도포하고, 타측면은 배면처리하여 코팅하는 점착제 도포단계와;A pressure-sensitive adhesive coating step of completely applying the pressure-sensitive adhesive on one side of the fabric film, and coating the other side by treating the back surface; 상기 원단필름에 도포된 점착제를 열풍건조시키고, 점착제가 도포된 원단필름을 지관에 감아 점착테이프롤을 형성하는 건조 및 권취단계와;A drying and winding step of drying the pressure-sensitive adhesive applied to the fabric film and winding the fabric-coated film to which the pressure-sensitive adhesive is applied to a paper tube to form an adhesive tape roll; 상기 점착테이프롤을 테이프 재단기를 이용하여 일정폭을 가지는 점착테이프로 절단하되, 상기 테이프 재단기는 단부의 측방향으로 미세돌기가 형성된 링나이프가 구비되어 상기 링나이프에 의해 상기 점착테이프는 측단에 미세절단홈이 형성되면서 절단되는 절단단계와;The adhesive tape roll is cut into an adhesive tape having a predetermined width by using a tape cutting machine, and the tape cutting machine is provided with a ring knife formed with fine protrusions in a lateral direction of an end portion, and the adhesive tape is finely formed at a side end by the ring knife. A cutting step of cutting while the cutting groove is formed; 상기 절단된 점착테이프를 단위별로 포장하고 출고하는 포장·완료단계를 포함하여 이루어지며;It comprises a packing and completion step of packing and shipping the cut adhesive tape for each unit; 상기 점착테이프의 측단에 형성된 미세절단홈에 의해 절단이 용이한 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법. Method for producing a pressure-sensitive adhesive tape, characterized in that the cutting is easy by the fine cutting groove formed on the side end of the adhesive tape. 제 5항에 있어서, The method of claim 5, 상기 원단필름은, 상기 원단필름은, 폴리프로필렌(PP)을 이축으로 연신하여 제조한 BOPP필름인 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법. Wherein the raw film, the raw film is a BOPP film produced by stretching polypropylene (PP) biaxially characterized in that the adhesive tape free cutting. 제 5항에 있어서, 상기 절단단계는, The method of claim 5, wherein the cutting step, 점착테이프롤을 테이프 재단기의 고정장치 회전축에 끼워 삽입하는 권취된 점착테이프롤 고정과정과, A wound adhesive tape roll fixing process for inserting the adhesive tape roll into the rotating shaft of the fixing device of the tape cutting machine, 상기 회전축을 회전시켜 점착테이프롤이 일정한 회전속도를 가지며 회전하는 점착테이프롤 회전과정과,A pressure-sensitive adhesive tape roll rotating process in which the pressure-sensitive adhesive tape roll rotates by rotating the rotary shaft; 상기 회전하는 점착테이프롤을 상기 테이프 재단기의 절단장치 링나이프를 이용하여 폭을 가지도록 절단하여 단일 점착테이프로 생산하는 링나이프에 의한 점착테이프롤 절단과정과, Cutting the rotating adhesive tape roll to have a width using a cutting device ring knife of the tape cutting machine, and cutting the adhesive tape roll by a ring knife to produce a single adhesive tape; 상기 절단과정에서 링나이프의 미세돌기에 의해 절단되는 점착테이프의 절단면에 두께방향으로 미세절단홈을 형성시키는 링나이프 돌기에 의한 미세절단홈 형성과정과,Forming a fine cutting groove by a ring knife protrusion to form a fine cutting groove in the thickness direction on the cutting surface of the adhesive tape cut by the fine protrusion of the ring knife in the cutting process; 상기 미세절단홈이 형성된 다수개의 점착테이프로 절단된 점착테이프롤을 회전축에서 제거하는 완료 점착테이프 회수과정을 포함하여 이루어지는 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법. And a completed adhesive tape recovery process for removing the adhesive tape roll cut into a plurality of adhesive tapes having the fine cutting grooves formed on the rotating shaft. 제 5항에 있어서, 상기 절단단계에서 사용되는 테이프 재단기는, According to claim 5, The tape cutting machine used in the cutting step, 점착테이프롤이 끼워져 삽입되는 회전축이 구비된 본체와, 상기 본체의 일측에 구비되어 상기 회전축의 회전속도와 점착테이프롤의 절단폭을 제어하는 자동제어반이 형성된 고정장치와, A fixing device having a main body provided with a rotating shaft into which the adhesive tape roll is inserted, an automatic control panel provided at one side of the main body to control the rotation speed of the rotating shaft and the cutting width of the adhesive tape roll; 상기 점착테이프롤의 개수에 대응되는 수의 링나이프와, 상기 링나이프를 지지하는 회동축이 구비된 몸체가 형성된 절단장치를 포함하여 구성된 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법. And a cutting device having a body having a number of ring knives corresponding to the number of the adhesive tape rolls, and a rotating shaft supporting the ring knives. 제 5항, 제 7항 또는 제 8항 중 어느 한 항에 있어서, The method according to any one of claims 5, 7, or 8, 상기 링나이프는, 원형몸체부와, 상기 원형몸체부의 외주면을 형성하는 원형칼날부와, 상기 원형칼날부의 단부를 따라 등간격으로 측방향 돌출된 미세돌기를 포함하여 구성된 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법. The ring knife comprises a circular body portion, a circular blade portion forming the outer circumferential surface of the circular body portion, and free cutting is characterized in that it comprises a micro projection protruding laterally at equal intervals along the end of the circular blade portion Adhesive tape manufacturing method. 제 9항에 있어서, The method of claim 9, 상기 링나이프는, 상기 원형칼날부의 단부를 따라 등간격으로 형성된 요홈을 더 포함하며, 상기 미세돌기는 상기 요홈을 형성하기 위한 외부충격에 의해 상기 원형칼날부가 밀려나면서 측방향으로 돌출되어 형성된 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법. The ring knife further includes grooves formed at equal intervals along the ends of the circular blade portion, wherein the fine protrusion is formed by protruding laterally while the circular blade portion is pushed out by an external impact to form the groove. Adhesive tape manufacturing method to be cut freely. 제 9항에 있어서, The method of claim 9, 상기 미세돌기는, 3∼5 마이크론(micron)의 크기로 원형칼날부의 일측방향으로 이웃하는 미세돌기와 10㎜의 간격을 가지고 돌출되게 형성된 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법.The fine projection is a cut-free adhesive tape, characterized in that formed to protrude at a spacing of 10 mm with the neighboring fine projection in one direction of the circular blade portion in the size of 3 to 5 microns (micron). 제 9항에 있어서, The method of claim 9, 상기 미세돌기는, 3∼5 마이크론(micron)의 크기로 원형칼날부의 양측방향으로 이웃하는 미세돌기와 10㎜의 간격을 가지고 돌출되게 형성된 것을 특징으로 하는 절단이 자유로운 점착테이프 제조방법.The fine projection is a cut-free adhesive tape manufacturing method, characterized in that formed to protrude at intervals of 10 mm with neighboring fine projections in both sides of the circular blade portion in the size of 3 to 5 microns (micron).
KR1020070081093A 2007-08-13 2007-08-13 Adhesive-tape be easy to cut and manufacturing method the same KR100795949B1 (en)