KR100647259B1 - The manufacturing method of the play card - Google Patents

The manufacturing method of the play card Download PDF

Info

Publication number
KR100647259B1
KR100647259B1 KR1020060017413A KR20060017413A KR100647259B1 KR 100647259 B1 KR100647259 B1 KR 100647259B1 KR 1020060017413 A KR1020060017413 A KR 1020060017413A KR 20060017413 A KR20060017413 A KR 20060017413A KR 100647259 B1 KR100647259 B1 KR 100647259B1
Authority
KR
South Korea
Prior art keywords
silver foil
paper
printing
coating
ink
Prior art date
Application number
KR1020060017413A
Other languages
Korean (ko)
Other versions
KR20060022308A (en
Inventor
홍진남
Original Assignee
(주)도원씨엔피
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by (주)도원씨엔피 filed Critical (주)도원씨엔피
Priority to KR1020060017413A priority Critical patent/KR100647259B1/en
Publication of KR20060022308A publication Critical patent/KR20060022308A/en
Application granted granted Critical
Publication of KR100647259B1 publication Critical patent/KR100647259B1/en

Abstract

본 발명은 놀이용 카드의 제조방법에 관한 것으로, 놀이용 카드를 제작할 때에 원지 위에 은박을 먼저 형압한 후, 그 상에 UV 잉크를 이용하여 인쇄함으로써 은박에 명암의 효과를 나타낼 수 있어서 입체감이 증대되며, 형압된 부분과 인쇄된 부분이 정밀하게 일치하여 고품질의 제품을 얻을 수 있는 특징이 있다.The present invention relates to a method of manufacturing a playing card, in which a silver foil is first pressed on a sheet of paper when a playing card is produced, and then printed using UV ink thereon, thereby exhibiting the effect of light and shade on the silver foil, thereby increasing the three-dimensional effect. The press-formed part and the printed part are precisely matched to obtain a high quality product.

본 발명은 크게 네 단계를 거쳐 완성되는바, 인쇄기(A)를 이용하여 원지(10) 상에 은박(20)을 110℃의 온도와 130kgf/cm2의 압력으로 형압하는 은박 형성공정(S1)과, 상기 형성된 은박(20) 상면에 남색(cyan), 자홍색(magenta), 노란색(yellow), 검은색(black)으로 구성된 UV 잉크(30)를 UV 인쇄기(B)를 통해 인쇄한 후 UV 경화장치(C)로 건조하는 UV 인쇄공정(S2)과, 상기 경화가 완료된 원지(10) 상에 코팅액(40)을 도포하는 코팅공정(S3)과, 코팅액(40)의 도포가 완료된 원지(10)를 상온에서 건조시키고, 소정의 크기로 재단하는 건조 및 재단공정(S4)으로 구성되어, 카드(50)에 형성된 은박(20) 상면에 명암을 표현할 수 있어 입체감이 증대되고 일층 미려한 구성을 갖는다.The present invention is largely completed through four steps, using a printing machine (A) to form a silver foil 20 on a sheet of paper 10 at a temperature of 110 ℃ and pressure of 130kgf / cm 2 (S1) And, after printing the UV ink 30 consisting of cyan, magenta, yellow, black on the upper surface of the formed silver foil 20 through a UV printing machine (B), UV curing UV printing process (S2) drying with the apparatus (C), the coating process (S3) for applying the coating liquid 40 on the hardened paper 10, and the base paper 10, the application of the coating liquid 40 is completed ) Is dried at room temperature, and the drying and cutting process (S4) is cut to a predetermined size, the contrast can be expressed on the upper surface of the silver foil 20 formed on the card 50, the three-dimensional effect is increased and has a more beautiful configuration. .

상기와 같이 구성된 본 발명은, 놀이용 카드를 제작할 때에 원지 위에 은박을 먼저 형압한 후, 그 상에 UV 잉크를 이용하여 인쇄함으로써 은박에 명암의 효과 를 나타낼 수 있어서 입체감이 증대되며, 형압된 부분과 인쇄된 부분이 정밀하게 일치하여 고품질의 제품을 얻을 수 있는 효과가 있다.The present invention configured as described above can press the silver foil on a sheet of paper first when producing a playing card, and then print using UV ink thereon, thereby producing the effect of contrast on the silver foil. And printed parts are precisely matched to have a high quality product.

또한, 외형이 미려하여 장기간 사용하여도 싫증을 유발하지 않으며, 대형브로마이드 형태로 제작할 경우 장식성이 뛰어나 소장가치를 높일 수 있는 또 다른 효과가 있다.In addition, the appearance is beautiful and does not cause tiredness even after long-term use, and when produced in the form of large bromide, there is another effect that can increase the small collection value because of excellent decoration.

놀이용 카드, 은박인쇄, UV 인쇄, 형압, 코팅액, 브로마이드 Playing cards, silver foil printing, UV printing, mold pressure, coating solution, bromide

Description

놀이용 카드의 제조방법 { The manufacturing method of the play card }The manufacturing method of the play card}

도 1은 본 발명의 공정 순서도1 is a process flow chart of the present invention

도 2는 본 발명의 제조 공정도2 is a manufacturing process diagram of the present invention

도 3은 본 발명 은박공정의 완료상태를 나타낸 상태도Figure 3 is a state diagram showing the completion state of the present invention silver foil process

도 4는 본 발명 UV 인쇄공정의 완료상태를 나타낸 상태도Figure 4 is a state diagram showing the completion state of the present invention UV printing process

[도면의 주요 부분에 대한 부호의 설명][Description of Symbols for Main Parts of Drawing]

10: 원지 20: 은박10: base 20: foil

30: UV 잉크 40: 코팅액30: UV ink 40: coating liquid

50: 카드 A: 인쇄기50: card A: printing press

B: UV 인쇄기 C: UV 경화장치B: UV Printing Machine C: UV Curing Equipment

D: 코팅액 도포기 E: 재단기D: Coating liquid applicator E: Cutting machine

S1: 은박형성 공정 S2: UV 인쇄공정S1: silver foil forming process S2: UV printing process

S3: 코팅공정 S4: 건조 및 재단공정S3: Coating Process S4: Drying and Cutting Process

본 발명은 놀이용 카드의 제조방법에 관한 것으로, 더욱 상세하게 설명하면, 놀이용 카드를 제작할 때에 원지 위에 은박을 먼저 형압한 후, 그 상에 UV 잉크를 이용하여 인쇄함으로써 은박에 명암의 효과를 나타낼 수 있어서 입체감이 증대되며, 형압된 부분과 인쇄된 부분이 정밀하게 일치하여 고품질의 제품을 얻을 수 있는 놀이용 카드의 제조방법에 관한 것이다.The present invention relates to a method of manufacturing a playing card, and in more detail, when producing a playing card, the silver foil is first pressed on a sheet of paper, and then printed using UV ink thereon to effect the contrast on the silver foil. The present invention relates to a manufacturing method of a playing card, in which a three-dimensional effect is increased, and a molded part and a printed part are precisely matched to obtain a high quality product.

일반적으로 놀이용 카드라 함은 여러 장의 카드로 구성된 한 벌 또는 여러 벌의 카드를 가지고 여러 사람이 놀이용으로 즐기기 위해 제작된 것으로, 그 대표적인 예로 어린이용 캐릭터 카드를 들 수 있다.In general, a playing card is a one or a plurality of cards composed of a number of cards that are produced for the enjoyment of several people, a typical example is a character card for children.

상기와 같은 어린이용 캐릭터 카드의 종래 제조방법을 살펴보면, 동판을 제작한 후, 인쇄기를 이용하여 인쇄 원단 위에 다양한 색상의 그림과 문자를 인쇄한 다음, 그에 은박을 형성시킴으로써 그림 상에는 단순히 은색으로만 은박이 표현되는 단점이 있었다.Looking at the conventional manufacturing method of the character card for children as described above, after manufacturing the copper plate, using a printing machine to print a picture and characters of various colors on the printed fabric, and then to form a silver foil on the picture simply silver foil on the picture There were drawbacks to this.

이로 인해 그 전체적인 형태가 은박과 그림이 서로 분리된 형태로 보여져 미려치 않으며, 명암의 효과가 전혀 나타나지 않아 입체감을 느낄 수 없는 문제점을 내포하고 있었으며, 사용자로 하여금 금방 싫증을 유발시키는 문제점을 내포하고 있었다.Because of this, the overall shape is not intriguing because silver foil and the picture are separated from each other, and the effect of contrast does not appear at all, which implies that the user cannot feel the three-dimensional effect. there was.

이에 본 발명은 상기와 같은 문제점을 감안하여 발명한 것으로, 놀이용 카드를 제작할 때에 원지 위에 은박을 먼저 형압한 후, 그 상에 UV 잉크를 이용하여 인쇄함으로써 은박에 명암의 효과를 나타낼 수 있어서 입체감이 증대되며, 형압된 부분과 인쇄된 부분이 정밀하게 일치하여 고품질의 제품을 얻을 수 있도록 함을 목적으로 한다.Therefore, the present invention was invented in view of the above problems, and when producing a playing card, the silver foil was first pressed on a sheet of paper, and then printed using UV ink thereon, thereby producing the effect of contrast on the silver foil. This is to be increased, and the pressed part and the printed part are precisely matched to obtain a high quality product.

또한, 외형이 미려하여 장기간 사용하여도 싫증을 유발하지 않으며, 대형브로마이드 형태로 제작할 경우 장식성이 뛰어나 소장가치를 높일 수 있도록 함을 목적으로 한다.In addition, it is beautiful in appearance and does not cause boring even for long-term use, and when manufactured in the form of large bromide, it is aimed at improving the small collection value because of its excellent decorativeness.

본 발명은 놀이용 카드의 제조방법에 관한 것으로, 놀이용 카드를 제작할 때에 원지 위에 은박을 먼저 형압한 후, 그 상에 UV 잉크를 이용하여 인쇄함으로써 은박에 명암의 효과를 나타낼 수 있어서 입체감이 증대되며, 형압된 부분과 인쇄된 부분이 정밀하게 일치하여 고품질의 제품을 얻을 수 있는 특징이 있다.The present invention relates to a method of manufacturing a playing card, in which a silver foil is first pressed on a sheet of paper when a playing card is produced, and then printed using UV ink thereon, thereby exhibiting the effect of light and shade on the silver foil, thereby increasing the three-dimensional effect. The press-formed part and the printed part are precisely matched to obtain a high quality product.

본 발명은 크게 네 단계를 거쳐 완성되는바, 인쇄기(A)를 이용하여 원지(10) 상에 은박(20)을 110℃의 온도와 130kgf/cm2의 압력으로 형압하는 은박 형성공정(S1)과, 상기 형성된 은박(20) 상면에 남색(cyan), 자홍색(magenta), 노란색(yellow), 검은색(black)으로 구성된 UV 잉크(30)를 UV 인쇄기(B)를 통해 인쇄한 후 UV 경화장치(C)로 건조하는 UV 인쇄공정(S2)과, 상기 경화가 완료된 원지(10) 상에 코팅액(40)을 도포하는 코팅공정(S3)과, 코팅액(40)의 도포가 완료된 원지(10)를 상온에서 건조시키고, 소정의 크기로 재단하는 건조 및 재단공정(S4)으로 구성되어, 카드(50)에 형성된 은박(20) 상면에 명암을 표현할 수 있어 입체감이 증대되고 일층 미려한 구성을 갖는다.The present invention is largely completed through four steps, using a printing machine (A) to form a silver foil 20 on a sheet of paper 10 at a temperature of 110 ℃ and pressure of 130kgf / cm 2 (S1) And, after printing the UV ink 30 consisting of cyan, magenta, yellow, black on the upper surface of the formed silver foil 20 through a UV printing machine (B), UV curing UV printing process (S2) drying with the apparatus (C), the coating process (S3) for applying the coating liquid 40 on the hardened paper 10, and the base paper 10, the application of the coating liquid 40 is completed ) Is dried at room temperature, and the drying and cutting process (S4) is cut to a predetermined size, the contrast can be expressed on the upper surface of the silver foil 20 formed on the card 50, the three-dimensional effect is increased and has a more beautiful configuration. .

이하 본 발명의 실시 예를 첨부된 도면을 참조하여 상세히 설명하면 다음과 같다.Hereinafter, an embodiment of the present invention will be described in detail with reference to the accompanying drawings.

도 1은 본 발명의 전체 공정도를 나타낸 것이고, 도 2는 본 발명의 제조공정도를 나타낸 것으로, 도시한 바와 같이, 네 단계를 거침으로 본 발명의 놀이용 카드가 제조되는바, 우선, 제 1공정은 동판에 인쇄하고자 하는 그림의 조각한 후, 이를 인쇄기(A)에 장착하고, 원지(10)를 공급하여 은박(20)을 형압시키는 은박 형성공정(S1)을 완료한다.Figure 1 shows the overall process diagram of the present invention, Figure 2 shows a manufacturing process diagram of the present invention, as shown, the playing card of the present invention is manufactured through four steps, first, first step After engraving the picture to be printed on the silver copper plate, it is mounted on the printing machine (A), and the raw paper 10 is supplied to complete the silver foil forming process (S1) for pressing the silver foil 20.

상기 은박(20)을 형성시키기 위한 바람직한 조건은 110℃의 온도와 130kgf/cm2의 압력으로 형압하는바, 이로써 은박(20)이 동판에 형성된 문양대로 원 지(10)에 형성될 수 있도록 구성된다.Preferred conditions for forming the silver foil 20 is to mold at a temperature of 110 ℃ and pressure of 130kgf / cm 2 , whereby the silver foil 20 can be formed on the base paper 10 as a pattern formed on the copper plate do.

상기 은박(20)이 형성된 형태가 도 3에 잘 도시되어 있는바, 은박(20)뿐만 아니라 필요에 따라 금박 등에도 동일한 형태로 작업이 가능한 구성을 갖는다.The form in which the silver foil 20 is formed is well illustrated in FIG. 3, and not only the silver foil 20 but also a gold foil or the like as required, has a configuration capable of working in the same form.

그런 다음 행해지는 제 2공정은, 은박(20)이 형압된 원지(10)를 UV 인쇄기(B)에 투입하여 은박(20)이 형성된 부위와 원지(10) 상에 제작하고자 하는 문양대로 UV 잉크(30)를 사용하여 인쇄하는 UV 인쇄공정(S2)을 완료한다.Then, the second step is carried out by putting the base paper 10 on which the silver foil 20 is pressurized into the UV printing machine B, UV ink according to the portion where the silver foil 20 is formed and the pattern to be produced on the base paper 10. The UV printing process S2 for printing using 30 is completed.

상기 UV 인쇄 시에는 남색(cyan), 자홍색(magenta), 노란색(yellow), 검은색(black)으로 구성된 4색 UV 잉크(30)를 사용하며, UV 인쇄 후 UV 경화장치(C)를 통과시킴으로써 순간적으로 UV 잉크(30)가 건조되는 구성을 갖는다.In the UV printing, a four-color UV ink 30 composed of cyan, magenta, yellow, and black is used. After UV printing, the UV curing apparatus C is passed through Instantly, the UV ink 30 is dried.

상기 UV 잉크(30)는 도 4에 도시된 바와 같이, 일반 종이뿐만 아니라 은박 및 합성수지에도 인쇄가 가능하여 상기 원지(10)뿐만 아니라 은박(20) 상에도 깨끗하게 인쇄되도록 구성된다.As shown in FIG. 4, the UV ink 30 may be printed on silver foil and synthetic resin as well as plain paper, so that the UV ink 30 may be cleanly printed on not only the base paper 10 but also the silver foil 20.

그 후 행해지는 제 3공정은, 상기 은박(20) 상에 인쇄된 UV 잉크(30)가 완전히 건조된 후에 그 표면 전체에 코팅액 도포기(D)로 코팅액(40)을 균일하게 도포하여 코팅을 완료하는 코팅공정(S3)을 완료한다.After the third step is carried out, after the UV ink 30 printed on the silver foil 20 is completely dried, the coating liquid 40 is uniformly applied with the coating liquid applicator D on the entire surface to apply the coating. Complete the coating process (S3) to complete.

상기 공정에서 주로 사용되는 코팅액(40)은 수성 바니스를 주로 사용하는바, 주로 사진이나 그림이 많이 인쇄된 곳에 사용이 적합하며, 원지(10) 전체를 코팅할 경우에는 별도의 필름이 필요치 않아 제작 비용과 제작 속도가 향상되는 구성을 가 지며, 부분적인 코팅도 세밀하게 코팅되는 특징이 있다.The coating liquid 40 mainly used in the above process is mainly used for the aqueous varnish, which is suitable for use mainly where a lot of pictures or pictures are printed, and when coating the entire base paper 10, a separate film is not required. It has a structure that improves cost and manufacturing speed, and the partial coating is characterized by fine coating.

마지막 공정인 제 4공정은, 상기 도포된 코팅액(40)을 상온에서 건조시킨 후, 재단기(E)를 이용하여 소정의 크기로 재단하는 건조 및 재단공정(S4)을 완료한다.The fourth step, which is the last step, is to dry the coated coating liquid 40 at room temperature, and then complete the drying and cutting process (S4) of cutting to a predetermined size using the cutting machine (E).

상기 코팅액(40)이 완전히 건조되면 전체 광택이 반광정도로 코팅된 면이 부드럽고 고급스러우며, 장기간 사용시에도 코팅된 면이 훼손되지 않아 인쇄된 그림과 은박이 벗겨지지 않는 구성을 갖는다.When the coating liquid 40 is completely dried, the surface is coated with a gloss of semi-gloss and is soft and luxurious, and the coated surface is not damaged even after long-term use, so that the printed picture and silver foil are not peeled off.

상기와 같이 코팅이 완료되면, 카드의 크기에 맞게 자동으로 재단되어 한 벌의 카드(50)를 완성하도록 하며, 완성된 카드(50)는 이후에 행해지는 별도의 정렬 및 포장공정으로 이송되는바, 제품의 자동 정렬기와 제품의 자동 공급장치를 통해 완제품이 완성되는 구성을 갖는다.When the coating is completed as described above, it is automatically cut to fit the size of the card to complete a set of cards 50, the completed card 50 is transferred to a separate alignment and packaging process to be performed later The finished product is completed through the automatic aligner of the product and the automatic supply of the product.

상기와 같이 구성된 본 발명은 놀이용 카드에 국한되어 사용되지 않고, 원지(10)의 전체에 캐릭터 형태 등의 다양한 은박(20)을 형성시키고, 그 위에 4색 UV 잉크(30)를 사용하여 그림을 인쇄한 다음, 코팅액(40)을 도포하여 대형 브로마이드를 제작함으로써 상품성과 보존성이 우수한 브로마이드 제작에도 적합하도록 구성된다.The present invention configured as described above is not limited to a playing card, and forms various silver foils 20, such as character shapes, on the whole of the base paper 10, and uses four-color UV ink 30 thereon for painting. After printing, by coating the coating liquid 40 to produce a large bromide is configured to be suitable for the production of bromide excellent in merchandise and storage properties.

상기와 같이 구성된 본 발명은, 놀이용 카드를 제작할 때에 원지 위에 은박을 먼저 형압한 후, 그 상에 UV 잉크를 이용하여 인쇄함으로써 은박에 명암의 효과를 나타낼 수 있어서 입체감이 증대되며, 형압된 부분과 인쇄된 부분이 정밀하게 일치하여 고품질의 제품을 얻을 수 있는 효과가 있다.According to the present invention configured as described above, when producing a playing card, the silver foil is first pressed on a sheet of paper, and then printed using UV ink thereon, so that the effect of contrast on the silver foil can be exhibited so that a three-dimensional feeling is increased, and the pressed portion And printed parts are precisely matched to have a high quality product.

또한, 외형이 미려하여 장기간 사용하여도 싫증을 유발하지 않으며, 대형브로마이드 형태로 제작할 경우 장식성이 뛰어나 소장가치를 높일 수 있는 또 다른 효과가 있다.In addition, the appearance is beautiful and does not cause tiredness even after long-term use, and when produced in the form of large bromide, there is another effect that can increase the small collection value because of excellent decoration.

Claims (2)

놀이용 카드의 제조방법에 있어서,In the manufacturing method of the playing card, 인쇄기(A)를 이용하여 원지(10) 상에 은박(20)을 110℃의 온도와 130kgf/cm2의 압력으로 형압하는 은박 형성공정(S1)과,Silver foil forming process (S1) which press-presses silver foil 20 on the base paper 10 using the printing machine A at the temperature of 110 degreeC, and the pressure of 130 kgf / cm <2> , 상기 형성된 은박(20) 상면에 남색(cyan), 자홍색(magenta), 노란색(yellow), 검은색(black)으로 구성된 UV 잉크(30)를 UV 인쇄기(B)를 통해 인쇄한 후 UV 경화장치(C)로 건조하는 UV 인쇄공정(S2)과,After the UV ink 30 composed of cyan, magenta, yellow, and black on the upper surface of the formed silver foil 20 is printed through a UV printer B, a UV curing device ( UV printing process (S2) to dry in C), 상기 경화가 완료된 원지(10) 상에 코팅액(40)을 도포하는 코팅공정(S3)과,A coating step (S3) of coating the coating liquid 40 on the hardened paper 10, and 코팅액(40)의 도포가 완료된 원지(10)를 상온에서 건조시키고, 소정의 크기로 재단하는 건조 및 재단공정(S4)으로 구성되어, 원지(10)에 형성된 은박(20) 상면에 명암을 표현할 수 있도록 함을 특징으로 하는 놀이용 카드의 제조방법.It is composed of a drying and cutting process (S4) for drying the paper 10, the coating of the coating liquid 40 is completed at room temperature, and cut to a predetermined size, to express the contrast on the upper surface of the silver foil 20 formed on the paper 10 Method of manufacturing a playing card, characterized in that to enable. 제 1항에 있어서,The method of claim 1, 코팅공정(S3) 시 도포하는 코팅액(30)은 수성 바니스를 사용함을 특징으로 하는 놀이용 카드의 제조방법.The coating solution 30 applied during the coating process (S3) is a manufacturing method of a playing card, characterized in that using an aqueous varnish.
KR1020060017413A 2006-02-22 2006-02-22 The manufacturing method of the play card KR100647259B1 (en)