JPS6487002A - Rolling method for clad metal sheet - Google Patents
Rolling method for clad metal sheetInfo
- Publication number
- JPS6487002A JPS6487002A JP24419187A JP24419187A JPS6487002A JP S6487002 A JPS6487002 A JP S6487002A JP 24419187 A JP24419187 A JP 24419187A JP 24419187 A JP24419187 A JP 24419187A JP S6487002 A JPS6487002 A JP S6487002A
- Authority
- JP
- Japan
- Prior art keywords
- rolling
- stock
- preformative
- clad
- rear end
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To reduce elongation difference defect and clad ratio defect parts in the top and rear end parts of a clad stock by performing usual rolling after performing preformative rolling in a specific lengthwise range from the stock top and rolling by a larger draft than that of the preformative rolling. CONSTITUTION:As for hot rolling of a clad stock, the lengthwise range of 0.2-0.8 times the total length of the stock from the stock top end is preformatively rolled. Defining a combination of the preformative rolling with a rolling by a larger draft than that of the preformative rolling from the stock rear end is one pass, then at least two passes rollings are performed. Respective peripheral speeds of upper and lower rolling rolls are made to be different; a material having less extensibility is put at a high speed roll side and rolling is performed in the above-mentioned way. Hence, the yield of the stock is improved.
Priority Applications (4)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP24419187A JPS6487002A (en) | 1987-09-30 | 1987-09-30 | Rolling method for clad metal sheet |
AU22903/88A AU608064B2 (en) | 1987-09-30 | 1988-09-28 | Rolling process for clad steel |
DE19883878620 DE3878620T2 (en) | 1987-09-30 | 1988-09-29 | METHOD FOR ROLLING PLATED STEEL. |
EP19880309025 EP0310376B1 (en) | 1987-09-30 | 1988-09-29 | Rolling process for clad steel |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP24419187A JPS6487002A (en) | 1987-09-30 | 1987-09-30 | Rolling method for clad metal sheet |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS6487002A true JPS6487002A (en) | 1989-03-31 |
Family
ID=17115127
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP24419187A Pending JPS6487002A (en) | 1987-09-30 | 1987-09-30 | Rolling method for clad metal sheet |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6487002A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7546756B2 (en) | 2001-08-24 | 2009-06-16 | Corus Technology Bv | Method for processing a metal slab or billet, and product produced using said method |
-
1987
- 1987-09-30 JP JP24419187A patent/JPS6487002A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7546756B2 (en) | 2001-08-24 | 2009-06-16 | Corus Technology Bv | Method for processing a metal slab or billet, and product produced using said method |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2063679A1 (en) | Apparatus and method for the manufacture of hot-rolled steel | |
JPS53106367A (en) | Continuous rolling mill | |
JPS6487002A (en) | Rolling method for clad metal sheet | |
JPS6487001A (en) | Rolling method for clad metal sheet | |
JPS6444204A (en) | Production of seamless titanium pipe | |
JPS55106604A (en) | Hot rolling method | |
JPS54149352A (en) | Rolling method by changing friction forces of upper and lower rolls | |
JPS5752504A (en) | Improving method for crop in hot strip mill | |
Migda | Improved Tolerances of the Wall Thickness at High Alloy Seamless Steel Tubes | |
JPS6440102A (en) | Method for hot edging of metal slab | |
Golubchik et al. | Selecting the Optimum Ratio of Roll to Billet Diameter for Skew Rolling | |
JPS5775206A (en) | Rolling method with rolls having different diameters | |
JPS6411008A (en) | Manufacture of seamless pipe | |
JPS56111503A (en) | Rolling method for strip | |
JPS5772701A (en) | Rolling method for giving high rolling reduction to material to be rolled | |
JPS55103201A (en) | Rolling method for steel sheet | |
JPS5561308A (en) | Controlling method for elongation length of pipe in continuous elongator | |
JPS57195505A (en) | Production of thin steel sheet of irregular thickness in width direction | |
JPS55139101A (en) | Method and apparatus for strong width-reducing rolling | |
Matsumoto et al. | Effect of Hot Rolling Condition on Mechanical Properties of Cold-Rolled Extra-Low-Carbon Steel Sheet With Titanium and/or Niobium Addition | |
JPS54157755A (en) | Blooming mill roll | |
JPS57121811A (en) | Rolling method for seamless steel pipe | |
Kazanecki et al. | Possibilities of Rolling Tube Blanks X 20 CrMoV 121 Steel in Skew Rolling Mills | |
JPS5514172A (en) | Skin-pass rolling method of original tin plate | |
Kotsar | Impactless Bite of Strip in Finishing Train Stands |