JPS648244A - Highly corrosion resistant cermet - Google Patents
Highly corrosion resistant cermetInfo
- Publication number
- JPS648244A JPS648244A JP16217187A JP16217187A JPS648244A JP S648244 A JPS648244 A JP S648244A JP 16217187 A JP16217187 A JP 16217187A JP 16217187 A JP16217187 A JP 16217187A JP S648244 A JPS648244 A JP S648244A
- Authority
- JP
- Japan
- Prior art keywords
- cermet
- phase
- carbide
- corrosion resistance
- corrosion resistant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To improve the corrosion resistance of titled cermet obtd. by incorporating Ni and/or Mo as a bond phase into the cermet contg. the carbide, etc., of Ti as a hard phase and adding Cr thereto. CONSTITUTION:The cermet which contains >=1 kinds of the carbide, nitride and carbonitride of Ti as the hard phase and contains 18-45% Ni and/or Mo and 3-13% Cr is prepd. The cermet contains further preferably the elements of group IV, V or VI of the periodic table or the carbide, nitride or carbonitride of said elements. Cr is solutionized in the bond phase by this constitution, by which the potential difference between the hard phase and the bond phase is decreased and since the passive state of Cr is further formed, the elution of the metal is suppressed and the corrosion resistance of this cermet is improved. This cermet is, therefore, adequate as a frame of a wrist watch for which the high corrosion resistance is demanded.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16217187A JPS648244A (en) | 1987-06-29 | 1987-06-29 | Highly corrosion resistant cermet |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16217187A JPS648244A (en) | 1987-06-29 | 1987-06-29 | Highly corrosion resistant cermet |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS648244A true JPS648244A (en) | 1989-01-12 |
Family
ID=15749368
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16217187A Pending JPS648244A (en) | 1987-06-29 | 1987-06-29 | Highly corrosion resistant cermet |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS648244A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO1989002106A1 (en) * | 1987-08-26 | 1989-03-09 | Fanuc Ltd | Preparation of nc data for groove cutting |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS49106409A (en) * | 1973-02-16 | 1974-10-09 | ||
JPS5913045A (en) * | 1982-07-14 | 1984-01-23 | Seiko Epson Corp | External decorative parts for timepiece |
-
1987
- 1987-06-29 JP JP16217187A patent/JPS648244A/en active Pending
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS49106409A (en) * | 1973-02-16 | 1974-10-09 | ||
JPS5913045A (en) * | 1982-07-14 | 1984-01-23 | Seiko Epson Corp | External decorative parts for timepiece |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO1989002106A1 (en) * | 1987-08-26 | 1989-03-09 | Fanuc Ltd | Preparation of nc data for groove cutting |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS56500748A (en) | ||
ES2149939T3 (en) | PROCESS OF ELABORATION OF A TITANIUM STEEL AND STEEL OBTAINED. | |
TW208044B (en) | ||
JPS6428340A (en) | Cermet alloy | |
JPS57207145A (en) | Wear resistant alloy | |
JPS56136951A (en) | Brazing al material | |
JPS648244A (en) | Highly corrosion resistant cermet | |
JPS6473038A (en) | Corrosion-resistant zirconium alloy | |
JPS5389809A (en) | Superhard alloy for bit | |
ES8502167A1 (en) | Nickel-chromium-molybdenum alloy. | |
DE3587365T2 (en) | NICKEL-TITANIUM-NIOB MOLDED ALLOY ALLOY AND ITEM MADE FROM IT. | |
JPS5524803A (en) | Tool part for surface covering | |
BR8704718A (en) | ALLOY WITH NICKEL-CHROME-MOLIBDENE BASE | |
JPS6468443A (en) | Cermet alloy | |
JPS5798671A (en) | Hard external parts for timepiece | |
JPS5428217A (en) | Corrosion resistant high tensile aluminum alloy with superior workability | |
JPS6425934A (en) | High corrosion-resistant amorphous aluminum alloy | |
JPS57116726A (en) | External parts for timepiece | |
JPS54121222A (en) | Heat resistant cast alloy having excellent anti- cementation property and weldability | |
JPS5358919A (en) | Low alloy steel with hydrogen stress cracking resistance | |
JPS57164955A (en) | Alloy with 2-phase structure for decoration and lock | |
JPS6447854A (en) | Zn-mn alloy vapor deposition plated metallic material excellent in corrosion resistance and workability | |
JPS6442541A (en) | Wear-resistant intermetallic compound type alloy having excellent toughness | |
ES8801709A1 (en) | High carbon, low alloy steel comprising niobium | |
JPS57143461A (en) | Corrosion resistant alloy for decoration |