JPS6434524A - Ironing die - Google Patents

Ironing die

Info

Publication number
JPS6434524A
JPS6434524A JP62193035A JP19303587A JPS6434524A JP S6434524 A JPS6434524 A JP S6434524A JP 62193035 A JP62193035 A JP 62193035A JP 19303587 A JP19303587 A JP 19303587A JP S6434524 A JPS6434524 A JP S6434524A
Authority
JP
Japan
Prior art keywords
die
ceramics
ironing
pipe stock
reduced
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP62193035A
Other languages
Japanese (ja)
Inventor
Kishin Sukimoto
Haruo Arima
Masao Yokoyama
Hiromune Chiyuuma
Takashi Mukasa
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Showa Aluminum Can Corp
Original Assignee
Showa Aluminum Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Showa Aluminum Corp filed Critical Showa Aluminum Corp
Priority to JP62193035A priority Critical patent/JPS6434524A/en
Publication of JPS6434524A publication Critical patent/JPS6434524A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To prevent the sticking of an aluminum onto a die bearing face and to improve the surface roughness of a pipe stock by using ceramics as the component material of the die for ironing. CONSTITUTION:The thickness of a pipe stock is thinned by ironing by passing a die 1 by engaging the tip of a punch 3 with the bend part 2a formed on one end of the pipe stock 2 by curling. A ceramics is used as the component material of this ironing die. There are partially stabilized zirconia formed by adding a stabilizing agent of specified concentration to ZrO2, silicon nitride, alumina, sialon, etc., as for the ceramics. By using these ceramics, the die wear is reduced, the die life is extended, the use of a low viscosity lubrication oil is enabled and the consumption of oils can be reduced.
JP62193035A 1987-07-31 1987-07-31 Ironing die Pending JPS6434524A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP62193035A JPS6434524A (en) 1987-07-31 1987-07-31 Ironing die

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP62193035A JPS6434524A (en) 1987-07-31 1987-07-31 Ironing die

Publications (1)

Publication Number Publication Date
JPS6434524A true JPS6434524A (en) 1989-02-06

Family

ID=16301080

Family Applications (1)

Application Number Title Priority Date Filing Date
JP62193035A Pending JPS6434524A (en) 1987-07-31 1987-07-31 Ironing die

Country Status (1)

Country Link
JP (1) JPS6434524A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US9527128B2 (en) 2013-06-28 2016-12-27 Nisshin Steel Co., Ltd. Ironing mold and formed material manufacturing method

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US9527128B2 (en) 2013-06-28 2016-12-27 Nisshin Steel Co., Ltd. Ironing mold and formed material manufacturing method

Similar Documents

Publication Publication Date Title
TR200101557T2 (en) Device for combining a container and a container and a ready-to-use set containing them.
AR248423A1 (en) Method of removing sludge from lubricating oils
EP1167825A3 (en) Polished gear surfaces
ATE238218T1 (en) DEVICE FOR THE NON-CONTACT GUIDING OR TREATING OF A RUNNING MATERIAL WEB, IN PARTICULAR PAPER OR CARDBOARD WEB, METAL OR PLASTIC FILM
KR910002527A (en) Die assembly
DK1163113T3 (en) Rakel
DE3864515D1 (en) PRESSURE-OPERATED DISC CLUTCH OR BRAKE.
DE69020087D1 (en) Bearings.
SE9302868L (en) Bearings Arrangements
KR840005672A (en) Applicator nozzle
JPS6434524A (en) Ironing die
JPS5596316A (en) Valve stem seal
BR0007619A (en) Semi-spherical shoe
BR0315279A (en) Compression cylinder
JPS6448625A (en) Forming tool for container member
SE9702934L (en) slide plate
AU583171B2 (en) The use of alkylbenzoyl acrylic acids as corrosion inhibitors
HiRa et al. Frictional Behavior of Coated Steels in Sheet Forming
ES292859U (en) Piston.
BR9902554A (en) Ionic-covalent ceramics for surface finishing
JP2000197901A (en) Caliber rolling method by solid lubrication
JPS57145971A (en) Member for sliding part
Maurin-Perrier et al. Wear reduction of ceramics by lubrication
Woydt Contribution to the Environment--Developments in Tribological Materials for Engineering Ceramics Reduce Friction and Wear
Felgentreu Flattened--Smoothening of Surfaces by Rolling