JPS6418563A - Method for casting alloy without any segregation - Google Patents
Method for casting alloy without any segregationInfo
- Publication number
- JPS6418563A JPS6418563A JP17396287A JP17396287A JPS6418563A JP S6418563 A JPS6418563 A JP S6418563A JP 17396287 A JP17396287 A JP 17396287A JP 17396287 A JP17396287 A JP 17396287A JP S6418563 A JPS6418563 A JP S6418563A
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- melting
- temp
- pressure
- deltat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To produce an alloy without any segregation by adding the specific pressure at the temp. of just above the solidified temp. of the alloy at the time of solidifying after melting the alloy and solidifying the alloy under over-cooling condition. CONSTITUTION:At the time of solidifying after melting the alloy, at the temp. of just above the m.p. of this alloy, the pressure deltap (atm) is added to the atmospheric pressure so as to become deltaT>=50 deg.C as shown in the equation deltaT=k( v/ h)Tf.deltap and solidification of the alloy is completed before distribution of solute is widely developed by making over-cooling state of the alloy. In the equation, each term shows as follows. deltaT: over-cooling temp. ( deg.C) v: volume change according to melting of the element having the largest wt.% among components composing the alloy (cm<3>/mol) h: enthalpy change according to melting of the element having the largest wt.% among components composing the alloy (cal/mol) Tf: m.p. of the element having the largest wt.% among components composing the alloy ( deg.C) deltap: pressure to be added to the atmospheric pressure (atm) k: coefficient according to the unit change (41.30)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP17396287A JPH07112620B2 (en) | 1987-07-14 | 1987-07-14 | Casting method of alloy without segregation |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP17396287A JPH07112620B2 (en) | 1987-07-14 | 1987-07-14 | Casting method of alloy without segregation |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6418563A true JPS6418563A (en) | 1989-01-23 |
JPH07112620B2 JPH07112620B2 (en) | 1995-12-06 |
Family
ID=15970268
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP17396287A Expired - Lifetime JPH07112620B2 (en) | 1987-07-14 | 1987-07-14 | Casting method of alloy without segregation |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH07112620B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6207302B1 (en) | 1997-03-04 | 2001-03-27 | Denso Corporation | Electroluminescent device and method of producing the same |
-
1987
- 1987-07-14 JP JP17396287A patent/JPH07112620B2/en not_active Expired - Lifetime
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6207302B1 (en) | 1997-03-04 | 2001-03-27 | Denso Corporation | Electroluminescent device and method of producing the same |
Also Published As
Publication number | Publication date |
---|---|
JPH07112620B2 (en) | 1995-12-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB8305066D0 (en) | Casting of material | |
JPS6418563A (en) | Method for casting alloy without any segregation | |
JPS56109144A (en) | Pour-casting method | |
JPS5565351A (en) | Manufacture of aluminum-silicon type alloy with superior toughness | |
Ishihara et al. | Formation of a High Pressure Phase in In--Bi Alloys Solidified From Highly Undercooled Liquid at Atmospheric Pressure | |
Hiraoka | Commercial Application of" Hot Top" Ingot Casting Method | |
JPS56114552A (en) | Metal mold for casting | |
JPS52142611A (en) | Heating method in soaking pit | |
JPS5377813A (en) | Converter slag separating method | |
JPS5620117A (en) | Manufacture of billet by continuous casting | |
Lohberg et al. | Contributions to the Directional Solidification of Iron--Carbon--Silicon Alloy. I.--Structure, Mechanical and Physical Properties of Directionally Solidified Cast Iron | |
Kamio et al. | Formation manner of monotectic solidification structure in Al-In alloys solidified unidirectionally | |
Jin et al. | Thermal analysis of solidification of aluminium alloys during continuous casting | |
Saucedo et al. | The development of surfaces in steel ingots and strands | |
Zhernov et al. | Experimental Casting of D 16 Alloy Ingots Into a Low Hot Topped Mold | |
Stern | Methods of Making Aluminum-Lead Alloys | |
Olivari | Semicontinuous Casting of Flat Products of Alloy AlCuMg 2 | |
Spaic et al. | Characterization of the Cu-Cr-Zr-Alloy Starting Cast Structure.(In German.) | |
JPS5597848A (en) | Internal segregation reducing method of steel ingot | |
Koritta | Concentration Changes During the Solidification of AlMg 5 Alloy in an Electromagnetic Mold.(Translation: VR/2193/82) | |
Binczewski | Composite Ingot Casting | |
Belov | Development in the Casting Technology for Aluminium Alloys | |
JPS57174429A (en) | Judging method for modification of al-si alloy | |
Ueshima et al. | Method for Mitigating Solidification Segregation of Steel and Continuous Casting Machine Using Said Method | |
Yamshchikov et al. | Thermodynamic Properties of Melts of Indium and Gallium Containing Dysprosium |