JPS63893Y2 - - Google Patents

Info

Publication number
JPS63893Y2
JPS63893Y2 JP16476578U JP16476578U JPS63893Y2 JP S63893 Y2 JPS63893 Y2 JP S63893Y2 JP 16476578 U JP16476578 U JP 16476578U JP 16476578 U JP16476578 U JP 16476578U JP S63893 Y2 JPS63893 Y2 JP S63893Y2
Authority
JP
Japan
Prior art keywords
block
styrene
pigment
similar
oya
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP16476578U
Other languages
Japanese (ja)
Other versions
JPS5580411U (en
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP16476578U priority Critical patent/JPS63893Y2/ja
Publication of JPS5580411U publication Critical patent/JPS5580411U/ja
Application granted granted Critical
Publication of JPS63893Y2 publication Critical patent/JPS63893Y2/ja
Expired legal-status Critical Current

Description

【考案の詳細な説明】 この考案は、建築用化粧ブロツクに関するもの
で、天然の大谷石に似た人造の化粧ブロツクを作
り出すべく考案されたものである。
[Detailed description of the invention] This invention relates to decorative blocks for construction, and was devised to create an artificial decorative block that resembles natural Oya stone.

従来の商品の化粧ブロツク中には、天然の大谷
石特有のクレーター状の凹溝模様が見られないの
に、オーヤブロツクとして販売されているものが
ある。
Some of the decorative blocks of conventional products are sold as Oya blocks even though they do not have the crater-like groove pattern that is unique to natural Oya stones.

本考案のものは、大谷石によく似たクレーター
状の凹溝模様を作ると同時に、凹溝模様内面に、
大谷石と同様の、ブロツク部分とは色彩のちがう
色模様を作り出すべく考案されたものである。
The product of this invention creates a crater-shaped groove pattern similar to Oya stone, and at the same time, the inner surface of the groove pattern has a
Similar to Oya stone, it was devised to create a pattern with different colors from the block part.

これを図面について説明すれば、先ずセメント
と、大谷石の凹溝模様内面の色彩に似た色素(必
ずしも単一色のものとはかぎらない)をよくまぜ
合わせたものを、発泡スチロールを粉粒としたも
のの表面にまぶしつけ、これを乾燥させておく。
To explain this in terms of drawings, first, we mix cement and a pigment similar to the color of the grooved inner surface of Oya stone (not necessarily a single color), and then turn Styrofoam into powder particles. Sprinkle it on the surface of the object and let it dry.

一方、大谷石によく似た色素を適当に混合して
ブロツク素材を作り、これを前記スチロールにセ
メント、色素をまぶし乾燥させたものとを、互に
よく混合してねり合わせ、ブロツクの型の中に入
れ、圧力を加えて後型から取り出し、適当に乾燥
させて後、ブロツクの前面部4、後面部5をサン
ダーペーパーで平滑にすり落し、発泡スチロール
の面が表面に出るようにする。
On the other hand, a block material is made by suitably mixing pigments similar to Oya stone, and this is mixed well with the above-mentioned styrene, coated with cement and pigment, and dried. After applying pressure and taking it out from the mold and drying it properly, the front part 4 and the rear part 5 of the block are sanded off smoothly with sanding paper so that the styrofoam surface is exposed.

次に、第一種石油類のシンナーをこの面にふき
付け、この表面に出ている発泡スチロール部分を
溶解除去すると、第1図、第2図で示すような凹
溝模様2が表面に表われてくる。
Next, when first-class petroleum thinner is applied to this surface to dissolve and remove the styrofoam portions that are exposed on the surface, a concave groove pattern 2 as shown in Figures 1 and 2 will appear on the surface. It's coming.

一方、凹溝模様2内面側には、スチロール表面
にセメントと共にまぶしつけられた色素が、色彩
模様3となつて、凹溝模様内面に表われてくる。
On the other hand, on the inner surface of the groove pattern 2, the pigment sprinkled on the styrene surface with cement becomes a colored pattern 3 and appears on the inner surface of the groove pattern.

即ち、化粧ブロツク1は大谷石によく似た色素
を混入してあるので大谷石に似たブロツク1とな
り、シンナーに洗い流されたスチロール部分は、
大谷石と同じクレーター状の凹溝模様2が表わ
れ、その凹溝の内面側には、大谷石と似た色彩模
様3を顕出されたものを作ることができた。
In other words, the makeup block 1 is mixed with a pigment similar to Oya stone, so it becomes Block 1 similar to Oya stone, and the styrene part washed away with thinner is
A crater-shaped concave groove pattern 2 similar to that of Oya stone appeared, and a color pattern 3 similar to Oya stone was created on the inner surface of the concave groove.

また、ブロツク素材に混入する色素、スチロー
ル部分にまぶしつける色素を適当に配合すること
によつて、大谷石とは少しく趣の変つた化粧ブロ
ツクも容易に作ることができるものである。
Furthermore, by appropriately mixing the pigments mixed into the block material and the pigments sprinkled on the styrene parts, it is possible to easily create decorative blocks that are slightly different from Oya stone.

このように、この考案によるものは、大谷石と
同じような化粧ブロツクも、また少しく趣の変つ
たものも、人造で、容易に、安価に提供できる有
用な考案となつたものである。
In this way, this invention has become a useful invention that allows decorative blocks similar to Oya stone, as well as ones with a slightly different taste, to be manufactured, easily, and inexpensively.

【図面の簡単な説明】[Brief explanation of drawings]

第1図は本考案ブロツクの斜視図、第2図は本
考案ブロツクの一部を破断して示した斜視図、第
3図は本考案のブロツクの平面図、第4図は本考
案のブロツクの側面図である。 1……化粧ブロツク、2……凹溝模様、3……
色彩模様、4……前面側、5……後面側。
Fig. 1 is a perspective view of the block of the invention, Fig. 2 is a perspective view of the block of the invention partially cut away, Fig. 3 is a plan view of the block of the invention, and Fig. 4 is the block of the invention. FIG. 1... Makeup block, 2... Concave groove pattern, 3...
Color pattern, 4...front side, 5...rear side.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] セメントと色素とをまぜ合わせたものを発泡ス
チロールの粉粒としたものの表面にまぶしつけて
乾燥させ、また一方、別に色素をまぜてねり合わ
せて作つたブロツク素材を用意し、これらを互に
混合させて化粧ブロツクを作り、ブロツクの前面
側及び後面側を平にすり落し、表面に表われたス
チロール部分を、第一種石油類のシンナーを吹き
つけて、スチロール部分を溶解除去して作つた建
築用化粧ブロツク。
A mixture of cement and pigment is sprinkled onto the surface of styrofoam powder and allowed to dry.Meanwhile, a block material made by mixing pigment and kneading is prepared separately, and these are mixed together. A building made by making a decorative block, rubbing the front and back sides of the block flat, and spraying class 1 petroleum thinner on the styrene that appeared on the surface to dissolve and remove the styrene. Makeup block.
JP16476578U 1978-11-29 1978-11-29 Expired JPS63893Y2 (en)