JPS6248734B2 - - Google Patents
Info
- Publication number
- JPS6248734B2 JPS6248734B2 JP58183899A JP18389983A JPS6248734B2 JP S6248734 B2 JPS6248734 B2 JP S6248734B2 JP 58183899 A JP58183899 A JP 58183899A JP 18389983 A JP18389983 A JP 18389983A JP S6248734 B2 JPS6248734 B2 JP S6248734B2
- Authority
- JP
- Japan
- Prior art keywords
- dust
- less
- powder
- collected
- water content
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02P10/00—Technologies related to metal processing
- Y02P10/20—Recycling
Landscapes
- Manufacture And Refinement Of Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58183899A JPS6075527A (ja) | 1983-09-30 | 1983-09-30 | 製鉄工場で発生する製鉄粉塵の処理方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58183899A JPS6075527A (ja) | 1983-09-30 | 1983-09-30 | 製鉄工場で発生する製鉄粉塵の処理方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6075527A JPS6075527A (ja) | 1985-04-27 |
| JPS6248734B2 true JPS6248734B2 (OSRAM) | 1987-10-15 |
Family
ID=16143756
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58183899A Granted JPS6075527A (ja) | 1983-09-30 | 1983-09-30 | 製鉄工場で発生する製鉄粉塵の処理方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6075527A (OSRAM) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3004265B1 (ja) * | 1998-11-24 | 2000-01-31 | 株式会社神戸製鋼所 | 炭材内装ペレット及び還元鉄製造方法 |
| JP4237965B2 (ja) * | 2002-02-25 | 2009-03-11 | 新日本製鐵株式会社 | Cr含有スラッジや焼却残渣等の処理方法およびそれにより得られる製鋼用ペレット |
-
1983
- 1983-09-30 JP JP58183899A patent/JPS6075527A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6075527A (ja) | 1985-04-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN104694760B (zh) | 一种处理赤泥回收铁精粉的方法及系统 | |
| CN108504855A (zh) | 一种以菱铁矿为还原剂悬浮磁化焙烧生产铁精矿的方法 | |
| CN109295299A (zh) | 一种利用回转窑工艺添加石灰石制备高赤铁矿自熔性球团矿的方法 | |
| CN108411104A (zh) | 一种基于低能耗热分解的脱硫灰资源化方法 | |
| US3313617A (en) | Iron-containing flux material for steel-making process | |
| CN102618718B (zh) | 钢厂含铁粉尘制备高强度生球的方法 | |
| CN103952540B (zh) | 利用含铁尘泥和高硅铁精矿生产金属化炉料的工艺 | |
| CN111647753B (zh) | 一种利用熔融气化炉直接还原回收锌的方法 | |
| CN108380360A (zh) | 一种优质钢渣铁精粉生产工艺 | |
| JP2005111394A (ja) | 有機系廃棄物の処理方法 | |
| JPH10192894A (ja) | 含油含鉄スラッジの処理方法 | |
| CN101259969B (zh) | 一种氧化铝的制备工艺 | |
| JPS6248734B2 (OSRAM) | ||
| US4091545A (en) | Method for removing water and grease deposit from rolling mill sludge | |
| JP2706142B2 (ja) | スクラップ予熱炉を有する電気炉における製鋼ダスト類の再利用方法 | |
| CN106591571A (zh) | 一种由赤泥制备含铁球团的方法 | |
| CN103274612A (zh) | 不锈钢污泥制水泥熟料添加剂的方法 | |
| CA2877061A1 (en) | Method and plant for recovering material and/or energy from phosphorus-containing waste | |
| JPH09279258A (ja) | 製鉄ダストの塊成化方法 | |
| JP3666940B2 (ja) | 下水汚泥のセメント原料化方法 | |
| CN112110659A (zh) | 一种利用钢渣捕集CO2消除游离CaO的方法和装置 | |
| CN101717855A (zh) | 一种铁矿石脱除铜砷的方法 | |
| CN108642240B (zh) | 一种利用废旧除尘布袋制备的铁水保温覆盖剂及制备方法 | |
| SU1669884A1 (ru) | Способ получени извести в обжиговой печи | |
| CN121270044A (zh) | 一种钢厂污泥固废资源化利用方法 |