JPS6237383A - ホツトコイルのスケ−ル抑制方法 - Google Patents
ホツトコイルのスケ−ル抑制方法Info
- Publication number
- JPS6237383A JPS6237383A JP17740685A JP17740685A JPS6237383A JP S6237383 A JPS6237383 A JP S6237383A JP 17740685 A JP17740685 A JP 17740685A JP 17740685 A JP17740685 A JP 17740685A JP S6237383 A JPS6237383 A JP S6237383A
- Authority
- JP
- Japan
- Prior art keywords
- hot coil
- hot
- coil
- scale
- sealing material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Winding, Rewinding, Material Storage Devices (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP17740685A JPS6237383A (ja) | 1985-08-12 | 1985-08-12 | ホツトコイルのスケ−ル抑制方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP17740685A JPS6237383A (ja) | 1985-08-12 | 1985-08-12 | ホツトコイルのスケ−ル抑制方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6237383A true JPS6237383A (ja) | 1987-02-18 |
| JPH0567713B2 JPH0567713B2 (enrdf_load_stackoverflow) | 1993-09-27 |
Family
ID=16030373
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP17740685A Granted JPS6237383A (ja) | 1985-08-12 | 1985-08-12 | ホツトコイルのスケ−ル抑制方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6237383A (enrdf_load_stackoverflow) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5750290A (en) * | 1995-04-20 | 1998-05-12 | Nec Corporation | Photo mask and fabrication process therefor |
| JP2018043247A (ja) * | 2016-09-12 | 2018-03-22 | Jfeスチール株式会社 | 熱間圧延コイルおよび無方向性電磁鋼板の製造方法 |
-
1985
- 1985-08-12 JP JP17740685A patent/JPS6237383A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5750290A (en) * | 1995-04-20 | 1998-05-12 | Nec Corporation | Photo mask and fabrication process therefor |
| JP2018043247A (ja) * | 2016-09-12 | 2018-03-22 | Jfeスチール株式会社 | 熱間圧延コイルおよび無方向性電磁鋼板の製造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0567713B2 (enrdf_load_stackoverflow) | 1993-09-27 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR20040030960A (ko) | 스퍼터 타겟 | |
| JPS6237383A (ja) | ホツトコイルのスケ−ル抑制方法 | |
| US2927371A (en) | Method of continuously forming welded coated steel tubing | |
| CN102560044A (zh) | 一种铜带表面处理方法及装置 | |
| JP3246748B2 (ja) | 深紋り成型用鋼ストリップもしくはシートの製造方法 | |
| US4319610A (en) | Process for coating metal tubes and use of the coated tubes | |
| USRE31354E (en) | Process for coating metal tubes and use of the coated tubes | |
| JPH05177240A (ja) | 熱延コイルの冷却方法 | |
| JPH11276981A (ja) | 無機質成形体の塗装方法及び無機質成形体 | |
| JPH01313108A (ja) | 熱延線材の均一急冷方法 | |
| US20030145914A1 (en) | Method and installation for hot dip coating metal strips | |
| JP3197269B2 (ja) | 無酸素鍛造方法 | |
| JPS625213B2 (enrdf_load_stackoverflow) | ||
| RU2774913C1 (ru) | Установка и способ для обработки прокатываемого материала | |
| JPH0287422A (ja) | 積層されかつ波形に成形された長尺の超電体およびその製造方法 | |
| CN115338265B (zh) | 一种带钢卷取工艺 | |
| JPS5877702A (ja) | 熱間圧延ステンレス鋼帯の製造方法および装置 | |
| JPS60251232A (ja) | 焼結鉱の品質管理方法 | |
| JPS58138517A (ja) | ホツトストリツプの高温巻取方法 | |
| JP3197270B2 (ja) | 無酸素鍛造装置 | |
| JPS5945018A (ja) | スケ−ルの少ない熱延鋼板の製造方法 | |
| JPS60115305A (ja) | 熱間薄板材の圧延法および圧延設備 | |
| JPH01219128A (ja) | 薄スケール熱延鋼板の製造方法 | |
| JPS625214B2 (enrdf_load_stackoverflow) | ||
| JPS62227034A (ja) | 連続ラインにおける高珪素鋼帯の製造方法 |