JPS6156119B2 - - Google Patents

Info

Publication number
JPS6156119B2
JPS6156119B2 JP192382A JP192382A JPS6156119B2 JP S6156119 B2 JPS6156119 B2 JP S6156119B2 JP 192382 A JP192382 A JP 192382A JP 192382 A JP192382 A JP 192382A JP S6156119 B2 JPS6156119 B2 JP S6156119B2
Authority
JP
Japan
Prior art keywords
layer
metallic luster
luster material
material layer
transparent film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP192382A
Other languages
Japanese (ja)
Other versions
JPS58119885A (en
Inventor
Mamoru Shimizu
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NICHEI KAKO KK
Original Assignee
NICHEI KAKO KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NICHEI KAKO KK filed Critical NICHEI KAKO KK
Priority to JP192382A priority Critical patent/JPS58119885A/en
Publication of JPS58119885A publication Critical patent/JPS58119885A/en
Publication of JPS6156119B2 publication Critical patent/JPS6156119B2/ja
Granted legal-status Critical Current

Description

【発明の詳細な説明】 この発明は、優れた装飾的効果を目的とした感
圧性粘着シートに関するものである。
DETAILED DESCRIPTION OF THE INVENTION This invention relates to a pressure-sensitive adhesive sheet intended for superior decorative effects.

従来、感圧性粘着シートに美麗な金属性光沢模
様を現出させる目的で、金属蒸着層を用いようと
する技術は広く知られているところである。たと
えば、実公昭45―3085号公報には、透明フイルム
の表面に光沢性材料の蒸着層を介して所望の文字
や図柄の印刷インク層が施され、その印刷インク
層以外の透明フイルムの表面部分を露出させ、か
つ上記透明フイルムの裏面に感圧接着剤層を介し
て離型紙が粘着された構造の光沢性文字模様入り
感圧接着シートが示されているが、従来用いられ
ている光沢性文字模様入り感圧接着シートのほと
んどは、この公報に示されているものと同様に、
フイルムもしくはシートの片面に金属光沢性材料
を蒸着、貼着もしくは塗布した程度のものでしか
ないので、折角の金属光沢性材料を用いても、そ
の効果は充分であるとは言えない。
BACKGROUND ART Conventionally, the technique of using a metal vapor deposited layer for the purpose of creating a beautiful metallic luster pattern on a pressure-sensitive adhesive sheet is widely known. For example, in Japanese Utility Model Publication No. 45-3085, a printing ink layer with desired characters or designs is applied to the surface of a transparent film through a vapor deposited layer of a glossy material, and the surface of the transparent film other than the printing ink layer is A pressure-sensitive adhesive sheet with a glossy character pattern is shown in which the transparent film is exposed and a release paper is adhered to the back side of the transparent film via a pressure-sensitive adhesive layer. Most of the pressure-sensitive adhesive sheets with character patterns are similar to those shown in this publication.
Since the metallic luster material is merely vapor-deposited, pasted or coated on one side of a film or sheet, even if a lot of effort is made to use the metallic lustrous material, the effect cannot be said to be sufficient.

したがつて、この発明は、このような現状に着
目してなされたものであり、透明フイルム層の上
下両面に金属光沢性材料層が形成され、下面金属
光沢性材料層の下には、さらに粘着剤層および離
型紙が積層され、一方、上面金属光沢性材料層の
上には、さらに適宜インキ層が設けられて、この
インキ層が被覆していない上面金属光沢性材料層
の部分が、化学的処理等によつて溶解除去され、
透明フイルム層の上面が露出している構造である
ことを特徴とする感圧性粘着シートを提供するも
のである。以下に、図面を用いながら、その詳細
を述べる。
Therefore, the present invention has been made in view of the current situation, and a metallic luster material layer is formed on both the upper and lower surfaces of a transparent film layer, and a metallic luster material layer is further formed under the lower surface metallic luster material layer. The adhesive layer and the release paper are laminated, and on the other hand, an appropriate ink layer is further provided on the upper surface metallic luster material layer, and the portion of the upper surface metallic luster material layer that is not covered by this ink layer is Dissolved and removed by chemical treatment, etc.
The present invention provides a pressure-sensitive adhesive sheet characterized by having a structure in which the upper surface of a transparent film layer is exposed. The details will be described below with reference to the drawings.

この発明における透明フイルム層2とは、ポリ
塩化ビニル、ポリエチレン、ポリプロピレン、ポ
リスチレン、ポリエステル、酢酸セルロース、そ
の他の透明性の優れたフイルム(シートも含む)
層をいい、金属光沢性材料層1および4とは、ア
ルミニウムを始めとする、亜鉛、金、銀、クロ
ム、ニツケル、銅、セレン、弗化マグネシウム、
硫化亜鉛、一酸化珪素等のような通常の真空蒸着
法に用いられる金属もしくは無機化合物の蒸着
層、電気化学的もしくは純化学的方法による金属
メツキ層、または、圧延した金属箔、さらには金
属粉を混入した合成樹脂フイルム(シート)や塗
膜であつてもよい。したがつて、透明フイルム層
2の上下両面に設ける金属光沢性材料層1および
4は、それぞれが同質のものであつても、また、
異質のものであつてもよく、たとえば、上面金属
光沢性材料層1は、後述するインキ層7で被覆さ
れない部分を後で溶解除去するために、酸、アル
カリ、水、その他の溶剤に溶けやすくしておくこ
とが望ましい。なお、透明フイルム層2と上下両
面の金属光沢性材料層1および4とは、蒸着法の
ように直接被覆させる方法、上下両面の金属光沢
性材料層1および4上に透明フイルムを押出し成
形する方法、または、両者を接着剤等で圧着させ
る方法等、いずれの方法で貼り合わせてもよい
が、接着剤を用いるときは、当然のことながら透
明の接着剤である方が望ましい。
The transparent film layer 2 in this invention refers to polyvinyl chloride, polyethylene, polypropylene, polystyrene, polyester, cellulose acetate, or other highly transparent films (including sheets).
The metallic luster material layers 1 and 4 are made of aluminum, zinc, gold, silver, chromium, nickel, copper, selenium, magnesium fluoride,
Deposited layers of metals or inorganic compounds used in ordinary vacuum deposition methods such as zinc sulfide, silicon monoxide, etc., metal plating layers by electrochemical or pure chemical methods, rolled metal foils, and even metal powders. It may also be a synthetic resin film (sheet) or coating film mixed with. Therefore, even if the metallic luster material layers 1 and 4 provided on both the upper and lower surfaces of the transparent film layer 2 are of the same quality,
For example, the upper metallic luster material layer 1 may be easily soluble in acids, alkalis, water, or other solvents in order to later dissolve and remove the portions not covered with the ink layer 7, which will be described later. It is desirable to keep it. The transparent film layer 2 and the metallic luster material layers 1 and 4 on both the upper and lower surfaces can be formed by direct coating such as a vapor deposition method, or by extrusion molding a transparent film on the metallic luster material layers 1 and 4 on the upper and lower surfaces. They may be bonded together by any method, such as a bonding method or a method of pressing the two together with an adhesive or the like, but when an adhesive is used, it is naturally preferable to use a transparent adhesive.

ここで、透明フイルム層2の下面に、予め、エ
ツチング、ワイヤーブラシ、サンドブラスト等に
よつて掻き傷を付けたり、エンボツシング等によ
つて凹凸模様を付けたり、透明インキで着色した
り、さらには、文字や図柄模様を印刷したりし
て、透明フイルム層2の下面の全面もしくは一部
に加工層3を形成しておけば、この発明の効果を
一層高めることができる。
Here, the lower surface of the transparent film layer 2 may be scratched in advance by etching, wire brushing, sandblasting, etc., an uneven pattern may be formed by embossing, etc., it may be colored with transparent ink, or further, The effects of the present invention can be further enhanced by forming a processed layer 3 on the entire or part of the lower surface of the transparent film layer 2 by printing letters or designs.

下面金属光沢性材料層4の下面にさらに積層す
る粘着剤層5および離型紙6は、この発明によつ
て得られる感圧性粘着シートから、離型紙6を剥
ぎ取り、粘着剤層5を露出させて、基材面に貼り
つけるためのものであるから、粘着剤および離型
紙の種類や性質を特に限定する必要はなく、通常
用いられる感圧性接着剤とそれに対応する離型紙
であればよい。
The adhesive layer 5 and release paper 6 to be further laminated on the lower surface of the lower surface metallic luster material layer 4 are obtained by peeling off the release paper 6 from the pressure-sensitive adhesive sheet obtained by the present invention and exposing the adhesive layer 5. Since it is intended to be attached to the surface of a base material, there is no need to particularly limit the types and properties of the adhesive and release paper, and any pressure-sensitive adhesive and release paper corresponding to the pressure-sensitive adhesive that are commonly used may be used.

つぎに、上面金属光沢性材料層1の上に形成す
るインキ層7とは、好ましくは透明性および付着
性のよいインクを用いて、加工層3に相応しい文
字や図柄模様を印刷したものである。この際の印
刷方法は、シートの面積の大小または長さの長短
によつて、オフセツト印刷、スクリーン印刷、グ
ラビヤ印刷等通常の凸版、平版、凹版、孔版等に
よる印刷法のいずれであつてもよい。このように
して、上面金属光沢性材料層1の上面にインキ層
7が印刷された後、インキ層7によつて被覆され
ていない上面金属光沢性材料層1の露出部分を、
酸、アルカリ、水、有機溶剤等によつて、溶解除
去し、インキ層7が形成されない部分に、透明フ
イルム層2の上面を露呈させれば、この発明の感
圧性粘着シートが得られる。なお、この感圧性粘
着シートの最上面を、たとえばポリエチレンテレ
フタレートフイルムのような透明な保護膜で積層
しても、この発明には何等の支障をも生じない。
Next, the ink layer 7 formed on the upper surface metallic luster material layer 1 is one in which letters and patterns suitable for the processed layer 3 are printed, preferably using an ink with good transparency and adhesion. . The printing method at this time may be any of the usual letterpress printing methods such as offset printing, screen printing, gravure printing, lithography, intaglio printing, stencil printing, etc., depending on the size of the area or length of the sheet. . After the ink layer 7 is printed on the upper surface of the upper metallic luster material layer 1 in this way, the exposed portion of the upper metallic lustrous material layer 1 that is not covered by the ink layer 7 is
The pressure-sensitive adhesive sheet of the present invention can be obtained by dissolving and removing the transparent film layer 2 with an acid, alkali, water, an organic solvent, etc., and exposing the upper surface of the transparent film layer 2 in the area where the ink layer 7 is not formed. Note that even if the uppermost surface of this pressure-sensitive adhesive sheet is laminated with a transparent protective film such as a polyethylene terephthalate film, no problem will arise in the present invention.

いま、一例としてポリプロピレンフイルム
(200μm厚)の上下両面に0.3〜0.5μmのアルミ
ニウム蒸着膜を形成したときの状態を示すと、上
面金属光沢性材料層1に相当するアルミ蒸着膜の
溶解除去には10%以下、たとえば、6%程度の苛
性ソーダ水溶液に浸漬すれば充分である。また、
加工層3を着色によつて形成するときも、インキ
層7を設けるときも全く同様であるが、淡黄色の
透明インキを用いたときは、それぞれの層の下層
のアルミニウム箔の色(銀色)は金色に、濃黄色
の透明インキを用いると銅色に見え、薄い半透明
の白色インキを用いるとアルマイト様の色調を与
え、木目状の透かし模様とすれば、金属感のある
木目模様に変化させることができるというよう
に、上下2層の蒸着膜および透明フイルムである
ポリプロピレンフイルムによる反射光線、屈折光
線、さらには、加工層3、インキ層7等の透過光
線もしくは反射光線等が交錯して、きわめて多種
多様の装飾的効果を現わす。色彩、色調の組み合
わせの変化のみならず、透明フイルム層2の厚さ
に応じて、インキ層7の文字や図柄模様を浮き上
がつた状態に見せることも可能であるので、金属
光沢性材料層1の一層のみを用いる従来の感圧性
粘着シートでは容易には得られない優れた装飾的
効果を示すことが明白であり、この発明の意義は
きわめて大きいと言える。
Now, as an example, we will show the state when a 0.3 to 0.5 μm vapor deposited aluminum film is formed on both the top and bottom surfaces of a polypropylene film (200 μm thick). It is sufficient to immerse it in a caustic soda aqueous solution of 10% or less, for example, about 6%. Also,
The process is exactly the same when forming the processed layer 3 by coloring and when providing the ink layer 7, but when using pale yellow transparent ink, the color of the aluminum foil below each layer (silver) If you use a dark yellow transparent ink, it will look like a copper color. If you use a thin semi-transparent white ink, it will give an alumite-like tone, and if you create a wood grain-like watermark pattern, it will change to a wood grain pattern with a metallic feel. As can be seen, the reflected and refracted rays from the upper and lower vapor deposited films and the transparent polypropylene film, as well as the transmitted or reflected rays from the processing layer 3, ink layer 7, etc., intersect. , exhibiting an extremely wide variety of decorative effects. In addition to changing the combination of colors and tones, it is also possible to make the letters and designs on the ink layer 7 appear raised depending on the thickness of the transparent film layer 2, so the metallic luster material layer It is clear that this invention exhibits excellent decorative effects that cannot be easily obtained with conventional pressure-sensitive adhesive sheets using only one layer of No. 1, and the significance of this invention is extremely great.

【図面の簡単な説明】[Brief explanation of the drawing]

図はこの発明の構造を示すための拡大断面図で
ある。 1……上面金属光沢性材料層、2……透明フイ
ルム層、3……加工層、4……下面金属光沢性材
料層、5……粘着剤層、6……離型紙、7……イ
ンキ層。
The figure is an enlarged sectional view showing the structure of the present invention. DESCRIPTION OF SYMBOLS 1...Top metallic luster material layer, 2...Transparent film layer, 3...Processing layer, 4...Bottom metallic luster material layer, 5...Adhesive layer, 6...Release paper, 7...Ink layer.

Claims (1)

【特許請求の範囲】 1 透明フイルム層の上下両面に金属光沢性材料
層が形成され、下面金属光沢性材料層の下には、
さらに粘着剤層および離型紙が積層され、一方、
上面金属光沢性材料層の上には、さらに適宜イン
キ層が設けられて、このインキ層が被覆していな
い上面金属光沢性材料層の部分が、化学的処理等
によつて溶解除去され、透明フイルム層の上面が
露出している構造であることを特徴とする感圧性
粘着シート。 2 下面金属光沢性材料層が、透明フイルムの下
面を加工、着色もしくは印刷すること等によつて
形成された加工層を介して密着していることを特
徴とする特許請求の範囲第1項記載の感圧性粘着
シート。
[Claims] 1. Metallic luster material layers are formed on both upper and lower surfaces of the transparent film layer, and below the lower metallic luster material layer,
Furthermore, an adhesive layer and release paper are laminated, while
An appropriate ink layer is further provided on the upper metallic luster material layer, and the portion of the upper metallic lustrous material layer that is not covered by this ink layer is dissolved and removed by chemical treatment etc. to make it transparent. A pressure-sensitive adhesive sheet characterized by a structure in which the upper surface of the film layer is exposed. 2. Claim 1, characterized in that the lower surface metallic luster material layer is in close contact with the lower surface of the transparent film through a processed layer formed by processing, coloring, printing, etc. pressure-sensitive adhesive sheet.
JP192382A 1982-01-09 1982-01-09 Pressure-sensitive adhesive sheet Granted JPS58119885A (en)