JPS6129818B2 - - Google Patents
Info
- Publication number
- JPS6129818B2 JPS6129818B2 JP54157456A JP15745679A JPS6129818B2 JP S6129818 B2 JPS6129818 B2 JP S6129818B2 JP 54157456 A JP54157456 A JP 54157456A JP 15745679 A JP15745679 A JP 15745679A JP S6129818 B2 JPS6129818 B2 JP S6129818B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- slab
- continuous casting
- cracks
- amount
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Continuous Casting (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15745679A JPS5680354A (en) | 1979-12-06 | 1979-12-06 | Method of suppressing cracking of b-containing steel ingot continuously cast |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15745679A JPS5680354A (en) | 1979-12-06 | 1979-12-06 | Method of suppressing cracking of b-containing steel ingot continuously cast |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5680354A JPS5680354A (en) | 1981-07-01 |
| JPS6129818B2 true JPS6129818B2 (show.php) | 1986-07-09 |
Family
ID=15650049
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15745679A Granted JPS5680354A (en) | 1979-12-06 | 1979-12-06 | Method of suppressing cracking of b-containing steel ingot continuously cast |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5680354A (show.php) |
Family Cites Families (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5534332B2 (show.php) * | 1972-07-27 | 1980-09-05 | ||
| JPS5938060B2 (ja) * | 1975-05-28 | 1984-09-13 | 新日本製鐵株式会社 | 表面割れの少ない連続鋳造キルド鋼片 |
| JPS5266815A (en) * | 1975-12-01 | 1977-06-02 | Nippon Steel Corp | Steel improved sulfide corrosion cracking resistance |
| JPS52104412A (en) * | 1976-03-01 | 1977-09-01 | Sumitomo Metal Ind Ltd | Temper type high tensile steel superior in weldability |
| JPS54135616A (en) * | 1978-04-12 | 1979-10-22 | Nippon Steel Corp | Manufacture of cold rolled steel plate with superior formability |
| JPS55107733A (en) * | 1979-02-15 | 1980-08-19 | Kawasaki Steel Corp | Cold rolled steel plate having superior press workability |
-
1979
- 1979-12-06 JP JP15745679A patent/JPS5680354A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5680354A (en) | 1981-07-01 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4379482A (en) | Prevention of cracking of continuously cast steel slabs containing boron | |
| US2562467A (en) | Armor plate and method for making same | |
| CN107438487B (zh) | 热轧轻型马氏体钢板及其制作方法 | |
| US20080164003A1 (en) | Method and Installation for Producing Light Gauge Steel with a High Manganese Content | |
| WO1995007780A1 (en) | Method of manufacturing thin cast piece through continuous casting | |
| US5662748A (en) | Thin cast strip and thin steel sheet of common carbon steel containing large amounts of copper and tin and process for producing the same | |
| KR20060130745A (ko) | 고동 저합금 강판 | |
| JPH0688125A (ja) | 連続鋳造片及び鋼塊の熱間加工法 | |
| JPS626635B2 (show.php) | ||
| JPS63123556A (ja) | 鋳造過程および熱間圧延過程で割れを起こし難いCr−Ni系ステンレス鋼の製造方法 | |
| JPS6129818B2 (show.php) | ||
| JPS626615B2 (show.php) | ||
| JP3518517B2 (ja) | 高クロム・フェライト系耐熱鋼材の製造方法 | |
| KR102882744B1 (ko) | 표면 품질이 개선된 합금강 제조 방법 | |
| JPS6364516B2 (show.php) | ||
| JPH022925B2 (show.php) | ||
| CN102312162A (zh) | 内燃机气阀用精炼马氏体合金及其生产工艺 | |
| JPS5852444B2 (ja) | 熱間圧延時の鋼片表面割れ抑制法 | |
| JPS61193758A (ja) | 表面性状の良好な熱間加工鋼材の製造法 | |
| JP4466335B2 (ja) | 鋼の連続鋳造方法 | |
| JPS6121301B2 (show.php) | ||
| JPH0668127B2 (ja) | 異方性が小さく表面性状が優れたCr−Ni系ステンレス鋼板の製造方法 | |
| JPS6364490B2 (show.php) | ||
| JPS6358215B2 (show.php) | ||
| JP2024139391A (ja) | 鋳片およびその連続鋳造方法 |