JPS6125669A - Method for filling caulking material into joint part of facing material - Google Patents

Method for filling caulking material into joint part of facing material

Info

Publication number
JPS6125669A
JPS6125669A JP14544384A JP14544384A JPS6125669A JP S6125669 A JPS6125669 A JP S6125669A JP 14544384 A JP14544384 A JP 14544384A JP 14544384 A JP14544384 A JP 14544384A JP S6125669 A JPS6125669 A JP S6125669A
Authority
JP
Japan
Prior art keywords
caulking material
caulking
masking agent
exterior
filling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP14544384A
Other languages
Japanese (ja)
Inventor
Atsushi Nakamura
敦 中村
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
National House Industrial Co Ltd
Original Assignee
National House Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by National House Industrial Co Ltd filed Critical National House Industrial Co Ltd
Priority to JP14544384A priority Critical patent/JPS6125669A/en
Publication of JPS6125669A publication Critical patent/JPS6125669A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To prevent the bulging out of a caulking material onto a facing material and to improve the operability by filling the caulking material into a joint part, and surface-finishing with use of a masking agent. CONSTITUTION:A masking agent 3 is coated on the surface of a facing material 1 in the vicinity of a joint part 2 with a coating roller 9 such as a roller sponge to form a protective film 11. Then a caulking material 4 is filled into the joint part 2 from a nozzle 12, the surface of the caulking material 4 is pressed with a finishing jig 6 such as a pallet, and the surplus caulking material 4 is scraped off. The protective film 11 and the caulking material 4 deosited on the film are then released from the surface of the facing material 1 by using a releasing rubber roller.

Description

【発明の詳細な説明】 [技術分野J 本発明は一対の外装材間で形成される目地部内ヘコーキ
ング材を充填する際の、外装材の目地部へのコーキング
材の充填方法に関するものである。
Detailed Description of the Invention [Technical Field J] The present invention relates to a method of filling caulking material into the joints of exterior materials when filling the joints formed between a pair of exterior materials. .

r背景技術J 従来上り、外装材間で形成される目地部内にコーキング
材を充填して外装材の熱膨張等による伸縮を目地部で吸
収すると共に外装材間の防水性を確保するということが
行なわれている。従来、外装材の目地部内にコーキング
材を充填するにあたっては、コーキング材吐出装置のノ
ズルからコーキング材を目地部内に吐出した後、ヘフな
どの仕上げ用治具を用いてコーキング材表面を押さえ付
は表面を平滑に仕上げると共に、余分なコーキング材を
かきとっているものであった。ところが、仕上げ用泊兵
でコーキング材表面を仕上げする際に、コーキング材が
目地部からはみ出して外装材表面を汚すという欠点があ
った。
Background technology J Conventionally, caulking material is filled in the joints formed between exterior materials to absorb expansion and contraction due to thermal expansion of the exterior materials at the joints and to ensure waterproofness between the exterior materials. It is being done. Conventionally, when filling caulking material into the joints of exterior materials, the caulking material was discharged from the nozzle of a caulking material dispensing device into the joints, and then the surface of the caulking material was pressed down using a finishing jig such as a Hef. The surface was smoothed and excess caulking was scraped off. However, when finishing the surface of the caulking material with a finishing coat, the caulking material protrudes from the joints and stains the surface of the exterior material.

【発明の目的」 本発明は上記の点に鑑みで成されたものであって、コー
キング材表面を仕上げする、際に、コーキング材が外装
材の目地部からはみ出すことがなく、コーキング材の充
填精度及び作業性を向上することができる外装材の目地
部へのコーキング材の充填方法を提供することを目的と
するものである。
[Object of the Invention] The present invention has been made in view of the above points, and it is possible to prevent the caulking material from protruding from the joints of the exterior material when finishing the surface of the caulking material, and to fill the caulking material with the filling material. It is an object of the present invention to provide a method of filling caulking material into joints of exterior materials, which can improve accuracy and workability.

[発明の開示] すなわち、本発明の外装材の目地部へのコーキング材の
充#X1方法は、一対の外装材1.1の端面間で形成さ
れる目地部2の近傍における外装材1の表面にマスキン
グ剤3を塗布し、次いで目地部2内にコーキング材4を
充填し、次にコーキング材4表面を仕上げ用治具6で仕
上げた後、上記マスキング剤3を外装材1表面から剥離
することを特徴とするもので、目地部2の外装材1表面
を予めマスキング剤3で保護しておいて目地部2からは
み出したコーキング材4が外装材1表面に直に付着しな
いようにし、上記目的を達成したもので尻る。
[Disclosure of the Invention] In other words, method #X1 of filling the joints of the exterior material with caulking material according to the present invention involves filling the joints of the exterior material 1 in the vicinity of the joints 2 formed between the end faces of the pair of exterior materials 1.1. Masking agent 3 is applied to the surface, then caulking material 4 is filled in the joints 2, and then the surface of the caulking material 4 is finished with a finishing jig 6, and then the masking agent 3 is peeled off from the surface of the exterior material 1. The surface of the exterior material 1 at the joint part 2 is protected in advance with a masking agent 3 to prevent the caulking material 4 protruding from the joint part 2 from directly adhering to the surface of the exterior material 1, I'm satisfied with something that achieves the above objectives.

以下本発明゛を実施例に基づいて詳述する。第1図に示
すように、一対の外装材1.1の端面間で目地部2が形
成されるように、一対の外装材1は枠材等の取付部材7
に固定され、外壁パネル8が形成されている。外装材1
の目地部2内にコーキング材4を充填するにあたっては
、第1図に示すように、まず初めに目地部2の近傍にて
外装材1の表面にマスキング剤3を塗布する。このマス
キング剤3はアクリルエマルノランクイプの一時保護塗
料で、一般名ストリッパプルペイントと呼ばれており、
このものを外装材1表面に塗布すると速やかに保lフィ
ルム11を形成し、外装材1表面を保護すると共に一方
軸離が容易なものである。
The present invention will be described in detail below based on examples. As shown in FIG. 1, the pair of exterior materials 1.
is fixed to form an outer wall panel 8. Exterior material 1
When filling the caulking material 4 into the joint 2, as shown in FIG. 1, the masking agent 3 is first applied to the surface of the exterior material 1 in the vicinity of the joint 2. This masking agent 3 is a temporary protective paint of acrylic emulsion type and is commonly called stripper pull paint.
When this material is applied to the surface of the exterior material 1, it quickly forms a lubricating film 11, which protects the surface of the exterior material 1 and at the same time facilitates axis separation.

このマスキング剤3はスプレーや刷毛塗り、あるいはロ
ーラー塗り等で塗布することが可能であるが、図のよう
にローラースボンノ等の塗布用、ローラー9で塗布する
のが好ましい。次に、ノズル12よりコーキング材4を
目地部2内に充填し、次いで、ヘラなどの仕上げ用治具
6番用いてコーキング材4の表面を押さえ付けると同時
に余分なコーキング材4をかきとる0次いで、マスキン
グ剤3が硬化して保護フィルム11を形成した後、剥離
用ゴムローラー10を用いて保!1フィルム11及1コ
ーキング材4を外装材1表面から剥離するのである。こ
のゴムローラー10は外装材1上を回転させながら移動
させることにより、ゴムローラー10の回りに保Il!
フィルム11が付着し、保II!フィルム11を巻き取
ることができるのである。
This masking agent 3 can be applied by spraying, brushing, or roller coating, but it is preferable to apply it with a roller 9, such as a roller bonnet, as shown in the figure. Next, the caulking material 4 is filled into the joint part 2 through the nozzle 12, and then the surface of the caulking material 4 is pressed down using a finishing jig No. 6 such as a spatula, and at the same time, the excess caulking material 4 is scraped off. Next, after the masking agent 3 is cured to form the protective film 11, it is held using a peeling rubber roller 10! 1 film 11 and 1 caulking material 4 are peeled off from the exterior material 1 surface. By rotating and moving the rubber roller 10 on the exterior material 1, the rubber roller 10 can be secured around the rubber roller 10!
The film 11 is attached, and it is preserved! The film 11 can be wound up.

しかして、マスキング剤3を目地部2の近傍にて外装材
1表面に塗布した後、目地部2内にコーキング材4を充
填して表面を仕上げることによ、ワ、外装材1表面はマ
スキング剤3で保護されて直にコーキング材が外装材1
表面に付着するということがないものであり、その後マ
スキング剤3を目地部2表面から剥ぎ取ることで目地部
2からはみ出たコーキング材4を除去することができる
ものである。特に、塗布用ローラー9を用いてマスキン
グ剤3を塗布し、また剥離用のゴムローラー10で剥離
することにより、マスキング剤3の塗布作業及び剥離作
業が極めて容易に行えるものである。上記方法は特に工
場内でのコーキング材施工に適し、コーキング材光項作
業が能率良く行え外壁パネル8の生産性が向上できるも
のである。
By applying the masking agent 3 to the surface of the exterior material 1 near the joints 2 and then filling the joints 2 with caulking material 4 to finish the surface, the surface of the exterior material 1 is masked. The caulking material is immediately applied to exterior material 1 after being protected by agent 3.
It does not adhere to the surface, and by subsequently peeling off the masking agent 3 from the surface of the joint 2, the caulking material 4 protruding from the joint 2 can be removed. In particular, by applying the masking agent 3 using the coating roller 9 and peeling it off using the peeling rubber roller 10, the coating and peeling operations of the masking agent 3 can be performed extremely easily. The above-mentioned method is particularly suitable for applying caulking material in a factory, and allows the caulking material work to be carried out efficiently and the productivity of the outer wall panel 8 to be improved.

〔発明の効果1 上記のように本発明は、目地部の開口縁における外装材
の表面にマスキング剤を塗布し、次いで目地部内にコー
キング材を充填し、このコーキング材表面を仕上げ用泊
兵で仕上げた後、マスキング剤を外装材表面から剥離す
るようにしたので、マスキング剤で外装材の表面を保護
した状態でコーキング材がかき取られることになり、そ
の後マスキング剤を外装材から剥離することではみ出た
コーキング材も同時に除去することかでト、コーキング
材が目地部からはみ出すことなくコーキング材表面を平
滑に仕上げることができ、従来の如く後処理でコーキン
グ材を除去する必要がなくなって充填作業の能率が向上
できる共に充填精度を向上することができるものである
[Effect of the invention 1 As described above, the present invention applies a masking agent to the surface of the exterior material at the opening edge of the joint, then fills the joint with caulking material, and then coats the surface of this caulking material with a finishing coat. After finishing, the masking agent was peeled off from the surface of the exterior material, so the caulking material was scraped off while the surface of the exterior material was protected by the masking agent, and then the masking agent was peeled off from the exterior material. By removing the protruding caulking material at the same time, the surface of the caulking material can be smoothed without the caulking material protruding from the joints, and there is no need to remove the caulking material in post-processing as in the past. This not only improves work efficiency but also improves filling accuracy.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図及び第2図はそれぞれ本発明一実施例のコーキン
グ材の充填方法を示す説明図である。 1は外装材、2は目地部、3はマスキング剤、4はコー
キング材、6は仕上げ用泊兵、9は塗布用ローラー、1
0は剥離用ローラーである。 代理人 弁理士 石 1)艮 七 第 1図 第2図 手続補正書(方式) %式% 2、発明の名称 外装材の目地部へのコーキング材の充填方法3、補正を
する者 事件との関係  特許出願人 住  所 大阪府豊中市新千里西町1丁目1番12号名
  称 (467>ナショナル住宅産業株式会社代表者
  西  尾   稔 4、代理人 郵便番号 530 5、補正命令の日付 昭和59年10月9日 6、補正の対象 明細書
FIGS. 1 and 2 are explanatory diagrams each showing a caulking material filling method according to an embodiment of the present invention. 1 is an exterior material, 2 is a joint, 3 is a masking agent, 4 is a caulking material, 6 is a finishing coat, 9 is an application roller, 1
0 is a peeling roller. Agent Patent attorney Ishi 1) Ai 7 Figure 1 Figure 2 Procedural amendment (method) % formula % 2. Name of the invention Method of filling caulking material into the joints of exterior materials 3. Connection with the case of the person making the amendment Related Patent Applicant Address 1-1-12 Shinsenri Nishimachi, Toyonaka City, Osaka Name (467> National Housing Industry Co., Ltd. Representative Minoru Nishio 4, Agent Zip Code 530 5, Date of Amendment Order 1982) October 9th 6, Specification subject to amendment

Claims (3)

【特許請求の範囲】[Claims] (1)一対の外装材の端面間で形成される目地部の近傍
における外装材の表面にマスキング剤を塗布し、次いで
目地部内にコーキング材を充填し、このコーキング材表
面を仕上げ用治具で仕上げた後、上記マスキング剤を外
装材表面から剥離することを特徴とする外装材の目地部
へのコーキング材の充填方法。
(1) Apply a masking agent to the surface of the exterior material near the joint formed between the end faces of a pair of exterior materials, then fill the joint with caulking material, and use a finishing jig to finish the surface of the caulking material. A method for filling a joint part of an exterior material with a caulking material, which comprises peeling off the masking agent from the surface of the exterior material after finishing.
(2)マスキング剤が塗布用ローラーにて塗布されるこ
とを特徴とする特許請求の範囲第1項記載の外装材の目
地部へのコーキング材の充填方法。
(2) A method for filling a caulking material into a joint of an exterior material according to claim 1, wherein the masking agent is applied using a coating roller.
(3)マスキング剤が剥離用ローラーにて外装材から剥
離されることを特徴とする特許請求の範囲第1項記載の
外装材の目地部へのコーキング材の充填方法。
(3) A method for filling a joint part of an exterior material with a caulking material according to claim 1, wherein the masking agent is peeled off from the exterior material using a peeling roller.
JP14544384A 1984-07-13 1984-07-13 Method for filling caulking material into joint part of facing material Pending JPS6125669A (en)