JPS60108332A - 板ガラスの強化方法 - Google Patents
板ガラスの強化方法Info
- Publication number
- JPS60108332A JPS60108332A JP21417383A JP21417383A JPS60108332A JP S60108332 A JPS60108332 A JP S60108332A JP 21417383 A JP21417383 A JP 21417383A JP 21417383 A JP21417383 A JP 21417383A JP S60108332 A JPS60108332 A JP S60108332A
- Authority
- JP
- Japan
- Prior art keywords
- cooling
- glass
- baffle plate
- flat glass
- strengthening
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 239000005357 flat glass Substances 0.000 title claims abstract description 43
- 238000000034 method Methods 0.000 title claims description 19
- 238000005496 tempering Methods 0.000 title abstract 3
- 238000001816 cooling Methods 0.000 claims abstract description 49
- 239000002826 coolant Substances 0.000 claims abstract description 10
- 238000005728 strengthening Methods 0.000 claims description 23
- 239000011521 glass Substances 0.000 claims description 13
- 238000005507 spraying Methods 0.000 claims description 2
- 239000005341 toughened glass Substances 0.000 abstract description 10
- 238000010438 heat treatment Methods 0.000 abstract description 4
- 238000010791 quenching Methods 0.000 abstract 1
- 230000000171 quenching effect Effects 0.000 abstract 1
- 230000002787 reinforcement Effects 0.000 description 10
- 238000009826 distribution Methods 0.000 description 5
- 230000000694 effects Effects 0.000 description 4
- 229920003023 plastic Polymers 0.000 description 4
- 230000002093 peripheral effect Effects 0.000 description 3
- 239000012634 fragment Substances 0.000 description 2
- 238000000465 moulding Methods 0.000 description 2
- 230000003187 abdominal effect Effects 0.000 description 1
- 238000005452 bending Methods 0.000 description 1
- 238000007664 blowing Methods 0.000 description 1
- 230000007547 defect Effects 0.000 description 1
- 238000010586 diagram Methods 0.000 description 1
- 230000000977 initiatory effect Effects 0.000 description 1
- 238000004519 manufacturing process Methods 0.000 description 1
- 239000003595 mist Substances 0.000 description 1
- 239000006058 strengthened glass Substances 0.000 description 1
- 230000002195 synergetic effect Effects 0.000 description 1
- 125000000391 vinyl group Chemical group [H]C([*])=C([H])[H] 0.000 description 1
- 229920002554 vinyl polymer Polymers 0.000 description 1
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 description 1
Landscapes
- Re-Forming, After-Treatment, Cutting And Transporting Of Glass Products (AREA)
Priority Applications (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21417383A JPS60108332A (ja) | 1983-11-16 | 1983-11-16 | 板ガラスの強化方法 |
| GB08427114A GB2149777B (en) | 1983-11-16 | 1984-10-26 | Method of toughening glass sheet by quenching |
| FR848416587A FR2554805B1 (fr) | 1983-11-16 | 1984-10-30 | Procede pour tremper une feuille de verre par refroidissement brusque, et feuille de verre obtenue |
| DE19843439871 DE3439871A1 (de) | 1983-11-16 | 1984-10-31 | Verfahren zum haerten einer glasschicht durch abschrecken |
| US06/842,723 US4662926A (en) | 1983-11-16 | 1986-03-20 | Method of toughening glass sheet by quenching |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP21417383A JPS60108332A (ja) | 1983-11-16 | 1983-11-16 | 板ガラスの強化方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS60108332A true JPS60108332A (ja) | 1985-06-13 |
| JPS6247819B2 JPS6247819B2 (enExample) | 1987-10-09 |
Family
ID=16651440
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP21417383A Granted JPS60108332A (ja) | 1983-11-16 | 1983-11-16 | 板ガラスの強化方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS60108332A (enExample) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN102557415A (zh) * | 2010-09-22 | 2012-07-11 | 格拉斯顿服务有限公司 | 喷嘴箱组件 |
| JP2017206433A (ja) * | 2016-05-17 | 2017-11-24 | グラストン フィンランド オイGlaston Finland Oy | ガラス板を強化するための方法および装置 |
| JP2020506865A (ja) * | 2017-02-20 | 2020-03-05 | サン−ゴバン グラス フランス | ガラスペインの熱による強化処理のための強化処理フレーム |
-
1983
- 1983-11-16 JP JP21417383A patent/JPS60108332A/ja active Granted
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN102557415A (zh) * | 2010-09-22 | 2012-07-11 | 格拉斯顿服务有限公司 | 喷嘴箱组件 |
| JP2017206433A (ja) * | 2016-05-17 | 2017-11-24 | グラストン フィンランド オイGlaston Finland Oy | ガラス板を強化するための方法および装置 |
| JP2020506865A (ja) * | 2017-02-20 | 2020-03-05 | サン−ゴバン グラス フランス | ガラスペインの熱による強化処理のための強化処理フレーム |
| US11332402B2 (en) | 2017-02-20 | 2022-05-17 | Saint-Gobain Glass France | Tempering frame for thermal tempering of glass panes |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6247819B2 (enExample) | 1987-10-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4128690A (en) | Toughened glass sheets | |
| US2042610A (en) | Method and apparatus for tempering glass | |
| EP2280097B1 (en) | Method of generating cracks in polycrystalline silicon rod and crack generating apparatus | |
| US4198463A (en) | Toughened glass sheets | |
| US2309290A (en) | Cooling nozzle for tempering hollow glassware | |
| US4662926A (en) | Method of toughening glass sheet by quenching | |
| CN102143920A (zh) | 玻璃板的风冷强化装置及风冷强化方法 | |
| JP2018524535A (ja) | 温度調節されるべき非無端表面の均一な非接触温度調節方法およびその装置 | |
| US1951950A (en) | Method and apparatus for cooling glass articles | |
| EP0000269B1 (en) | Method for thermally toughening glass sheets and glass sheets obtained by this method, in particular to be used as motor vehicle side or rear windows. | |
| US4178414A (en) | Method of toughening glass sheets | |
| JP2653708B2 (ja) | 強化ガラス板の製造方法 | |
| JPS60108332A (ja) | 板ガラスの強化方法 | |
| KR0145060B1 (ko) | 룰러 반송된 유리판을 냉각하는 장치 | |
| JPH0623068B2 (ja) | 板ガラスの強化方法 | |
| US3294519A (en) | Glass sheet tempering apparatus | |
| US20160201156A1 (en) | Nozzle for cooling vacuum heat treatment furnace | |
| CN108483885B (zh) | 一种2mm玻璃的钢化方法 | |
| JPS6343327B2 (enExample) | ||
| CN208038518U (zh) | 一种退火炉喷口装置 | |
| CN206858429U (zh) | 一种钢化炉用风栅结构 | |
| JPS6250416B2 (enExample) | ||
| CN105886736A (zh) | 一种大截面轴类锻件热处理方法 | |
| CN212533069U (zh) | 一种分段式淬火冷却设备 | |
| JPS56102567A (en) | Hardening method for aluminum strip |