JPS595158B2 - ソイルセメントトシテノスラグノリヨウホウホウ - Google Patents

ソイルセメントトシテノスラグノリヨウホウホウ

Info

Publication number
JPS595158B2
JPS595158B2 JP50005749A JP574975A JPS595158B2 JP S595158 B2 JPS595158 B2 JP S595158B2 JP 50005749 A JP50005749 A JP 50005749A JP 574975 A JP574975 A JP 574975A JP S595158 B2 JPS595158 B2 JP S595158B2
Authority
JP
Japan
Prior art keywords
slag
cement
electric furnace
black
converter
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP50005749A
Other languages
English (en)
Japanese (ja)
Other versions
JPS5181409A (enExample
Inventor
任 鴛海
正雄 伯
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Jiryoku Senko Co Ltd
Original Assignee
Nippon Jiryoku Senko Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Jiryoku Senko Co Ltd filed Critical Nippon Jiryoku Senko Co Ltd
Priority to JP50005749A priority Critical patent/JPS595158B2/ja
Publication of JPS5181409A publication Critical patent/JPS5181409A/ja
Publication of JPS595158B2 publication Critical patent/JPS595158B2/ja
Expired legal-status Critical Current

Links

Classifications

    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02WCLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT
    • Y02W30/00Technologies for solid waste management
    • Y02W30/50Reuse, recycling or recovery technologies
    • Y02W30/91Use of waste materials as fillers for mortars or concrete

Landscapes

  • Soil Conditioners And Soil-Stabilizing Materials (AREA)
JP50005749A 1975-01-09 1975-01-09 ソイルセメントトシテノスラグノリヨウホウホウ Expired JPS595158B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP50005749A JPS595158B2 (ja) 1975-01-09 1975-01-09 ソイルセメントトシテノスラグノリヨウホウホウ

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP50005749A JPS595158B2 (ja) 1975-01-09 1975-01-09 ソイルセメントトシテノスラグノリヨウホウホウ

Publications (2)

Publication Number Publication Date
JPS5181409A JPS5181409A (enExample) 1976-07-16
JPS595158B2 true JPS595158B2 (ja) 1984-02-02

Family

ID=11619745

Family Applications (1)

Application Number Title Priority Date Filing Date
JP50005749A Expired JPS595158B2 (ja) 1975-01-09 1975-01-09 ソイルセメントトシテノスラグノリヨウホウホウ

Country Status (1)

Country Link
JP (1) JPS595158B2 (enExample)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS63108093A (ja) * 1986-10-23 1988-05-12 Nippon Jiryoku Senko Kk 廃棄物並びに軟弱土固化材

Also Published As

Publication number Publication date
JPS5181409A (enExample) 1976-07-16

Similar Documents

Publication Publication Date Title
Baghdadi et al. The potential of cement kiln dust for the stabilization of dune sand in highway construction
KR101700017B1 (ko) 황 제강-슬래그 골재 콘크리트
KR101246114B1 (ko) Tbm 공법에 적용되는 세그먼트용 콘크리트 조성물 및 이에 의하여 제조된 고성능 콘크리트 세그먼트
JP2014080367A (ja) フライアッシュ・コンクリート
KR20100071272A (ko) 용선예비처리 슬래그를 이용한 시멘트 혼화재 제조방법
JPS595158B2 (ja) ソイルセメントトシテノスラグノリヨウホウホウ
CN108840635A (zh) 一种将固废炉渣制作成非烧结砖的配方及制备方法
Zain et al. Influence of different curing conditions on strength and durability of high-performance concrete
Kersh et al. Repair mixture for limestone-shell buildings
US2898220A (en) Process for manufacturing steamcured light-weight concrete with low shrinkage
JP2020011871A (ja) 耐久性を有するコンクリート
US2127451A (en) Hardening and waterproofing composition for concrete or mortar
JP7652144B2 (ja) 水和固化体の製造方法
Rajeshkumar et al. Performance of Rice Husk Ash and Groundnut Shell Ash in Sustainable Concrete
JPS60166249A (ja) セメントモルタル系硬化体の成形方法
CN120864852B (zh) 一种用于生态护坡的固废基多孔性材料及其制备方法
JPH0421549A (ja) 透水性コンクリート
KR102488082B1 (ko) 자철광 미분말과 석회석 미분말을 혼화재로 사용한 27MPa급 순환 굵은 골재 콘크리트 조성물
JPS61238398A (ja) 深層ヘドロ硬化材の製造方法
JPH04114942A (ja) コンクリート用乾燥収縮低減剤及び乾燥収縮低減剤配合セメント
CN110683817A (zh) 一种钛渣路基材料及其制备方法和应用
JPS6253468B2 (enExample)
RU1815256C (ru) В жущее
JPS60137496A (ja) ヘドロ用固化材
RU1813759C (ru) В жущее дл строительных растворов и бетонов