JPS5946696B2 - Metal molding manufacturing method - Google Patents

Metal molding manufacturing method

Info

Publication number
JPS5946696B2
JPS5946696B2 JP15021480A JP15021480A JPS5946696B2 JP S5946696 B2 JPS5946696 B2 JP S5946696B2 JP 15021480 A JP15021480 A JP 15021480A JP 15021480 A JP15021480 A JP 15021480A JP S5946696 B2 JPS5946696 B2 JP S5946696B2
Authority
JP
Japan
Prior art keywords
metal plate
molding
metal
decorative tape
metal molding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP15021480A
Other languages
Japanese (ja)
Other versions
JPS5775232A (en
Inventor
淳男 鈴木
謹也 安塚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hashimoto Forming Industry Co Ltd
Original Assignee
Hashimoto Forming Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hashimoto Forming Industry Co Ltd filed Critical Hashimoto Forming Industry Co Ltd
Priority to JP15021480A priority Critical patent/JPS5946696B2/en
Publication of JPS5775232A publication Critical patent/JPS5775232A/en
Publication of JPS5946696B2 publication Critical patent/JPS5946696B2/en
Expired legal-status Critical Current

Description

【発明の詳細な説明】 本発明は金属モールディングの製造方法、特にモールデ
ィング端末の処理方法に関するものである。
DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a method for manufacturing metal moldings, and more particularly to a method for treating molding ends.

従来金属モールディングは金属板材をプレス成形して成
るモールディングの表面にメッキ、蒸着、スパッタリン
グ、或いは塗装などの方法により装飾層を設けるように
しているが、これによれば公害などの問題が発生し、ま
た量産化を図ることが; できないという欠点を有して
いる。
Conventionally, metal molding is made by press-forming a metal plate material, and a decorative layer is provided on the surface of the molding using methods such as plating, vapor deposition, sputtering, or painting, but this causes problems such as pollution. It also has the disadvantage of not being able to be mass-produced.

そこで近時本出願人による第1図に示すような例えばピ
ラーカバーになどの金属モールディングを製造する場合
において、第2図に示すように予め平板状の金属板材1
の表面側に着色された装飾oテープ2を被着しておき、
この被着した平担状の部材を一定形状にブランクするよ
うにしてモールディングとして製造している。
Therefore, recently, when manufacturing a metal molding such as a pillar cover as shown in FIG. 1 by the present applicant, a flat metal plate material 1 is prepared in advance as shown in FIG.
A colored decorative o-tape 2 is applied to the front side of the
This adhered flat member is blanked into a predetermined shape to produce a molding.

これによれば装飾テープ2を平担な金属板材1の表面に
貼着するので、この作業が著しく簡単となりしかもプレ
ス成5形後何ら他の処理を施す必要がないので量産化を
図ることができ、かつ公害が発生しない。しかしながら
このような方法によれば予め金属板材1の表面に相当な
テンションをもつて装飾テープ2を被着しているので、
第3図、第4図に示・oすように長期間の使用において
装飾テープ2が次第に収縮することに依りその端末3が
内側方向に移動し金属板材1より成るモールディング1
0の端末11が外側に露出してしまいこれにより装飾効
果が著しく失われ、しかもこの露出した部分か・5ら錆
などが発生してしまう。
According to this method, since the decorative tape 2 is attached to the surface of the flat metal plate material 1, this work becomes extremely simple, and there is no need to perform any other processing after press forming, making mass production possible. It is possible to do so without causing any pollution. However, according to this method, since the decorative tape 2 is applied to the surface of the metal plate 1 with considerable tension in advance,
As shown in FIGS. 3 and 4, as the decorative tape 2 gradually shrinks during long-term use, its ends 3 move inward, causing the molding 1 made of the metal plate 1
The terminal 11 of 0 is exposed to the outside, resulting in a significant loss of decorative effect, and furthermore, rust etc. occur from this exposed portion.

なおモールディング10において第3図に示す如くその
端末11が内側方向に折り返された場合(カバーにの中
央部)においてはこの露出した部分が外部から目視され
ないので装飾上は問題とならないのであるが、第■04
図に示すように金属板材1を内側に折曲げない部分(カ
バーにの端部)についてはこの端末11がそのまま外部
から目視されてしまうので上記問題が大きくなる。本発
明の目的は装飾テープの端末を金属板材よ■5 り成る
金属モールディングの端末よりも外側方向に突出せしめ
この突出した部分を内側に折り返して金属モールディン
グの端末を被うようにして上記欠点を除去するものであ
り、以下実施例を用いて詳細に説明する。
In addition, when the terminal 11 of the molding 10 is folded back inward as shown in FIG. 3 (at the center of the cover), this exposed part is not visible from the outside, so there is no problem in terms of decoration. No. ■04
As shown in the figure, the above-mentioned problem is exacerbated in the portion where the metal plate material 1 is not bent inward (the end portion of the cover) because the terminal 11 is visible from the outside. An object of the present invention is to make the end of the decorative tape protrude outward from the end of the metal molding made of metal plate material, and to fold this projecting part inward so as to cover the end of the metal molding. This will be explained in detail below using examples.

第5図ないし第8図は本発明による金属モールデイング
の製造方法の一実施例を示す製造工程図であり、第3図
、第4図と同じものは同一符号を用いている。
5 to 8 are manufacturing process diagrams showing an embodiment of the method for manufacturing metal molding according to the present invention, and the same parts as in FIGS. 3 and 4 are denoted by the same reference numerals.

本発明においてはまず平担状の金属板材1の表面に装飾
テープ2を被着せしめついで第1図に示すように例えば
ピラーカバーなどの形状にこの板材1をブランクするの
であるが、この場合、第6図の如くモールデイング10
における内側に折り返さない端末Sにおいて金属板材1
、装飾テープ2の長さがlだけ多少長くなるようにブラ
ンクし、しかもこの端末Sに対応する個所における金属
板材1にブランクを行なうときに或いはブランクの前の
工程において切欠12を設けておく。
In the present invention, a decorative tape 2 is first applied to the surface of a flat metal plate 1, and then the plate 1 is blanked into the shape of, for example, a pillar cover, as shown in FIG. Molding 10 as shown in Figure 6
Metal plate material 1 at the terminal S that is not folded back inward in
The decorative tape 2 is blanked so that its length is slightly longer by l, and a notch 12 is provided when blanking the metal plate 1 at a location corresponding to the terminal S or in a step before blanking.

ブランク終了後において切欠12よりモールデイング1
0の端末Sに相当する個所より突出する部分の金属板材
を折るようにして除去しこれによりモールデイング10
の端末Sに相当する個所より装飾テープ2は外側に突出
するのでこの突出した部分20を内側に折り返しモール
デイング10としての金属板材1の端末をこの突出した
部分20によつて被うようにする。この場合装飾テープ
2の裏面に粘接着層を設けておくことにより突出部20
を裏側に折り返すだけで金属板材1の端末側にこの突出
部20を被着することができる。以上説明したように本
発明によれば金属モールデイングの端末を、その表面側
に被着される装飾テープの端末を裏側に折り返すことに
よりこの折り返した部分で被うようにしたので装飾テー
プに経時的な収縮が発生しても金属モールデイングの端
末が外部に露出することがなく従来に比較して装飾性を
高めることができ、しかも端末に錆などが発生するとい
う欠点を除去できる。
Molding 1 from notch 12 after blanking
The part of the metal plate that protrudes from the part corresponding to the terminal S of 0 is folded and removed, thereby forming the molding 10.
Since the decorative tape 2 protrudes outward from a portion corresponding to the terminal S, this protruding portion 20 is folded inward so that the terminal end of the metal plate material 1 serving as the molding 10 is covered by this protruding portion 20. . In this case, by providing an adhesive layer on the back side of the decorative tape 2, the protruding portion 20
The protrusion 20 can be attached to the end side of the metal plate 1 by simply folding it back. As explained above, according to the present invention, the end of the metal molding is covered by the folded part by folding the end of the decorative tape applied to the front side of the metal molding to the back side. Even if mechanical shrinkage occurs, the ends of the metal molding will not be exposed to the outside, making it possible to improve the decorativeness compared to the conventional method, and eliminate the disadvantage of rust on the ends.

従つて金属モールデイングの長寿命化を図ることができ
る。また、装飾部材の端末よりも内側の金属板材に薄肉
部を形成して、プレス成形後に金属板材の端末側をこの
薄肉部より除去することにより、より迅速かつ正確に装
飾テープの端末を外側に突出させることができる。なお
本発明においてピラーカバーより成る金属モールデイン
グについて説明したが本発明はこれに限定されず金属材
より成る車輛用外装品であれば如何なるものであつても
本発明を適用できる。
Therefore, it is possible to extend the life of the metal molding. In addition, by forming a thin part on the metal plate material inside the end of the decorative member and removing the end side of the metal plate material from this thin part after press forming, the end of the decorative tape can be moved outward more quickly and accurately. It can be made to stand out. Although the present invention has been described with respect to a metal molding made of a pillar cover, the present invention is not limited thereto, and the present invention can be applied to any vehicle exterior product made of a metal material.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図ないし第4図は従来の金属モールデイングの製造
方法の一例を示す平面図および断面図、第5図ないし第
8図は本発明による金属モールデイングの製造方法の一
実施例を示す斜視図および断面図である。 1・・・・・・金属部材、2・・・・・・装飾テープ、
3・・・・・・端末、10・・・・・・金属モールデイ
ング、20・・・・・・装飾テープの突出部。
1 to 4 are plan views and sectional views showing an example of a conventional metal molding manufacturing method, and FIGS. 5 to 8 are perspective views showing an embodiment of a metal molding manufacturing method according to the present invention. FIG. 2 is a diagram and a cross-sectional view. 1... Metal member, 2... Decorative tape,
3...Terminal, 10...Metal molding, 20...Protrusion of decorative tape.

Claims (1)

【特許請求の範囲】[Claims] 1 金属板材の表面側に装飾テープを貼着した部材をプ
レス成形して金属モールディングとして製造するように
した金属モールディングの製造方法において、プレス成
形時またはプレス成形の前の工程において、装飾テープ
の端末よりも内側の金属板材に薄肉部を形成しておき、
プレス成形後に金属板材の端末側をこの薄肉部より除去
することにより金属板材における端末よりも装飾テープ
の端末を外側に突出せしめ、この突出した部分を内側に
折り返すようにして金属板材の端末を被うようにしたこ
とを特徴とする金属モールディングの製造方法。
1. In a metal molding manufacturing method in which a member with a decorative tape pasted on the surface side of a metal plate material is press-molded to produce a metal molding, the end of the decorative tape is Form a thin wall part on the metal plate material inside the
After press forming, the end of the metal plate is removed from this thin wall part so that the end of the decorative tape protrudes outward from the end of the metal plate, and this protruding part is folded back inward to cover the end of the metal plate. A method for manufacturing a metal molding, characterized in that:
JP15021480A 1980-10-28 1980-10-28 Metal molding manufacturing method Expired JPS5946696B2 (en)