JPS5932803Y2 - Equipment for observing corrosion inside a multi-tubular once-through boiler - Google Patents
Equipment for observing corrosion inside a multi-tubular once-through boilerInfo
- Publication number
- JPS5932803Y2 JPS5932803Y2 JP764180U JP764180U JPS5932803Y2 JP S5932803 Y2 JPS5932803 Y2 JP S5932803Y2 JP 764180 U JP764180 U JP 764180U JP 764180 U JP764180 U JP 764180U JP S5932803 Y2 JPS5932803 Y2 JP S5932803Y2
- Authority
- JP
- Japan
- Prior art keywords
- boiler
- header
- test piece
- equipment
- corrosion inside
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【考案の詳細な説明】
この考案は、上下管寄せを多数の木管で連通した多管式
貫流ボイラにおける罐内腐食状態観察装置に関するもの
である。[Detailed description of the invention] This invention relates to an apparatus for observing the state of corrosion inside a can in a multi-tube once-through boiler in which the upper and lower headers are connected through a large number of wooden tubes.
多管式貫流ボイラにおいて、水処理が不適当であると、
下部管寄せ等にピッチング等の腐食が発生する。In a multi-tubular once-through boiler, if water treatment is inadequate,
Corrosion such as pitting occurs on the lower header, etc.
これは、給水中に含まれている溶存酸素等が原因で゛あ
る。This is caused by dissolved oxygen, etc. contained in the water supply.
そこで従来においては、検査孔等から内部を覗いて腐食
状態を推定していた。Conventionally, therefore, the state of corrosion was estimated by looking into the interior through an inspection hole or the like.
ピッチングの深さ等は測定することができなかった。It was not possible to measure pitching depth, etc.
この考案は、管寄せと同質材料から戊る試験片を下部管
寄せ内へ挿入配置しておき、この試験片を観察すること
によって、罐内の腐食状態を推定できるようにしようと
するものである。This idea aims to make it possible to estimate the state of corrosion inside the can by inserting a test piece made of the same material as the header into the lower header and observing this test piece. be.
ピッチングの深さ等も、この試験片を測定することによ
って、推定できるようにしようとするものである。The depth of pitting and the like can also be estimated by measuring this test piece.
以下この考案の実施例を図面にもとづいて説明する。Examples of this invention will be described below based on the drawings.
この考案の多管式貫流ボイラは、上部管寄せ1および下
部管寄せ2が多数の水管3によって連通されている。In the multi-tubular once-through boiler of this invention, an upper header 1 and a lower header 2 are communicated through a large number of water pipes 3.
下部管寄せ2の一部に試験片挿入口4が設けられている
。A test piece insertion port 4 is provided in a part of the lower header 2.
管寄せと同質材料から成る試験片5が挿入口4から下部
管寄せ2内へ挿入配置されている。A test piece 5 made of the same material as the header is inserted into the lower header 2 through the insertion port 4.
試験片5は管寄せと同質材料であるから、ボイラを長期
間運転後取り出し、これを観察することによって、罐内
の状態を推定することができる。Since the test piece 5 is made of the same material as the header, the condition inside the can can be estimated by taking the boiler out after a long period of operation and observing it.
この考案は多管式貫流ボイラについて記したが、他のボ
イラにおいても適用可能である。Although this idea has been described for a multi-tubular once-through boiler, it can also be applied to other boilers.
以上説明したようにこの考案は、構造簡単で効果的な罐
内腐食状態観察装置を提供することができるものである
。As explained above, this invention can provide an apparatus for observing corrosion inside a can that is simple in structure and effective.
第1図は、この考案の実施例を示した概略縦断面図であ
る。
第2図は、要部拡大縦断面図である。
1・・・・・・上部管寄せ、2・・・・・・下部管寄せ
、3・・・・・・水管、4・・・・・・試験片挿入口、
5・・・・・・管寄せと同質材料から成る試験片。FIG. 1 is a schematic vertical sectional view showing an embodiment of this invention. FIG. 2 is an enlarged longitudinal sectional view of the main part. 1... Upper header, 2... Lower header, 3... Water pipe, 4... Test piece insertion port,
5...Test piece made of the same material as the header.
Claims (1)
した多管式貫流ボイラにおいて、下部管寄せ2の一部に
試験片挿入口4を設け、管寄せと同質材料から戊る試験
片5を挿入口4から下部管寄せ2内へ挿入配置したこと
を特徴とする多管式貫流ボイラの罐内腐食状能観察装置
。In a multi-tube once-through boiler in which an upper header 1 and a lower header 2 are connected through a large number of water pipes 3, a test piece insertion port 4 is provided in a part of the lower header 2, and a test piece is cut from the same material as the header. 5 inserted into the lower header 2 through the insertion port 4.