JPS5930781A - アルミニウムダイカスト部品圧洩れ欠陥の含浸密封方法 - Google Patents
アルミニウムダイカスト部品圧洩れ欠陥の含浸密封方法Info
- Publication number
- JPS5930781A JPS5930781A JP13738582A JP13738582A JPS5930781A JP S5930781 A JPS5930781 A JP S5930781A JP 13738582 A JP13738582 A JP 13738582A JP 13738582 A JP13738582 A JP 13738582A JP S5930781 A JPS5930781 A JP S5930781A
- Authority
- JP
- Japan
- Prior art keywords
- acid
- water glass
- aluminum die
- die
- defects
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Ceramic Products (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13738582A JPS5930781A (ja) | 1982-08-09 | 1982-08-09 | アルミニウムダイカスト部品圧洩れ欠陥の含浸密封方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP13738582A JPS5930781A (ja) | 1982-08-09 | 1982-08-09 | アルミニウムダイカスト部品圧洩れ欠陥の含浸密封方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5930781A true JPS5930781A (ja) | 1984-02-18 |
JPS6411411B2 JPS6411411B2 (enrdf_load_stackoverflow) | 1989-02-23 |
Family
ID=15197447
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP13738582A Granted JPS5930781A (ja) | 1982-08-09 | 1982-08-09 | アルミニウムダイカスト部品圧洩れ欠陥の含浸密封方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5930781A (enrdf_load_stackoverflow) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6247490A (ja) * | 1985-08-26 | 1987-03-02 | Shiramizu Sangyo:Kk | ダイカスト製品の含浸方法および含浸装置 |
GB2501896A (en) * | 2012-05-09 | 2013-11-13 | Uk Sport | Aerodynamic fork |
-
1982
- 1982-08-09 JP JP13738582A patent/JPS5930781A/ja active Granted
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6247490A (ja) * | 1985-08-26 | 1987-03-02 | Shiramizu Sangyo:Kk | ダイカスト製品の含浸方法および含浸装置 |
GB2501896A (en) * | 2012-05-09 | 2013-11-13 | Uk Sport | Aerodynamic fork |
Also Published As
Publication number | Publication date |
---|---|
JPS6411411B2 (enrdf_load_stackoverflow) | 1989-02-23 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
TWI525217B (zh) | Aluminum alloy article, aluminum alloy member and manufacturing method thereof | |
US4439241A (en) | Cleaning process for internal passages of superalloy airfoils | |
JP2001003184A (ja) | 基体からアルミニドコーティングを除去する方法 | |
KR970074977A (ko) | 금속과 복합물을 결합시키는 신규한 방법 | |
JPS616287A (ja) | 耐熱合金製品用化学的酸洗い浴 | |
JP6543037B2 (ja) | 金属‐樹脂複合体の製造方法 | |
JPS5930781A (ja) | アルミニウムダイカスト部品圧洩れ欠陥の含浸密封方法 | |
JPS6133752A (ja) | 複合アルミニウム部材の製造方法 | |
CN101560657B (zh) | 一种镁合金表面化学转化处理的方法 | |
CN112519099A (zh) | 一种注塑前铝合金表面处理方法 | |
CN109321928A (zh) | 一种超级奥氏体不锈钢卷连续酸洗方法 | |
WO2015045595A1 (ja) | 流体機械用部材の製造方法、及び、流体機械用部材 | |
JPH0134737B2 (enrdf_load_stackoverflow) | ||
JPS649128B2 (enrdf_load_stackoverflow) | ||
CN104923520A (zh) | 经磨粒流加工后的涡轮叶片残留磨料的清洗方法 | |
US4444804A (en) | Flame sprayed coatings | |
CN115475608B (zh) | 一种废弃氧化铝干燥剂低温浸渍原位再生方法 | |
JP2000245115A (ja) | アルミ製回転体の製造方法 | |
CN101818353B (zh) | 一种防止气孔的钛及钛合金焊接表面前处理工艺 | |
CN114635124B (zh) | 一种铝合金小口径深腔内表面可焊性镀层的制作方法 | |
CN118773613A (zh) | 一种防腐蚀剂及其制备方法、应用 | |
CN115522209B (zh) | 一种钢材强化处理液及钢材处理工艺 | |
JPH1161054A (ja) | 電子部品の樹脂部材接合面の前処理方法 | |
US4550761A (en) | Mold coating | |
JPH06122065A (ja) | 鋳型材の化学的除去方法およびその装置 |