JPS59124832A - Mold for producing glove - Google Patents

Mold for producing glove

Info

Publication number
JPS59124832A
JPS59124832A JP57234759A JP23475982A JPS59124832A JP S59124832 A JPS59124832 A JP S59124832A JP 57234759 A JP57234759 A JP 57234759A JP 23475982 A JP23475982 A JP 23475982A JP S59124832 A JPS59124832 A JP S59124832A
Authority
JP
Japan
Prior art keywords
mold
glove
face
semi
sand
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP57234759A
Other languages
Japanese (ja)
Inventor
Hiroshi Fujii
弘 藤井
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ST KAGAKU KOGYO KK
Original Assignee
ST KAGAKU KOGYO KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ST KAGAKU KOGYO KK filed Critical ST KAGAKU KOGYO KK
Priority to JP57234759A priority Critical patent/JPS59124832A/en
Publication of JPS59124832A publication Critical patent/JPS59124832A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To provide good apparent feelingness for a mold for glove by a method in which fine particles of graze and sand are sprayed onto the outer surface of unfinished product in a semi-dried state during the molding process to form a fine uneven (particles-shaped) face on the outer surface, and the mold is completely dried and baked. CONSTITUTION:Fine particles of a graze and sand are sprayed onto the outer surface of a mold in a semi-dried state during the mold-manufacuring stage to form a fine uneven (particle-shaped) face 1, and the mold is completely dried and baked. The film 3 of a soft synthetic resin is formed on the surface of the mold 2 by a dipping method and gelled, and the film 3 is separated from the mold 2 to obtain a glove. In forming the fine uneven face on the outer surface of the mold by a dipping method, the dripping of the soft synthetic resin or rubber is avoided. A well-flexible and less-sticky glove having a thick feelingness for the weight can thus be obtained.

Description

【発明の詳細な説明】 本発明はゴム、軟質合成樹脂等製の手袋を浸漬法により
製する際に使用する新規の手袋製造用型に関するもので
あって、製作工程中に於て半乾燥の状態にある未完品の
外表面に釉薬および砂等粒子を吹付けて同面を微細な粒
状の凹凸面とし、然るのちに完全に乾燥して焼成するこ
とを要旨とするものである。
DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a new glove manufacturing mold used when manufacturing gloves made of rubber, soft synthetic resin, etc. by the dipping method. The gist of this method is to spray particles such as glaze and sand onto the outer surface of an unfinished product to create a finely granular uneven surface, which is then completely dried and fired.

尚、図示せる実施例は型製作段階に於て半乾燥の状態に
あるうちに後述する被膜(3)が被着する外表面に第1
11薬および微粒の砂を吹付けて同面を微細な粒状凹凸
面(1)とし、この半乾燥物を完全乾燥して焼成するこ
とによって構成した手袋製造用型(2)である。
In addition, in the illustrated embodiment, during the mold manufacturing stage, while the mold is in a semi-dry state, the first layer is applied to the outer surface to which the coating (3) described later is applied.
This is a glove manufacturing mold (2) constructed by spraying chemical No. 11 and fine sand to make the same surface a fine granular uneven surface (1), and completely drying this semi-dried product and firing it.

また、本発明手袋製造用型(2)は当該型(2)の上記
外表面に軟質合成樹脂の被膜(3)をσ債法により被膜
して当該被膜(3)をゲル化する。
In addition, in the glove manufacturing mold (2) of the present invention, a soft synthetic resin coating (3) is coated on the outer surface of the mold (2) by the sigma bonding method, and the coating (3) is gelled.

然るのち、上記のゲル化した被膜(3)を手袋用型(2
)より反転して剥離し仕上加工を施して完成品(イ)を
得る等の用法に供するものである。
After that, the above gelled coating (3) was molded into a glove mold (2).
), then peeled off, and subjected to finishing processing to obtain the finished product (a).

本発明は斜上の如く製作工程中に於て半乾燥の状態にあ
る未完品の外表面に柚系および砂等粒子を吹付けて同面
を微細な粒Vの凹凸面とし然るのち完全に乾燥して焼成
することを要旨とするので、温雅さを視覚に与える微粒
子状凹凸を外表面に備えた](■品価値が高い手袋の実
施を可能とする著効かあるは勿論であるが、特に型の外
表面に設けた微粒子状凹凸は浸αを法の実施時には軟合
成樹脂、ゴム等の流下を抑え、重さの割には厚手窓があ
り、且つ屈曲性がよく更に所R1’llペタつきがない
特性を製品に享有せしめる機能を果す等の効果な葵する
ものである。
In the present invention, particles such as citron and sand are sprayed onto the outer surface of an unfinished product that is in a semi-dry state during the manufacturing process, such as the one shown on the slope, to make the same surface an uneven surface with fine grains V, and then the product is completely finished. Since the main purpose is to dry and fire the gloves, the outer surface is provided with fine particulate irregularities that give a sense of elegance to the eye. In particular, the particulate irregularities provided on the outer surface of the mold suppress the flow of soft synthetic resin, rubber, etc. during the immersion method, and it has a thick window for its weight, and has good flexibility, and is It is an effective material that has the function of making the product enjoy a non-sticky property.

【図面の簡単な説明】[Brief explanation of the drawing]

図は本発明手袋製造用型の実施例を示すものであって、
第1図は全体を示す一部拡太1#r tf+1付き正面
図、第2図は使用の一状態を示す一部拡大断面付正面囚
、第3図は本発明により得た完成品を示す一部拡大断面
付き正面図である。 (1)・・・凹凸面、(2)・・・手袋製造用型、(3
)・・・被膜、(イ)・・・完成品。 特 許 出 願 人 エステ−化学株式会社?y4s 
1図
The figure shows an embodiment of the glove manufacturing mold of the present invention,
Fig. 1 is a front view with a partially enlarged 1#r tf+1 showing the whole, Fig. 2 is a front view with a partially enlarged section showing one state of use, and Fig. 3 is a finished product obtained by the present invention. It is a front view with a partially enlarged cross section. (1)...Uneven surface, (2)...Glove manufacturing mold, (3
)...Coating, (a)...Finished product. Patent applicant: Esthe Chemical Co., Ltd.? y4s
Figure 1

Claims (1)

【特許請求の範囲】[Claims] 製作工程中に於て半乾燥の状態にある未完品の外表面に
釉薬および砂等粒子を吹付けて同面を微細な粒状の凹凸
面とし、然るのちに完全に乾燥して焼成することを特徴
とする手袋製造用型。
During the production process, particles such as glaze and sand are sprayed onto the outer surface of an unfinished product that is in a semi-dry state to create a fine granular uneven surface, which is then completely dried and fired. A glove manufacturing mold featuring:
JP57234759A 1982-12-29 1982-12-29 Mold for producing glove Pending JPS59124832A (en)