JPS5881954A - 耐摩耗性および自己潤滑性にすぐれた高強度鉄基焼結合金 - Google Patents
耐摩耗性および自己潤滑性にすぐれた高強度鉄基焼結合金Info
- Publication number
- JPS5881954A JPS5881954A JP17933081A JP17933081A JPS5881954A JP S5881954 A JPS5881954 A JP S5881954A JP 17933081 A JP17933081 A JP 17933081A JP 17933081 A JP17933081 A JP 17933081A JP S5881954 A JPS5881954 A JP S5881954A
- Authority
- JP
- Japan
- Prior art keywords
- self
- wear resistance
- high strength
- sintered alloy
- content
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Powder Metallurgy (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP17933081A JPS5881954A (ja) | 1981-11-09 | 1981-11-09 | 耐摩耗性および自己潤滑性にすぐれた高強度鉄基焼結合金 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP17933081A JPS5881954A (ja) | 1981-11-09 | 1981-11-09 | 耐摩耗性および自己潤滑性にすぐれた高強度鉄基焼結合金 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5881954A true JPS5881954A (ja) | 1983-05-17 |
JPS6133056B2 JPS6133056B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1986-07-31 |
Family
ID=16063947
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP17933081A Granted JPS5881954A (ja) | 1981-11-09 | 1981-11-09 | 耐摩耗性および自己潤滑性にすぐれた高強度鉄基焼結合金 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5881954A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6244556A (ja) * | 1985-08-21 | 1987-02-26 | Mitsubishi Metal Corp | 耐摩耗性およびなじみ性のすぐれた銅合金溶浸Fe基焼結材料 |
US4909843A (en) * | 1986-10-04 | 1990-03-20 | Etablissement Supervis | Highly wear-resistant iron-nickel-copper-molybdenum sintered alloy with addition of phosphorous |
JPH04124248A (ja) * | 1990-09-14 | 1992-04-24 | Isamu Kikuchi | 含油軸受用焼結合金およびその製造方法 |
JP2011085163A (ja) * | 2009-10-14 | 2011-04-28 | Porite Corp | 非含油性焼結歯車体 |
CN103639405A (zh) * | 2013-12-03 | 2014-03-19 | 江苏大学 | 一种金属基高温自润滑复合材料及其制备方法 |
CN104907554A (zh) * | 2014-03-12 | 2015-09-16 | 北京有色金属研究总院 | 一种粉末冶金用粉体材料及其制备方法与应用 |
CN108385029A (zh) * | 2018-01-17 | 2018-08-10 | 瑞安市迦勒汽车部件有限公司 | 一种一体化成型的汽车水泵同步带轮生产工艺 |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03122462U (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) * | 1990-03-26 | 1991-12-13 | ||
US20230038219A1 (en) | 2020-01-27 | 2023-02-09 | Mitsubishi Materials Corporation | Tin or tin alloy electroplating solution, method for forming bumps, and method for producing circuit board |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5141607A (ja) * | 1974-10-07 | 1976-04-08 | Sumitomo Electric Industries | Taimamoseijudozairyo |
JPS5419406A (en) * | 1977-07-15 | 1979-02-14 | Teikoku Piston Ring Co Ltd | Heattanddwear resistant sintered ferrous alloy for valve seat ring having good processability |
-
1981
- 1981-11-09 JP JP17933081A patent/JPS5881954A/ja active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5141607A (ja) * | 1974-10-07 | 1976-04-08 | Sumitomo Electric Industries | Taimamoseijudozairyo |
JPS5419406A (en) * | 1977-07-15 | 1979-02-14 | Teikoku Piston Ring Co Ltd | Heattanddwear resistant sintered ferrous alloy for valve seat ring having good processability |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6244556A (ja) * | 1985-08-21 | 1987-02-26 | Mitsubishi Metal Corp | 耐摩耗性およびなじみ性のすぐれた銅合金溶浸Fe基焼結材料 |
US4909843A (en) * | 1986-10-04 | 1990-03-20 | Etablissement Supervis | Highly wear-resistant iron-nickel-copper-molybdenum sintered alloy with addition of phosphorous |
JPH04124248A (ja) * | 1990-09-14 | 1992-04-24 | Isamu Kikuchi | 含油軸受用焼結合金およびその製造方法 |
JP2011085163A (ja) * | 2009-10-14 | 2011-04-28 | Porite Corp | 非含油性焼結歯車体 |
CN103639405A (zh) * | 2013-12-03 | 2014-03-19 | 江苏大学 | 一种金属基高温自润滑复合材料及其制备方法 |
CN104907554A (zh) * | 2014-03-12 | 2015-09-16 | 北京有色金属研究总院 | 一种粉末冶金用粉体材料及其制备方法与应用 |
CN108385029A (zh) * | 2018-01-17 | 2018-08-10 | 瑞安市迦勒汽车部件有限公司 | 一种一体化成型的汽车水泵同步带轮生产工艺 |
Also Published As
Publication number | Publication date |
---|---|
JPS6133056B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1986-07-31 |