JPS5858198A - ヘドロまたは汚泥の固化方法 - Google Patents
ヘドロまたは汚泥の固化方法Info
- Publication number
- JPS5858198A JPS5858198A JP56156417A JP15641781A JPS5858198A JP S5858198 A JPS5858198 A JP S5858198A JP 56156417 A JP56156417 A JP 56156417A JP 15641781 A JP15641781 A JP 15641781A JP S5858198 A JPS5858198 A JP S5858198A
- Authority
- JP
- Japan
- Prior art keywords
- sludge
- alkali metal
- blast furnace
- hydroxide
- granulated slag
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Treatment Of Sludge (AREA)
- Processing Of Solid Wastes (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56156417A JPS5858198A (ja) | 1981-10-01 | 1981-10-01 | ヘドロまたは汚泥の固化方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56156417A JPS5858198A (ja) | 1981-10-01 | 1981-10-01 | ヘドロまたは汚泥の固化方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5858198A true JPS5858198A (ja) | 1983-04-06 |
| JPH0124559B2 JPH0124559B2 (cg-RX-API-DMAC7.html) | 1989-05-12 |
Family
ID=15627292
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56156417A Granted JPS5858198A (ja) | 1981-10-01 | 1981-10-01 | ヘドロまたは汚泥の固化方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5858198A (cg-RX-API-DMAC7.html) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100436396B1 (ko) * | 2002-01-29 | 2004-06-16 | 주식회사 포스코건설 | 유기성슬러지의 고형화, 안정화를 통한 자원화 방법 및이를 위한 장치 |
| WO2005039702A1 (en) * | 2003-10-28 | 2005-05-06 | Nanyang Technological University | A method and composition for stabilizing waste mercury compounds using ladle furnace slag |
-
1981
- 1981-10-01 JP JP56156417A patent/JPS5858198A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR100436396B1 (ko) * | 2002-01-29 | 2004-06-16 | 주식회사 포스코건설 | 유기성슬러지의 고형화, 안정화를 통한 자원화 방법 및이를 위한 장치 |
| WO2005039702A1 (en) * | 2003-10-28 | 2005-05-06 | Nanyang Technological University | A method and composition for stabilizing waste mercury compounds using ladle furnace slag |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0124559B2 (cg-RX-API-DMAC7.html) | 1989-05-12 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP6137850B2 (ja) | 水硬性組成物 | |
| JP5946107B2 (ja) | セメント組成物の製造方法 | |
| Chindaprasirt et al. | Characterizations of FBC/PCC fly ash geopolymeric composites | |
| JP5800387B2 (ja) | 土質改良材 | |
| Zhang et al. | Preparation and hydration process of copper slag-granulated blast furnace slag-cement composites | |
| JPS63289498A (ja) | 放射性廃棄物の固化剤 | |
| JP5874695B2 (ja) | 重金属類を含有する固形廃棄物の無害化方法 | |
| KR102306318B1 (ko) | 연약지반용 고화제 조성물 및 그 제조방법 | |
| JP2004315303A (ja) | セメント組成物、コーティング材料、及びそれを用いた遮塩方法 | |
| KR101937772B1 (ko) | 알칼리 자극제를 활용한 친환경 고성능 콘크리트 조성물 | |
| JPH0337145A (ja) | セメント用急結剤 | |
| JP6957922B2 (ja) | 石炭灰硬化物 | |
| JP6292257B2 (ja) | 脱硫スラグを用いた水和固化体 | |
| JPS6336840B2 (cg-RX-API-DMAC7.html) | ||
| JP2009227549A (ja) | セメント添加材及びセメント組成物 | |
| JPS5858198A (ja) | ヘドロまたは汚泥の固化方法 | |
| JPH10165920A (ja) | 泥状物の団粒化剤、それを用いた固化剤 | |
| JPH0214308B2 (cg-RX-API-DMAC7.html) | ||
| GB2077251A (en) | Slag Cement Composition | |
| JP2004352596A (ja) | 水硬性材料の製造方法および水硬性建築材料 | |
| JP2006143990A (ja) | 固化材 | |
| JP2018203583A (ja) | 石炭灰組成物 | |
| JP2008029937A (ja) | 副生物の処理方法 | |
| JP2503235B2 (ja) | 硬化促進材 | |
| JP3549635B2 (ja) | 混合セメントの刺激材及び混合セメント組成物 |