JPS5847978Y2 - Roll with uneven pattern on wall surface - Google Patents
Roll with uneven pattern on wall surfaceInfo
- Publication number
- JPS5847978Y2 JPS5847978Y2 JP4991379U JP4991379U JPS5847978Y2 JP S5847978 Y2 JPS5847978 Y2 JP S5847978Y2 JP 4991379 U JP4991379 U JP 4991379U JP 4991379 U JP4991379 U JP 4991379U JP S5847978 Y2 JPS5847978 Y2 JP S5847978Y2
- Authority
- JP
- Japan
- Prior art keywords
- roll
- uneven pattern
- wall surface
- naps
- pattern
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【考案の詳細な説明】
従来から壁面に塗材を塗り付けた直後に、凹凸模様を表
面に形成した連通気泡性のポリウレタンスポンジ又は部
分アセタール化ポリビニールアルコールスポンジを局面
に貼着したロールを転圧し、塗材表面に凹凸模様をつげ
る施工法がある。[Detailed explanation of the invention] Conventionally, immediately after applying a coating material to a wall surface, a roll with an open-cell polyurethane sponge or partially acetalized polyvinyl alcohol sponge pasted on the surface with an uneven pattern formed on the surface is rolled. There is a construction method that involves pressing and creating an uneven pattern on the surface of the coating material.
しかしこれらのロールは何れも高価であるにかかわらず
、部分アセタール化ポリビニールアルコールスポンジロ
ールは使用に際して予め水で膨潤軟化させておかねばな
らず、しかも吸水膨潤と乾繰収縮を繰り返しているうち
に次第に変形し、ロールの直径が部分的に狂い塗材面に
均一な接触をしなくなったり、模様が変形する等の欠点
があった。However, although all of these rolls are expensive, partially acetalized polyvinyl alcohol sponge rolls must be swollen and softened with water before use, and moreover, as they repeatedly absorb water, swell and shrink, they dry out and shrink. There were drawbacks such as the roll becoming gradually deformed, the diameter of the roll being partially out of alignment and not making uniform contact with the surface of the coating material, and the pattern being deformed.
またこれらの凹凸模様付ロールは塗材液を含み易い点が
長所ではあるが、スポンジのセルを大きく、且連続的に
しなげればならないため気孔を構成する殻が薄く、ある
いは細くなり易く、その結果耐久性が低下し、特にポリ
ウレタンスポンジロールはその傾向が大ぎい。The advantage of these textured rolls is that they easily contain the coating liquid, but because the sponge cells have to be made large and continuous, the shells that make up the pores tend to become thin or thin. As a result, durability decreases, and this tendency is particularly severe for polyurethane sponge rolls.
本考案はこれらのスポンジを構成する材料より遥かに強
靭な繊維を用い、同繊維の立毛部分と立毛欠除部とによ
り凹凸模様を形成し、安価で耐久性に富み、かつ液含み
の良い凹凸型付はロールを容易かつ安価に製作し得るよ
うにしたものであり、以下実施例を添付図面について説
明する。The present invention uses fibers that are much stronger than the materials that make up these sponges, and forms an uneven pattern with the raised portions and missing portions of the same fibers, making it inexpensive, durable, and highly absorbent. The molding method allows rolls to be manufactured easily and inexpensively, and examples will be described below with reference to the accompanying drawings.
比較的腰の強い立毛2を密生させた基布3をロール基体
1の周面に捲装貼着し、立毛2の所要部分を欠除した立
毛欠除部4と立毛2とにより凹凸模様を形成する。A base fabric 3 in which relatively stiff naps 2 are densely grown is wound and adhered to the circumferential surface of the roll base 1, and an uneven pattern is created by the naps 2 and the naps 2 and the naps 2. Form.
上記立毛2はナイロン、アクセル、ポリエチレン、ポリ
プロピレン、ポリ塩化ビニールのような熱可塑性合成樹
脂の繊維、細いテープ、獣毛、植物性繊維等任意の繊維
の立毛又はループを密生させたもの、植毛布等を利用す
ることができ、立毛欠除部4は、熱或いは化学的方法に
よる溶融圧着、電気植毛、或いは機械的切断によるほか
、織成による凹凸織模様布を利用することができる。The nap 2 mentioned above is a fiber of thermoplastic synthetic resin such as nylon, accelerator, polyethylene, polypropylene, or polyvinyl chloride, thin tape, animal hair, vegetable fiber, etc. made of dense nap or loops of any fiber, or flocked cloth. The raised raised portion 4 can be formed by melt-pressing using heat or chemical methods, electro-flocking, mechanical cutting, or by weaving an uneven woven pattern cloth.
又欠除部4の形成はロール基体1への捲装前、又は捲装
後の伺れでも良い。Further, the cutout portion 4 may be formed before or after winding onto the roll base 1.
尚図中5は−・ンドル、6は支軸である。In the figure, 5 is a handle, and 6 is a support shaft.
本考案は上記のように凹凸模様が立毛繊維と立毛繊維の
欠除部により形成され、繊維の性質、太さ、長さ等によ
り硬軟は自由に調節することができ、吸収性も立毛繊維
の密度により調整し得るので塗装材料、模様に応じ最適
の硬さの凹凸模様を有する型付ロールを簡単安価に製作
することができ、使用後の洗滌も容易に行える効果があ
る。In this invention, as mentioned above, the uneven pattern is formed by the napped fibers and the missing parts of the napped fibers, and the hardness and softness can be freely adjusted depending on the fiber properties, thickness, length, etc., and the absorbency is also the same as the napped fibers. Since the density can be adjusted, it is possible to easily and inexpensively produce a molded roll having an uneven pattern with the optimum hardness depending on the coating material and pattern, and it also has the effect of being easy to wash after use.
図面は本考案の実施例を示すもので、第1図は正面図、
第2図は縦断側面図である。
1・・・・・・ロール基体、2・・・・・・立毛、3・
・・・・基布、4・・・・・・立毛欠除部。The drawings show an embodiment of the present invention, and FIG. 1 is a front view;
FIG. 2 is a longitudinal side view. 1... Roll base, 2... Napped, 3.
...Foundation fabric, 4...Fleece missing part.
Claims (1)
ール基体の周面に捲装貼着してなる壁面の凹凸模様型付
ロール。A roll with an uneven pattern on the wall surface, which is formed by winding and pasting a base fabric having an uneven pattern formed by raised naps and missing raised parts around the circumferential surface of a roll base.