JPS5847535A - Recessed mark working of welded pipe material - Google Patents

Recessed mark working of welded pipe material

Info

Publication number
JPS5847535A
JPS5847535A JP14809581A JP14809581A JPS5847535A JP S5847535 A JPS5847535 A JP S5847535A JP 14809581 A JP14809581 A JP 14809581A JP 14809581 A JP14809581 A JP 14809581A JP S5847535 A JPS5847535 A JP S5847535A
Authority
JP
Japan
Prior art keywords
band plate
welded pipe
pipe
cylindrical roll
roll
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP14809581A
Other languages
Japanese (ja)
Inventor
Yasushi Teramoto
寺本 靖
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SANKO KUKI SOCHI KK
Teijin Engineering Ltd
Original Assignee
SANKO KUKI SOCHI KK
Teijin Engineering Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SANKO KUKI SOCHI KK, Teijin Engineering Ltd filed Critical SANKO KUKI SOCHI KK
Priority to JP14809581A priority Critical patent/JPS5847535A/en
Publication of JPS5847535A publication Critical patent/JPS5847535A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To manufacture a transport pipe of a desired diameter which has executed recessed mark working to its inside surface, by making a welded pipe manufacturing band plate press-contact in advance with a roll having a linear or dot-like projecting pattern, making it pass through, giving a desired pressed mark to one side, and after that, executing its forming. CONSTITUTION:A band plate 4 for manufacturing a welded pipe is made to pass through under necessary pressing force between a cylindrical roll 1 having a linear or dot-like projecting pattern 2 on its outside circumferential surface, and a cylindrical roll 3 whose outside circumferential surface is smooth, and a band plate 5 which has carved the projecting pattern 2 of the cylindrical roll 1 on one surface of the band plate 4 is obtained. This band plate 5 is formed to a pipe which has set the recessed mark side to its inside, by which it is possible to obtain a transport pipe which has executed recessed mark working to its inside surface so as to be used for air transport of a pulverulent and/or granular body.

Description

【発明の詳細な説明】 本発明は粉粒体“の空気輸送に使世する凹痕加工を内面
に施した輸送管の製作方法に関するものである。
DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a method of manufacturing a transport pipe whose inner surface is provided with concave markings useful for pneumatic transport of powder and granular materials.

粉粒体、特にd成樹脂のベレット等を空気輸送する場合
、輸送管内壁との磨擦で被輸送物の表面が溶融し、フイ
A/A状のフラッフが生成されることは広く知られると
ころである。またこれの発生−防止策として輸送管内壁
面を粗くし、あるいは凹凸を作り、または条痕状の加工
を施すことも又周知である。
It is widely known that when powder and granular materials, especially pellets of d-plastic resin, are transported by air, the surface of the transported material melts due to friction with the inner wall of the transport pipe, and fluff in the form of A/A is generated. be. It is also well known that as a measure to prevent this from occurring, the inner wall surface of the transport pipe is made rough, has irregularities, or is processed in the form of striations.

しかして、その加工方法としては、−ンドブラストによ
って管内壁面を梨地にするもの、あるいけ管内にローレ
ットのごときを通過せしめて圧痕を陰刻するなどが杖表
例である。
Examples of processing methods include making the inner wall surface of the tube a satin finish by sandblasting, and passing a knurling or the like through a knurling tube to create indentations.

しかるにこれらの方法はいずれも管に成形されのちに加
工されるため、管径毎に加、工具を備えなければならぬ
煩雑さがある。
However, in all of these methods, the tube is formed and then processed, so it is complicated to prepare tools for each diameter of the tube.

またサンドプラス、ト法によるものは、フィルム状のフ
ラッフの発生は抑制される代り粉状物の発生が増加し、
また耐用台数が短く、数年毎の再加工を必要4とするな
どの欠点があシ、ローーツートのごときを使用する加工
方法においては、管、内壁に所望深さの凹痕を与えるた
めには相当強力な圧着生し、その修整に困難する場合も
出て来る。
In addition, when using the Sand Plus and To methods, the generation of film-like fluff is suppressed, but the generation of powdery substances increases.
In addition, there are disadvantages such as short service life and the need for reprocessing every few years, and machining methods that use a low tool are difficult to make indentations of the desired depth on the pipe and inner wall. There are cases where the crimping is quite strong and it is difficult to repair it.

本発明は、以上に述べた不都合を解消する目的をもらで
、輸送管に使用す2る溶接管の製造工程において管に成
形する前の素材の段階における帯板着し通過させて、該
帯板の一側面に所望の圧痕を連続して与え、しかるのち
これを成形して内壁面に凹痕をもつ溶接管に仕上げるの
である。
The present invention aims to eliminate the above-mentioned disadvantages, and in the manufacturing process of two welded pipes used for transport pipes, the material is attached to a strip at the stage of the material before being formed into a pipe, and the strip is passed through. Desired indentations are continuously made on one side of the plate, which is then formed into a welded pipe with concave indentations on the inner wall surface.

本発明の実施例を図面によって説明すると、第1図は、
帯板4の片面に凹痕加工を施すロール装置の斜視跨明図
である。
An embodiment of the present invention will be described with reference to the drawings. FIG. 1 shows the following:
FIG. 3 is a perspective straddle view of a roll device that applies concave marks to one side of a strip 4. FIG.

ターン)のエツジ2が陽刻されており、該エツジ2を含
むエツジロール1の円周表面は繰り返される圧痕加工に
耐えるように、゛焼入等によって充分の硬度が与えられ
ている。、受口−/L’8の円周面は平滑であり特に硬
度は必要としない。エツジロール1および受ローtv8
Fi帯板4を挾んで所要の押圧力に耐える強度を持って
軸支さhている。
The edge 2 of the turn is engraved, and the circumferential surface of the edge roll 1 including the edge 2 is given sufficient hardness by hardening or the like so as to withstand repeated indentations. , the circumferential surface of the socket -/L'8 is smooth and does not require particular hardness. Edgeroll 1 and Ukero tv8
It is pivotally supported with the strength to withstand the required pressing force by sandwiching the Fi band plate 4.

両口−μに挾まれ所望の押圧力を加えられた帯板4は、
図示しない牽引装置によってローμ軸に直角方向に進行
し、進行に従ってエツジ口、j/l/ 1および受ロー
ル8は回転し、該ロールの圧着部をターン)が凹痕とし
て陰刻される。
The strip plate 4, which is held between both ends -μ and a desired pressing force is applied,
It travels in a direction perpendicular to the low μ axis by a traction device (not shown), and as it advances, the edge opening, j/l/1, and receiving roll 8 rotate, and the crimped portion of the roll (turn) is inscribed as a concave mark.

第2図は、エツジローlL/1のエツジ2によって凹瘍
5が陰刻される状態を説明する側断面部分図であり、第
8図は同じく正面部分図である。
FIG. 2 is a partial side cross-sectional view illustrating the state in which the recess 5 is inscribed by the edge 2 of the edge roller IL/1, and FIG. 8 is a partial front view.

また第4図は、帯板4に陰刻された凹痕5の模様(パタ
ーン)の−例を示す平面部分図であ・る。
FIG. 4 is a partial plan view showing an example of a pattern of concave marks 5 intaglio-engraved on the band plate 4. As shown in FIG.

このようにして−側面に凹痕加工を施された帯゛板4V
i以後凹痕加ニーを内壁面とし・て通常の溶接管の成形
工程が行われる。
In this way - band plate 4V with concave markings on the side surface
After i, a normal welded pipe forming process is performed using the concave knee as the inner wall surface.

以上のようにして加工される本発明の一痕加工は、従来
の加工方法に比べて次の利点がある。
The single-mark machining of the present invention performed as described above has the following advantages over conventional machining methods.

第1K所要最大径用帯板が加工できるロール設備があれ
ば各種経用帯板′が加工できるので、従来方法のように
各管径毎に加工器具を揃える必要がなく経済的である。
If there is roll equipment capable of processing the 1K required maximum diameter strip, it is possible to process various warp strips, so it is economical as there is no need to prepare processing tools for each pipe diameter as in the conventional method.

またとの凹痕加工の工程は、帯板を所要中に裁断する工
程に含まれて同時に行うことができるので、従来の管の
製作工程が本発明の実施によって増加することけない。
Since the step of forming the concave marks can be carried out simultaneously with the step of cutting the strip as required, the conventional pipe manufacturing steps will not be increased by implementing the present invention.

第2に加工される凹痕の深さと模様(パターン)゛こと
かで・きることである。従来方法では凹痕の深さくある
・いけ強さ)にもまたその模様にも選択の巾が狭かった
が、本発明の方法では必要に応じた選択ができて凹痕加
工の効果を大きく向上させることかできる。
Secondly, it is possible to determine the depth and pattern of the concave marks to be processed. In the conventional method, there was a narrow range of choices regarding the depth and strength of the dents and the pattern, but with the method of the present invention, selections can be made according to needs, greatly improving the effectiveness of dent processing. I can do it.

第8に、凹痕加工で万一帯板が変形したり歪を起1.て
も、管に球形する前であるのでその修整は容易であり、
正確な形状の管を作ることができる。
Eighth, in the unlikely event that the strip plate is deformed or distorted due to the machining of the concave marks, 1. However, since it has not yet become a spherical shape, it is easy to correct it.
Can create tubes with precise shapes.

【図面の簡単な説明】[Brief explanation of drawings]

第1゛図は本発明実施例の凹痕加工用50−ル装置の斜
視説明図であり、第2図は凹痕陰刻の状態を説明する側
断面部分図、第8図は第2図の正面部分図である。また
第4図は凹痕の模様の一例を示す平面部分図である。 1・・・エツジロール。2・・・エツジ。8・・・受け
ロール。4・・・帯板。6・・・凹痕。 特   許   出   願   人 三興空気装置株式会社 代表取締役 森 山 有 恒 手続補正書(自発) 昭和57年2月/7 日 特許庁長官 島田春樹 殿 11事件の表示 昭和56年特許願第148095号 2、発明の名称 溶接管材の凹痕加工 3、補正をする者 4、補正の対象 l、第4頁第、7行の次に下記の記述を挿入。 [第5図は第4図と異った模様(パターン)を示す平面
部分図であり、この場合はロールを複数回通過させて施
工する。」 2、第5頁15行の次に下記の記述を挿入[また第5図
はロールら複数回通過させて得た凹痕の模様の一例を示
す部分図である。 3、別紙図面(第5図)追加。 1115図
FIG. 1 is a perspective explanatory view of a 50-hole device for machining concave marks according to an embodiment of the present invention, FIG. FIG. Further, FIG. 4 is a partial plan view showing an example of a pattern of concave marks. 1... Etsujirol. 2...Etsuji. 8...Receive roll. 4...Strip plate. 6... Concave marks. Patent application Hitoshi Sanko Air Equipment Co., Ltd. CEO Yu Moriyama Procedural amendment (spontaneous) February 7, 1980 Commissioner of the Patent Office Haruki Shimada Indication of case 11 Patent application No. 148095 2 of 1982 , Title of the invention: Machining of concave marks on welded pipe material 3, Person making the correction 4, Subject of correction 1, Page 4, page 4, next to line 7, insert the following description. [FIG. 5 is a partial plan view showing a pattern different from that in FIG. 4, and in this case, the work is performed by passing the roll multiple times. 2. Insert the following description next to line 15 on page 5 [FIG. 5 is a partial view showing an example of the pattern of concave marks obtained by passing the roll several times. 3. Added attached drawing (Figure 5). Figure 1115

Claims (1)

【特許請求の範囲】[Claims] 溶接管製作用の帯板を、外周面に線状または点状の凸起
模様をもつ円柱形ロールと外周面が平滑な円柱形ロール
の間を所要の押圧力のもとに通過させて、該帯板の片面
に円柱形ロールの凸起模様を陰刻した凹痕を施し、しか
るのち前記帯板を凹痕側を内側として管に成形すること
を特1徴とする溶接管材の凹痕加工。
A strip plate for welded pipe production is passed between a cylindrical roll having a linear or dotted convex pattern on its outer circumferential surface and a cylindrical roll having a smooth outer circumferential surface under the required pressing force, Indentation processing of a welded pipe material, characterized in that one side of the strip is provided with indentations in which a convex pattern of a cylindrical roll is inscribed, and then the strip is formed into a tube with the indentation side facing inside. .
JP14809581A 1981-09-18 1981-09-18 Recessed mark working of welded pipe material Pending JPS5847535A (en)