JPS5831134U - コルク粒と合成樹脂接着剤とより成る弾性成形物 - Google Patents
コルク粒と合成樹脂接着剤とより成る弾性成形物Info
- Publication number
- JPS5831134U JPS5831134U JP12563181U JP12563181U JPS5831134U JP S5831134 U JPS5831134 U JP S5831134U JP 12563181 U JP12563181 U JP 12563181U JP 12563181 U JP12563181 U JP 12563181U JP S5831134 U JPS5831134 U JP S5831134U
- Authority
- JP
- Japan
- Prior art keywords
- synthetic resin
- resin adhesive
- cork
- cork grains
- molded product
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
第1図は本考案弾性成形物の外面を示す説明図である。
Claims (2)
- (1)コルク粒群と、硬化剤を含む常温硬化性接着剤と
を1:0.5乃至1:1.2の割合で混合したものを室
温に於て容積が約173〜176程度になるまで加圧圧
縮硬化したものを室温で5日乃至7日間養生することに
より得られる弾性体で、少なくともコルクが全体に占め
る割合が約75%以上で、且つ引張り強度が14kg/
cffl〜19に9−/cIft1伸び率15糎〜30
%、引裂強度5に9f/cm〜7kgf/cmであるこ
とを特徴とするコルク粒と合成樹脂接着剤とより成る弾
性成形物。 - (2)成形物を薄板状にスライスして成る実用新案登録
請求の範囲第(1)項記載のコルク粒と合成樹脂接着剤
とより成る弾性成形物。