JPS5822169A - Method of correcting warp of melamine decorative board - Google Patents
Method of correcting warp of melamine decorative boardInfo
- Publication number
- JPS5822169A JPS5822169A JP56120955A JP12095581A JPS5822169A JP S5822169 A JPS5822169 A JP S5822169A JP 56120955 A JP56120955 A JP 56120955A JP 12095581 A JP12095581 A JP 12095581A JP S5822169 A JPS5822169 A JP S5822169A
- Authority
- JP
- Japan
- Prior art keywords
- decorative board
- melamine decorative
- melamine
- correcting warp
- correcting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
【発明の詳細な説明】
本発明は洗面化粧台等のポストフオーム用メラミン化粧
板の反り矯正方法に関し、芯材への貼り合わせ、曲げ加
工時に生ずる不良を々〈すことを目的とする。DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a method for correcting warpage of melamine decorative boards for post-forms such as bathroom vanities, and an object of the present invention is to eliminate defects that occur during bonding to a core material and during bending.
一般に化粧板に反りが発止すると芯材への貼り合わせ時
に化粧板の割れ等の不良が発生することが知られている
。特に自動貼り合わせの場合、化粧板を吸盤で吸着し、
て芯材のある場所へ移動するか、吸盤でうまく吸着し々
い、コンベアテ移動の際方向が変わる、乾燥炉にひっか
かる等の不都合廃があった。又、手貼りの場合でも貼り
合わせの位d決めがしにくいという欠点があった。更に
曲は加工時にも化粧板の反りによって化粧板とヒーター
との距離が変わり加熱過多、不足が生じ易く温度コント
ロールが難しいという欠点を有していた。It is generally known that if a decorative board begins to warp, defects such as cracking of the decorative board will occur when it is bonded to a core material. Especially in the case of automatic lamination, the decorative board is adsorbed with a suction cup,
There were inconvenient wastes, such as the core material being moved to a place with the core material, the suction cup not adsorbing properly, the direction changing when moving on the conveyor belt, and getting caught in the drying oven. Furthermore, even when pasting is done by hand, it is difficult to determine the position of pasting. Moreover, during processing, the warping of the decorative board changes the distance between the decorative board and the heater, which tends to cause overheating or underheating, making it difficult to control the temperature.
本発明は軟土の如き実情KI!みて為されたものである
。以下実施例として示した図面に基づき本発明を詳述す
る。The present invention is a reality like soft soil! It was done by looking at it. The present invention will be described in detail below based on the drawings shown as examples.
図はメラミン化粧板の反り矯正装置を示し、榛数枚のメ
ラミン化粧板3け積層して定盤4上に載置され、ヒータ
一部2によりその表面(プレス面)が100℃前後に加
熱されたプレス装置1 hcよりメラミン化粧板3は熱
圧保持されている。The figure shows a warpage correction device for melamine decorative boards. Three melamine decorative boards are laminated and placed on a surface plate 4, and the surface (pressed surface) is heated to around 100°C by the heater part 2. The melamine decorative board 3 is held under heat and pressure by the press device 1 hc.
ヒータ一部2dプレス装に1に熱板を取イ」けて形成し
たものであってもよい。A part of the heater may be formed by attaching a hot plate to a 2D press equipment.
プレス面を100℃前後にしているのは、それ以下では
反りの矯正効果が少なく、それ以上で−1を又メラミン
化粧板か灰地、L、てしま込、後の曲げ加工に影醤を与
えるか7らである。このように100℃前後で熱圧保持
することが本発明の1つの特長と々っ−Cいる。The reason why the press surface is kept at around 100℃ is that if it is lower than that, there is little effect of correcting the warpage, and if it is higher than that, it will be -1 again, and if it is melamine decorative board or gray board, L, teshimakomi, it will affect the bending process later. It's 70 to give. One of the features of the present invention is that it is maintained under heat and pressure at around 100°C.
以上のようにメラミン化粧板を定盤上に複数枚kl!j
i截+dt L、、、プレス面を100℃前後に加熱し
たプレス装置により熱圧保持させて成るのでメラミン化
粧板の反りがなくなり、化粧板の貼り合わせ、曲は加工
が容易になるという特長を有する。As shown above, put multiple melamine decorative boards on the surface plate! j
i cutting + dt L,,,The pressed surface is held under heat and pressure using a press device heated to around 100℃, which eliminates warping of the melamine decorative board, and makes it easy to bond and curve the decorative board. have
しIはメラミン化粧板の反り矯正装置を示す概略図であ
る。
1・・・プレス装置 2・・・ヒータ一部 3・・・メ
ラミン化粧板 4・・・定盤。
特許量−人
松下電工株式会社1 is a schematic diagram showing a warpage correction device for melamine decorative board. 1...Press device 2...Part of the heater 3...Melamine decorative board 4...Surface plate. Patent amount - Matsushita Electric Works Co., Ltd.
Claims (1)
’L/ス面を100℃前後に加熱したプレス装置により
熱圧保持させて成るメラミン化粧板の反り矯正方法。(Place multiple sheets of 11 melamine decorative boards on a surface plate,
A method for straightening the warpage of a melamine decorative board by holding the L/S surface under heat and pressure using a press device heated to around 100°C.