JPS5820730A - 強磁性鉱石粉の製造法 - Google Patents
強磁性鉱石粉の製造法Info
- Publication number
- JPS5820730A JPS5820730A JP56111566A JP11156681A JPS5820730A JP S5820730 A JPS5820730 A JP S5820730A JP 56111566 A JP56111566 A JP 56111566A JP 11156681 A JP11156681 A JP 11156681A JP S5820730 A JPS5820730 A JP S5820730A
- Authority
- JP
- Japan
- Prior art keywords
- particle size
- magnetic
- powder
- ore
- iron oxide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Compounds Of Iron (AREA)
- Hard Magnetic Materials (AREA)
- Soft Magnetic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56111566A JPS5820730A (ja) | 1981-07-18 | 1981-07-18 | 強磁性鉱石粉の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56111566A JPS5820730A (ja) | 1981-07-18 | 1981-07-18 | 強磁性鉱石粉の製造法 |
Related Child Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP60007036A Division JPS60171224A (ja) | 1985-01-18 | 1985-01-18 | 強磁性酸化鉄 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5820730A true JPS5820730A (ja) | 1983-02-07 |
| JPH024536B2 JPH024536B2 (enrdf_load_stackoverflow) | 1990-01-29 |
Family
ID=14564618
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56111566A Granted JPS5820730A (ja) | 1981-07-18 | 1981-07-18 | 強磁性鉱石粉の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5820730A (enrdf_load_stackoverflow) |
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE3536735A1 (de) * | 1984-10-16 | 1986-05-07 | Sumitomo Metal Industries, Ltd., Osaka | Verfahren zur herstellung von feinteiligem eisenoxidpulver |
| JPS61215220A (ja) * | 1985-03-19 | 1986-09-25 | Tetsugen:Kk | 鉄鉱石からのフエライト原料用酸化鉄の製造方法 |
| JPS62138331A (ja) * | 1985-12-13 | 1987-06-22 | Tetsugen:Kk | 鉄鉱石からのフエライト原料用酸化鉄の製造方法 |
| JPS62138332A (ja) * | 1985-12-13 | 1987-06-22 | Tetsugen:Kk | 鉄鉱石からのフエライト原料用酸化鉄の製造方法 |
| US5061412A (en) * | 1989-03-31 | 1991-10-29 | Sumitomo Special Metal Co. Ltd. | Process for producing a magnet of strontium ferrite having high performance |
| JP2017154925A (ja) * | 2016-03-01 | 2017-09-07 | 太平洋セメント株式会社 | アルカリ土類金属窒化物粒子の製造法 |
-
1981
- 1981-07-18 JP JP56111566A patent/JPS5820730A/ja active Granted
Cited By (7)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE3536735A1 (de) * | 1984-10-16 | 1986-05-07 | Sumitomo Metal Industries, Ltd., Osaka | Verfahren zur herstellung von feinteiligem eisenoxidpulver |
| DE3536735C2 (de) * | 1984-10-16 | 1987-05-07 | Sumitomo Metal Industries, Ltd., Osaka | Verfahren zur Herstellung von feinteiligem Eisenoxidpulver |
| JPS61215220A (ja) * | 1985-03-19 | 1986-09-25 | Tetsugen:Kk | 鉄鉱石からのフエライト原料用酸化鉄の製造方法 |
| JPS62138331A (ja) * | 1985-12-13 | 1987-06-22 | Tetsugen:Kk | 鉄鉱石からのフエライト原料用酸化鉄の製造方法 |
| JPS62138332A (ja) * | 1985-12-13 | 1987-06-22 | Tetsugen:Kk | 鉄鉱石からのフエライト原料用酸化鉄の製造方法 |
| US5061412A (en) * | 1989-03-31 | 1991-10-29 | Sumitomo Special Metal Co. Ltd. | Process for producing a magnet of strontium ferrite having high performance |
| JP2017154925A (ja) * | 2016-03-01 | 2017-09-07 | 太平洋セメント株式会社 | アルカリ土類金属窒化物粒子の製造法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH024536B2 (enrdf_load_stackoverflow) | 1990-01-29 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Kaczmarek et al. | Preparation of Fe/sub 3/O/sub 4/and/spl gamma/-Fe/sub 2/O/sub 3/powders by magnetomechanical activation of hematite | |
| US4067953A (en) | Process for upgrading ores containing baddeleyite | |
| JPWO2006075763A1 (ja) | 単結晶質ダイヤモンド微粉及びその製造方法 | |
| JPS5820730A (ja) | 強磁性鉱石粉の製造法 | |
| EP0502612B1 (en) | High-purity iron oxide, and method for production thereof | |
| CN116832949A (zh) | 一种基于分级磁选工艺综合回收铁锂云母的方法 | |
| Ibrahim et al. | Dry magnetic separation of nepheline syenite ores | |
| US5496526A (en) | Production of intermediate grade manganese concentrate from low grade manganiferous ores | |
| Hallbauer, DK & Joughin | The size distribution and morphology of gold particles in Witwatersrand reefs and their crushed products | |
| JPH01294801A (ja) | 扁平状Fe−Ni系合金微粉末の製造方法 | |
| KR100334295B1 (ko) | 고령토에 함유된 산화철과 이산화티탄 제거를 위한 건식정제 방법 | |
| JPS60171224A (ja) | 強磁性酸化鉄 | |
| Tang et al. | Polycrystalline Nd2Fe14B/α-Fe nanocomposite flakes with a sub-micro/nanometre thickness prepared by surfactant-assisted high-energy ball milling | |
| Bajorek et al. | Synthesis of nanostructured Ho (Ni0. 5Fe0. 5) 3 compound via ball-milling | |
| JPH01294802A (ja) | 扁平状Fe−Si−Al系合金微粉末の製造方法 | |
| JPH10506365A (ja) | 活性ボール・ミリングを使用した金属酸化物粉体の作成 | |
| JPH09253517A (ja) | 粉末粒子の粉砕方法と粒子修飾方法 | |
| CN111836909B (zh) | 锰原料的制造方法及含锰钢的熔炼方法 | |
| Adi et al. | Nanomagnetite Extraction from Iron Sand Prepared by Mechanical Alloying Method | |
| Sitek et al. | On the preparation of precursors and carriers of nanoparticles by water jet technology | |
| Van Weert et al. | Selective pressure leaching of zinc and manganese from natural and man-made spinels using nitric acid | |
| Jalil et al. | Natural magnetite characterization from beach sand prepared by using planetary ball milling | |
| Kwon | Anisotropy and magnetic properties of Nd/sub 16/Fe/sub 76/B/sub 8/and Nd/sub 16/Fe/sub 75.3/B/sub 8/Zr/sub 0.1/HDDR materials | |
| Fitriana et al. | Structural modification of strontium hexaferrite through destruction process and ionic substitution | |
| JPS61215220A (ja) | 鉄鉱石からのフエライト原料用酸化鉄の製造方法 |