JPS58180245A - コンクリ−ト等の静的破砕方法および膨張錠剤 - Google Patents
コンクリ−ト等の静的破砕方法および膨張錠剤Info
- Publication number
- JPS58180245A JPS58180245A JP6200782A JP6200782A JPS58180245A JP S58180245 A JPS58180245 A JP S58180245A JP 6200782 A JP6200782 A JP 6200782A JP 6200782 A JP6200782 A JP 6200782A JP S58180245 A JPS58180245 A JP S58180245A
- Authority
- JP
- Japan
- Prior art keywords
- crushing
- agent
- concrete
- hole
- static
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Disintegrating Or Milling (AREA)
- Piles And Underground Anchors (AREA)
- Working Measures On Existing Buildindgs (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6200782A JPS58180245A (ja) | 1982-04-14 | 1982-04-14 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6200782A JPS58180245A (ja) | 1982-04-14 | 1982-04-14 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS58180245A true JPS58180245A (ja) | 1983-10-21 |
JPH0148059B2 JPH0148059B2 (enrdf_load_stackoverflow) | 1989-10-17 |
Family
ID=13187662
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6200782A Granted JPS58180245A (ja) | 1982-04-14 | 1982-04-14 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS58180245A (enrdf_load_stackoverflow) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5945379A (ja) * | 1982-09-07 | 1984-03-14 | Denki Kagaku Kogyo Kk | 破砕剤及びそれを用いた破砕工法 |
JPS6013172A (ja) * | 1983-07-04 | 1985-01-23 | 旭化成株式会社 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
JPS62195074A (ja) * | 1986-02-21 | 1987-08-27 | Ube Ind Ltd | 静的破砕剤およびその製造方法 |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS4943416A (enrdf_load_stackoverflow) * | 1972-08-31 | 1974-04-24 | ||
JPS5667059A (en) * | 1979-11-01 | 1981-06-05 | Onoda Cement Co Ltd | Destroying agent for brittle matter |
-
1982
- 1982-04-14 JP JP6200782A patent/JPS58180245A/ja active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS4943416A (enrdf_load_stackoverflow) * | 1972-08-31 | 1974-04-24 | ||
JPS5667059A (en) * | 1979-11-01 | 1981-06-05 | Onoda Cement Co Ltd | Destroying agent for brittle matter |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5945379A (ja) * | 1982-09-07 | 1984-03-14 | Denki Kagaku Kogyo Kk | 破砕剤及びそれを用いた破砕工法 |
JPS6013172A (ja) * | 1983-07-04 | 1985-01-23 | 旭化成株式会社 | コンクリ−ト等の静的破砕方法および膨張錠剤 |
US4600154A (en) * | 1983-07-04 | 1986-07-15 | Asahi Kasei Kogyo Kabushiki Kaisha | Static expansive demolition agent in the three-dimensional form and process for demolishing brittle material using the same |
JPS62195074A (ja) * | 1986-02-21 | 1987-08-27 | Ube Ind Ltd | 静的破砕剤およびその製造方法 |
Also Published As
Publication number | Publication date |
---|---|
JPH0148059B2 (enrdf_load_stackoverflow) | 1989-10-17 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
IE792109L (en) | Composite material. | |
DE2819086A1 (de) | Verfahren zur endlagerreifen, umweltfreundlichen verfestigung von waessrigen, radioaktiven abfallfluessigkeiten der mittelaktiven kategorie (maw), der niedrigaktiven kategorie (law) und der kategorie der tritiumverbindungen enthaltenden fluessigkeiten | |
EP2784039B1 (en) | Cement curing formulation and method for high-level radioactive boron waste resins from nuclear reactor | |
US3723338A (en) | Method of reducing the release of mobile contaminants from granular solids | |
JPS58180245A (ja) | コンクリ−ト等の静的破砕方法および膨張錠剤 | |
KR100221516B1 (ko) | 라디칼 경화형 화합물용 입상 피복 경화제 및 이를 이용한 앵커볼트 고정용 조성물 | |
DE2531056C3 (de) | Verfahren zum Verfestigen einer radioaktive oder toxische Abfallstoffe enthaltenden wäßrigen Lösung | |
JPS6013172A (ja) | コンクリ−ト等の静的破砕方法および膨張錠剤 | |
US4622175A (en) | Process for solidifying radioactive waste | |
CH662123A5 (it) | Composizione per l'immobilizzazione di residui radioattivi ed impiego della composizione. | |
US2935189A (en) | Stop leak package | |
JP2804213B2 (ja) | 固体から液体までの固さを有する産業廃棄物を(メタ)アクリル樹脂中に封入する方法 | |
KR20090080713A (ko) | 방사성 폐기물 과립화 방법 및 처리장치 | |
JPS5815000B2 (ja) | 放射性廃棄物処理方法 | |
US5180542A (en) | Container | |
Peevy | Effects of some liming materials and calcium sulfate on soil reaction and exchangeable calcium and magnesium | |
DE814453C (de) | Presslinge aus Bodenverbesserungsmitteln | |
RU2048438C1 (ru) | Способ получения жидкого натриевого стекла | |
EP1050521A1 (de) | Ausgangsgemisch für natürlich aushärtenden zellenbeton ohne hilfe einer autoklav und verfahren und vorrichtung zur herstellung von gegenständen aus zellenbeton | |
JPS5528858A (en) | Method of producing ornament | |
DE2856875A1 (de) | Verfahren zum erhoehen des sicherheitsgrades einer in einem unterirdischen hohlraum eines salzstockes befindlichen, mit verfestigten radioaktiven abfaellen gefuellten endlagerstaette gegen unvorhersehbare verschiebungen im salzgestein und/oder wassereinbruch in vorhandene hohlraeume innerhalb des bereichs der endlagerstaette | |
JPS62267699A (ja) | 放射性廃棄物の固化処理方法 | |
Tvergaard et al. | Fatigue crack evolution in a metal reinforced by short fibres | |
JPS62179585A (ja) | 静的破砕剤 | |
JPS6081277A (ja) | 静的破砕方法および静的破砕用膨脹性錠剤 |