JPS5744477A - Horizontal fillet two electrode submerged arc welding method - Google Patents
Horizontal fillet two electrode submerged arc welding methodInfo
- Publication number
- JPS5744477A JPS5744477A JP12011180A JP12011180A JPS5744477A JP S5744477 A JPS5744477 A JP S5744477A JP 12011180 A JP12011180 A JP 12011180A JP 12011180 A JP12011180 A JP 12011180A JP S5744477 A JPS5744477 A JP S5744477A
- Authority
- JP
- Japan
- Prior art keywords
- welding
- weld
- plate
- wires
- beads
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To obtain a weld zone of good quality extremely efficiently with the smallest number of passes by specifying the aiming position and spacing of both electrode wires and electric power source characteristics respectively at the welding of beads covering only the vertical plate to a lower plate in the multilayer weld zone.
CONSTITUTION: After ordinary welding of the 1st layer W1, two electrode submerged arc welding wherein at least one pole is not DC is carried out. At the welding of the 2nd layer W2 covering the lower plate B side, it is essential for facilitating the subsequent bead welding that the beads are as flat as possible and that the toes of weld are aligned. Therefore, the aiming positions of precedent and succeeding electrode wires 1, 2 are set respectively at distances d1, d2 from a vetrtical plate S, and the spacing d4 in the weld line direction W.D. of both wires is set at ≤30mm. Next, the beads of the smooth shape wherein there are no undercuts and the toes of weld are algined are necessary for the 3rd layer covering only the vertical plate S side. Therefore, the positions of the wires 1, 2 are set respectively remote from the plate S contrary from before and the spacing d4 is set at ≥40mm.
COPYRIGHT: (C)1982,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12011180A JPS5744477A (en) | 1980-08-30 | 1980-08-30 | Horizontal fillet two electrode submerged arc welding method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12011180A JPS5744477A (en) | 1980-08-30 | 1980-08-30 | Horizontal fillet two electrode submerged arc welding method |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5744477A true JPS5744477A (en) | 1982-03-12 |
Family
ID=14778203
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP12011180A Pending JPS5744477A (en) | 1980-08-30 | 1980-08-30 | Horizontal fillet two electrode submerged arc welding method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5744477A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103785929A (en) * | 2014-01-15 | 2014-05-14 | 上海交通大学 | GMAW horizontal welding method for board with large thickness |
-
1980
- 1980-08-30 JP JP12011180A patent/JPS5744477A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103785929A (en) * | 2014-01-15 | 2014-05-14 | 上海交通大学 | GMAW horizontal welding method for board with large thickness |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE3163032D1 (en) | Process for producing rounded edges welded along the longitudinal seam | |
JPS5744477A (en) | Horizontal fillet two electrode submerged arc welding method | |
JPS5527417A (en) | Vertical downward build-up welding method | |
JPS5524749A (en) | Method of padding and welding pipe | |
JPS53130241A (en) | Welding method for manufacture of thick walled steel pipe | |
JPS5666376A (en) | Multielectrode arc welding method | |
JPS53103956A (en) | Arc welding method | |
JPS56111578A (en) | Gas shielded arc welding method using alternating current multiple electrode | |
JPS5262943A (en) | Process for building large cyclindrical structure | |
JPS57181763A (en) | Vertical narrow groove mag welding method for short size | |
JPS5768268A (en) | Horizontal fillet submerged arc welding method | |
JPS5584274A (en) | Automatic intermittent welding method | |
JPS5785690A (en) | Automatic welding method for aluminum alloy pipe | |
JPS5433243A (en) | Methof and apparatus for consumable electrode type three o'clock automatic welding | |
JPS53131941A (en) | Method of forming gap of thick pipe welded portion | |
JPS5492536A (en) | Submerged arc welding method | |
EP0050092A3 (en) | Method for the butt welding of high current conductors of large cross section area | |
JPS5411861A (en) | Automatic arc welding process and device therefor | |
JPS5736084A (en) | Terminating method in electron beam welding | |
JPS5791881A (en) | Automatic welding device for segment | |
JPS53127346A (en) | High speed submerged arc welding method for groove | |
JPS5762863A (en) | One side welding method | |
JPS53114751A (en) | Arc welding method | |
JPS57134292A (en) | Welding method for finned tube | |
Klug et al. | Possibilities of Improving Productivity in Submerged Arc Welding and Its Effect on Mechanical and Technological Qualities |